FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER SECOND PREMOLAR |
Kim Hee-Jin
(Department of Prosthodontics, School of dentistry, Wonkwang University)
Lee Hae-Hyoung (Department of Biomaterials, School of dentistry, Wonkwang University) Nam Young-Sung (Department of Prosthodontics, School of dentistry, Wonkwang University) Dong Jin-Keun (Department of Prosthodontics, School of dentistry, Wonkwang University) |
1 | Beham G. IPS-Empress. A new ceramic technology. Ivoclar-Vivadent Report 1990; 6:1-13 |
2 | Paek SJ. Yang JH. A study on the fracture strength of all-ceramic crowns. J Korean Acad Prosthodont 1995:33:611--633 |
3 | Wohlwend A., Strub JR., Scharer P. Metal ceramic and all porcelain restorations: Current consideration. Int J Prosthodont 1989;2: 13-26 |
4 | Claus H. Das Hi-Ceram-Verfahren-metallfrere Kronen auf einem Keramikgerust. Dent Labor 1987;35:479 |
5 | Hobo S, Iwata T. Castable apatite ceramics as a new biocompatible restorative material. I. Theoretical considerations. Quintessence Int 1985: 16: 135 |
6 | Schwickerath H. Was der Zahntechniker each ten sollte Herstellung von vollkeramischem Zahnersatz. Dent Labor. 1992:40: 1501 |
7 | Craig RG. Restorative dental materials. pp65. St Louis. CV Mosby. 1989 |
8 | Probster L. Survival rate of In-Coram restoration. Int J Prosthodont 1993;259-263 |
9 | Southan DE, Jorgensen KD. Faulty porcelain jacket crowns. Aust Dent J 1973; 18:152-156 DOI ScienceOn |
10 | Mackert JR Jr, Russel C. Leucite crystallization of a heat-pressed dental ceramic. Int J Prosthodont. 1996: 9: 261 |
11 | Yu HW, Song CY, Bae TS, Song KY, Park CW. A comparative study on the flexure strength of the ceramics for all-ceramic crowns. J Korean Acad Prosthodont 1994;32: 195-211 |
12 | Vintage manual. Shofu Co. Tokyo, Japan |
13 | Mclean JW. Ceramics in clinical dentistry. Br Dent J 1988;187 |
14 | Tidehag P, Gunne J. A 2-year clinical follow-up study of IPS-Empress ceramic inlay. Int. J. Prosth 1995:8:456-460 |
15 | Seghi RR. Sorensen JA. Relative flexural strength of six new ceramic materials. Int. J. Prosth. 1995:8:239-24 |
16 | Sozio RB, Riley EJ. Shrink free ceramic. Dent Clin North Am 1985:29:705-717 |
17 | Faber KT, Evans AG. Crack deflection processes, I Theory. Acta Metall. 1983: 31:565-576 |
18 | Grossman DG, Nelson JW. The bonded Dicor crown. J Dent Res. abstr No.800. 1987:66:206 |
19 | Oh SC, Choi DG, Woo YH, Choi BB. A study on the flexure strength and microstructure of IPS Empress ceramics according to the sprue types. Kyunghee Dent J 1997; 19: 391-418 |
20 | Optec Hsp laboratory technique manual. Jeneric/Pentro Inc Wallingford CN January 1988 |
21 | Kelly JR, Giordana R, Prober R, Gima MJ. Fracture surface analysis of dental ceramics. Clinically failed restorations. Int J Prosthodont. 1990;3:430 |
22 | Friedlander LD, Munoz CA, Goodacre CJ, Doyle MG, Moor BK . The effect of tooth preparation design on breaking strenth of Dicor crowns. Part 1. Int J Prosthodont 1990: 3: 159 |
23 | Dong JK, Oh SC, Kim SD. Fracture strength of the IPS Empress crown: The effect of occlusal depth and axial inclination on upper first premolar crowns. J Korean Acad Prosthodont 1999;37: 127-133 |
24 | Mutobe Y, Maruyama T, Kataoka S. In harmony with nature. Esthetic restoration of a nonvital tooth with IPS-Empress all-ceramic material. QDT 1997;83-85 |
25 | Claus H. Vita In-ceram, A new system for producing aluminum oxid crown and bridge substructures. Quintessz Zahntech 1990; 16:35 |
26 | Green DJ. Microcracking mechanisms in ceramics. In. Bradt RC, Evans AG, Lange FF, Hasselman DP(des), Fracture Mechanics of ceramics. Vol.5. New York. plenum press. 1983:457-478 |
27 | Dong JK. Luthy H, Wohelwend A, Scharer P. Heat-Pressed Ceramics. Technology and strength. Int J Prosthodont 1992:5:916 |
28 | Dicor laboratory manual. Densply international. York Pa 1987 |
29 | Adair PJ, Grossman DG. The castable ceramic crown. Int J Periodont Rest Dent 1984:4:32 |
30 | Anusavice KJ, Hojjatie B. Tensile stress in glass-ceramic crowns. Effect of flaws and cement voids. Int J Prosthodont 1992:5:351 |
31 | Schwickerrath H. Die In-Ceram Aluminiumoxid-Kerarniken Innova-tiver dentalke laischer Werkstoff. Dent Labor 1989: 37:1597 |
32 | Green DJ, Hannink FHJ, Swain MV. Transformation toughening of ceramics. Boca Raton FL. CRC Press. 1989:57-91 |
33 | Brodbeck D, Studer S, Lehner C. Six-year clinical experience with an all-ceramic restoration system. Dental-Labor 1995;Ill |
34 | Yamamoto M. Metal-Ceramics. Chicago. Quintessence Int 1987;219 |
35 | Hobo S, Iwata T. Castable apatite ceramics as a new biocompatible restorative material. II. Fabrication of the restoration. Quintessence Int 1985; 16: 207 |
36 | Krejci I. Krejci D, Lutz F. Clinical evaluation of a new pressed glass ceramic inlay material over 1.5 years. Quintessence int.1992:23:181-6 |
37 | Oh SC, Dong JK. A study on the flexural strength of heat-pressed ceramics according to sprue designs, J Korean Acad Prosthodont 1997; 35: 130-140 |