Browse > Article

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER FIRST MOLAR  

Kim Sung-Hoon (Department of Prosthodontics, College of Dentistry, Wonkwang University)
Lee Jin-Han (Department of Prosthodontics, College of Dentistry, Wonkwang University)
Kim Yu-Lee (Department of Prosthodontics, College of Dentistry, Wonkwang University)
Dong Jin-Keun (Department of Prosthodontics, College of Dentistry, Wonkwang University)
Publication Information
The Journal of Korean Academy of Prosthodontics / v.41, no.1, 2003 , pp. 48-60 More about this Journal
Abstract
The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower First Molar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement(Bistite resin cement, Tokuyama Soda Co. LTD., Japan). The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine(Zwick Z020, Zwick, Germany)was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1789 N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (1091 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth. Size of fragment was affected by the amount of occlusal reduction.
Keywords
Axial inclination; Fracture strength; IPS Empress Crown; Occlusal depth;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Dicor laboratory manual, Dentsply Int., York., PA, 1987
2 Beham G. IPS-Empress. A new ceramic technology. Ivoclar-Vivadent report 1990;6:1-13
3 Kern M, Doglas WH, Fechtig T, Strub JR, Delong R. Fracture strength of all-porcelain Resin bonded bridges after testing in an artificial oral environment. J Prosthet Dent 1993;21:117-21
4 Doyle MG, Goodacre CJ, Andres CJ. The effect of tooth preparation design on the breaking strength of Dicor crown: Part 3. Int J Prosthodont 1990;3:327-31   PUBMED
5 Eden GT, Kacic JM. Dicor crown strength improvement due to bonding. J Dent Res 1987;66:207 abstr No. 802
6 Wohlwend A, Scharer P. The Empress technique. Quintessenz Zahntech 1990;16:966-78
7 Luthy H, Dong JK, Wohlwend A, Scharer P. Effects of veneering and glazing on the strength of heat-pressed ceramics. Schweiz Monatsschr Zahnmed 1993;103:1257-60   PUBMED
8 Mackert JR, Russel CM. Leucite crystallization during Empress proessing, Abstract. J Dent Res 1995;74:166
9 Krejci I, Krejci D, Lutz F. Clinical evaluation of a new pressed glass ceramic inlay material over 1.5 years. Quintessense int 1992;23:181-6
10 김병훈 외 9명. 세라믹스 총론. 반도출판사 1987
11 Green DJ. Microcracking mechanisms in ceramics. In. Bradt RC, Evans AG, Lange FF, Hasselman DP(eds). Fracture Mechanics of ceramics. Vol.5. New York. plenum press. 1983;457-78
12 Green DJ, Hannink RHJ, Swain MV. Transformation toughening of ceramics. Boca Raton FL. CRC Press. 1989;57-91
13 Anusavice KJ, Hojjatie B. Tensile stress in glassceramic crowns: Effect of flaws and cement voids. Int J Prosthodont 1992;5:351-4   PUBMED
14 Hobo S, Iwata T. Castable apatite ceramics as a new biocompatible restorative material. 1. Teoretical considerations. Quintessence Int 1985;16:135-41
15 Rodrigues A, Nathanson D, Goldstein R. Fracture resistance of different porcelain crowns system in vitro. Abstract No.1311. J Dent Res (special issue)1987;66:270
16 McInnes-Ledoux PM, Ledoux WR, Weinberg R, Pappold A. Luting castable ceramic restorations-a bond strength study 'Abstract'. J Dent Res1987;66:245
17 Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. J Prothet Dent 1999;81(6):652-61   DOI   PUBMED   ScienceOn
18 Song BK, Lee HH, Dong JK. Fracture Strength of the IPS Empress Crown : The effect of occlusal depth and axial inclination on upper central incisor. J Korean Academy Stomatognathic Function and occlusion 2000;16:237-44
19 Fiedlander LD, Munoz CA, Goodacre CJ, Doyle MG, Moor BK. The effect of tooth preparation design on breaking strength of Dicor crowns: Part 1. Int J Prosthodont 1990;3:159-64
20 Yoshinari M, Derand T. Fracture strength of all-ceramic crowns. Int J Prosthodont 1994;7:329-38   PUBMED
21 Mutobe Y, Maruyama T, Kataoka S. In harmony with nature. Esthetic restoration of a nonvital tooth with IPS-Empress all-ceramic material. QDT 1977;83-5
22 Kelly JR, Giordana R, Prober R, Gima MJ. Fracture surface analysis of dental ceramics: Clinically failed restorations. Int J Prosthodont 1990;3:430-4   PUBMED
23 Doering J, Jensen ME, Sheth J, Tolliver D, Chan D. Fracture resistance of resinbonded etched-porcelain full veneer crowns 'Abstract'. J Dent Res 1987;66:207
24 Dong JK, Luthy H, Wohlwend A, Scharer P. Heat-pressed ceramics : Technology and strength. Int J Prosthodont 1992;5:9-16   PUBMED
25 Craig RG. Restorative dental materials, pp65, St Louis, CV Mosby,1989
26 Shinohara N, Minesaki Y, Mukoyoshi N, Moriyama, Jimi T. The effect of the cementing material on the strength of the all-ceramic crown. J JPN Prosthodont S 1989;33:416
27 Grey NJA, Piddock V, Wilson MA. In vitro comparison of conventional crowns and a new all-ceramic system. J Dent 1993; 21:47-51   DOI   ScienceOn
28 Grossman DG, Nelson JW. The bonded Dicor crown. J Dent Res 1987;66:206 abstr No. 800
29 Probster L. Compressive strength of two modern all-ceramic crowns. Int J Prosthodont 1992;5:409-14   PUBMED
30 Mackert JR, Russell CM. Leucite crystallitation during processing of a heat-pressed dental ceramic. Int J Prosthodont 1996;9: 261-5   PUBMED
31 Sozio RB, Riley EJ. Shrink free ceramic. Dent Clin North Am 1985;29:705-17   PUBMED
32 이준근. 세라믹의 기계적 특성. 반도출판사 1994
33 Mackert JR Jr, Russel C. Leucite crystallization of a heat-pressed dental ceramic. Int J Prosthodont 1996;9:261
34 Sorensen JA, Fanuscu MI, Choi C, Mifo W. Status of clinical trial on Empress crown. J Dent Res 1995;74:159-62
35 Chan C, Weber H. Plaque retention on teeth restored with full-ceramic crowns: A comparative study. J Prosthet Dent 1986;56:666-71   DOI   ScienceOn
36 Josephson BA, Schulman A, Dunn ZA, Hurwitz W. A compressive strength study of complete ceramic crowns, Part II. J Prosthet Dent 1991;65:388-91   DOI   ScienceOn
37 Dicor laboratory manual. Densply international, York., Pa, 1987
38 Okeson JP. Management of Temporomandibular Disorders and Occlusion. MosbyYear Book 1993;69
39 Anusavice KJ. Degradability of dental ceramics. Adv Dent Res 1992;6:82-9   DOI   PUBMED
40 Land CH. A new system of restoring badly decayed teeth by means of an enamelled metallic coating. Independent Practitoner 1886;7:407-8
41 Anusavice KJ, Hojjatie B. Tensile stress in glassceramic crowns: Effect of flaws and cement voids. Int J Prosthodont 1992;5:351-4   PUBMED
42 Probster L. Compressive strength of two modern all-ceramic crowns. Int J Prosthodont 1992;5:409-14   PUBMED
43 Clause H. Vita In-Ceram a new system for producing aluminum oxide crown and bridge substructures. Quintessenz Zahntech 1990;16:35-46
44 오상천, 최대균, 우이형, 최부병. 주입선에 따른 IPS Empress도재의 굽힘강도와 미세구조에 관한 연구. 경희치대논문집 1997;19:391-418
45 Southan DE, Jorgensen KD. Faulty porcelain jacket crowns. Aust Dent J 1973; 18: 152-6   DOI   ScienceOn
46 Kelly JR, Giordano R, Pober R, Michael J. Fracture surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont 1990;3:430-4   PUBMED
47 Hsinenberg BJ. IPS-Empress mit neuer keramik technologie. Quintessenz Zahntech 1991;17:475-9
48 Richards MW, Kelly JR. Indentation-strength of unpressed and pressed Empress disk, Abstract. J Dent Res 1994;74:159
49 Tidehag P, Gunne J. A 2-year clinical follow-up study of IPS-Empress ceramic inlay. Int J Prosthodont 1995;8:456-60   PUBMED
50 Seghi RR, Sorensen JA. Relative flexural stength of six new ceramic materials. Int J Prosthodont 1995;8:239-46   PUBMED
51 Choi TR, Lee HH, Dong JK. Fracture Strength of the IPS Empress Crown : The effect of occlusal depth and axial inclination on upper first molar. J Korean Academy Prosthodontics 2001;39:171-683
52 Vita Zahnfabrik. Vita Hi-Ceram working instruction. Bad Sackingen, Germany, 1988
53 Kim HS, Ju TH, Oh SC, Dong JK. A study on the fracture strength of the IPS-Empress ceramin crown according to margin type. J Korean Academy Prosthodontics 1997;35:296-307
54 김경남 외 6명. 치과재료학. 군자출판사 1995
55 Ching-Cheng L, O'Brien WJ. Strength of magnesia-core crown with different body porcelain. Int J Prosthodont 1993;6:60-4
56 Optec HSP laboratory technique manual. Jeneric/pentro Inc, Wallingford. Conn, January, 1988
57 Grossman DG, Nelson JW. The bonded Dicor crown. J Dent Res 1987;66:206, bstr No. 800
58 Uctasli S, Wilson HJ, Unterbrunk G, Zaimoglu A. The strength of a heat-pressed all-ceramic restorative material. J Oral Rehabilitation 1996;23:257-61   DOI
59 Dong JK, Oh SH, Kim SD. Fracture strength of the IPS Empress crown : The effect of occlusal depth and axial inclinationon upper first premolar crowns. J Korean Academy Prosthodontics 1999;37:127-33
60 IPS-Empress manual. Ivoclar Com., Schann, Liechtenstein
61 Friedlander LD, Munoz CA, Goodacre CJ, Doyle MG, Moore BK. The effect of tooth preparation design on the breaking strength of Dieor crowns. Int J Prosthodont 1993;3:159-68