부유선별법에 의한 제련용 몰리브덴 정광의 회수 (Recovery of Roasting-Molybdenite Concentrate by Froth Flotation)

  • 박철현;전호석;김병곤;한오형
    • 한국재료학회지
    • /
    • 제19권12호
    • /
    • pp.661-666
    • /
    • 2009
  • Froth flotation has been carried out in order to produce roasting-molybdenite concentrate from molybdenite ore in the Shin-yeomi mine. In our study, roasting-molybdenite (Mo 0.43%) from Shin-yeomi mine was recovered by varying the conditions of regrinding time, dosage of collector and alkalinity. Liberation and flotation efficiency more were effective at regrinding time of six minutes than at single grinding. Mo recovery curves increased considerably as dosage of kerosene increased, whereas Mo grade curves decreased gradually. The separation efficiency of molybdenite was effective when the dosage of collector (kerosene) was adjusted to 300 g/t. The molybdenite concentrate was agglomerated in the range of pH 5-7 and its separation efficiency increased to pH 9-10. The concentrate of 49.5% Mo grade ($MoS_2$, 82.6%) with 81.5% recovery from Shin-yeomi molybdenite ores was obtained under conditions of 20% pulp concentration, 300 g/t kerosene 325 g/t frother (AF65), 2.5 kg/t depressant ($Na_2SiO_3$), pH 9-10 and four cleaning times. In the future, a trial run that can separate up to 50% Mo grade from Shin-yeomi molybdenite ores will be performed.

Magnetron Sputtering법에 의해 증착한 MoS$_2$ 박막의 고진공하에서의 트라이볼로지적 특성 (Tribological characteristics of sputtered MoS$_2$films with Magnetron Sputtering Method in High Vacuum)

  • 안찬욱;김석삼;이상로
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2000년도 제32회 추계학술대회 정기총회
    • /
    • pp.406-413
    • /
    • 2000
  • The friction and wear behaviors of Magnetron Sputtered MoS$_2$films were investigated by using a pin on disk type tester which was designed and manufactured for this experiment. The experiment was conducted by using silicon nitride (Si$_3$N$_4$) as a pin material and Magnetron Sputtered MoS$_2$on bearing steel (STB2) as a disk material, under operating conditions that include different surface roughness (Polishing specimen, Grinding specimen)(2types), linear sliding velocities in the range of 22, 44, 66mm/sec (3types), normal loads vary from 9.8N, 19.6N, 29.4N(3types), corresponding to contact pressures of 1.9∼2.7GPa and atmospheric conditions of high vacuum( 1.3${\times}$10$\^$-4/Pa), medium vacuum( 1.3${\times}$10$\^$-l/Pa), ambient air(10$\^$5/Pa)(3types). We investigated fracture mechanism in magnetron sputtered MoS$_2$films with Magnetron Sputtering method in each experiment.

  • PDF

Construction of Abalone Sensory Texture Evaluation System Based on BP Neural Network

  • Li, Xiaochen;Zhao, Yuyang;Li, Renjie;Zhang, Ning;Tao, Xueheng;Lee, Eung-Joo
    • 한국멀티미디어학회논문지
    • /
    • 제22권7호
    • /
    • pp.790-803
    • /
    • 2019
  • The effects of different heat treatments on the sensory characteristics of abalones are studied in this study. In this paper, the sensory evaluation of abalone samples under different heat treatment conditions is carried out, and the evaluation results are analyzed. The three-dimensional (3D) scanning and reverse engineering are used in tooth modeling of the sensory evaluation of abalone samples under different heat treatment conditions. Besides, the chewing movement models are simplified into three modes, including the cutting mode, compressing mode and grinding mode, which are simulated using finite element simulation. The elastic modulus of the abalone samples is obtained through the compression testing using a texture analyzer to distinguish their material properties under different heat treatments and to obtain simulated mechanical parameters. Finally, taking the mechanical parameters of the finite element simulation of abalone chewing as input and sensory evaluation parameters as the output, BP neural network is established in which the sensory texture evaluation model of abalone samples is obtained. Through verification, the neural network prediction model can meet the requirements of food texture evaluation, with an average error of 9.12%.

불소 첨가/미첨가 인공타액 용액에서 연마 및 마스킹 조건이 적층제조 Ti-6Al-4V 합금의 동전위분극시험 결과에 미치는 영향 (Effects of Grinding and Masking Conditions on the Potentiodynamic Polarization Curves of Additively Manufactured Ti-6Al-4V Alloy in Artificial Saliva Solution with or Without Fluoride Ions)

  • 안경빈;장희진
    • Corrosion Science and Technology
    • /
    • 제20권6호
    • /
    • pp.475-483
    • /
    • 2021
  • Additively manufactured titanium alloy is one of the promising materials in advanced medical industries. However, these additively manufactured alloys show corrosion properties different from those of conventional materials due to their unique microstructure. In this study, the effect of surface roughness and masking conditions on the results of the potentiodynamic polarization tests on additively manufactured or conventional Ti-6Al-4V alloys in artificial saliva solution with or without fluoride was investigated. The results showed that the corrosion potential was slightly lower with a flat cell with an O-ring than with masking tape. The corrosion rate was decreased with decreases in the surface roughness. Localized corrosion involving delamination of the surface layer occurred at 7 ~ 9 V (SSC) on the additively manufactured alloy in solution with or without fluoride when the samples were finished with 1000-grit SiC paper, whereas localized corrosion was not observed in the specimens finished with 1-㎛ alumina paste.

다결정 다이아몬드의 와이어방전가공에 관한 연구 (The Study on the WEDM of Polycrystalline Diamond)

  • 김창호;강재원;오장욱;서재봉
    • 한국기계가공학회지
    • /
    • 제7권3호
    • /
    • pp.67-74
    • /
    • 2008
  • Polycrystalline diamonds(PCD) tools are widely used in machining a large variety of advanced materials. However, the manufacture of PCD tool blanks is not an economical process. The shaping of PCD blanks with conventional machining methods(such a grinding) is long, labor-intensive process. This paper reports experimental investigation of the influence of electrical machining conditions on the metal removal rate of WEDM of PCD. Experimental results show that the longer pulse-on time and the shorter pulse-off time increase the metal removal rate and worsen the surface quality. The smaller grain size of diamond yields the metal removal rate and shows the better surface quality. Higher electrical conductivity of water yields worse surface roughness.

  • PDF

Job Stress at the Shipbuilding Industry

  • Lee, Kwan-Suk;Chung, Da-Yeh
    • 대한인간공학회지
    • /
    • 제31권1호
    • /
    • pp.177-183
    • /
    • 2012
  • Objectives: The objectives of this study are to discuss the importance of job stress and to introduce a model of job stress at the shipbuilding industry considering the characteristics of the shipbuilding works. Background: Shipbuilding works consist of grinding, painting, interior works, welding, and assembling and using heavy equipment in narrow space or work at outside or at high and dangerous places. The working environments aggravate the stress to the workers. Methods: Studies of job stress in industries including shipbuilding industries were reviewed and the characteristics of jobs of shipbuilding were analyzed to find causes of job stress. Results: A model was constructed based upon these findings and reviews. Conclusions: Job stress of shipbuilding workers are very high and thus job and working conditions need to be improved to attenuate the level of job stress of shipbuilding workers. Applications: This model can be used to identify the highly stressed workers and sources of stress.

유리질 결합 CBN공구 제조시 기공량 변화 (The Change of Porosity During the Fabrication of Vitreous Bonded CBN Tools)

  • 양진
    • 한국세라믹학회지
    • /
    • 제35권9호
    • /
    • pp.988-994
    • /
    • 1998
  • In the manufacturing of vitreous bonded CBN tool the porosity change associated with various processing conditions, I. e. the sintering temperature and the size and the amount of abrasive grits was observed. In the case of sintering of vitreous bond material only the specimen density reached the maximum at 950$^{\circ}C$ and then the total porosity was increased slightly with the temperature above 950$^{\circ}C$. In the sintering of a-brasive grits and the vitreous bond material together a marked increase in the total porosity was found with the temperature above 950$^{\circ}C$ Reducing the grit size at the constant volume fraction of abrasive grits showed an increase in the total porosity at whole sintering temperature. On the contrary. it was observed that increasing the volume fraction of abrasive grits with a same size showed the increased open porosity simultaneously with decreased closed porosity at whole sintering temperature.

  • PDF

고강성 병렬형 로봇의 최적 여유 구동 (Optimal Redundant Actuation of Parallel Manipulators with High Operational Stiffness)

  • 김성복
    • 제어로봇시스템학회논문지
    • /
    • 제6권2호
    • /
    • pp.181-189
    • /
    • 2000
  • This paper presents the optimal redundant actuation of parallel manipulators for complicated robotic applications such as cutting grinding drilling and digging that require a high degree of operational stiffness as well as the balance between force applicability and dexterity. First by taking into account the distribution(number and location) of active joints the statics and the operational stiffness of a redundant parallel manipulator are formulated and the effects of actuation redundancy are analyzed, Second for given task requirements including joint torque limit task force maximum allowable disturbance and maximum allowable deflection the task execution conditions of a redundant parallel manipulator are derived and the efficient testing formulas are provided. Third to achieve high operational stiffness while maintaining moderate dexterity the redundant actuation of a parallel manipulator is optimized which determines the optimal distribution of active joints and the optimal internal joint torque, Finally the simulation results for the optimal redundant actuation of a planar parallel manipulator are given.

  • PDF

볼브레이커시험에 의한 실리콘 다이의 표면조건에 따른 파단강도 평가 (Evaluation of Fracture Strength of Silicon Die with Surface Condition by Ball Breaker Test)

  • 변재원
    • 열처리공학회지
    • /
    • 제26권4호
    • /
    • pp.178-184
    • /
    • 2013
  • The effects of thickness and surface grinding condition on the fracture strength of Si wafer with a thickness under $100{\mu}m$ were investigated. Fracture strength was measured by ball breaker test for about 330 dies (size: $4mm{\times}4mm$) per each wafer. For statistical analysis of the fracture strength, scale factor was determined from Weibull plot. Ball breaker fracture strength was observed to increase with decreasing thickness of silicon die. For the silicon dies of different surface conditions, ball breaker fracture strength was high in the order of polished, ground (#4800), and ground (#320 grit) specimen. Probabilistic fracture strength (i.e., scale factor) increased with decreasing surface roughness of silicon die.

Optimization of Food Waste Fermentation for Probiotic Feed Production with Yeast Kluyveromyces marxianus

  • Lee, Ki-Young;Yu, Sung-Jin;Yu, Seung-Yeng
    • 한국자원리싸이클링학회:학술대회논문집
    • /
    • 한국자원리싸이클링학회 2001년도 정기총회 특별강연 및 춘계학술연구발표회(2)
    • /
    • pp.121-125
    • /
    • 2001
  • For the probiotic feed production, aerobic liquid fermentation of pulverized food wastes was attempted with a yeast Kluyveromyces marxianus. After grinding finely, optimal fermentation conditions of the substrate was investigated by shaking culture. The most active growth of the yeast was shown at solid content of 10%. The proper addition of urea(0.5g/l), o-phosphate(0.4g/l), molasses(4g/l), and yeast extract (1g/1) increased cell growth rate and viable cell count. For optimizing, the nutrients were all added to substrate and fermentation was carried in 2 litre jar fermenter. For the stimulation of hydrolyzing enzyme excretion, mixed culture with Aspersillus oryzae was also conducted. In 12 hours of fermentation, viable cell count of the yeast Kluyveromyces marxianus amounted to the number of 1.4 $\times$10$^{10}$ /1 in the culture medium.

  • PDF