Effect of Sintering Time on Microwave Dielectric Properties of Layered Mg0.93Ca0.07TiO3-(Ca0.3Li0.14Sm0.42)TiO3 Ceramics (소결시간에 따른 적층형 Mg0.93Ca0.07TiO3-(Ca0.3Li0.14Sm0.42)TiO3 세라믹스의 마이크로파 유전특성)

  • Cho, Joon-Yeob;Yoon, Ki-Hyun;Kim, Eung-Soo;Kim, Tae-Hong
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.9
    • /
    • pp.890-895
    • /
    • 2002
  • Effect of the sintering time on the microwave dielectric properties of the layered Functionally Graded Materials(FGMs) of the Mg0.93Ca0.07TiO3(MCT) with (Ca0.3Li0.14Sm0.42)TiO3(CLST) ceramics was investigated. The dielectric constant of layered FGMs specimens showed a nearly constant value and did not change significantly with sintering time. The quality factor, however, was affected by the relative density and thermal stress developed in each dielectric layer. With an increase of the relative density and the decrease of the induced thermal stresses, quality factor of the layered FGMs specimens increased and the quality factor was incluenced sensitively by the change of compressive stress developed in MCT layers which had a lower thermal expansion coefficient than that of CLST. For the layered FGMs specimen sintered at 1300$^{\circ}C$ for 9h, the compressive stress developed in MCT layer showed the maximum value, which, in turn, the quality factor of the specimen was the minimum value.

Hydrothermal Preparation and Sintering of Fine PSZT Powder (미세 PSZT분말의 수열합성 및 소결)

  • Oh, Jung Kang;Seo, Kyung Won
    • Applied Chemistry for Engineering
    • /
    • v.9 no.5
    • /
    • pp.654-660
    • /
    • 1998
  • In preparing PSZT powder by hydrothermal synthesis, effects of reaction temperature, concentration of raw materials and mineralizer on crystallinity, particle size distribution, and dielectric constant were investigated. By varying the concentration of mineralizer and the ratio of Pb to Sr or Zr to Ti, crystalline PSZT powder, having the mean particle size of $0.3{\sim}15{\mu}m$, was prepared by hydrothermal synthesis in the temperature range of $120{\sim}200^{\circ}C$ for a 2h reaction. PSZT ceramics, having dielectric constant of 1000~3000, were prepared at $1150^{\circ}C$ for a 2h sintering reaction of the PSZT powders. Experimental results showed that the weight mean particle size of $0.5{\mu}m$ was obtained when the concentration of KOH in the solution was 10 wt % and the ratio of Pb to Sr was 0.95/0.05, that of Zr to Ti was 0.52/0.48. It also showed that the ceramics of dielectric constant of 2900 were prepared through sintering of this PSZT powder. Size of PSZT particles became smaller with its narrow distribution as the concentration of KOH increased up to 10 wt %. However, it came to be larger at this concentration and above. By adding small amount of Sr that would not affect that crystallinity of particles we can improve dielectric property of sintered materials. Addition of Zr may shift the major crystal phase of synthetic PSZT powder from tetragonal to rhombohedral phase.

  • PDF

Low-Temperature Sintering and Microwave Dielectric Properties of the $B_2O_3-$ and CuO-added $Ba(Mg_{1/3}Nb_{2/3})O_3$ Ceramics ($B_2O_3$ 와 CuO가 첨가된 $Ba(Mg_{1/3}Nb_{2/3})O_3$ 세라믹스의 저온소결과 마이크로파 유전특성 연구)

  • Lim, Jong-Bong;Son, Jin-Ok;Nahm, Sahn;Yu, Myeong-Jae;Lee, Woo-Sung;Kang, Nam-Kee;Lee, Hwack-Joo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.838-841
    • /
    • 2004
  • [ $B_2O_3$ ] added $Ba(Mg_{1/3}Nb_{2/3})O_3$ (BBMN) ceramics were not sintered below $900^{\circ}C$. However, when CuO was added to the BBMN ceramic, it was sintered even at $850^{\circ}C$. The amount of the $Ba_2B_2O_5$ second phase decreased with the addition of CuO. Therefore, the CuO additive is considered to react with the $B_2O_3$ inhibiting the reaction between $B_2O_3$ and BaO. Moreover, it is suggested that the solid solution of CuO and $B_2O_3$ might be responsible for the decrease of the sintering temperature of the specimens. A dense microstructure without pores was developed with the addition of a small amount of CuO. However, a porous microstructure with large pores was formed when a large amount of CuO was added. The bulk density the dielectric constant $({\varepsilon}_r)$ and the Q-value increased with the addition of CuO but they decreased when a large amount of CuO was added. The variations of those properties are closely related to the variation of the microstructure. The excellent microwave dielectric properties of Qxf=21500 GHz, ${\varepsilon}_r=31$ and temperature coefficient of resonance frequency$({\tau}_f)=21.3\;ppm/^{\circ}C$ were obtained for the $Ba(Mg_{1/3}Nb_{2/3})O_3+2.0\;mol%B_2O_3+10.0$ mol%CuO ceramic sintered at $875^{\circ}C$ for 2h.

  • PDF

Dielectric and Piezoelectric Properties of Microwave Sintered BNT-ST Ceramics (마이크로파 소성법으로 제조한 BNT-ST 세라믹스의 유전 및 압전 특성)

  • Lee, Sang-Hun;Kim, Seong-Hyun;Erkinov, Farrukh;Nguyen, Hoang Thien Khoi;Duong, Trang An;Han, Hyoung-Su;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.33 no.1
    • /
    • pp.37-44
    • /
    • 2020
  • This study investigated the microstructure and piezoelectric properties of lead-free 0.74(Bi1/2Na1/2)TiO3-0.26SrTiO3 (BNST26) piezoelectric ceramics sintered using a microwave furnace. For comparison, specimens were also prepared using a conventional furnace sintering (CFS). Average grain sizes of 2.4 ㎛ and 3.2 ㎛ were obtained in the sample sintered at 1,100℃ for 5 min using microwave sintering (MWS) and at 1,175℃ for 2 h using CFS, respectively. To quantify the changes in the microstructures and electrical properties according to the sintering conditions, the polarization hysteresis, bipolar and unipolar strain curves, and temperature dependence of permittivity were evaluated. As a result, it was determined that the Pmax (maximum polarization), Pr (remanent polarization) and Smax (maximum strain) values tend to increase with the average grain size. Based on these results, it is concluded that the MWS method can produce lead-free ceramics with superior performance in a relatively short time compared to the conventional CFS method.

Low Temperature Sintering of BNKT Lead-Free Piezoelectric Ceramics Using CuO-Coated Na0.5Bi4.5Ti4O15 Templates (산화구리가 피복된 Na0.5Bi4.5Ti4O15 틀입자를 이용한 BNKT 무연 압전 세라믹스의 저온소성 연구)

  • Jeong, Gwang-Hwi;Lee, Sang-Seop;Ahn, Chang Won;Han, Hyoung Su;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.33 no.5
    • /
    • pp.337-343
    • /
    • 2020
  • This study investigated the low temperature sintering with various templates of Bi-based lead-free piezoelectric ceramics. The effects of using CuO-coated Na0.5Bi4.5Ti4O15 templates on the sintering behavior as well as the dielectric, ferroelectric, and piezoelectric properties of Bi1/2(Na0.78K0.22)1/2TiO3 (BNKT) ceramics have been examined. In comparison with the specimens sintered with the Na0.5Bi4.5Ti4O15 templates without CuO coating, those sintered with the CuO-coated Na0.5Bi4.5Ti4O15 templates showed larger template sizes as well as a larger electric field induced strain (Smax/Emax) of 422 pm/V after sintering at temperatures as low as 975℃. These results are promising for low-cost multilayer ceramic actuator applications.

Dielectric and Piezoelectric Properties of [Li0.04(Na0.5K0.5)0.96](Nb0.86Ta0.10Sb0.04)O3 Ceramics Doped with SrO (SrO의 첨가에 따른 [Li0.04(Na0.5K0.5)0.96](Nb0.86Ta0.10Sb0.04)O3세라믹스의 유전 및 압전 특성)

  • Park, Min-Ho;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.25 no.3
    • /
    • pp.198-203
    • /
    • 2012
  • In this study, $[Li_{0.04}(Na_{0.5}K_{0.5})_{0.96}](Nb_{0.86}Ta_{0.10}Sb_{0.04})O_3+xSrO$ (x=0, 0.0025, 0.005, 0.0075) ceramics were synthesized by the conventional mixed oxide method. The X-ray diffraction patterns demonstrated that ceramics possessed single perovskite structure. The SEM images indicate that microstructure can be obviously affected by a small amount of added SrO. The phase transition temperature tetragonal-cubic($T_c$) and orthorhombic-tetragonal($T_{o-t}$) shifts downward and upward with the increase of Sr addition, respectively. The excellent piezoelectric properties of $d_{33}=170[pC/N]$, $k_p=0.37$, $Q_m=64.12$, $T_{o-t}=153^{\circ}C$ and $T_c=370^{\circ}C$ were obtained from the 0.25 mol% Sr added ceramics sintered at $1,120^{\circ}C$ for 1 h.

Effect of Ta Doping on Piezoelectric Properties of Lead-Free (K0.5Na0.5)NbO3 Ceramics ((K0.5Na0.5)NbO3 세라믹스의 압전 특성에 대한 Ta 도핑 효과)

  • Kang, Jin-Kyu;Lee, Yong-Hui;Heo, Dae-Jun;Lee, Hyun-Young;Dinh, Thi Hinh;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.5
    • /
    • pp.292-296
    • /
    • 2014
  • We investigated the effect of Ta doping on the dielectric and piezoelectric properties of lead-free $(K_{0.5}Na_{0.5})NbO_3$ ceramics prepared using a conventional ceramic processing. X-ray diffraction analysis revealed that Ta was perfectly substituted into Nb-sites in the range of 0 to 20 at%. As Ta content in the KNN increased, the sinterability of KNN ceramics was significantly degraded while the Ta doping enhanced the piezoelectric constant $d_{33}$, planar mode piezoelectric coupling coefficient ($k_p$), and electromechanical quality factor ($Q_m$). The highest values for $d_{33}$, $k_p$, and $Q_m$ was found to be 156 pC/N, 0.37, and 155, respectively.

The Piezoelectric Properties of (Na0.5K0.5)NbO3-K4CuNb8O23 Ceramics with Various K4CuNb8O23 Doping and Sintering Temperatures

  • Yoon, Jung-Rag;Lee, Chang-Bae;Lee, Kyung-Min;Lee, Heun-Young;Lee, Serk-Won
    • Transactions on Electrical and Electronic Materials
    • /
    • v.11 no.3
    • /
    • pp.126-129
    • /
    • 2010
  • (1-X) $(Na_{0.5}K_{0.5})NbO_3-X$ $K_4CuNb_8O_{23}$ (NKN-X KCN) ceramics were produced using the conventional solid state sintering method, and their sinterability and electric properties were investigated. The density, dielectric constant (${\varepsilon}_r$), piezoelectric constant $d_{33}$, electromechanical coupling factor $k_p$ and mechanical quality factor $Q_m$ value of the NKN ceramics depended upon the KCN content and the sintering temperature. In particular, the KCN addition to the NKN greatly improved the mechanical quality factor $Q_m$ value. The ceramic with X = 2.0 mol% sintered at $1,150^{\circ}C$ possesses the optimum properties (${\varepsilon}_r=241$, $d_{33}=78$, $k_p=0.34$ and $Q_m=1,121$). These results indicate that the ceramic is a promising candidate material for applications in lead free piezoelectric transformer and filter materials.

The Piezoelectric Properties of (Na0.5K0.5)NbO3-K5.4Cu1.3Ta10O29 Ceramics with Various K5.4Cu1.3Ta10O29 Doping and Sintering Temperatures

  • Yoon, Jung Rag;Lee, Chang-Bae;Lee, Serk Won;Lee, Heun-Young
    • Transactions on Electrical and Electronic Materials
    • /
    • v.13 no.6
    • /
    • pp.283-286
    • /
    • 2012
  • (1-X)$(Na_{0.5}K_{0.5})NbO_3-XK_{5.4}Cu_{1.3}Ta_{10}O_{29}$ (NKN-KCT) lead-free piezoelectric ceramics have been synthesized by the conventional solid state sintering method, and their sinterability and piezoelectric properties were investigated. Typically, this material is sintered between 1,025 and $1,100^{\circ}C$ for 2 hours to achieve the required densification. Crystalline structures and Microstructures were analyzed by X-ray diffraction and scanning electron microscope. The density, dielectric constant (${\varepsilon}_r$), piezoelectric constant $d_{33}$, electromechanical coupling factor $k_p$ and mechanical quality factor $Q_m$ value of the NKN ceramics depended upon the KCT content and the sintering temperature. In particular, the KCT addition to NKN greatly improved the mechanical quality factor $Q_m$ value. The ceramic with X = 1.0 mol% sintered at $1,050^{\circ}C$ exhibited optimum properties (${\varepsilon}_r$=246, $d_{33}$=95, $k_p$=0.38 and $Q_m$=1,826). These results indicate that the ceramic is a promising candidate material for applications in lead free piezoelectric transformer and filter materials.

Effect of Ta Substitution on the Dielectric and Piezoelectric Properties of (Li0.04(Na0.54K0.46)0.96(Nb0.96-xTaxSb0.04)O3Ceramics (Ta 치환이 (Li0.04(Na0.54K0.46)0.96(Nb0.96-xTaxSb0.04)O3 세라믹스의 유전 및 압전 특성에 미치는 영향)

  • Noh, Jung-Rae;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.8
    • /
    • pp.627-631
    • /
    • 2011
  • [ $[Li_{0.04}(Na_{0.54}K_{0.46})_{0.96}](Nb_{1-0.04-X}TaxSb_{0.04})O_3$ ]lead-free piezoelectric ceramics have been prepared by normal sintering at $1,100^{\circ}C$ for 5 h. X-ray diffraction analysis indicated that specimens demonstrate orthorhombic symmetry when $Ta\leq5$ mol%. While transforming into tetragonal symmetry when $x\geq20$ mol%. These suggest that the orthorhombic and tetragonal phases co-exist in the ceramics with 5 mol% $cm^3$. As the result of SEM images, the grain growth was decreased with the increase of Ta substitution. The ceramics become 'softening', leading to improvements in $k_p$, $\varepsilon_r$ and $d_{33}$, but a decrease in $Q_m$. Excellent properties of $k_p$= 0.46, $d_{33}$= 293 pC/N, ${\varepsilon}_r$= 1,583 and Tc= $340^{\circ}C$ were obtained when Ta= 15 mol%.