Synthesis and Characteristics of 2 Step-curable Shape Memory Polyurethane (2단계 경화형 형상기억 폴리우레탄의 합성 및 분석)

  • Noh, Geon Ho;Lee, Seungjae;Bae, Seong-Guk;Jang, Seong-Ho;Lee, Won-Ki
    • Journal of Environmental Science International
    • /
    • v.27 no.11
    • /
    • pp.1023-1028
    • /
    • 2018
  • Shape memory materials are widely used in high-tech industries. Although shape memory polymers have been developed, they have a disadvantage, only unidirectional resilience. Shape memory polymers with bi-directional recovery resilience have been actively studied. In this study, a bidirectional shape memory polyurethane was synthesized using poly(${\varepsilon}$-caprolactone) diol, methylene dicyclohexyl diisocyanate, and hydroxyethyl acrylate. The first physical curing occurred between hard segments and hydrogen bondings when the solution was dried. The second curing in acrylate groups was performed by UV exposure. A degree of curing was analyzed by infrared spectroscopy. The shape memory properties of 2 step-cured polyurethanes were investigated as a function of UV curing time.

THE CHANGES IN DEGREE OF CONVERSION OF COMPOSITE RESINS AFTER ADDITIONAL HEAT CURING (수종 복합레진의 추가적인 열중합 후의 중합률 변화)

  • Park, Seong-Ho
    • Restorative Dentistry and Endodontics
    • /
    • v.20 no.2
    • /
    • pp.827-831
    • /
    • 1995
  • This study was designed to etermine the changes in the degree of conversion for composite resins after heat curing following the methods proposed by Lee & Park(1995). 8-mm diameter hole was made in 1mm teflon plate and one of three types of composites (Charisma, Brilllant, Z100) was placed and light cured for 60seconds. The samples were devided into 3 groups according to the placing composites. After light curing, the samples were separated from the moulds. Using this method, 10 samples were prepared in each group; 5 samples from each group were heat cured according to the methods proposed by manutfactures, These samples were then thinned to 50-$70{\mu}m$ and analysed with a Fourier Transform Infrared Spectrometer. Standard baseline technique was used to calculate the degree of conversion. When the samples were light cured, the degrees of conversion in each groups were 47.1 % (charisma), 53.3% (Z100), and 70.1 % (Brilliant). The degree of conversion after heat curing were; 60.1 % (Charisma), 71.1 % (Z100), and 73.3 % (Brillant). Once the samples were heat cured, there were significant increases in degree of conversion.

  • PDF

AN EXPERIMENTAL STUDY OF THE DEGREE OF CONVERSION AND CYTOTOXICITY OF DUAL CURE RESIN CEMENTS (수종 이원중합 레진 씨멘트의 중합률 및 세포 독성에 관한 실험적 연구)

  • Roh, Byoung-Duck;Park, Seong-Ho;Lee, Chung-Suck
    • Restorative Dentistry and Endodontics
    • /
    • v.20 no.1
    • /
    • pp.33-54
    • /
    • 1995
  • The degree of conversion of composite resin was known to have influence on the mechanical properties of composite materials such as hardness, strength, wear resisitance, dimensional and color stability. Also unreacted monomer was reported to be harmful to the pulp. So the degree of conversion was a very important factor in the success of composite resin restorations. In recent, the dual cure resin cement was developed with the advocations that it could increase the curing rates in the sites where the curing ligt could not reach. Moreover many manufactors added some adhesive components in the resin cement. This study was undertaken to observe the effects of curing depth and light curing times on the degree of conversion of dual cure resin cements. CR INLAY CEMENT, DUAL CEMENT and OPTEC BOND, by the Fourier transform Infrared analysis, changing the curing depth 1mm, 2mm and 3mm, and varying the light curing time 20 seconds, 40 seconds and 80 seconds at each depth. The cytotoxicity of dual cure resin cements was tested by the in vitro MTT method using L929 cell. The results was evaluated and compared statistically. The results were obtained as follows : 1. The dual cure resin cements reavealed various degree of conversion, CR INLAY CEMENT and DUAL CEMENT had a tendency to be more reactive to the light cure and OPTEC BOND was a more chemical one. 2. CR INLAY CEMENT and DUAL CEMENT showed the lowest degree of conversion in 2 mm depth, and in 3mm depth the degree of conversion increased, which were due to the chemical cure of dual cures, but OPTEC BOND showed decreasing degree of conversion with increasing curing dept h and all experimental groups showed lower degree of conversion than CHEMICAL group which cured in dark room with no light, so the weak light-curing of dual cure resin cement prevented the chemical cure. (P<0.05) 3. CR INLAY CEMENT and DUAL CEMENT showed increasing degree of conversion in 1 mm and 3 mm, according to the increasing cure times, but in 2 mm depth the degree of conversion decreased with increasing light-curing times and OPTEC BOND showed contrary tendency, but there was no ststistical importance in the differences among the experimental group.(P>0.05) 4. The optical density by MTT assay of extractions of CR INLAY CEMENT, DUAL CEMENT and OPTEC BOND revealed no statitically important differences comparing with optical density of negative control.(P>0.05) 5. CR INLAY CEMENT showed a tendency of increaing cytotoxicity with days and DUAL CEMENT and OPTEC BOND showed higher cytotoxicity in 2 days than in 4 days, but there was no statistical importance in the differences.(P>0.05).

  • PDF

Heating & Drying Characteristics of Coating Layer by Induction Heating and Short-wave Infrared Heating (유도가열 및 근적외선 가열방법에 의한 표면처리 강판 도포층의 가열 및 건조 특성)

  • Kim T. S.;Yang J. W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.08a
    • /
    • pp.249-257
    • /
    • 2004
  • Drying and curing characteristics of PCM resins using the induction heater and short-wave infrared emitter module was studied to develop a compact oven system for the high speed CCL and post-treatment equipment. Drying of the polyester resins using the induction heater and infrared heater showed that the blistering tendency of polyester resin coating increased regardless of additives and colors of resins as the heating rate and/or dry film thickness increased. The blistering of polyester resin coating layer occurred when the heating speed was over than $25^{\circ}C/sec$ for the dry film thickness of $19\~20um$, which is the typical thickness of finish coating in CCL. So did it when the heating speed was over than $40^{\circ}C/sec$ for the dry film thickness over than 10 um. The heating efficiency of paint coated steels by the infrared heating was strongly dependent on the colors of paint coating and generally increased for the dark surface and/or coating. But the faster drying of the PCM resin coatings increased the blistering tendency of coating layer. The blistering limit for the typical finish coating by the infrared heating was estimated as the heating rate slower than $20^{\circ}C/sec$ regardless of colors of PCM resins.

  • PDF

Preparation and dielectric properties of polyimide thin films by vapor deposition polymerization method (진공증착중합에 의한 Polyimide 박막의 제조와 유전특성)

  • 이덕출;김형권
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.45 no.3
    • /
    • pp.380-385
    • /
    • 1996
  • Thin films of polyamic acid(PAA) were fabricated by vapor deposition polymerization(VDP) from pyromellitic dianhydride(PMDA) and 4,4'-diamino diphenyl ether(DDE). Thin films of polyimide(PI) were obtained by curing PAA, and their dielectric properties have been measured. The uniform thin films of PI formed by curing PAA at 300 .deg. C for 1 hr. which was confirmed by Fourier transform Infrared spectroscopy(FT-IR) absorption at 720, 1380, 1780c $m_{-1}$. Relative permittivity and tan .delta. were 3.9 and 0.008 at 10kHz, respectively. (author). 8 refs., 11 figs., 1 tab.1 tab.

  • PDF

Effect of Electron Beam and ${\gamma}$-Ray Irradiation on the Curing of Epoxy Resin

  • Kang, Phil-Hyun;Park, Jong-Seok;Nho, Young-Chang
    • Macromolecular Research
    • /
    • v.10 no.6
    • /
    • pp.332-338
    • /
    • 2002
  • The effect of an electron beam and ${\gamma}$-ray irradiation on the curing of epoxy resins was investigated. Diglycidyl ether of bisphenol A (DGEBA) and diglycidyl ether of bisphenol F (DGEBF) as epoxy resin were used. The epoxy resins containing 1.0-3.() wt% of triarylsulphonium hexafluoroantimonate(TASHFA) and triarylsulphonium hexafluorophosphate(TASHFP) as initiator were irradiated under nitrogen at room temperature with different dosage of EB and ${\gamma}$-rays from a Co$^{60}$ u source. The chemical and mechanical characteristics of irradiated epoxy resins were compared after curing of EB and ${\gamma}$-ray irradiation. The thermal properties of cured epoxy were investigated using dynamic mechanical thermal analysis. The chemical structures of cured epoxy were characterized using near infrared spectroscopy. Mechanical properties such as flexural strength, modulus were measured. The gel fraction of DGEBA with ${\gamma}$-ray was higher than that of the epoxy with EB at the same dose. Young's modulus of the sample irradiated by ${\gamma}$-ray is higher than that of sample cured by EB. From the result of strain at yield, it was found that the epoxy cured by ${\gamma}$-ray had a higher stiff property compared with the irradiated by EB.

Comparing volumetric and biological aspects of 3D-printed interim restorations under various post-curing modes

  • Song, Gun;Son, Ji-Won;Jang, Ji-Hyun;Choi, Sung-Hyeon;Jang, Woo-Hyung;Lee, Bin-Na;Park, Chan
    • The Journal of Advanced Prosthodontics
    • /
    • v.13 no.2
    • /
    • pp.71-78
    • /
    • 2021
  • Purpose. This study aims to compare the volumetric change, degree of conversion (DOC), and cytotoxicity of 3D-printed restorations post-cured under three different conditions. Materials and Methods. 3D-printed interim restorations were post-cured under three different conditions and systems: 5 min, 30 min, and 24 h. Three-unit and six-unit fixed dental prostheses (n = 30 for each case) were printed; ten specimens from each group were post-cured and then scanned to compare their volumetric changes. Root-mean-squared (RMS) values of the data were acquired by superimposing the scanned files with original files. Thirty disk-shaped specimens were printed to evaluate the DOC ratio. Fourier transform infrared spectroscopy was used to compare the DOCs of 10 specimens from each group. Human gingival fibroblasts were used to measure the cell viability of every specimen (n = 7). The data from this experiment were employed for one-way analysis of variance and Tukey's post-hoc comparisons. Results. Differences between the three-unit restorations were statistically insignificant, regardless of the post-curing conditions. However, for the six-unit restorations, a high RMS value was acquired when the post-curing duration was 30 min. The average DOC was approximately 56 - 62%; the difference between each group was statistically insignificant. All the groups exhibited cell viability greater than 70%, rendering them clinically acceptable. Conclusion. The post-curing conditions influenced the volume when the length of the restoration was increased. However, this deviation was found to be clinically acceptable. Additionally, post-curing did not significantly influence the DOC and cytotoxicity of the restorations.

Curing Properties of UV-LED Curable Color Coating (UV-LED 경화형 칼라 코팅의 경화특성 연구)

  • Ho, Shin-Chan;Kim, Jong-Gu;Hong, Jin-Who;Ahn, Tae-Jung;Kim, Hyun-Kyoung
    • Journal of Adhesion and Interface
    • /
    • v.13 no.1
    • /
    • pp.31-37
    • /
    • 2012
  • In this study, we investigated the curing properties of UV-LED curable color coating. Specially, the effects of UV-LED wavelength (365, 395, and 405 nm), inert gas, the concentration of photosensitizer, and dual curing on the curing behavior of UV-LED coating systems were studied. The photopolymerization behaviors and the unreacted acrylate groups at Film-air (FA) interface and Film-substrate (FS) interface were investigated by photo differential scanning calorimetry (Photo-DSC) and Fourier-transform infrared spectroscopy with attenuated total reflection (FT-IR/ATR), respectively. Photo-DSC results showed that the heat flow and the ultimate conversion for coating system cured by 405 nm UV-LED were higher than the corresponding values for coating systems cured by 395 and 365 nm UV-LED. FT-IR/ATR results showed that the UV-LED curing systems improved interior and through curing of the coating film, but significantly are affected by oxygen inhibition at FA-interface. The inert environment such as nitrogen purging and the dual curing improved the surface and interior curing of the coating films.

SOLUTION CHARACTERISTICS AND MEMBRANE FORMATION OF PARTIALLY IMIDIZED POLY (AMIC ACID)

  • Lee, Hyuck-Jai;Won, Jong-Ok;Park, Hyun-Chae;Lee, Hoo-Sung;Kang, Yong-Soo
    • Proceedings of the Membrane Society of Korea Conference
    • /
    • 1999.07a
    • /
    • pp.83-86
    • /
    • 1999
  • The imidization effect of a poly (amic acid) dope solution on membrane formation has been investigated. Poly (amic acid) solution in S-methyl-2-pyrrolidione hs been thermally imidized at $120^{\circ}C$ with different curing time and its degree of imidization was determined by infrared spectroscopy. The solution properties have been studied as a function of concentration and curing time by dynamic light scattering. The quality of a solvent was changed from good to poor with increasing imidization of poly(amic acid).The reduced polymer-solvent interaction diminishes the membrane formation time. The morphology of a membrane was able to be controlled by the characteristics of dope solution.

  • PDF

Dual-Curable Acrylic Pressure-Sensitive Adhesives Based on UV and Thermal Processes

  • Kim, Yang-Bae;Park, Su-Cheol;Kim, Hyun-Kyoung;Hong, Jin-Who
    • Macromolecular Research
    • /
    • v.16 no.2
    • /
    • pp.128-133
    • /
    • 2008
  • Several dual-curable acrylic pressure-sensitive adhesives (PSA) were synthesized by the radical polymerization of acrylic monomers containing benzophenone, hydroxyl, and alkyl groups. The optimum extent of UV-induced cure was determined by varying the content of the benzophenone groups (the photoinitiator) from 0.5 to 1.5 wt%. The weight average molecular weight of the polymers obtained ranged from 300,000 to 700,000 amu. The coated pressure-sensitive adhesives were cured either by short UV exposure to induce the grafting of acrylic polymers, or by heating for 6 hat $60^{\circ}C$ to promote the reactions between the polyisocyanates and hydroxyl groups. The dual-curing behavior was determined by monitoring both processes quantitatively by infrared spectroscopy. The developed dual-curable acrylic pressure-sensitive adhesives were found to compensate for the limitations in UV-induced curing of thick coatings.