• Title/Summary/Keyword: High-temperature compression test

Search Result 136, Processing Time 0.033 seconds

High Temperature Plastic Deformation Behaviors of the Bulk Metallic Glass Zr-Ti-Cu-Ni-Be Alloy (벌크 비정질 Zr-Ti-Cu-Ni-Be 합금의 고온 소성 변형 특성)

  • Lee K. S.;Ha T. K.;Ahn S. H.;Chang Y. W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.10a
    • /
    • pp.272-276
    • /
    • 2001
  • Multicomponent $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ bulk matallic glass alloy shows good bulk glass forming ability due to its high resistance to crystallization in the undercooled liquid state.1) In this study, DSC and X-ray diffractometry have been performed to confirm the amorphous structure of the master $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ alloy. To investigate the mechanical properties and deformation behaviors of the bulk metallic $Zr_{41.2}Ti_{13.8}Cu_{12.5}Ni_{10}Be_{22.5}$ alloy, a series of compression tests has been carried out at the temperatures ranging from $351^{\circ}C$ to $461^{\circ}C$ and at the various initial strain rates from $2{\times}10^{-4}s^{-1}\;to\;2{\times}10^{-2}s^{-1}$. There are two types of nominal stress-strain curves. The one shows linear stress-strain relationship meaning fracture at maximum stress, the other shows plastic deformation including steady-state flow. Also DSC analysis for the compressed specimens has been performed to investigate the change of thermal stability and crystallization behavior for the various test conditions.

  • PDF

A Study on the Development of Non-PC High-Early-Strength Concrete Without Steam Curing (증기양생이 불필요한 PC부재용 조강형 콘크리트 개발에 관한 연구)

  • Jun, Woo-Chul;Lee, Ji-Hwan;Park, Hee-Gon;Lee, Jae-Sam;Kim, Kyung-Min;Cho, In-Sung
    • Journal of the Korea Institute of Building Construction
    • /
    • v.14 no.2
    • /
    • pp.156-162
    • /
    • 2014
  • This study aims to develop a rapidly hardening type of concrete to achieve the removal of form intensity (more than 10MPa) using the method of curing at room temperature in order to solve some economic environmental problems by omitting the steam curing process involved in producing PC (Precast Concrete). Therefore, this study evaluated a rapidly hardening cement containing a high amunt of C3S, which is very responsive in expressing early intensity, and a rapidly hardening type of concrete which uses some hardening accelerator to increase thehydration reaction of $C_3S$. The results of the experiment on concrete using some hardening accelerator are asfollows. In the slump flow experiment for identifying the liquidity and the air test, the desired values were met. The compression strength showed rapid expression response by 12 hours, and met the desired value within 6~9 hours. Its drying shrinkage value and Autogenous shrinkage value were measured as below ($-754.5{\times}10^{-6}$),and satisfied the requirements. In addition, in the Semi-Adiabatic Temperature Test, it was found that the concrete rose to its peak temperature within 24 hours and then its temperature dropped.

Investigation of the Cryogenic Performance of the High Density Polyurethane Foam (고밀도 폴리우레탄 폼의 극저온 성능 분석)

  • Jeong-Hyeon Kim;Jeong-Dae Kim;Tae-Wook Kim;Seul-Kee Kim;Jae-Myung Lee
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.26 no.6_3
    • /
    • pp.1289-1295
    • /
    • 2023
  • Polyurethane foam insulation required for storing and transporting cryogenic liquefied gas is already widely used as a thermal insulation material for commercial LNG carriers and onshore due to its stable price and high insulation performance. These polyurethane foams are reported to have different mechanical performance depending on the density, and the density parameter is determined depending on the amount of the blowing agent. In this study, density-dependent polyurethane foam was fabricated by adjusting the amount of blowing agent. The mechanical properties of polyurethane foam were analyzed in the room temperature and cryogenic temperature range of -163℃ at 1.5 mm/min, which is a quasi-static load range, and the cells were observed through microstructure analysis. The characteristics of linear elasticity, plateau, and densification, which are quasi-static mechanical behaviors of polyurethane foam, were shown, and the correlation between density and mechanical properties in a cryogenic environment was confirmed. The correlation between mechanical behavior and cell size was also analyzed through SEM morphology analysis. Polyurethane foam with a density of 180 kg/m3 had a density about twice as high as that of a polyurethane foam with a density of 96 kg/m3, but yield strength was about 51% higher and cell size was about 9.5% smaller.

Effects of Zr-hydride distribution of irradiated Zircaloy-2 cladding in RIA-simulating pellet-clad mechanical interaction testing

  • Magnusson, Per;Alvarez-Holston, Anna-Maria;Ammon, Katja;Ledergerber, Guido;Nilsson, Marcus;Schrire, David;Nissen, Klaus;Wright, Jonathan
    • Nuclear Engineering and Technology
    • /
    • v.50 no.2
    • /
    • pp.246-252
    • /
    • 2018
  • A series of simulated reactivity-initiated accident (RIA) tests on irradiated fully recrystallized boiling water reactor Zircaloy-2 cladding has been performed by means of the expansion-due-to-compression (EDC) test method. The EDC method reproduces fuel pellet-clad mechanical interaction (PCMI) conditions for the cladding during RIA transients with respect to temperature and loading rates by out-of-pile mechanical testing. The tested materials had a large variation in burnup and hydrogen content (up to 907 wppm). The results of the EDC tests showed variation in the PCMI resistance of claddings with similar burnup and hydrogen content, making it difficult to clearly identify ductile-to-brittle transition temperatures. The EDC-tested samples of the present and previous work were investigated by light optical and scanning electron microscopy to study the influence of factors such as azimuthal variation of the Zr-hydrides and the presence of hydride rims and radially oriented hydrides. Two main characteristics were identified in samples with low ductility with respect to hydrogen content and test temperature: hydride rims and radial hydrides at the cladding outer surface. Crack propagation and failure modes were also studied, showing two general modes of crack propagation depending on distribution and amount of radially oriented hydrides. It was concluded that the PCMI resistance of irradiated cladding under normal conditions with homogenously distributed circumferential hydrides is high, with good margin to the RIA failure limits. To further improve safety, focus should be on conditions causing nonfavorable hydride distribution, such as hydride reorientation and formation of hydride blisters at the cladding outer surface.

Evaluation on Mechanical Properties of High Strength Light-Weight Concrete with Elevated Temperature and loading (하중조건과 고온에 의한 고강도 경량 콘크리트의 역학적 특성 평가)

  • Kim, Gyu-Yong;Kim, Young-Sun;Choe, Gyeong-Cheol;Park, Hyun-Gil;Lee, Tae-Gyu
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.6
    • /
    • pp.723-730
    • /
    • 2011
  • It is very important to experimentally evaluate concrete behavior at elevated temperature because aggregates make up approximately 80 percent of volume in concrete. In this study, an experiment to evaluate mechanical properties of normal weight and light weight concrete of 60 MPa was conducted. Based on loading level of 0, 20 and 40 percent, the tests of 28 days compressive strength, elastic modulus, thermal strain, total strain, and transient creep using ${\phi}100{\times}200mm$ cylindrical specimens at elevated temperature were performed. Then, the results were compared with CEB (Committes Euro-international du Beton) model code. The results showed that thermal strain of light weight concrete was smaller than normal weight concrete. Also, the results showed that compressive strength of light concrete at $700^{\circ}C$ was higher than normal weight concrete and CEB code, similar to that obtained at ambient temperature. Transient creep developed from loading at a critical temperature of $500^{\circ}C$ caused the concrete strains to change from expansion to compression. The transient creep test result showed that internal force was high when the ratio of shrinkage between concrete and aggregate was more influential than thermal expansion.

Development and testing of multicomponent fuel cladding with enhanced accidental performance

  • Krejci, Jakub;Kabatova, Jitka;Manoch, Frantisek;Koci, Jan;Cvrcek, Ladislav;Malek, Jaroslav;Krum, Stanislav;Sutta, Pavel;Bublikova, Petra;Halodova, Patricie;Namburi, Hygreeva Kiran;Sevecek, Martin
    • Nuclear Engineering and Technology
    • /
    • v.52 no.3
    • /
    • pp.597-609
    • /
    • 2020
  • Accident Tolerant Fuels have been widely studied since the Fukushima-Daiichi accident in 2011 as one of the options on how to further enhance the safety of nuclear power plants. Deposition of protective coatings on nuclear fuel claddings has been considered as a near-term concept that will reduce the high-temperature oxidation rate and enhance accidental tolerance of the cladding while providing additional benefits during normal operation and transients. This study focuses on experimental testing of Zr-based alloys coated with Cr-based coatings using Physical Vapour Deposition. The results of long-term corrosion tests, as well as tests simulating postulated accidents, are presented. Zr-1%Nb alloy used as nuclear fuel cladding serves as a substrate and Cr, CrN, CrxNy layers are deposited by unbalanced magnetron sputtering and reactive magnetron sputtering. The deposition procedures are optimized in order to improve coating properties. Coated as well as reference uncoated samples were experimentally tested. The presented results include standard long-term corrosion tests at 360℃ in WWER water chemistry, burst (creep) tests and mainly single and double-sided high-temperature steam oxidation tests between 1000 and 1400℃ related to postulated Loss-of-coolant accident and Design extension conditions. Coated and reference samples were characterized pre- and post-testing using mechanical testing (microhardness, ring compression test), Thermal Evolved Gas Analysis analysis (hydrogen, oxygen concentration), optical microscopy, scanning electron microscopy (EDS, WDS, EBSD) and X-ray diffraction.

Standardization of the Preparation Methods for Hwajeun (I) - focused on the volume and temperature of water added- (화전 조리법의 표준화를 위한 조리과학적 연구 (I) - 첨가하는 물의 양과 온도를 중심으로 -)

  • 이승현;장명숙
    • Korean journal of food and cookery science
    • /
    • v.17 no.3
    • /
    • pp.237-245
    • /
    • 2001
  • The purpose of this study was to develop a standardized recipe of Hwajeun(glutinous rice pancake with flower) by evaluating various methods appeared in the literature. For this purpose, the effects of the volume and temperature of water used to make dough on the sensory and rheological characteristics of Hwajeun were investigated. This experiment consisted of sensory evaluation in acceptance and intensity(appearance, color, moistness, softness, chewiness, adhesiveness, taste and overall preference), objective evaluation by using texture analyser, color difference meter and measurement of water content and oil absorption ratio. The loss ratio of moisture contents between dough and cooked Hwajeun were 2.4 ~2.8%, and the oil absorption ratio of Hwajeun made by 2$0^{\circ}C$water for kneading increased in proportion to the increment of water added(p<0.01). In terms of color, b value of Hwajeun made by 104$^{\circ}C$ salted water for kneading showed higher value compared to the others. In the two bite compression test, adhesiveness, springiness, gumminess and chewiness of Hwajeun made by 2$0^{\circ}C$ water(36%) for kneading showed significantly(p<0.05) high value among the samples. As a result of sensory evaluation, Hwajeun made with 27% of 104$^{\circ}C$ salted water for kneading was most preferred in softness, chewiness, taste and overall preference

  • PDF

High Temperature Compressive Deformation Behavior of Ti-6Al-2Sn-4Zr-6Mo Alloy (Ti-6Al-2Sn-4Zr-6Mo 합금의 고온압축 변형거동)

  • Hyun, Yong-Taek;Lee, Yong-Tai;Lee, Chan-Gyu
    • Korean Journal of Materials Research
    • /
    • v.11 no.2
    • /
    • pp.82-87
    • /
    • 2001
  • The hot deformation behavior of Ti-6Al-2Sn-4Zr-6Mo(Ti6246) alloy was investigated in both the $\alpha$+$\beta$ and $\beta$-phase fields by conducting compression tests over a strain rate range of $10^{-3}s^{-1}$ to $10^0s^{-1}$. The flow stress was increased with increasing strain rate and decreasing test temperature. The flow curves obtained at temperatures below 90$0^{\circ}C$ exhibited a flow softening. However, in the $\beta$-phase field, above 95$0^{\circ}C$, the flow stress increased monotonically with plastic strain approaching steady state values. Constitutive equations for the dependence of flow stress on strain, strain rate, and temperature were developed through the analysis of the flow curves.

  • PDF

Effects of Swirl and Combustion Parameters on the Performance and Emission in a Turbocharged D.1. Diesel Engine (선회유동 및 연소인자가 터보과급 디젤엔진의 성능 및 배기가스특성에 미치는 영향)

  • 윤준규;차경옥
    • Journal of Energy Engineering
    • /
    • v.11 no.2
    • /
    • pp.90-98
    • /
    • 2002
  • The effects of swirl and combustion parameters on the performance and emission in a turbo-charged D.I. diesel engine of the displacement 9.4L were studied experimentally in this paper. Generally the swirl in the combustion process of diesel engine promotes mixing of the injection fuel and the intake air. It is a major factor to improve the engine performance because the fuel consumption and NO$_{x}$ is trade-off according to the high temperature and high pressure of combustion gas in a turbocharged D.I. diesel engine, it's necessary to thinking over the intake and exhaust system, the design of combustion bowl and so on. In order to choose a turbocharger of appropriate capacity. As a result of steady flow test, when the swirl ratio is increased, the mean flow coefficient is decreased, whereas the gulf factor is increased. Also, through engine test its can be expected to meet performance and emissions by optimizing the main parameter's; the swirl ratio is 2.43, injection timing is BTDC 13$^{\circ}$ CA, compression ratio is 16, combustion bowl is re-entrant 5$^{\circ}$, nozzle hole diameter is $\Phi$0.28*6, turbocharger is GT40 model which are compressor A/R 0.58 and turbine A/R 1.19.

Die Life Estimation of Hot Forging for Surface Treatment and Lubricants (표면처리 및 윤활제에 따른 열간 단조 금형의 수명 평가)

  • 이현철;김병민;김광호
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.20 no.7
    • /
    • pp.26-35
    • /
    • 2003
  • This study explains the effects of lubricant and surface treatment on hot forging die life. The mechanical and thermal load, and thermal softening which is happened by the high temperature of die, in hot and warm forging, cause die wear, heat checking and plastic deformation, etc. This study is fur the effects of solid lubricants and surface treatment condition for hot forging die. Because cooling effect and low friction are essential to the long life of dies, optimal surface treatment and lubricant are very important to improve die life for hot forging process. The main factors, which affect die hardness and heat transfer, are surface treatments and lubricants, which are related to thermal diffusion coefficient and heat transfer coefficient, etc. For verifying these effects, experiments are performed for hot ring compression test and heat transfer coefficient in various conditions as like different initial billet temperatures and different loads. The effects of lubricant and surface treatment for hot forging die life are explained by their thermal characteristics. The new developed technique in this study for predicting tool life can give more feasible means to improve the tool life in hot forging process.