Effect of Nano Grain Growth on Coefficient of Thermal Expansion in Electroplated Fe-Ni Invar Alloy (Fe-Ni Invar 합금에서 나노 결정립 성장이 열팽창계수에 미치는 영향)

  • Yim, Tai Hong;Choe, Byung Hak;Jeong, Hyo Tae
    • Korean Journal of Materials Research
    • /
    • v.24 no.10
    • /
    • pp.515-519
    • /
    • 2014
  • The aim of this paper is to consider the effect of annealing on the coefficient of thermal expansion (CTE) of electroplated Invar Fe-Ni alloy. The CTE of the as-electroplated alloy is lower than those of alloys annealed at $400^{\circ}C$ and $800^{\circ}C$. XRD peaks become sharper as the as-electroplated alloy is annealed, which means the grain growth. The average grain sizes of as-electroplated and as-annealed alloys at $400^{\circ}C$ and $800^{\circ}C$ are 10 nm, 70 nm, and $2{\mu}m$, respectively, as determined by TEM and EBSD analyses. The CTE variation for the various grain sizes after annealing may come from the magnetostriction effect, which generates strain due to changes in the magnetization state of the alloys. The thermal expansion coefficient is considered to be affected by nano grain size in electroplated Fe-Ni Invar alloys. As grain size decreases, ferromagnetic forces might change to paramagnetic forces. The effect of lattice vibration damping of nano grain boundaries could lead to the decrease of CTE.

Carbon Nanotube Growth on Invar Alloy using Coal Tar Pitch (콜타르피치를 이용한 Invar 합금 위 탄소나노튜브의 합성)

  • Kim, Joon-Woo;Jeong, Goo-Hwan
    • Journal of the Korean institute of surface engineering
    • /
    • v.50 no.6
    • /
    • pp.516-522
    • /
    • 2017
  • We report the growth of carbon nanotubes (CNT) on Invar-42 plates using coal tar pitch (CTP) by chemical vapor deposition (CVD) method. The solid phase CTP is used as an inexpensive carbon source since it produces a bunch of hydrocarbon gases such as $CH_4$ and other $C_xH_v$ by thermal decomposition over $450^{\circ}C$. The Invar-42 is a representative Ni-based ferrous alloy and can be used repetitively as a substrate for CNT growth because Ni and Fe are used as very active catalytic elements. We changed mixing ratio of carrier gases, argon and hydrogen, and temperature of growth region. It was found that the optimum gas ratio and temperature for high quality CNT growth are $Ar:H_2=400:400$ sccm and $1000^{\circ}C$, respectively. In addition, the carbon nanoball (CNB) was also obtained by just changing the mixing ratio to $Ar:H_2=100:600$ sccm. Finally, CTP can be employed as a versatile carbon source to produce various carbon-based nanomaterials, such as CNT and CNB.

A Study on AK Shadow Mask with Fe-Ni Alloy Coating for Flat CPTs

  • Kim, Sang-Mun
    • Journal of Information Display
    • /
    • v.5 no.4
    • /
    • pp.27-30
    • /
    • 2004
  • This paper investigates the effects of coating such as Invar (Fe-36% Ni), Fe-Ni Alloys and $WO_3$ on the doming property of aluminum killed (AK) shadow masks, which may be used for flat CPTs. Invar and Fe-Ni Alloys are deposited on AK shadow mask in plasma atmosphere and annealed. $WO_3$ is screen-printed on the deposited layer. The coating is observed to cause a decrease in the doming property of the shadow masks due to their lower thermal expansion coefficients and anti-doming properties.

Study on Precipitation and Mechanical Properties of High Strength Invar Alloy (고강도 인바합금의 석출거동과 기계적 특성 연구)

  • Jeong, J.Y.;Lee, K.D.;Ha, T.K.;Jeong, H.T.
    • Transactions of Materials Processing
    • /
    • v.17 no.7
    • /
    • pp.507-510
    • /
    • 2008
  • Effect of V addition on the precipitation behavior and strength of Fe-36Ni based high strength Invar alloy for power transmission wire was investigated. Fe-36Ni Invar alloy plates were fabricated using conventional ingot casting followed by hot rolling. High strength can be obtained through precipitation hardening and strain hardening by cold rolling. Simulation using FactSage$^{(R)}$ revealed that equilibrium phases which can be formed are two kinds of MC-type precipitates, $Mo_{2}C$ and $M_{23}C_6$ carbide. The latter stoichiometric carbide was expected to be formed at relatively lower temperature of $800^{\circ}C$.

Effect of Aging on fatigue of Al Clad INVAR Core Wire for High Capacity and Low Sag(STACIR/AW) Conductor ( 1 ) (경년열화가 가공송전선(STACIR/AW)용 강심소재 Al Clad Invar 강선의 피로에 미치는 영향 ( 1 ))

  • Kim Shang-Shu;Kim Byung-Geol;Hyun Suk-Kyu;Sin Goo-Yong;Lee Dong-Il;Min Byung-Uk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.1
    • /
    • pp.91-99
    • /
    • 2006
  • Fatigue properties of INVAR/AW wires have been investigated under the heat exposure in order to ensure stable operation and to estimate life span of their power line. In the case of heat exposure for 10000 hr, fatigue life and limit increased. For further heat exposure, fatigue limit decreased due to the decrease in yield strength. The variation fatigue of strand wire was strongly dependent on its amplitude. Also, cracks in wires of 7 strands were caused by stress concentration at the outer surface and fretting between each wire during vibration.

Relationship Between Texture and Deformability in Fe-Ni Invar Alloy Strips (Fe-Ni 인바(Invar) 합금 박판의 가공성 향상을 위한 방향성 조직 제어)

  • Park, S.Y.;NamGung, J.;Kim, M.C.;Kim, S.S.;Lee, S.S.;Park, C.G.
    • Transactions of Materials Processing
    • /
    • v.15 no.8 s.89
    • /
    • pp.586-590
    • /
    • 2006
  • 42Ni-Fe Invar alloy strips were fabricated using conventional ingot casting and melt drag casting followed by rolling. Mechanical properties such as tensile strength, elongation and blanking deformability of the strips were evaluated. The properties were strongly depended on fabrication methods. Tensile strength and elongation of all strips were in the range of $40-60kg/mm^{2}$ and 26-35%, respectively, which are enough values for the manufacture of the final products. In some of the strips, however, burrs occurred at deformed surface. The properties of strips were explained in terms of microstructure such as grain size and texture formation during rolling. Additionally, strips by melt drag casting method were compared to those by conventional ingot casting.

Black oxide coating on Invar steel (인바강재의 흑화처리)

  • Kim, H. G.;Kang, T.
    • Journal of the Korean institute of surface engineering
    • /
    • v.26 no.3
    • /
    • pp.109-114
    • /
    • 1993
  • Black magnetite film could be formed on Invar steel for shadows mask by iron electroplating in thickness of 0.46~0.63$\mu\textrm{m}$ on Invar steel and subsequent oxidation of iron by immersion in strongly alkaline soution for 30~60 minutes. blackness degreed of magnetite oxide film on Invar was C20BL90 in comparision of color chart of Dainippon Ink & Chemicals Inc. Co. and adhesion test showed excellent adhesion of oxide film on substrate. Magnetite oxide film grew up on iron in hot strongly alkaline solution according to 'Sato-Cohen' oxide film growth model.

  • PDF

Effect Of The Microstructure And Aging Treatment Conditions On Strength Of High Strength Invar Alloy (고강도 인바합금의 강도에 미치는 미세구조와 시효처리 조건의 영향)

  • Jung, J.Y.;Lee, K.D.;Ha, T.K.;Jeong, H.T.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.10a
    • /
    • pp.322-325
    • /
    • 2007
  • Precipitation characteristics of the Fe-36Ni based high strength Invar alloy for power transmission wire was investigated in this study. High strength can be obtained in this alloy through solution hardening, precipitation hardening and strain hardening by cold working. In the present study, ingots of Fe-36Ni based Invar alloys with the contents of C, Mo and V varied. Microstructure observations by OM, SEM, and TEM were carried out to validate the simulation results. BCC phase and $FeNi_3$ phase are also expected at lower temperatures below $500^{\circ}C$. Aging treatments were carried out at temperatures ranging from 400 to $900^{\circ}C$ for time intervals from 3 min to 100hrs. Peak aging condition was obtained as $400^{\circ}C$ and 1 hr. With temperature increased, peak strength was decreased abruptly. Microstructure observation was conducted by optical microscopy, scanning electron microscopy, and transmission electron microscopy.

  • PDF