• 제목/요약/키워드: Low temperature annealing

검색결과 686건 처리시간 0.043초

Size and Density of Graphene Domains Grown with Different Annealing Times

  • Jung, Da Hee;Kang, Cheong;Nam, Ji Eun;Kim, Jin-Seok;Lee, Jin Seok
    • Bulletin of the Korean Chemical Society
    • /
    • 제34권11호
    • /
    • pp.3312-3316
    • /
    • 2013
  • Single crystals of hexagonal graphenes were successfully grown on Cu foils using the atmospheric pressure chemical vapor deposition (CVD) method. We investigated the effects of reaction parameters, such as the growth temperature and annealing time, on the size, coverage, and density of graphene domains grown over Cu foil. The mean size of the graphene domains increased significantly with increases in both the growth temperature and annealing time, and similar phenomena were observed in graphene domains grown by low pressure CVD over Cu foil. From the comparison of micro Raman spectroscopy in the graphene films grown with different annealing times, we found that the nucleation and growth of the domains were strongly dependent on the annealing time and growth temperature. Therefore, we confirmed that when reaction time was same, the number of layers and the degree of defects in the synthesized graphene films both decreased as the annealing time increased.

Low Temperature Annealed Sol-Gel Aluminum Indium Oxide Thin Film Transistors

  • Hwang, Young-Hwan;Jeon, Jun-Hyuck;Seo, Seok-Jun;Bae, Byeong-Soo
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.396-399
    • /
    • 2009
  • Thin-film transistors (TFTs) with an aluminum indium oxide (AIO) channel layer were fabricated via a simple and low-cost sol-gel process. Effects of annealing temperature and time were investigated for better TFT performance. The sol-gel AIO TFTs were annealed as low as $350^{\circ}C$. They exhibit n-type semiconductor behavior, a mobility higher than 19 $cm^2/V{\cdot}s$ and an onto-off current ratio greater than $10^8$.

  • PDF

Effective Annealing and Crystallization of Si Film for Advanced TFT System

  • Noguchi, Takashi
    • Journal of Information Display
    • /
    • 제11권1호
    • /
    • pp.12-16
    • /
    • 2010
  • The effect of the crystallization and activated annealing of Si films using an excimer laser and the new CW blue laser are described and compared with furnace annealing for application in advanced TFTs and for future applications. Pulsed excimer laser annealing (ELA) is currently being used extensively as a low-temperature poly-silicon (LTPS) process on glass substrates as its efficiency is high in the ultra-violet (UV) region for thin Si films with thickness of 40-60 nm. ELA enables extremely low resistivity relating to high crystallinity for both the n- and p-type Si films. On the other hand, CW blue laser diode annealing (BLDA) enables the smooth Si surface to have arbitral crystal grains from micro-grains to an anisotropic huge grain structure only by controlling its power density. Both annealing techniques are expected to be applied in the future advanced TFT systems.

HNx 분위기가스중에서 BAF소둔시 코일의 온도변화에 관한 연구 (A Study on Temperature Variation of Coil on BAF Annealing in HNx Atmospheric Gas)

  • 전언찬;김순경
    • 대한기계학회논문집
    • /
    • 제18권5호
    • /
    • pp.1227-1234
    • /
    • 1994
  • A cold spot temperature control system for the batch annealing furnace has been established in order to reduce energy consumption which is essential to improve productivity and stabilize the properties of products. A relationship between annealing cycle time and gas flow rate is developed and also for the variation of coil cold spot temperature with time during heating, and actual temperature measurements at mid-width of each coil during soaking. The results of the temperature variation effect on the cold rolled steel sheet batch annealing are as follows. (1) Cooling rate increasing gradually with increasing atmospheric gas flow, but heating rate is hardly increasing without atmospheric gas component change. (2) In case of short time heating, the slowest heating part is the center of B coil and in case of ling time heating, the low temperature point moves from the center of coil to inside coil. (3) The outside of top coil is the highest temperature point under heating, which becomes the lowest temperature point under cooling. (4) Soaking time determination depends on the input coil width, and soaking time for quality homogenization of 1214 mm width coil must be 2 hours longer than that of 914 mm width coil.

Low-temperature crystallization of high-dielectric (Ba,Sr)$TiO_3$ thin films for embedded capacitors

  • Cho, Kwang-Hwan;Kang, Min-Gyu;Kang, Chong-Yun;Yoon, Seok-Jin
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 춘계학술회의 초록집
    • /
    • pp.21-21
    • /
    • 2010
  • (Ba,Sr)$TiO_3$ (BST) thin film with a perovskite structure has potential for the practical application in various functional devices such as nonvolatile-memory components, capacitor, gate insulator of thin-film transistors, and electro-optic devices for display. Normally, the BST thin films derived from sol-gel and sputtering are amorphous or partially crystalline when processed below $600^{\circ}C$. For the purpose of integrating BST thin film directly into a Si-based read-out integrated circuit (ROIC), it is necessary to process the BST film below $400^{\circ}C$. The microstructural and electrical properties of low-temperature crystallized BST film were studied. The BST thin films have been fabricated at $350^{\circ}C$ by UV-assisted rapidly thermal annealing (RTA). The BST films are in a single perovskite phase and have well-defined electrical properties such as high dielectric constant, low dielectric loss, low leakage current density, and high breakdown voltage. Photoexcitation of the organics contained in the sol-gel-derived films by high-intensity UV irradiation facilitates elimination of the organics and formation of the single-crystalline phase films at low temperatures. The amorphous BST thin film was transformed to a highly (h00)-oriented perovskite structure by high oxygen pressure processing (HOPP) at as low as $350^{\circ}C$. The dielectric properties of BST film were comparable to (or even better than) those of the conventionally processed BST films prepared by sputtering or post-annealing at temperature above $600^{\circ}C$. When external pressure was applied to the well-known contractive BST system during annealing, the nucleation energy barrier was reduced; correspondingly, the crystallization temperature decreased. The UV-assisted RTA and HOPP, as compatible with existing MOS technology, let the BST films be integrated into radio-frequency circuit and mixed-signal integrated circuit below the critical temperature of $400^{\circ}C$.

  • PDF

Excimer Laser Annealing 결정화 방법 및 고유전 게이트 절연막을 사용한 poly-Si TFT의 특성 (Characteristics of poly-Si TFTs using Excimer Laser Annealing Crystallization and high-k Gate Dielectrics)

  • 이우현;조원주
    • 한국전기전자재료학회논문지
    • /
    • 제21권1호
    • /
    • pp.1-4
    • /
    • 2008
  • The electrical characteristics of polycrystalline silicon (poly-Si) thin film transistor (TFT) crystallized by excimer laser annealing (ELA) method were evaluated, The polycrystalline silicon thin-film transistor (poly-Si TFT) has higher electric field-effect-mobility and larger drivability than the amorphous silicon TFT. However, to poly-Si TFT's using conventional processes, the temperature must be very high. For this reason, an amorphous silicon film on a buried oxide was crystallized by annealing with a KrF excimer laser (248 nm)to fabricate a poly-Si film at low temperature. Then, High permittivity $HfO_2$ of 20 nm as the gate-insulator was deposited by atomic layer deposition (ALD) to low temperature process. In addition, the solid phase crystallization (SPC) was compared to the ELA method as a crystallization technique of amorphous-silicon film. As a result, the crystallinity and surface roughness of poly-Si crystallized by ELA method was superior to the SPC method. Also, we obtained excellent device characteristics from the Poly-Si TFT fabricated by the ELA crystallization method.

YBCO 박막선재용 Ni 기판의 집합도에 미치는 제조공정 변수효과 (Effect of Processing Variables on the Texture of Ni Substrate for YBCO Coated Conductor)

  • 지봉기;임준형;이동욱;주진호;나완수;김찬중;홍계원
    • 한국전기전자재료학회논문지
    • /
    • 제16권10호
    • /
    • pp.938-945
    • /
    • 2003
  • We fabricated Ni-substrate for YBCO coated conductors and evaluated the effects of pressing and annealing temperature and time on texture. Ni substrate was fabricated by powder metallurgy technique and compacts were prepared by applying uniaxial or isostatic pressure. The texture of substrate made by applying cold isostatic pressure (CIP) was stronger than that by uniaxial pressure which we attribute to the fact that the CIP method provided higher density and more uniform density distribution. It was observed that the substrate annealed at 400 C showed both retained texture and recrystallized texture. On the other hand, the texture of substrate significantly improved at annealing temperature above 500 C, forming strong 4-fold symmetry, [111] II ND texture, and FWHM of 9∼10 . It is to be noted that the degree of texture was almost independent of annealing temperature (500∼1000 C) and annealing time(1∼54 min, at 1000 C). EBSD and AFM analysis indicated that 99% of grain boundaries was low angle grain boundary and RMS was approximately 3 nm, respectively. Development of strong cube texture and high fraction of low angle grain boundary of Ni-substrate made by powder metallurgy technique in our study is considered to be suitable for the application of YBCO coated conductors.

$90\%$ 단면감소율로 인발된 전해동의 어닐링시 집합조직과 미세조직 발달에 미치는 전단 변형의 영향 (Effects of Shear Strains on the Developement of Texture and Microstructure of $90\%$ Drawn Copper Wire during Annealing)

  • 박현;이동녕
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 제4회 압출 및 인발가공 심포지엄
    • /
    • pp.55-62
    • /
    • 2001
  • An electrolytic copper rod was drawn up to $90\%$ in area reduction and annealed under various conditions. The EBSD measurement of the drawn wire showed that in the center region the <111> + <100> fiber duplex texture was dominant, while in the middle and surface regions relatively defused textures developed with a little higher density in <11w>//wire axis. The inhomogeneous texture in the deformed wire gave rise to the inhomogeneous microstructure and texture after annealing. The annealing texture could be classified into the recrystallization texture developed during low temperatures and at the early stage at a high temperature and the growth texture developed after a prolonged annealing at the high temperature. The recrystallization temperature could be explained by the strain energy release maximization model and the growth texture was discussed based on the grain boundary mobility anisotropy.

  • PDF

투명전극용 ZnO/Ti/ZnO 박막의 급속열처리 효과 (Effect of Rapid Thermal Annealing on the Properties of Transparent Conducting ZnO/Ti/ZnO Thin Films )

  • 장진규;김대일
    • 열처리공학회지
    • /
    • 제35권6호
    • /
    • pp.314-318
    • /
    • 2022
  • Transparent conducting ZnO/Ti/ZnO tri-layer films deposited on glass substrate with DC and RF magnetron sputtering were rapid thermal annealed at 150, 300 and 450℃ for 5 minutes and then effect of annealing temperature on the structural and optoelectronics properties of the films were investigated. The structural properties are strongly related to annealing temperature and the largest grain size is observed in the films annealed at 450℃. The electrical resistivity also decreases as low as 7.7 × 10-4 Ωcm. The visible transmittance also depends on the annealing temperature. The films annealed at 450℃ show a higher transmittance of 80.6% in this study.

CVD법을 이용한 보론 포스파이드의 저온 층착과 특성에 관한 연구 (A Study on the Deposition of Boron Phosphide at the Low Temperature using CVD Method and its Characteristics)

  • 윤여철;김순영;박윤권;강재경;김철주
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.103-107
    • /
    • 2000
  • Boron Phosphide films were deposited on the glass substrate at the low temperature, 55$0^{\circ}C$, by the reaction of B$_2$H$_{6}$ with PH$_3$ using CVD. $N_2$ was employed as carrier gas. The optimal gas rates were 50 $m\ell$/min for B$_2$H$_{6}$, 50 $m\ell$/min for PH$_3$ $m\ell$/min and 1.5 $\ell$/min for $N_2$. To investigate the annealing effect, the films were annealed for 1hour, 3hours in $N_2$ambient at 55$0^{\circ}C$ and tested. The deposition rate was 1000$\AA$/min and the refractive index of film was 2.6. The measurement of X-RD shows that the films have the preferred orientation of (1 0 1) and the intensity of the peak for (1 0 1) orientation decreases according to the annealing time. The data of VIS spectrophotometer proved that the films are transparent in the visible range and the maximal transmittance increases according to the annealing time; 75.49% for as-deposited, 76.71% for 1hr-annealed and 86.4 % for 3hrs-annealed. The measurement of AFM shows that the average surface roughness increases according to the annealing time; 73$\AA$ for as-deposited, 88.9$\AA$ for 1hr-annealed and 220$\AA$ for 3hrs-annealed. Also, The data of the secondary electron emission rate(Υ) shows that the secondary electron emission rate increases according to the annealing time; 0.317 for 1hr-deposited, 0.357 for 1hr-annealed and 0.537 for 3hrs-annealed. And, The measurement of FT-IR that the characteristic of transmittance in the infrared range was stabilized through annealing.ing.

  • PDF