Thermal, Curing, Elastic, and Mechanical Properties of Ethylene Propylene Diene Monomer/Polybutadiene/Carbon Black Composites

  • Tae-Hee Lee;Keon-Soo Jang
    • Elastomers and Composites
    • /
    • v.58 no.3
    • /
    • pp.142-151
    • /
    • 2023
  • In this study, we investigate the thermal and mechanical properties of composites comprising ethylene propylene diene monomer (EPDM) and polybutadiene (PB) obtained using carbon black (CB) as a reinforcing and compatibilizing filler. Owing to the significance of elastomeric materials in various industrial applications, blending of EPDM and PB has emerged as a strategic method to optimize the material properties for specific applications. This study offers insights into the blend composition, its microstructure, and the resulting macroscopic behaviors, focusing on the synergetic effects of composite materials. Furthermore, this study delves into curing and rheological behaviors, crosslink densities, and mechanical, thermal, and elastic properties of the elastomeric composites. Through systematic exploration, we believe that this study will be beneficial to material scientists and engineers working on developing advanced elastomeric composites.

Studies on Incombustibility Improvement of EPDM Rubber with $Al(OH)_3$ and $Sb_2O_3$ ($Al(OH)_3$$Sb_2O_3$의 첨가에 따른 EPDM계 고무의 난연성 향상 연구)

  • Kim, Jin-Yong;Lee, Won-Bok;Lim, Dae-Hyun;Suh, Hyuk;Rhee, Young-Woo
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 2009.11a
    • /
    • pp.449-452
    • /
    • 2009
  • In order to improve incombustibility of EPDM(Ethylene propylene diene monomer)-based rubber, inorganic materials as $Al(OH)_3$ and $Sb_2O_3$ were added. The mechanical and thermal properties have been measured for vulcanized rubber loaded with different concentrations of $Al(OH)_3$ and $Sb_2O_3$. As inorganic material contents increases from 5phr to 30phr, the specific gravity and hardness increase while elongation at break decreases. This study performed incombustibility test and thermal analysis through TGA(Thermogravimetric Analyzer). As a results, incombustible and thermal properties of EPDM-based rubber were improved as $Al(OH)_3$ and $Sb_2O_3$ contents increase.

  • PDF

Study on Manufacturing and Characteristics of Silicone/EPDM Rubber Blend (실리콘/EPDM고무 블렌드의 제조와 특성에 관한 연구)

  • 김진국;이형규
    • Polymer(Korea)
    • /
    • v.25 no.3
    • /
    • pp.406-413
    • /
    • 2001
  • Blending has become an interesting way for preparing new materials with tailored properties. Unfortunately, many materials are incompatible due to the difference in their viscoelastic properties, surface energy and interaction. Therefore, the properties of polymer blends are not obtained as expected levels. Silicone rubber has an excellent heat-resistance and electrical characteristics, and ethylene propylene diene monomer (EPDM) rubber also has good mechanical properties. The purpose of this study is to develop a new engineering material which has excellent electrical and mechanical properties through blending of silicone with EPDM rubber.

  • PDF

Mechanical Property, Thermal Conductivity, Rebound Resilience and Thermal Property of Chloro Isobutylene Isoprene Rubber/Ethylene Propylene Diene Monomer Blend

  • Hwang, Young-Bea;Lee, Won-Ki;Park, Chan Young
    • Elastomers and Composites
    • /
    • v.53 no.2
    • /
    • pp.80-85
    • /
    • 2018
  • Chloro isobutylene isoprene rubber (CIIR) and ethylene propylene diene monomer (EPDM) compounded with other formulation chemicals, depending on the polymer blend, were prepared by mechanical mixing. After manufacturing the rubber vulcanizate by compression molding with a hot press, the mechanical and thermal properties including thermal conductivity, rebound resilience of the CIIR/EPDM blends were measured. As the EPDM rubber content increased, hardness and tension set showed a tendency to increase. Pure CIIR exhibited the lowest tensile strength; however, tensile strength increased with loading of EPDM rubber. On the other hand, in CIIR rubber, which is usually a low-rebound elastomer owing to a high damping effect, rebound resilience exhibited an increasing trend as the content of EPDM rubber increased. As the EPDM rubber content increased, thermal stability was improved due to reduction of decomposition rate in the rubber region of the blend vulcanizate.

Studies on Incombustibility Improvement of EPDM-based Insulation with Al(OH)3 and Sb2O3 (EPDM계 내열재의 Al(OH)3와 Sb2O3 함량에 따른 난연 효과 연구)

  • Kim, Jinyong;Lim, Daehyun;Lee, Wonbok
    • Journal of Aerospace System Engineering
    • /
    • v.7 no.4
    • /
    • pp.36-41
    • /
    • 2013
  • In order to improve incombustibility of EPDM(Ethylene propylene diene monomer)-based rubber, inorganic materials as $Al(OH)_3$ and $Sb_2O_3$ were added. The mechanical and thermal properties have been measured for vulcanized rubber loaded with different concentrations of $Al(OH)_3$ and $Sb_2O_3$. As inorganic material contents increases from 5phr to 30phr, the specific gravity and hardness increase while elongation at break decreases. This study performed incombustibility test and thermal analysis through TGA(Thermogravimetric Analyzer). As a results, incombustible and thermal properties of EPDM-based rubber were improved as $Al(OH)_3$ and $Sb_2O_3$ contents increase.

Combustion Properties of Ethylene-propylene diene monomer/polypropylene/Clay Nanocomposites Based on EDPM/PP (EPDM/PP에 바탕을 둔 에칠렌-프로필렌 디엔 모노머/폴리프로필렌/클레이 나노복합체의 연소특성)

  • Chung, Yeong-Jin
    • Journal of the Korean Applied Science and Technology
    • /
    • v.28 no.4
    • /
    • pp.410-417
    • /
    • 2011
  • Effects of ethylene-propylene diene monomer (EPDM)/polypropylene (PP), zinc oxide, stearic acid, and clay on the combustive properties based on EDPM/PP were investigated. The EDPM/PP/clay nanocomposites was compounded to prepare specimen for combustive analysis by cone calorimeter (ISO 5660-1). It was found that the specific mass loss rate (SMLR) in the nanocomposites decreased due to the fire resistance compared with unfilled EDPM/PP, while the nanocomposites showed the higher total heat release (THR), higher CO production release, and higher specific extinction area (SEA) than those of virgin EPDM/PP. The stearic acid for softening ruber increased the THR and amount of smoke by itself, combustible.

Optimal Design for CLIP EPDM Rubber Products using a Flow Analysis

  • Huh, Young-Min;Lee, Kwang-O;Kang, Sung-Soo
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.7 no.4
    • /
    • pp.23-27
    • /
    • 2006
  • Rubber is used in many industrial products, such as hoses, rubber belts, and oil seals. In particular, more than 200 rubber parts are used in automobiles. The design technology of these parts is largely dependent on field experience, which leads to lengthy and expensive developing procedures. However, with the help of recent developments in nonlinear computer analysis, new rubber products can be developed at low cost. In this study, rubber injection molding design variables, such as location and number of gates, were optimized using computer-aided engineering with the cross-WLF equation to produce CLIP rubber products made from ethylene propylene diene monomer(EPDM). The validity of the proposed design was evaluated by comparison with actual forming results.

Cure Characteristics, Physical Properties and Ozone Resistance of Butyl Rubber and EPDM Rubber Blends (Butyl고무와 EPDM고무 블렌드의 경화특성, 물리적 성질 및 내오존성)

  • Park, Chan-Young;Hwang, Young-Bea
    • Elastomers and Composites
    • /
    • v.46 no.4
    • /
    • pp.329-334
    • /
    • 2011
  • In general, butyl rubber(IIR : isobutylene isoprene rubber) has excellent gas permeability resistance and impact absorbance property as low resilience elastomer. In this experiment butyl rubber blends with EPDM(ethylene propylene diene monomer) were prepared by mechanical mixing method. Curing behavior, physical properties and ozone resistance etc. were subsequently examined. Measurement results of gas transmission rate test shows that butyl rubber contents above 50 wt% showed significant decrease in gas permeability resistant property. However, in butyl rubber/EPDM blend, EPDM contents above 25 wt% indicates no surface change due to improvement of ozone resistance under the condition of 50 pphm, $50^{\circ}C$, 120 hrs.

Thermoplastic Polyurethane (TPU)/Ethylene-Propylene-Diene Monomer Rubber (EPDM) and TPU/Polybutadiene Rubber (BR) Blends for the Application of Footwear Outsole Materials (신발겉창 재료용 열가소성 폴리우레탄 (TPU)/에틸렌-프로필렌-디엔 고무와 TPU/부타디엔 고무 블렌드)

  • Kim, Ji-Hoo;Kim, Gue-Hyun
    • Elastomers and Composites
    • /
    • v.48 no.3
    • /
    • pp.195-200
    • /
    • 2013
  • The main objective of this study is to improve abrasion resistance and wet slip resistance of thermoplastic polyurethane (TPU) by blending with ethylene-propylene-diene monomer rubber (EPDM) or polybutadiene rubber (BR) for the application of the footwear outsole materials. With addition of 10 wt% of EPDM or BR, TPU/EPDM and TPU/BR blends exhibited higher NBS abrasion resistance, tensile properties and wet slip resistance than TPU. However, with further increasing content of EPDM and BR, abrasion resistance and tensile properties of the blends decreased. Improvement in abrasion resistance and tensile properties with 10 wt% of addition of EPDM or BR may be due to better microphase separation of TPU.

Melt Grafting of Citraconic Acid onto an Ethylene-Propylene-Diene Terpolymer (EPDM) -Effect of Reaction Conditions and Initiator Type on the Melt Grafting of Citraconic Acid onto EPDM- (EPDM고무와 씨트라코닉산의 melt grafting - 반응조건과 개시제에 따른 영향 연구 -)

  • Kim, Jung-Soo;Bae, Jong-Woo;Lee, Jin-Hyok;Oh, Sang-Taek;Kim, Gu-Ni;Lee, Young-Hee;Kim, Han-Do
    • Elastomers and Composites
    • /
    • v.48 no.1
    • /
    • pp.39-45
    • /
    • 2013
  • Melt grafting of citraconic acid (CCA) onto an ethylene-propylene-diene terpolymer (EPDM) with various peroxide initiators was performed using a Haake Rheocorder. Finding the optimum running condition and concentration is critical for effective grafting and performance of grafted material. Therefore, this study focused on the effects of mixing (reaction) condition and monomer/initiator dosages on the grafting degree, grafting efficiency and crosslinking degree (gel content), melt flow index and mechanical properties of CCA-g-EPDM. As the grafting degree/crosslinking degrees increased, the tensile strength increased significantly, but elongation at break and melt flow index decreased. The initiator 2,5-dimethyl-2,5-di(tert-butyl peroxy)-hexane (T-101) appeared to meet for the best grafting(2.31%). The grafting degree increased markedly with increasing monomer CCA/initiator T-101 contents. The grafting degree also increased with increasing mixing temperature/time, and then leveled off or decreased/increased a little. The optimum monomer/initiator dosages and reaction temperature/time were found to be about 5/0.05 wt% and $180^{\circ}C$/15min, respectively.