• Title/Summary/Keyword: Dry Shrinkage

Search Result 220, Processing Time 0.02 seconds

Nylon FDY와 ROY로 제조한 ATY의 물성에 관한 연구 (A Study on the Physical Properties of ATY Produced with Nylon FDY and ROY)

  • 김승진;김재우;홍상기
    • 한국염색가공학회지
    • /
    • 제16권6호
    • /
    • pp.35-43
    • /
    • 2004
  • This study surveys the physical properties of ATY produced with FDY and POY. ATY is made with 70d Nylon FDY and 80d Nylon POY using AIKI air jet texturing machines, respectively. The processing parameters such as air pressure and yam speed are varied, and air pressure is varied ranging with 8.5bar, l0.5bar and 1l.5bar, and yarn speed is varied ranging with 400m/mim, 450m/mim, and 500m/min. The various physical properties of ATY made by POY and FDY denier, wet shrinkage, dry shrinkage, tensile properties, thermal stress and instability are measured and discussed with air pressure and yam speed. The shrinkage simulation of ATY is performed for analysing the process shrinkage on the dyeing and finishing processes.

콘크리트의 Consistency 변화가 소성수축에 미치는 영향 (Influence on the Plastic Shrinkage of Concrete for a Varieties of Consistency)

  • 오무영
    • 한국농공학회지
    • /
    • 제20권1호
    • /
    • pp.4626-4630
    • /
    • 1978
  • The objective of this study is to investigate how the varieties of consistency of fresh concrete influence on the plastic shrinkage in dry condition. The test was conducted under the controlled chamber in which the temperature was kept at 25 ${\pm}$2$^{\circ}C$, the humidity 35 ${\pm}$3%, and the wind velocity 4.0 ${\pm}$0.5m/sec. The results obtained from the test are as follow. 1) The rate of evaporation was highest at 2-3 hour after casting, and decreased gradually. 2) The plastic shrinkage was increased as to the slump values. The shrinkage rate was very highest at 2-4 hour and hardly showed any changes after 6 hour. 3) The recommendation for good cloncrete is that slump value should be as low as possible in construction.

  • PDF

온돌바닥 모르터의 건조수축보상을 위한 팽창제의 품질특성 연구 (A Study on the Quality Properties of the Expansive For Dry-Shrinkage Compensation of the Floor Mortar)

  • 이웅종;이종열;정연식;이순기;정성철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.155-160
    • /
    • 2000
  • In this paper, we investigated quality properties for the expansive of the CaO-$CaSO_4$ family which used to compensate dry-shrinkage in the floor mortar of On-Dol heating System. This experimental study established the mix condition with quantity of the expansive and is to investigate the relativity between the compress strength and the length change and the relativity between the chemical properties and the length change with the analysis of the physical and chemical properties. As a result of the study, the expansive is controlled by more the CaO than the $CaSO_4$. The relativity between the compress strength and the length change is expressed by exponential function, showing that if the expansive performance is increased, the compress strength is decreased. And the relativity between the chemical properties and the length change is only relative the quantity of the F-CaO among the chemical properties, is expressed by the second order function, showing that if the F-CaO is increased, the expansive performance is increased.

  • PDF

연신공정 조건이 소모연신사의 물성에 미치는 영향 (II) (The Effects of Drawing Conditions on Physical Properties of the Drawn Worsted Yarns (II))

  • 한원희;김승진;조진황
    • 한국염색가공학회지
    • /
    • 제22권1호
    • /
    • pp.61-70
    • /
    • 2010
  • This effects of drawing conditions on the physical properties of the drawn worsted yarns were investigated. The drawn worsted yarns were made on the yarn drawing system with various drawing conditions such as concentration of reducing agent, draw ratio, setting time of drawn yarn and concentration of oxidizing agent. The dry and wet shrinkage, irregularity(CV%), thin and thick part, hairiness and abrasion resistance of these various specimens were measured and discussed in terms of various drawing conditions.

고슬럼프 보통강도 콘크리트의 실용화를 위한 시공특성에 관한 실험적 연구 (An Experimental Study on Workability for Practical Use of High Workable and Normal Strength Concrete)

  • 정양희;김용로;이도범;장선근
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 추계 학술논문 발표대회 논문집
    • /
    • pp.107-110
    • /
    • 2006
  • The purpose of this study is to suggest a reference data for the development of high workable and normal strength concrete using Polycarboxylate superplasticizer and granulated blast furnace slag as concrete admixtures. So in this study, it is quantitatively evaluated the workability, compressive strength, the heat of hydration and dry shrinkage of high workable concrete on normal compressive strength($21{\sim}27MPa$) for the practical use in construction field. As a result of this study, it is appeared that the performance of high workable and normal strength concrete is superior than that of ready-mixed concrete of the same strength through the B/P tests in the plants.

  • PDF

Polyethylene Glycol 주입방법과 건조방법이 목재 부피수축률에 미치는 효과 (Effects of the Methods of Polyethylene Glycol Impregnation and Drying on the Volumetric Shrinkage of Wood)

  • 이원희;강춘원;홍승현;강호양
    • 한국가구학회지
    • /
    • 제27권1호
    • /
    • pp.43-48
    • /
    • 2016
  • PEG (Polyethylene glycol) impregnation in wood reduces the occurrence of checking during kiln drying. The volumetric shrinkages of wood PEG impregnated by pressure (PEG-P) or soaking (PEG-S) methods, and oven-dried by vent (VD) or air-tight (AD) methods were measured and compared with the controls. The average oven-dry weight of PEG impregnated specimens was larger than that of the controls by 3.6 g, but was not influenced by the drying methods. The average of the total volumetric shrinkage of PEG-P-VD specimens was the least (2.3%), while that of CON-S-AD specimens was the largest (28.9%). Within a drying method the total volumetric shrinkage of the control was the largest followed by PEG-S and PEG-P specimens, which implied that residual PEG in wood restrained its shrinkage during drying.

콘크리트 배합조건에 따른 수축저감제의 건조수축 특성 (Drying Shrinkage Characteristics of the Concrete Incorporated Shrinkage Reducing Agent According to Mixed Proportion of Concrete)

  • 김영선;김광기;박순전;김정선
    • 한국건축시공학회지
    • /
    • 제17권3호
    • /
    • pp.245-252
    • /
    • 2017
  • 최근 소비패턴의 변화에 따라 대형마트, 아울렛 및 물류창고 등과 같은 구조물들이 증가하고 있다. 이와 같은 구조물들은 초평탄 바닥부재를 포함하고 있기 때문에 소성 및 건조수축에 의한 슬래브 부재의 균열 억제 관리를 철저하게 실시한다. 슬래브 부재의 균열을 억제하기 위한 방안으로 화학적 균열저감 방법을 사용하고 있으며, 특히 수축저감제에 대한 사용검토가 증가하고 있다. 그러나 이에 대한 국내 연구결과는 부족한 상황이다. 본 연구에서는 수축저감제를 사용한 콘크리트의 수축특성과 배합요인 변동에 따른 건조수축 특성을 검토하였다. 국내 수축저감제는 해외 고급형 수축저감제와 성능이 유사한 것으로 나타났으며, 수축저감제 사용량이 증가할수록 건조수축 억제 효과는 높아지는 것으로 나타났다. 수축저감제 1.5%를 사용한 시험체는 재령 100일에서 수축저감제를 사용하지 않은 시험체에 비해 건조수축량이 약 절반으로 나타났다. 또한, 혼화재료 사용에 대해 특별한 성능변화는 없는 것으로 확인되었다.

콘크리트 장기변형의 구속계수와 선압축력의 손실률 (Restraint Coefficient of Long-Term Deformation and loss Rate of Pre-Compression for Concrete)

  • 연정흠;주낙친
    • 콘크리트학회논문집
    • /
    • 제14권4호
    • /
    • pp.521-529
    • /
    • 2002
  • 콘크리트의 크리프와 건조수축에 의한 장기변형의 일부가 구속되는 합성단면에 대해 콘크리트에 발생되는 잔류응력과 이로 인한 콘크리트 단면에 선압축력의 손실을 계산하기 위해 콘크리트 장기변형의 구속계수가 유도되었으며, 선압축력의 손실률을 계산하기 위한 식을 제안하였다. 제안된 구속계수는 재령수정 유효탄성계수가 적용된 환산단면특성으로부터 계산되며, 복잡한 형태의 합성단면에 대해서도 쉽게 적용될 수 있다. 기존 설계기준에서 콘크리트의 장기변형과 관련된 조항을 검토하기 위해서 도로설계편람의 일반 합성단면에 대해 이 구속계수와 선압축력의 손실 계산식이 적용되었다. 부정정력과 신축이음량의 계산에 적용되는 건조수축변형률 $150 ~ 200$\times$10^{-6}$ 은 장기변형의 구속정도가 적은 경우에 과소 계산될 수 있으며, 잔류응력의 계산에 는 적용되는 $180$\times$10^{-6}$ 은 비정상적으로 작은 값이다. 이 논문에서 적용된 PSC 합성단면에 대한 도로교 설계기준의 손실률 16.3%는 ACI 209에 대해서는 안전측으로 계산되었으나 Eurocode 2에 대해서는 안전을 보장할 수 없었다. 강합성 단면의 콘크리트 바닥판에 일반 보강철근의 긴장에 의해 선압축력이 도입되면 철근비의 증가로 긴장에 의한 경우보다 상당히 큰 손실이 발생되었으며, 강재거더의 구속에 의해 긴장된 보강재 선인장력의 손실은 감소한 반면에, 콘크리트 선압축력의 손실은 증가하였다.

콘크리트 단면복구용 보수재료의 굵은 골재 최대치수 및 조립률에 따른 재료적 특성 (Material Properties Depending on the Maximum Aggregate Size and Fineness Modulus for Concrete Repair Materials)

  • 이선목;이병재;김윤용
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제27권6호
    • /
    • pp.62-69
    • /
    • 2023
  • 본 연구에서는 보수재료에 굵은 골재를 사용하게 되면서 얻을 수 있는 효과를 검토하기 위해 굵은 골재의 최대치수 및 조립률을 다양화 하면서 콘크리트의 특성을 파악하는 기초 연구를 수행하였다. 그 결과 콘크리트의 슬럼프는 굵은 골재 최대치수가 커질수록 증가하였고, 공기량은 최대 골재 치수가 10 mm 이상인 배합군에 비해 최대 골재 치수가 5 mm 의 골재를 사용한 배합에서 공기량이 1.88~2.35 배 높게 측정되었다. 압축강도는 굵은 골재의 실적률에 많은 영향을 받는 것으로 나타났다. 실적률이 가장 높은 최대치수 20 mm 의 굵은 골재를 사용한 배합에서 압축강도가 가장 높게 측정되었으며 실적률이 가장 낮은 배합의 압축강도보다 45% 이상 높게 나타났다. 건조수축 측정결과 굵은 골재 최대치수 및 조립률의 변화에 따라 굵은 골재의 실적률이 높아지면서 건조 수축이 가장 낮게 측정되었고, 실적률이 가장 낮은 배합에서 가장 크게 나타났다. 본 연구를 통해 콘크리트 구조물 보수용 재료에 사용되는 굵은 골재의 최대치수 및 조립률을 다양화해서 입도를 조정하게 되면 강도 및 작업성이 우수해지고 건조수축을 줄일 수 있는 것을 확인 할 수 있었다.

고로슬래그 미분말을 대량 사용한 고강도 콘크리트의 조기강도 및 길이변화 특성에 관한 실험적 연구 (An Experimental Study on Early Strength and Drying Shrinkage of High Strength Concrete Using High Volumes of Ground Granulated Blast-furnace Slag(GGBS))

  • 양완희;류동우;김우재;박동철;서치호
    • 한국건축시공학회지
    • /
    • 제13권4호
    • /
    • pp.391-399
    • /
    • 2013
  • 본 연구에서는 40 MPa 및 60 MPa급의 고강도 콘크리트를 제조함에 있어서, 보통 포틀랜드 시멘트에 대해 60~80%를 고로슬래그 미분말로 대체하고, 알카리 설페이트계(Modified Alkali Sulfate type) 자극제(Activator)를 활용하여 조기강도 개선효과 및 콘크리트의 길이변화 특성을 고찰하였다. 이에 따라 알카리 자극제를 결합재 대비 1%를 사용한 결과, 미소수화열은 72시간의 누적 발열량이 약 45%가 향상되어 초기의 강도 성능 향상에 기여하는 것으로 판단되며, 콘크리트의 유동성은 다소 감소하였으나, 3일과 7일 강도는 8~12% 향상되어 고로슬래그 미분말을 60% 수준으로 대체하여 고강도 콘크리트를 제조할 때 초기재령의 강도 확보에 알카리 설페이트계 자극제의 활용이 효과적인 것으로 나타났다. 또한 길이변화 시험 결과는, 40 MPa와 60 MPa 시험체 모두 BS40 > BS60 > BS60A > BS80A의 순으로 길이변화가 큰 것으로 나타났고, 알카리 자극제의 사용에 따라 길이변화가 다소 개선되는 것으로 나타났다.