FRACTURE STRENGTH OF THE IPS EMPRESS CROWN:THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON UPPER FIRST PREMOLAR CROWNS (IPS Empress 도재관의 파절강도 : 상악제1소구치에서 교합면 두께와 축면 경사도에 따른 영향)

  • Dong, Jin-Keun;Oh, Sang-Chun;Kim, Sang-Don
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.1
    • /
    • pp.127-133
    • /
    • 1999
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the upper first premolar. After 10 metal dies were made fir each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results were : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (630N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength(378N). There were no significant differences of the fracture strength by axial inclination in same occlusal depth group. 2. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth.

  • PDF

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN: THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON UPPER FIRST MOLAR (IPS Empress 도재관의 파절강도 : 상악 제1대구치에서 교합면 두께와 축면경사도에 따른 영향)

  • Choi Teak-Rim;Lee Hae-Young;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.2
    • /
    • pp.171-183
    • /
    • 2001
  • The purpose of this study was compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the upper first molar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and were cemented with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows: 1. The fracture strength of the ceramic crown with 2.5mm depth and $8^{\circ}$ inclination was the highest (1393N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (1015N) 2. There were no significant differences of the fracture strength according to occlusal depth and axial inclination. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth. 4. There was positive correlation between the fracture strength and the fracture surface area of crowns.

  • PDF

Crown Duplication Technique of Upper Central Incisor using IPS-Empress system (IPS-Empress system을 이용한 상악 중절치의 치관복제술)

  • Oh, Sang-Chun;Shin, Young-Ho
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.22 no.3
    • /
    • pp.243-250
    • /
    • 2006
  • Due to high esthetic demands from patients, we are driven to fabricate natural-looking(form and color) restorations. In the past decade, the glass-ceramic in dentistry has been used as a material with variable crystals that affects the appearance, characteristics, and mechanical properties of metal-free fixed restoration. The conventional IPS Empress glass-ceramic is a heat-pressed, leucite reinforced material using the "lost wax" principle. This glass-ceramic has been successfully used for esthetic restorations such as all-ceramic crowns, inlays/onlays, and veneers for about 15 years. This article presents that the form and surface texture of clinical crown are duplicated by IPS-Empress system using "lost-wax technique".

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECTS OF INCISAL REDUCTION AND AXIAL INCLINATION ON UPPER CANINE (IPS Empress 도재관의 파절강도 : 상악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Shin Dong-Kuk;Kang Han-Joong;Park Yong-Suck;Park Kwang-Soo;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.1
    • /
    • pp.30-40
    • /
    • 2005
  • Purpose. The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction (2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the upper canine. Material and methods. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and the universal testing machine was used to measure the fracture strength. Results. 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest (839N) Crowns of 2.0mm depth and $12^{\circ}$ inclination had the lowest strength (559N). 2. There was no significant difference in the fracture strength by axial inclination in the same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER SECOND PREMOLAR (IPS Empress 도재관의 파절강도 : 하악 제2소구치에서 교합면 두께와 축면 경사도에 따른 영향)

  • Kim Hee-Jin;Lee Hae-Hyoung;Nam Young-Sung;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.40 no.5
    • /
    • pp.441-450
    • /
    • 2002
  • The purpose of this study was compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower second premolar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement. The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1284 N). Crowns of 1.5mm depth and $8^{\circ}$ inclination had the lowest strength (951 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth.

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER FIRST MOLAR (IPS Empress 도재관의 파절강도: 하악 제1대구치에서 교합면 두께와 축면경사도에 따른 영향)

  • Kim Sung-Hoon;Lee Jin-Han;Kim Yu-Lee;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.41 no.1
    • /
    • pp.48-60
    • /
    • 2003
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower First Molar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement(Bistite resin cement, Tokuyama Soda Co. LTD., Japan). The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine(Zwick Z020, Zwick, Germany)was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1789 N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (1091 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth. Size of fragment was affected by the amount of occlusal reduction.

A STUDY ON THE FRACTURE STRENGTH OF THE IPS-EMPRESS CERAMIC CROWN ACCORDING TO MARGIN TYPE (IPS-Empress 도재관의 변연형태에 따른 파절강도에 관한 연구)

  • Kim, Hyun-Soo;Ju, Tae-Hun;Oh, Sang-Chun;Dong, Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.35 no.2
    • /
    • pp.296-307
    • /
    • 1997
  • The purpose of this study was to compare the fracture strength of the IPS-Empress ceramic crown according to margin types such as bevel, shoulder, rounded shoulder, shoulder with bevel, rounded shoulder with bevel and bevel with groove. After 10 metal dies were constructed for each group, the IPS-Empress ceramic crown were fabricated and each crown was cemented on each metal die with Bistite resin cement. The cemented crowns mounted in the testing jig were inclined 30 degree and universal testing machine (Zwick 1456 41, Zwick Co., Germany) was used to measure the fracture strength. The obtained results were as follows : 1. The fracture strength of the crown with rounded shoulder was the highest of all. The mean fracture strength was 484N in rounded shoulder, 357N in bevel, 341N in rounded shoulder with bevl, 300N in shoulder with bevel, 280N in shoulder and 275N in bevel with groove. 2. The fracture strength of rounded shoulder was statistically different from those of shoulder with bevel, shoulder and beve41 with groove. 3. In the strain at fracture, there was no significant difference among each group. 4. The fracture mode of the crown was similar and most of fracture line began at the loading area and extended through proximal surface perpendicularly to the margin, irrespective of margin type.

  • PDF

FRACTURE STRENGTH OF ZIRCONIA MONOLITHIC CROWNS (지르코니아 단일구조 전부도재관의 파절강도)

  • Jeong Hee-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.44 no.2
    • /
    • pp.157-164
    • /
    • 2006
  • Purpose: The purpose of this study was to compare the fracture strength of the zirconia monolithic all-ceramic crowns according to the thickness(0.5 mm, 0.8 mm, 1.1 mm) and IPS Empress II ceramic crown of 1.5 mm thickness. Material and method: Eight crowns for each of 3 zirconia crown groups were fabricated using CAD/CAM system(Kavo, Germany) and eight Empress II crowns were made from silicone mold and wax pattern. Each crown group was finished in accordance with the specific manufacturer s instruction. All crowns were luted to the metal dies using resin cement and mounted on the testing jig in a universal testing machine. The load was directed at the center of crown with perpendicular to the long axis of each specimen until catastrophic failure occurred. Analysis of variance and Tukey multiple comparison test(p<.05) were applied to the data. Results and Conclusion: 1. The fracture strength of the zirconia monolithic all-ceramic crown was higher thickness increased(p<.05). 2 The fracture strength of 1.1 mm thickness zirconia monolithic all-ceramic crown was higher than the fracture strength of 1.5 mm thickness IPS Empress II crown(p<.05). 3. The fracture strength of 0.5 mm thickness zirconia monolithic all-ceramic crown exceeded maximum occlusal forces.

Esthetic reconstruction of upper central incisor using immediate Frialit-2 implant placement, immediate temporary crown fabrication and IPS Empress 2 crown (즉시 Frialit-2 implant 식립, 즉시 임시치관 제작 그리고 IPS Empress 2 crown을 이용한 상악중절치의 심미적 수복)

  • Kim, Yu-Lee;Oh, Sang-Chun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.19 no.1
    • /
    • pp.43-48
    • /
    • 2003
  • During the past several years, significant advances have occurred in the utilization of osseointegrated implants for the treatment of partially edentulous patients. One of the biggest purposes for treating of these patients is the high demand for improved esthetics, especially in the anterior region. For this esthetics, the new trend in dental implants is the immediate placement and immediate superstructure fabrication. The refined surgical technique, the skillful soft tissue management, and the proper prosthetic coordination are the main factors to achieve natural looking of implant supported prosthesis. The customized provisional restoration and the customized impression coping are recommended for the optimal peri-implant soft tissue contour. The basic concept of Frialit 2 system was the immediate replacement of a tooth with root-analog fixture after extraction. This system guarantees an ideal result in function and esthetics. The ceramic abutment system offers improved quality in the respect of esthetics, fitness, translucency, and biocompatibility. In this clinical report, the final restoration made with IPS Empress 2 crown on the CeraBase abutmen of Frialit 2 system allowed the reproduction of the natural vitality of tooth and adjacent gingiva.

Fracture Strength of IPS Empress Crown : The Effect of Incisal Reduction and Axial Inclination on Lower Canine (IPS Empress 도재관의 파절강도 : 하악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Jung, Young-Chan;Shin, Dong-Kuk;Park, Eun-Ju;Kim, Min-Jeong;Dong, Jin-Keun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.20 no.1
    • /
    • pp.19-29
    • /
    • 2004
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction(2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the lower canine. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest(1377N). Crowns of 2.0mm depth and $4^{\circ}$ inclination had the lowest strength (731 N). 2. There were no significant differences of the fracture strength by axial inclination in same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.