Kim, Sung-Hoon;Kim, Woo-Seok;Choi, Kyeong-Dal;Joo, Hyeong-Gil;Hong, Gye-Won;Han, Jin-Ho;Hahn, Song-Yop;Song, Hee-Suck;Park, Jung-Ho
Proceedings of the KIEE Conference
/
2003.07b
/
pp.1015-1017
/
2003
In a research and development team of high temperature superconducting (HTS) transformer for power distribution, prior to manufacture a single phase 1MVA 22.9 kV/6.6 kV HTS transformer, a 1MVA transformer for insulation test with windings made of copper tapes with the same size as BSCCO-2223 HTS tape was manufactured. The test transformer was composed of both the copper windings of double pancake type and the shell type core of laminated silicon steel plates. The characteristics tests of the test transformer were performed, such as no load test, load test and short test at 77k using liquid nitrogen. Insulation tests, lightning impulse test, power-frequency voltage test and external insulation test, were accomplished also.
According to the improvement of HTS conductor, HTS tapes which have the high current capacity have been recently researched in several nations. For large power application, AC loss is the most important issue in the development of AC superconducting power devices because it is closely related to the system operation efficiency. In 1st generation wire of HTS conductor, BSCCO, AC loss is too large to use for power application. Also, It is well known in recently years that YBCO CC, the 2nd generation wire, has also too much AC loss to apply to AC power devices. There are many trials to develop the new HTS wire having the low AC loss around the world. In this research, we present the measurment result of magnetization losses in SmBCO coated conductors. We measured the magnetization loss generated by perpendicularly exposed external magnetic field and compared with the analytic value of the strip model. Also, we presented the results compared with measured magnetization loss of an YBCO coated conductor.
An HTS power cable is generally composed of 2 layers for conducting and 1 layer for shielding. For the analysis of AC loss of an HTS power cable, 2-dimensional magnetic field analysis is carried out. The magnetization loss in HTS cable core was calculated, and the transport current loss was obtained from the monoblock equation and the elliptical Norris Equation. And the total AC loss of the cable was expected by the sum of magnetization loss and transport current loss. The variation of ac loss with respect to the gap and uncertain factor between the superconducting tapes was investigated, and the ac loss of 22.9kV/50MVA high-Tc superconducting power cable was calculated. These results well agree with those of experiment.
The result of design and Partial fabrication of a 1 MVA single phase high temperature superconducting(HTS) transformer for power distributions are presented in this paper. The HTS windings are wound as double pancake windings which have advantages of uniform distribution of high voltage over the windings. the rated primary and secondary voltages are 22.9 kV and 6.6 kV respectively. Four HTS tapes are wound in parallel for secondary windings considering the rated currents of the transformer. The HTS windings will be cooled down to 65 K by natural convection of sub-cooled liquid nitrogen using a single-staged GM-cryocooler in order to make the stability of the HTS windings better. The iron core is designed as shell type and isolated from the liquid nitrogen by an FRP cryostat which have a room temperature bore. After the complete fabrication of the total HTS transformer system, performance test of the transformer will be carried out.
In this paper, 3-D nonlinear electromagnetic analysis of a single phase 1MVA 22.9 kV/6.6 kV high temperature superconducting(HTS) transformer with double pancake windings was accomplished. The characteristics of 1MVA HTS transformer such as The efficiency, voltage regulation and % impedance voltage drop were obtained by the 3-D non-linear electromagnetic analysis. And in order to verify the 3-D non-linear electromagnetic analysis of a single phase 1MVA HTS transformer, a 1MVA test transformer with windings made of copper tapes with the same size as BSCCO-2223 HTS tape was manufactured. The energy conservation method to perform the analysis of leakage impedances of both a 1MVA HTS transformer and test transformer was used. The characteristic analysis such as efficiency, voltage regulation and % impedance voltage drop of transformer was performed. And the obtained values of both 1MVA HTS transformer and test transformer were compared.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2003.07a
/
pp.573-576
/
2003
HTS superconducting tapes are now commercially available for practical applications such as magnets and cables. Since superconductors in such applications are subjected to high mechanical loads that can significantly degrade the superconducting properties, mechanical properties and the strain tolerance known as the strain effect on superconducting properties are needed to be estimated for developing superconducting devices. Influences of loading mode on the Ic degradation and the interaction on strain effect were discussed in this study.
Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
/
2003.10a
/
pp.63-66
/
2003
1 km length of Bi-2223/Ag superconducting wires were fabricated by stacking, drawing process with advanced heat-treatment schedules. Intermediate annealing was carried out to increase the homogeneity and uniformity of the superconducting filaments embedded in the silver matrix. Phase modification from tetragonal to orthorhombic Bi-2212 by pre heat treatment(PHT) was executed to improve the texture and phase transformation of Bi-2223. Drawing stress was measured to Predict the sausaging and stress limit, Rolling parameters such as thickness, width and winding tension were investigated to roll the tape with uniformity. Critical current of 1 km length of superconducting tapes was measured about 50 A continuously after final sintering.
Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
/
2003.10a
/
pp.142-145
/
2003
In order to investigate the effect of cryogenic rolling on the critical current density (Jc), 54 and 55-multi-filament Bi-2223/hg tapes have been fabricated using a PIT process including two different types of cooling methods. The densification of oxide filament was found to occur due to the cryogenic rolling, and this enhanced the critical current density. However, when the wire was fully immersed in liquid nitrogen used as the coolant in cryogenic rolling, Jc degradation appeared caused by the nitrogen penetration into the filament. The cryogenically rolled tape with an improved type of cooling showed approximately 10% Jc's increase.
Shin, Hyung-Seop;Dizon, John Ryan C;Kim, Tae-Young;Ko, Rock-Kil;Oh, Sang-Soo
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2006.06a
/
pp.93-94
/
2006
The $I_c$ degradation behavior of YBCO CC tapes due to torsional deformation has been investigated. Particularly, the influence of torsion angle on the $I_c$ in HTS tapes was examined at 77K (self-field). At low torsional angles or shear strains, the $I_c$ degradation was small and gradual. Also, a good consistency of the $I_c$ degradation behaviors was found along the longitudinal direction under torsion when multiple voltage terminals were adopted for investigating the homogeneity of the $I_c$ degradation.
Stability of a Bi-2223/Ag tape was studied by using a numerical model considering the temperature distribution of cross-sectional area. The dynamic evolution of normal zone of a HTS tape can be shown by the developed two-dimensional Program using finite difference method. Two kinds of analyses are compared to quantify the critical disturbance energy for quenching HTS tapes. One is the length-thickness(x-r) side and the other is the length-width(x-z) side. For each case. the governing energy balance equations and corresponding boundary conditions are formulated. The results of analyses shows that the critical disturbance energies for each cases seem to be very close for considered Bi-2223/Ag tape .
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.