The objectiveness of this study was to evaluate whether low-viscosity composite can bond effectively to dentin surface without bonding resin. The low-viscosity composites being 50wt% filler content were made by the inclusion of bonding resin of two self-etching systems(Cleafil SE Bond, Unifil Bond) varied with contents as 0, 10, 20, 30, 40, 50wt%. Exposed dentin surfaces of extracted 3rd molars are used. Dentin bond strengths were measured. The tests were carried out with a micro-shear device placed testing machine at a CHS of 1mm/min after a low-viscosity composite was filled into an iris cut from micro tygon tubing with internal diameter approximately 0.8mm and height of 1.0mm. 1 Flexural strength and modulus was increased with the addition of bonding resin. 2. Micro-shear bond strength to dentin was improved according to content of bonding resin irrespective of applying or not bonding resin in bonding procedure, and that of Clearfil SE Bond groups was higher than Unifil Bond. 3. There were no significant difference whether use of each bonding resin in bonding procedure for S-40, S-50, U-50(p>0.05). 4. In SEM examination, resin was well infiltrated into dentin after primed with self-etching primer only for S-50 and U-50 in spite of the formation of thinner hybrid layer. Low viscosity composite including some functional monomer may be used as dentin bonding resin without an intermediary bonding agent. It makes a simplified bonding procedure and foresees the possibility of self-adhesive restorative material.
Flowable resin composite is a relatively new restorative material. It has been reported that a low viscosity, low modulus intermediate resin applied between the bonding agent and restorative resin act as an "elastic buffer" that can relieve contraction stress. This in-vitro study aimed to evaluate the effect of flowable composite resin as a restorative material on regional tensile bond stredgth to cervical wedge shaped cavity walls. (omitted)
고분자계 치아 수복용 복합재에서 2,2-bis[4-(2-hydroxy-3-methacryloyloxy propoxy) phenyl] propane(Bis-GMA) 70 wt%와 희석제인 triethylene glycol dimethacrylate(TEGDMA)가 30 wt% 포함된 혼합물이 레진 기질로 사용되고 있다. Bis-GMA의 높은 점도로 인해 첨가되는 TEGDMA는 수복재의 높은 경화 수축과 물성 저하의 원인이 된다. 본 연구에서는 TEGDMA 첨가량을 감소시켜 우수한 특성을 나타내는 수복재를 제조하기 위해 저점도 Bis-GMA 유도체들을 이용하여 새로운 치과용 수복재를 제조하였다. 히드록실기를 포함하지 않는 Bis-GMA 유도체들의 경화 특성은 Bis-GMA와 비슷하였지만 이들의 흡습성과 점도는 Bis-GMA에 비해 크게 낮았다. Bis-GMA 유도체를 포함한 수복재를 제조하여 경화 수축률, 흡습성, 기계적 물성을 실험한 결과 기존 상업적으로 사용되는 수복재보다 낮은 흡습성과 탁월한 물성을 나타내었고, 경화 수축률도 약 25% 감소하였다.
Mechanical properties and water stability of HAC/PVA based MDF cement composite were investigated using polyurethane(PU) resin, silane coupling agent and various PVA. The results were as follows ; The flexural strength of MDF cement composite increased as increasing with PVA content. Low-viscosity PVA developed higher flexural strength than high-viscosity PVA under a drying curing condition. But the strength of water immersed specimen decreased. Water stability of MDF cement improved as increasing with content of PU. Consequently, water stability of polyurethane 7% added MDF cement was about 2 times higher than that of the controlled specimen. Furthermore, the strength and water stability of diamine group based silane couling agent in using MDF cement increased and improved dramatically.
이 연구의 목적은 자가 중합복합 레진과 두 단계 산 부식 접착제의 친화성에 대한 중간 접착제와흐름성 레진의 효과를 미세 인장 결합 강도를 통해 비교하는 것이었다. 20개의 발거된 대구치를 사용해 접착제와 부가적인 적용(활성제, 중간 접착제, 흐름성 레진)에 따라 XP bond 그룹 (XA, XB, XF 그룹), Prime & Bond NT 그룹 (NA, NB, NF 그룹), Optibond solo plus 그룹 (OA, OB OX 그룹)으로 나누었다. 접착제 적용 후 활성제, 중간 접착제, 흐름성 레진을 각각 적용하고 상부에 자가 중합 레진을 축성하였다. 24시간 동안 실온의 증류수에 보관 후 각 그룹당 10개의 시편을 준비하였다. 모든 시편의 미세인장 결합 강도를 측정하여 다음과 같은 결과를 얻었다. 1. 모든 그룹에서 중간 접착제와 흐름성 레진의 적용은 활성제 적용보다 더 높은 결합 강도를 보였다. 2. 선택된 방법에 관계없이, Optibond solo plus 그룹은 가장 낮은 미세인장 결합강도를 보였다. 3. 파절 양상은 대부분 접착성 파절을 보였고 일부 레진 내에서 응집성 파절을 보였다. 이번 연구의 결과로부터, 중간 접착제와 흐름성 레진의 적용이 낮은 pH를 가지는 두 단계 산 부식 접착제와 자가 중합복합 레진의 상아질 접착에 더 효과적이라 예상된다.
목적: 저점도 벌크필레진과 복합레진을 적층한 수복물의 색조를 평가하기 위함이다. 연구 재료 및 방법: 저점도 벌크필레진(SDR)과 A2, A3 색조의 미세혼합형 복합레진(A2, A3)을 4 mm 두께로 제작하여 광중합한 후 색차계를 이용하여 레진 시편의 CIE $L^*a^*b^*$ 값을 측정하였다. 이후 저점도 벌크필레진 상방에 2 mm 두께로 A2, A3 색조의 미세혼합형 복합레진을 적층하여(SA2, SA3) 광중합한 후 색측정을 하고(n = 10), 저점도 벌크필레진과 미세혼합형 복합레진, 그리고 이들을 적층한 시편의 색차(${\Delta}E$)를 계산하였다. 결과: $L^*$ 값은 SDR이 가장 컸고 SA2, SA3 그리고 A2, A3 순으로 감소했다. $a^*$ 값은 SDR이 가장 작았고 SA2, SA3 그리고 A2, A3 순으로 증가했다. $b^*$ 값은 SDR이 가장 작았으며 A2, SA2 그리고 A3, SA3 순으로 증가했다. 적층한 시편과 미세복합형 복합레진 시편의 ${\Delta}E$ 값은 A2와 SA2 사이에 ${\Delta}E=3.4$, A3와 SA3 사이에 ${\Delta}E=3.1$로 계산되었다. 결론: 저점도 벌크필레진과 미세혼합형 복합레진을 적층한 시편과 미세혼합형 복합레진만으로 제작한 시편의 색조의 차이는 일반적으로 인지하지 못할 정도로 작았다.
The purpose of this study was to evaluate and compare the effectiveness of various low-viscosity resin systems used as rebonding agents to prevent microleakage at the margins of class I composite resin restorations. Seventy sound human premolars were selected for experiment. Class I cavities were prepared and each cavity was conditioned with a 37% phosphoric acid for 15 sec, rinsed with water for 15 sec, and dried with compressed air. Bonding agent(Scotchbond Multipurpose, 3M Co.) was applied and a hybrid composite resin (Z-100, 3M Co.) was placed using an incremental technic. The excess cured composite resin was carefully removed with Sof-Lex discs(3M Co.) to expose the original margins of the cavity. The following seven groups were established : group 1 was not rebonded and used as control group ; group 2 was rebonded with a Scotchbond Multipurpose(3M Co.) and finished ; group 3 was rebonded with a Fortify(BISCO) and finished ; group 4 was rebonded with a Concise white sealant(3M Co.) and finished ; group 5 was rebonded with a Concise white sealant(3M Co.) and not finished ; group 6 was rebonded with a P&F sealant(BISCO) and finished; group 7 was rebonded with a P&F sealant(BISCO) and not finished. The specimens were then subjected to 500 thermocycles between 5 & 65 with a 10 see dwell time and immersed in 2% methylene blue dye solution for 24 hours and sectioned with low-speed diamond cutter into two part under water condition. The extent of microleakage at rebonded margins was evaluated microscopically and scored for dye penetration according to the following scale : 0=no dye penetration ; 1=dye penetration to half-way along axial wall between enamel surface and DEJ ; 2=dye penetration beyond halfway along axial wall between enamel surface and DEJ ; 3=dye penetration to the full depth of DEJ or beyond DEJ. Selected samples were prepared for SEM observation to determine the depth of penetration of the rebonding agent into the marginal interface. The obtained results were as follows: 1. In the group 2 and 3, which is rebonded with a Scotchbond Multipupose and Fortify, dye penetration score were decreased significantly than that of group 1 (P<0.05), but group 4 and 6 were not statistically different from group 1(P>0.05). 2. There were significant differences between group 4, 6 and group 5, 7 when compared by dye penetration score (P<0.05). 3. In the SEM observation, Scotchbond Multipurpose and Fortify were penetrated within $30-40{\mu}m$ depth of the outermost surface. However, both sealants were failed to penetrate into the debonded interface.
Phenolin resin, prepared form phenol and formaldehyde, is one of the oldest thermosetting resins available. Phenolic resins are cured via condensation polymerization with evolution of water, which in molding process is a big problem. The use of phenolic resins in glass fiber composites is growing, primarily due to their low flame spread, low smoke generation and low smoke toxicity properties. SMC of phenolics has been rearched since the 1986. The technology challenge was to match resin viscosity, handling and cure with those for the polyester SMC to avoid any special processing for fabricators and end users. Phenolic SMC was chosen because of the ease of molding to the required shape with light- weight, thin wall structure and with excellent fire protection.
본 연구는 물성의 단점이 많은 희석재인 TEGDMA의 사용을 줄이기 위해, Bis-GMA의 유도체로서 중합수축이 적고 점도가 낮은 새로운 단량체인 methoxlyated Bis-GMA (Bis-M-GMA)를 첨가한 복합레진의 법랑질과 상아질 변연에서의 미세누출을 비교하였다. 40개의 발거된 상하악 소구치의 협면과 설면에 $2\;mm\;{\times}\;2\;mm\;{\times}\;2\;mm$ 와동을 형성하여 4개 군으로 분류하였다. Clearfil SE bond와 복합레진을 이용하여 와동을 수복하였다. EX1군은 실험용 복합레진 1 (Bis-M-GMA/TEGDMA = 95/5wt% ,40 nm 나노필러 함유), EX2군은 실험용 복합레진 2 (Bis-M-GMA/TEGDMA = 95/5wt%, 20 nm 나노필러 함유), EX3군은 실험용 복합레진 3 (Bis-GMA/TEGDMA = 70/30wt%, 40 nm 나노필러 함유), Z250군은 Filtek 2250으로 각각 와동을 수복하였다. 모든 시편은 실온의 실온의 생리식염수에서 7일간 보관한 후, $5^{\circ}C$와 $55^{\circ}C$ 의 수조에서 500회의 열순환을 실시하고, 2% methylene blue염색 용액에 24시간 담근 후, 협설측으로 치아 장축에 평행하게 절단하고 광학입체현미경하에서 각 수복물의 법랑질과 상아질 변연부의 색소침투 정도를 관찰하여 미세누출점수로 기록한 후 각 군의 유의성을 검증하였다. 법랑질 변연이 상아질 변연보다 유의성있게 낮은 미세변연누출을 보였다 (p = 0.007). 각 변연에서 EX1, EX2보다 EX3, Z250군의 염색침투도가 증가하는 경향을 보였지만 통계적으로 유의성 있는 차이를 보이지는 않았다 (p > 0.05). 점도가 낮은 새로운 레진단량체인 Bis-M-GMA는 기존의 단량체인 Bis-GMA의 대체재로 고려될 수 있다.
MMA-modified fiberglass-reinforced plastic composite pipe was produced by using the binder of MMA-modified unsaturated polyester resin in which low viscosity MMA was added to unsaturated polyester resin. Sixteen specimens were made of polymer mortar and fiberglass-reinforced plastic by the centrifugal method. For these specimens the external strength tests were carried out by taking the core thickness consisting of polymer mortar and the fiberglass content per unit area as experimental variables to figure out the effect of variations of these variables influencing on flexural rigidity that is an important property for the composite pipe. Results of this study are believed to provide the basic data for more economical and practical design of MMA-modified fiberglass-reinforced plastic composite pipe.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.