An Experimental Study on Early Strength and Drying Shrinkage of High Strength Concrete Using High Volumes of Ground Granulated Blast-furnace Slag(GGBS)

고로슬래그 미분말을 대량 사용한 고강도 콘크리트의 조기강도 및 길이변화 특성에 관한 실험적 연구

  • Yang, Wan-Hee (Department of Architectural Engineering, Konkuk University) ;
  • Ryu, Dong-Woo (Department of Architectural Engineering, Daejin University) ;
  • Kim, Woo-Jae (Research & Engineering Division R&D CENTER, POSCO E&C) ;
  • Park, Dong-Cheol (R&D CENTER, Intchem Co., Ltd.) ;
  • Seo, Chee-Ho (Department of Architectural Engineering, Konkuk University)
  • Received : 2013.02.25
  • Accepted : 2013.04.16
  • Published : 2013.08.20

Abstract

For high strength concrete of 40~60 MPa, the effects on the early strength and concrete dry shrinkage properties replacing 60~80% of Ordinary Portland Cement with Blast Furnace Slag Powder and using the Alkali Activator (Modified Alkali Sulfate type) are considered in this study. 1% Alkali Activator to the binder, cumulative heat of hydration for 72 hours was increased approximately 45%, indicating that heat of hydration contributes to the early strength of concrete, and the slump flow of concrete decreased slightly by 3.7~6.6%, and the 3- and 7- strength was increased by 8~12%, which that the Alkali Activator (Modified Alkali Sulfate type) is effective for ensuring the early strength when manufacturing High Strength Concrete (60%) of Blast Furnace Slag Powder. Furthermore, the dry shrinkage test, both 40 MPa and 60 MPa specimens had level of length changes in order of BS40 > BS60 > BS60A > BS80A, and the use of the Alkali Activator somewhat improved resistance to dry shrinkage.

본 연구에서는 40 MPa 및 60 MPa급의 고강도 콘크리트를 제조함에 있어서, 보통 포틀랜드 시멘트에 대해 60~80%를 고로슬래그 미분말로 대체하고, 알카리 설페이트계(Modified Alkali Sulfate type) 자극제(Activator)를 활용하여 조기강도 개선효과 및 콘크리트의 길이변화 특성을 고찰하였다. 이에 따라 알카리 자극제를 결합재 대비 1%를 사용한 결과, 미소수화열은 72시간의 누적 발열량이 약 45%가 향상되어 초기의 강도 성능 향상에 기여하는 것으로 판단되며, 콘크리트의 유동성은 다소 감소하였으나, 3일과 7일 강도는 8~12% 향상되어 고로슬래그 미분말을 60% 수준으로 대체하여 고강도 콘크리트를 제조할 때 초기재령의 강도 확보에 알카리 설페이트계 자극제의 활용이 효과적인 것으로 나타났다. 또한 길이변화 시험 결과는, 40 MPa와 60 MPa 시험체 모두 BS40 > BS60 > BS60A > BS80A의 순으로 길이변화가 큰 것으로 나타났고, 알카리 자극제의 사용에 따라 길이변화가 다소 개선되는 것으로 나타났다.

Keywords

References

  1. Roy DM. Alkali-activated cements: Opportunities and challenges. Cement and Concrete Research. 1999 Feb;29(2):249-54. https://doi.org/10.1016/S0008-8846(98)00093-3
  2. ACI Committee 206. Ground granulated blast-furnace slag as cementations constituent in concrete. ACI Materials Journal. 2009;No.84-M34:327-42.
  3. Hester D, McNally C, Richardson MG. Study of influence of slag alkali level on the alkali-silica reactivity of slag concrete. Construction and Building Materials. 2005 Nov;19(9):661-5. https://doi.org/10.1016/j.conbuildmat.2005.02.016
  4. Leng F, Feng N, Lu X. An experiment study on the properties of resistance to diffusion of chloride ions of fly ash and blast furnace slag concrete. Cement and Concrete Research. 2000 Jun;30:989-92. https://doi.org/10.1016/S0008-8846(00)00250-7
  5. Ryu DW, Kim WJ, Yang WH, Park DC. An Experimental Study on the Carbonation and Drying Shrinkage of Concrete Using High Volumes of Ground Granulated Blast-furnace Slag. Korea Institute of building Construction. 2012 Aug;12(4):393-400. https://doi.org/10.5345/JKIBC.2012.12.4.393
  6. Park CB. Properties of high volume mineral admixture concrete with kind of inorganic activators [dissertation]. [Seoul (Korea)]: Konkuk University; 2012. 132 p.
  7. Shi C, Day RL. A calorimetric study of early hydration of alkali-slag cements. Cement and Concrete Research. 1995 Aug;25(6):1333-46. https://doi.org/10.1016/0008-8846(95)00126-W
  8. Bensted J, Barnes P. editors. Structure and Performance of Cements. 2nd ed. London and New York: Taylor & Francis; 2002. Chapter 3, Hydration of Portland Cement; p. 57-139.
  9. Collins FG, Sanjayan JG. Strength and shrinkage properties of alkali-activated slag concrete containing porous coarse aggregate. Cement and Concrete Research. 1999 Apr;29(4):607-10. https://doi.org/10.1016/S0008-8846(98)00203-8
  10. Douglas E, Bilodeau A, Malhotra VM. Properties and durability of alkali-activated slag concrete. ACI Materials Journal. 1992 Sep;89(5):509-16.
  11. Mehta PK, Monteiro PJM. CONCRETE Microstructure, Properties, and Materials. 3nd ed. New York: The McGraw-Hill Companies; 2006. Chapter 4, Dimensional Stability; p. 85-120.
  12. Bakharev T, Sanjayan JG, Cheng YB. Effect of admixtures on properties of alkali-activated slag concrete. Cement and Concrete Research. 2000 Sep;30(9):1367-74. https://doi.org/10.1016/S0008-8846(00)00349-5

Cited by

  1. Effect of Blast Furnace Slag on Rheological Properties of Fresh Mortar vol.14, pp.4, 2014, https://doi.org/10.5345/JKIBC.2014.14.4.285
  2. An Experimental Study on the Chloride Attack Resistibility of Alkali-Activated Ternary Blended Cement Concrete vol.16, pp.4, 2016, https://doi.org/10.5345/JKIBC.2016.16.4.321
  3. A study of the effect of light-burnt dolomite on the hydration of alkali-activated Portland blast-furnace slag cement vol.57, 2014, https://doi.org/10.1016/j.conbuildmat.2014.01.071
  4. Study on the characteristic of liner and cover material by accelerating agent type vol.27, pp.2, 2018, https://doi.org/10.5322/JESI.2018.27.2.75