• 제목/요약/키워드: Dissimilar aluminum alloy

검색결과 50건 처리시간 0.025초

구리-알루미늄 이종재료의 브레이징 특성 향상에 관한 연구 (Study on the Improvement of Brazeability for Copper-Aluminum Dissimilar Materials Joint)

  • 정호신;배동수;고성우
    • 한국해양공학회지
    • /
    • 제15권3호
    • /
    • pp.49-57
    • /
    • 2001
  • One of the most important considerations to braze Cu-Al dissimilar materials is control of brittle metallic compound which makes it difficult to obtain a sound brazed joint. Nowdays, several attempts were made to control the metallic compound. But effective method for controlling metallic compound was not established. In this point of view, commercially pure aluminum and copper were used as base metal and Al-Si-X and Zn-Al-X alloy systems were developed as filler metal. Brazing was carried out to find optimum conditions for Cu-Al dissimilar joint. The results obtained in this study were summarized as follows: 1) The joint brazed by Al-Si-X filler metal showed good brazeability and mechanical properties. The tensile strength of the joint brazed over solidus temperature was more than 90% of Al base metal. Especially, the joint brazed at liquidus temperature was fractured in the Al base metal. 2) Fluorides fluxes(a mixture of potassium fluoro-aluminates) were used to improve surface cleanliness of base metal and wettability of Al-Si-X filler metal. It was melted at the temperature about 1$0^{\circ}C$ lower than that of the filler metal, and made appropriate brazing environment. Therefore, it could be a proper selection as flux.

  • PDF

Al/Fe 이종금속 접합부의 부식특성 (Corrosion Assessment of Al/Fe Dissimilar Metal Joint)

  • 강민정;김철희;김준기;김동철;김종훈
    • Journal of Welding and Joining
    • /
    • 제32권4호
    • /
    • pp.55-62
    • /
    • 2014
  • The use of light-weight Al alloys in the automotive industry is increasing to meet requirements for fuel efficiency and emission reduction. Joining Al alloy to the conventional steel sheet is also very important issue with the increased use of Al alloy, and several joining processes have been introduced to enhance joining strength between dissimilar metals. This paper deals with a galvanic corrosion in the dissimilar metal joining. Salt spray tests up to 2000 hours were conducted on a self-piercing rivet, spot welded, adhesive bonded and weld-bonded joints, and cross-sections and tensile shear strength according the salt spray duration were analyzed at every 500-hour. Self-piercing rivet joint had relative low initial strength but the joint strength did not change regardless of the salt spray duration. The strength of other joints (spot welded, adhesive bonded and weld-bonded joints) decreased with the increase of salt spray duration and the corrosion behaviour of each joint was discussed.

초고장력강과 알루미늄 합금의 판재 접합을 위한 헬리컬 SPR 설계 (Design of Helical SPR for Joining Advanced High Strength Steel and Aluminum Alloy Sheets)

  • 김동범;김관우;조해용
    • Journal of Welding and Joining
    • /
    • 제33권6호
    • /
    • pp.55-59
    • /
    • 2015
  • Self-piercing riveting (SPR) is a sheet-joining method that can be used for materials that are difficult or unsuitable for weld, such as aluminum alloys and other steel sheet metals. The increased application of lightweight materials has initiated many investigations into new SPR conditions for riveting dissimilar materials. However, buckling of the semi-tubular rivet occurs during the riveting of AHSS. In this study, a helical SPR was designed for the riveting of AHSS and Al-alloy. In addition, the reinforced helical SPR which has straight parts was designed. The riveting of AHSS and Al-alloy was simulated. Simulated results were verified by comparison with experimental ones.

신소재 금형펀치의 이종재 마찰용접 개발과 AE품질평가를 위한 연구 (Friction Welding of Dissimilar Press Punch Materials and Its Evaluation by AE)

  • 오세규;박일동;이원석
    • Journal of Welding and Joining
    • /
    • 제15권2호
    • /
    • pp.43-53
    • /
    • 1997
  • The complete joining method for dissimilar press punch materials and its real-time evaluation method is not available at present. Brazing method has been used for joining them, but it is known that the welded joint by the brazing has the lower bonding efficiency and reliability than the diffusion welding. The friction welding with a diffusion mechanism in bonding was applied in this study. This work was carried out to determine the proper friction welding conditions and to analyze mechanical properties of friction welded joints of sintered carbide tool materials (SKNM50 for the blade part of press punch) to alloy steel (SCM440 for the shank part of press punch) using aluminum (A6061 for the interlayer material) as an insert material between the sintered carbide tool materials and the alloy steel. In addition, acoustic emission test was carried out during friction welding to evaluate the weld quality.

  • PDF

유리섬유 강화 플라스틱과 알루미늄 합금 접합을 위한 유한요소해석 (Finite element analysis for joining glass fiber reinforced plastic and aluminium alloy sheets)

  • 조해용;김동범
    • Journal of Welding and Joining
    • /
    • 제33권2호
    • /
    • pp.78-84
    • /
    • 2015
  • Self-piercing rivet(SPR) is mechanical joining methods and which can be joining dissimilar materials. Unlike conventional riveting, SPR also needs no pre-drilled holes. During plastically deformation, SPR pierces upper sheet and joins it to under sheet. SPR has been mainly applied to the joining the automobile body and some materials, such as glass fiber reinforced polymer and aluminum alloy, which represent the sheet-formed materials for lightweight automobile. Glass fiber reinforced plastic(GFRP) has been considered as a partial application of the automobile body which is lighter than steels and stronger than aluminium alloys. It is needed SPR to join Al alloy sheets and GFRP ones. In this paper, in order to design the rivet and anvil, which are suitable for GFRP, the joinability was examined through simulations of SPR joining between GFRP and Al alloy sheets. For this study, AutoCAD was used for the modeling and the simulated using commercial FEM code DEFORM-2D. The simulated results for SPR process joining between GFRP and Al alloys were confirmed by the same conditions as experimental trials.

알루미늄 기반 Advanced Multi-Material 기술의 선진 동향 (Trends of Advanced Multi-Material Technology for Light Materials based on Aluminum)

  • 이목영;정성훈
    • Journal of Welding and Joining
    • /
    • 제34권5호
    • /
    • pp.19-25
    • /
    • 2016
  • Global warming is hot issue to keep the earth everlastingly. Despite the increase of the world population and the energy demand, the world oil supply and the oil price are hold the steady state. If we are not decrease the world population and the energy consumption, unforeseeable energy crisis will come in the immediate future. AMT acronym of Advanced Materials for Transportation is a non-profitable IEA-affiliated organization to mitigate the oil consumption and the environment contamination for the transportation. In recent, Annex X Multi-materials Joining was added to enhance the car body weight reduction cause the high fuel efficiency and the low emission of exhaust gas. Multi-materials are the advanced materials application technology to optimize the weight, the performance and the cost with the combination of different materials such as Al-alloy, Mg- alloy, AHSS and CFRP. In this study, the trends of AMT strategy and Al-alloy based multi-materials joining technology were review. Also several technologies for Al-alloy dissimilar joining were investigated.

AL합금과 이종금속의 접합계면에서의 미세조직과 접합강도에 미치는 열처리조건의 영향 (The Effect of the Heat Treatment Conditions on the Strength and Microstructure in the Bonded Interface in Dissimilar Metal and Aluminum Alloy)

  • 김익수;최병영;강창룡
    • 열처리공학회지
    • /
    • 제16권1호
    • /
    • pp.2-9
    • /
    • 2003
  • The aluminum alloy which is light and has excellent thermal conductivity and iron base alloy that is remarkable heat-resistece and wear resistence properties were bonded together. The bond was created between a stationary and a rotating member by using the frictional heat generated between them while subjected to high normal forces on the interface of Al alloy and iron base alloy. The microstructure of the bonded interface of friction welding and the strength in the bonded interface formed under various bonding conditions were examined through TEM, SEM with EDX and triple bending test. In interface of bonding materials formed after various heat treatment, bonding strength was substantially different, resulting from formation of intermetallic compound or softening during annealing.

이종 알루미늄 합금 A6K31/A5J32 겹치기 마찰교반 접합부의 인장성질에 미치는 접합조건의 영향 (The effects of Welding Conditions on Tensile Properties of Friction Stir Lap Welded of Dissimilar Al Alloy, A6K31/A5J32)

  • 윤태진;김상주;송상우;홍재근;강정윤
    • Journal of Welding and Joining
    • /
    • 제29권2호
    • /
    • pp.72-79
    • /
    • 2011
  • The scope of this investigation is to evaluate the effect of joining parameters on the microstructural features and mechanical properties of dissimilar aluminum alloys, 1mm-thickness fixing AA6K31 at the top position and fixing AA5J32 at the bottom position. The friction stir lap welds were studied under various welding conditions, rotation speed of 1000, 1250, 1500rpm and welding speed of 100, 300, 500, 700mm/min, respectively. Mechanical test has been investigated in terms of tensile shear test and hardness test. The results showed that three type nugget shapes such as onion ring, zigzag type, hooking with the void, have been observed with revolutionary pitch. All welding conditions fractured at the HAZ of top plate, A6K31 and also the strength compare with base metal of lap joints were low efficiency, 52~63%. The thickness of fractured position was decreased with the lower heat input conditions. The relationships were excellent due to linear between the effective thickness of fractured position and peak load. The fractured position was the interface between joint area and not joint area. Also the strength efficiency compared with base metal was lower than decreasing rate of thickness because the hardness was decreased at fractured position due to softened material.

이종 알루미늄 합금 KS5J32/AA6K31 겹치기 마찰교반 접합부의 인장성질에 미치는 접합조건의 영향 (Effect of Welding Condition on Tensile Properties of Friction Stir Lap Joint of Dissimilar Al Alloy, KS5J32/AA6K31)

  • 김상주;윤태진;송상우;강정윤
    • Journal of Welding and Joining
    • /
    • 제30권6호
    • /
    • pp.98-105
    • /
    • 2012
  • The focus of this investigation is to evaluate the effect of joining parameter on the microstructure and mechanical properties of welds produced by friction stir lap welding. The dissimilar Al alloys, KS5J32 and AA6K31, were joined by friction stir lap welding technique under several welding conditions, and KS5J32 alloy was placed on the top of AA6K31 alloy. The tool rotation speeds were 1000, 1250, and 1500rpm, and the welding speeds were 100, 300, 500, 700mm/min, respectively. The results showed that two shapes of nugget, such as onion ring and irregular vortex type, were observed with various revolutionary pitch. In all welding conditions, fracture occurred at the soften region of bottom sheet(AA6K31) and the strengths were 64~78% of those of base metal. Fractured positions were classified into three types : HAZ, triple point, void depending on the revolutionary pitch. The actual thickness of specimen at the fractured location was decreased with decreasing heat input. A linear relationship exists between the effective thickness of fractured position and peak load.

이종재료 Self-Piercing Rivets 접합부의 인장-전단 피로강도 (Tensile-Shear Fatigue Strength of Self-Piercing Rivets Joining Dissimilar Metal Sheets)

  • 강세형;김택영;오만진;김호경
    • 한국안전학회지
    • /
    • 제30권4호
    • /
    • pp.1-7
    • /
    • 2015
  • Self-piercing riveting (SPR) process is gaining popularity due to its many advantages. The SPR does not require a pre-drilled hole and has capability to join a wide range of similar or dissimilar materials and combinations of materials. This study investigated the fatigue strength of self-piercing rivet joint with aluminum alloy (Al-5052) and steel (SPCC) sheets. Static and fatigue tests on tensile-shear specimens were conducted. From the static strength aspect, the optimal punching force for the specimen with upper SPCC (U.S) sheet and lower aluminum alloy(L.A) sheets was 34 kN. During static test the specimens fractured in pull-out fracture mode due to influence of plastic deformation of joining area. There was a relationship between applied load amplitude $P_{amp}$ and number of cycles N ; $P_{amp}=19588N_f^{-0.211}$ and $P_{amp}=4885N_f^{-0.083}$ for U.S-L.A and U.A-L.S specimens, respectively. U.A-L.S fatigue specimens failed due to fretting crack initiation around the rivet neck between upper and lower sheets.