The Study of Luppe Smelting with Converting Dust and Slag (제강전로 더스트와 슬래그를 이용한 루페제련에 관한 연구)

  • 황용길;이상화;김재일;김연수
    • Resources Recycling
    • /
    • v.7 no.2
    • /
    • pp.39-45
    • /
    • 1998
  • We smelted thc pellets made by mixing the distilled carbon from wlISte Lires, LD converter dust and slag with reduction process in the revcrberatory furnace. Thc obtained results are as follows 1) The removal mte of zinc appears above 97% after T reducing the pellets at $1300^{\circ}C$ for Ihr and the zinc content in the residue are 0.1~D.2%. 2) Under the mixing condition of 500 g LD dust. 150-200 g LD slag and 30-50 g distilled carbon of waste lires the removal raho of zinc shows above 95%, while t the 50-60% Fe remains in the residue. 3) After smelting at $1350^{\circ}C$ for 3hrs, the recovery ratio of pig iron reduced from lhe p pellets containing 15-20% LD slag and 4.1-7.2% distilled carbon of waste tires appears in the range of 89.3-92%. 4) Tbe c chemical composition of the recovered pig iron is 1.7%C, O.05%P, 0.05%S and balance Fe. 5) Tbe recovered dust from the d dust collcctor alter finishing the reduction rcaction appears as a crude zinc oxide conLaining 60% zinc.

  • PDF

Design and Fabrication of Reflection-type Pump LD Protection Filters for High Power Fiber Lasers by Using Ta2O5/SiO2 Thin Films (Ta2O5/SiO2를 이용한 고출력 광섬유 레이저의 펌프 LD 보호기용 반사형 필터 설계 및 제작)

  • Sung, Hamin;Kim, Jae Hun;Lee, Seok;Jhon, Young Min
    • Korean Journal of Optics and Photonics
    • /
    • v.23 no.3
    • /
    • pp.124-127
    • /
    • 2012
  • We designed and fabricated dichroic filters for high-power fiber lasers to protect the pumping laser diode from counterpropagating laser beams. The transmittance at laser diode wavelengths of 905 nm~925 nm was designed to be less than 0.1% and the transmittance at the fiber laser or Brillouin scattering wavelengths of 1020 nm ~ 1100 nm was designed to be more than 99.9%. Since oxide materials have good adhesion to the $SiO_2$ substrate, $SiO_2/Ta_2O_5$ were used as coating materials. The filter was fabricated according to our optimized design and its characteristics were compared with the theoretical design. As a result, the transmittance at laser diode wavelengths of 905 nm~925 nm was measured to be less than 0.1%, and the transmittance at the fiber laser or Brillouin scattering wavelengths of 1020 nm~1100 nm was measured to be more than 95.5%, which coincided well with the theoretical design considering processing errors. The filter was found to operate well over 1W of input laser power.

Leaching Behavior of LD Slag

  • Kim, Hyung-Suek;Han, Ki-Hyun;M. S. Oh;Byeon, Tae-Bong
    • Proceedings of the IEEK Conference
    • /
    • 2001.10a
    • /
    • pp.526-531
    • /
    • 2001
  • LD slag, that is, a by-product of steel making process, has been mainly used as land construction materials. Recently, the seashore application of LD slag was tried in Japan and Korea tut the reaction between LD slag and seawater was not studied yet. We tried to clarify the leaching reaction and/or mechanism of LD slag and the reaction between seawater and LD slag. We tried to apply these results to the decarbonization of seawater for seawater magnesia process. At first, LD slag was milled and classified into 5 grades, that is, (ⅰ)45${\mu}{\textrm}{m}$ under, (ⅱ)0.25~0.5mm (ⅲ)0.5~1mm(ⅳ)1~2mm, (ⅴ)2.36~3.35mm. These slags were leached in the distilled water. In case of 45${\mu}{\textrm}{m}$ under, the pH of the leached solution was over 12. The chemical analysis of leached solution showed that the $Ca^{+}$$^2$was main component and the S $i^{+}$$^4$was very low. On the other hand, the content of S $i^{+}$$^4$in leached solution was decreased with the increase of pH of this solution. The nearly pure calcium solution was made and the ultra high purity MgO could be made with this calcium solution. The leaching behavior of LD slag was different between the fine particle and coarse particle. The calcium was leached by bulk dissolution in the coarse particle and by surface controlled reaction in fine particle. The leaching rate was slow in coarse particle and fast in fine particle. Therefore, the high pH solution, that is, over 12, was obtained in fine particle.cle.e.

  • PDF

Acute Oral Toxicity Test in Japanese Quail (일본 메추리를 이용한 급성 경구독성시험법의 확립)

  • 최은실;박종환;홍정주;박재학
    • Toxicological Research
    • /
    • v.17 no.4
    • /
    • pp.287-296
    • /
    • 2001
  • The acute oral LD5O toxicity values of isazofos, pyraclofos, diazinon and methomyl were determined for Japanese quail based on OECD guideline. The $LD_{50}$ of isazofos, pyraclofos and diazinon was 16.26 mg/kg, and 7.11mg/kg body weight In female respectively. And the $LD_{50}$ of each chemical in male was 21.44, 35.64, 8.28 mg/kg body weight respectively. Diazinon was the most susceptible compounds to Japanese quail in both sexes. The $LD_{50}$ of methomyl was 21.24 mg/kg body weights in female, and 28.28 mg/kg body weight in male respectively. Diazinon, isazofos and methomyl were more toxic In the female than male. The symptoms of poisoning were similar in quails administrated with each chemicals. The clinical sign in Japanese quail were ataxia, salivation, diarrhea, ruffled feather and convulsion at dead point. There were severe hemorrhage and catarrhal inflammation from duodenum to ileum In all compounds. In Japanese quail treated with organophosphorus and carbamate compounds, brain acetylcholinesterase was inhibited by 88-96. The recovery was not observed after 5 h in sublethal dose.

  • PDF

The effect of thickness on luminous properties of ceramic phosphor plate for high-power LD (고출력 LD 용 형광체 세라믹 플레이트의 두께에 따른 광학 특성)

  • Ji, Eun Kyung;Lee, Chul Woo;Song, Young Hyun;Jeong, Byung Woo;Jung, Mong Kown;Yoon, Dae-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.26 no.2
    • /
    • pp.80-83
    • /
    • 2016
  • In the present paper, garnet structured $Y_3Al_5O_{12}:Ce^{3+}$ (YAG : Ce) ceramic phosphor plate (CPP) for high power laser diode (LD) was prepared and optical properties were analyzed. We synthesized monodispersed spherical nano-sized YAG : Ce particles by liquid phase method, fabricated phosphor ceramic plate with the addition of $Al_2O_3$. $75{\mu}m$ and $100{\mu}m$ thick YAG : Ce CPPs were compared in terms of the factors of conversion efficacy, thermal quenching, luminance and correlated color temperature (CCT). In conclusion, conversion efficacy decreased by 25 % in both samples and $100{\mu}m$ thick sample provides better optical properties of thermal quenching, maximum light conversion efficacy and maximum luminance value.

Proposan and Analysis of DR(Distributed Reflector)-LD/EA(electro-absorption)­Modulator Integrated Device (분포반사기 레이저 다이오드와 광흡수 변조기가 집적된 소자의 제안 및 해석)

  • 권오기;심종인
    • Korean Journal of Optics and Photonics
    • /
    • v.9 no.5
    • /
    • pp.333-341
    • /
    • 1998
  • The novel integrated device, 1.55 ${\mu}{\textrm}{m}$ DR-LD(distrbuted reflector laser diode) integrated EA-MOD (electro-absorption modulator) as light source, is proposed to improve the device yield and its operational performances. This device can be easily fabricated by the selective MOVPE technique and its fabrication processes are almost the same as the reported 1.55 ${\mu}{\textrm}{m}$ DFB-LD(distributed feedback laser diode) integrated EA-MOD except the asymmetric gratings. The static and dynamic properties are investigated simultaneously by solving the transfer matrix method for light propagation, the time-dependent rate equation for carrier change and schr$\"{o}$dinger equation for QCSE (Quantum-Confined Stark Effect). The performances of the proposed device such as output power, chirp, and extinction ratio are compared with those of DFB-LD integrated EA-MOD. Under 10Gb/s NRZ modulation, we obtain that DR-LD integrated EA-MOD. is 30% higher in output power on the on-state, about 50% lower in chirp, and slightly larger in extinction ratio than DFB-LD integrated EA-MOD.-MOD.

  • PDF

Design and Properties Related to Anti-reflection of 1.3μm Distributed Feedback Laser Diode (1.3μm 분포 괴환형 레이저 다이오드의 무반사 설계 및 특성)

  • Ki, Hyun-Chul;Kim, Seon-Hoon;Hong, Kyung-Jin;Kim, Hwe-Jong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.3
    • /
    • pp.248-251
    • /
    • 2009
  • We have investigated the effect of the quality of 1.3 um distributed feed back laser diode (DFB-LD) on the design of anti-reflection (AR) coatings. Optimal condition of AR coating to prevent internal feedback from both facets and reduce the reflection-induced intensity noise of laser diode was simulated with Macleod Simulator. Coating materials used in this work were ${Ti_3}{O_5}$ and $SiO_2$, of which design thickness were 105 nm and 165 nm, respectively. AR coating films were deposited by Ion-Assisted Deposition system. The electrical and optical properties of 1.3 um laser diode were characterized by Bar tester and Chip tester. Threshold current and slop-efficiency of DFB-LD were 27.56 mA 0.302 W/A. Far field pattern and wavelength of DFB-LD were $22.3^{\circ}(Horizontal){\times}24.4^{\circ}$ (Vertical), 1313.8 nm, respectively.

Acute Oral Toxicity of KDRD-002 in Rats (랫드에 대한 KDRD-002의 급성경구독성시험)

  • 김형식;이승기;김규봉;곽승준;안미영;최병천;이병무
    • Biomolecules & Therapeutics
    • /
    • v.4 no.4
    • /
    • pp.310-313
    • /
    • 1996
  • Acute oral toxicity studies of KDRD-002 (Coriolus versicolor polysaccharide :DDB= 19.2:1) were carried out in Sprague-Dawley rats of both sexes. In this study, we daily examined number of deaths, clinical signs, body weights and pathological examinations for 7 days after single oral administration of KDRD-002 with different dose levels. KDRD-002 did not show any toxic effect in rats and oral LD$_{50}$ value was over 3.25 g/kg in rats.s.

  • PDF

Thermal Stress Relief through Introduction of a Microtrench Structure for a High-power-laser-diode Bar (높은 광출력을 갖는 Laser Diode Bar의 열응력 개선: 마이크로-홈 도입을 통한 응력 분포 변화 분석)

  • Jeong, Ji-Hun;Lee, Dong-Jin;O, Beom-Hoan
    • Korean Journal of Optics and Photonics
    • /
    • v.32 no.5
    • /
    • pp.230-234
    • /
    • 2021
  • Relief of thermal stress has received great attention, to improve the beam quality and stability of high-power laser diodes. In this paper, we investigate a microtrench structure engraved around a laser-diode chip-on-submount (CoS) to relieve the thermal stress on a laser-diode bar (LD-bar), using the SolidWorks® software. First, we systematically analyze the thermal stress on the LD-bar CoS with a metal heat-sink holder, and then derive an optimal design for thermal stress relief according to the change in microtrench depth. The thermal stress of the front part of the LD-bar CoS, which is the main cause of the "smile effect", is reduced to about 1/5 of that without the microtrench structure, while maintaining the thermal resistance.

AlN를 도핑시킨 ZnO박막의 전기적 및 광학적 특성

  • Son, Lee-Seul;Kim, Gyeom-Ryong;Lee, Gang-Il;Jang, Jong-Sik;Chae, Hong-Cheol;Gang, Hui-Jae
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.88-88
    • /
    • 2011
  • ZnO는 직접 천이형 반도체로써, 상온에서 3.4eV에 해당하는 띠틈을 가지고 있다. 뿐만 아니라 60meV의 큰 엑시톤 결합에너지를 가지고 있어 단파장 광전 소자 영역의 LED(Light Emitting Diode)나 LD(Laser Diode)에 널리 사용되고 있다. 하지만 일반적으로 격자틈새 Zn(Zni2+)이온이나 O 빈자리(V02+)이온과 같은 자연적인 도너 이온이 존재하여 n-형 전도성을 나타낸다. 그러므로 ZnO계 LED와 LD의 개발에 있어서 가장 중요한 연구 과제는 재현성 있고 안정된 고농도의 p-형 ZnO박막을 성장시키는 것이다. 하지만, 자기보상효과나 얕은 억셉터 준위, 억셉터의 낮은 용해도로 인하여 어려움을 가지고 있다. 본 연구에서는 고품질의 p-형 ZnO박막을 제작하기 위해 AlN를 도핑시킨 ZnO박막을 RF 마그네트론 스퍼터링 법을 이용하여 Ar과 O2분위기에서 성장시켰다. ZnO와 AlN타겟을 동시에 사용하였으며, ZnO타겟에 걸어준 RF 파워는 80W, AlN타겟에 걸어준 RF 파워는 5~20W로 변화시켰다. 박막의 전기적, 광학적 특성은 XPS (X-ray Photoelectron Spectroscopy), REELS (Reflection Electron Energy Loss Spectroscopy), XRD (X-ray Diffraction), SIMS (Secondary Ion Mass Spectrometry), AES (Auger Electron Spectroscopy), Hall measurement를 이용하여 연구하였다. XPS측정결과, AlN를 도핑시킨 ZnO박막의 Zn2p3/2와 O1s피크는 undoped ZnO박막의 피크보다 낮은 결합에너지에서 측정되었다. 모든 박막이 결정화 되었으며, (002)방향으로 우선적으로 성장된 것을 확인할 수 있었다. 홀 측정 결과, 기판을 $200^{\circ}C$로 가열하면서 성장시킨 박막이 p-형을 나타내었으며, 비저항(Resistivity)이 $5.51{\times}10^{-3}{\Omega}{\cdot}m$, 캐리어 농도(Carrier Concentration)가 $1.96{\times}1018cm^{-3}$, 이동도(Mobility)가 $481cm^2$/Vs이었다. 또한 QUEELS -Simulation에 의한 광학적 특성분석 결과, 가시광선영역에서 투과율이 90%이상으로 투명전자소자로의 응용이 가능하다는 것을 보여주었다.