졸-겔법을 이용한 $(Ba_{1-x}Sr_x)TiO_3$ 박막의 제조 및 특성 (Preparation and Characteristics of $(Ba_{1-x}Sr_x)TiO_3$ Thin Films by the Sol-gel Process)

  • 황규석;김병훈
    • 한국세라믹학회지
    • /
    • 제32권4호
    • /
    • pp.516-524
    • /
    • 1995
  • In this study, to prepare the dielectric (Ba, Sr)TiO3 thin films by the sol-gel process, Titaminum (IV) sio-propoxide (Ti[OCH(CH3)2]4), Ba and Sr acetate were used for sol and thin films were prepared by dip-coating process. Stability of sol decreased with the increase of Sr, and thickness of thin films were obtained 0.13~0.17${\mu}{\textrm}{m}$ by 1 coating cycle. Transmittance of amorphous thin films heated at 500 and 55$0^{\circ}C$ was very good, and crystallization tendency of thin films according to heat-treatment temperature and crystallization characteristics of thin films heated at 11$0^{\circ}C$ for 3 hrs were analysed. As a result, good perovskite structure was obtained higher than 100$0^{\circ}C$, and tetragonality of thin film was decreased but pyrochlore was formed with increasing Sr. In case of addition to substitute 0.4mol% Sr for Ba, dielectric constant was 288 and loss factor (tan $\delta$) was 0.04.

  • PDF

$(Ba_xSr_{1-x})$TiO$_3$박막의 온도 변화에 따른 유전 특성 (Dielectric Properties with Temperature Variation of $(Ba_xSr_{1-x})$TiO$_3$Thin Films)

  • 김덕규;전장배;송민종;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 춘계학술대회 논문집
    • /
    • pp.309-313
    • /
    • 1997
  • (Ba$_{x}$Sr$_{l-x}$)TiO$_3$(BST) thin fi1ms with various Ba/Sr ratios were deposited on Pt(80nm)/SiO$_2$(100nm)/Si by RF magnetron sputtering. BST thin films which have x=0.6, 0.5, 0.4 were studied dielectric properties with temperature variation. The frequency was used from 100Hz to 1MHz for measuring dielectric constant. The measurement conditions of dielectric constant with Temperature Variation were 1KHz and 2$0^{\circ}C$. As a result, the dielectric constant of BST thin film was about 425 and loss factor was 0.013. Also, with increasing Temperature, the dielectric constants of BST thin films were gradually decreased.sed.

  • PDF

졸-겔법에 의한 강유전 BST 박막의 제조 및 특성 (Fabrication and properties of ferroelectric BST thin films prepared by sol-gel method)

  • 이진홍;박병옥
    • 한국결정성장학회지
    • /
    • 제11권2호
    • /
    • pp.60-66
    • /
    • 2001
  • ($Ba_x$$Sr_{1-x}$)$TiO_3$ (x=0.9, 0.7, 0.5)박막을 졸-겔법으로 ITO-coated glass기판 위에 제조하였다. BST의 perov-skite상 생성온도는 $600^{\circ}C$ 이상이며 Sr함량이 증가할수록, $Ba^{2+}$ 이온보다 작은 $Sr^{2+}$ 이온에 의해 perovskite상들의 피크가 높은 회절 각도로 이동하였다. 그리고 온도가 증가할수록 결정립은 조대화 되었고, Sr 함량이 증가할수록 결정립은 미세화 되었다. BST(50/50)의 유전상수 값은 다른 두 조성보다 큰 값을 나타내고 유전손실 값은 더 낮았다. 1 kHz때의 BST(50/50)박막의 유전상수 및 유전손실 값은 각각 652와 0.042였다.

  • PDF

캐패시터용 강유전체 박막의 제조 및 특성 (Fabrication and Properties of Ferroelectric Thin Film for Capacitor)

  • 소병문;박춘배
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 추계학술대회 논문집 전문대학교육위원 P
    • /
    • pp.31-34
    • /
    • 1999
  • In the present study, we fabricated stoichiometric $(Ba_{1-x}Sr_x)TiO_3$ thin films at various substrate temperature and contents using of magnetron sputtering method on optimized Pt-based electrodes (Pt/TiN/$SiO_2$/Si). The substate temperature deposited at 200[ $^{\circ}C$], 400[$^{\circ}C$] and 600[$^{\circ}C$] and crystalline BST thin films show above 400[$^{\circ}C$]. Also, the composition of $(Ba_{1-x}Sr_x)TiO_3$ thin films deposited on Si wafer substrate at 400[$^{\circ}C$] were closed to stoichiometry($1.015{\sim}1.093$ in A/B ratio), but compositional deviation from a stoichiometry is larger as $SrCO_3$ is added. The drastic decrease of dielectric constant and increase of dielectric loss in $(Ba_{1-x}Sr_x)TiO_3$thin films is observed above 100[kHz]. V-I characteristics of $(Ba_{1-x}Sr_x)TiO_3$ thin films show the decrease of leakage current with the increase of $SrCO_3$ contents.

  • PDF

Tunable microwave device에 사용될 수 있는 $(Ba,Sr)TiO_{3}$ 박막의 유전특성 향상에 관한 연구 (Enhanced dielectric properties of $(Ba,Sr)TiO_{3}$ thin films applicable to tunable microwave devices)

  • 박배호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.73-76
    • /
    • 2001
  • We deposited epitaxial $Ba_{0.6}Sr_{0.4}TiO_{3}(BST)$ films having thickness of 400 nm on MgO(001) substrates, where a 10 nm thick $Ba_{1-x}Sr_{x}TiO_{3}$ (x = 0.1 - 0.7) interlayer was inserted between BST and MgO to manipulate the stress of the BST films. Since the main difference of those epitaxial BST films was the lattice constant of the interlayers, we were very successful in controlling the stress of the BST films. BST films under small tensile stress showed larger dielectric constant than that without stress as well as those under compressive stress. Stress relaxation was investigated using epitaxial BST films with various thicknesses grown on different interlayers. For BST films grown on $Ba_{0.7}Sr_{0.3}TiO_{3}$ interlayers, the critical thickness was about 600 nm. On the other hand, the critical thickness of single-layer BST film was less than 100 nm.

  • PDF

Zr이 첨가된 $({Ba_{1-x}},{Sr_x})TiO_3$ 박막의 미세구조와 전기적 성질 (Microstructures and Electrical Properties of Zr Modified $({Ba_{1-x}},{Sr_x})TiO_3$ Thin Films)

  • 박상식
    • 한국재료학회지
    • /
    • 제10권9호
    • /
    • pp.607-611
    • /
    • 2000
  • 고밀도 DRAM에서 박막 커패시터로의 적용을 위해 Zr이 첨가된 (Ba(sub)1-x, Sr(sub)x)TiO$_3$<원문차조> 박막이 r.f. magnetron sputter-ing 법에 의해 제조되었다. 증착된 박막들은 다결정질 구조를 보였으며 증착압력이 감소함에따라 Zr/Ti의 비가 현저히 증가하였으며 본 연구에서는 얻어진 박막들은 100kHz에서 380∼525의 유전상수값을 나타냈다. 전압에 따른 커패시턴스와 분극량의 변화는 이력특성을 크게 보이지 않아 상유전상으로 형성되었음을 보였다. 누설전류밀도는 증착압력이 감소함에 따라 작아지는 경향을 보였고 10mTorr이상에서 증착된 박막의 경우 200kV/cm의 전계에서 10(sup)-7∼10(sup)-8A/$\textrm{cm}^2$의 차수를 갖는 누설전류밀도를 보여 본 연구에서 제조된 (Ba(sub)1-x, Sr(sub)x)(Ti(sub)1-x, Zr(sub)x)O$_3$<원문참조>박막은 고밀도 DRAm을 위한 커패시터에의 적용가능성을 보였다.

  • PDF

Tunable microwave device에 사용될 수 있는 (Ba,Sr)$TiO_3$ 박막의 유전특성 향상에 관한 연구 (Enhanced dielectric properties of (Ba.Sr)$TiO_3$ thin films applicable to tunable microwave devices)

  • 박배호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.73-76
    • /
    • 2001
  • We deposited epitaxial $Ba_{0.6}$S $r_{0.4}$Ti $O_3$(BST) films having thickness of 400 nm on MgO(001) substrates, where a 10 nm thick $Ba_{1-x}$S $r_{x}$Ti $O_3$(x=0.1-0.7) interlayer was inserted between BST and MgO to manipulate the stress of the BST films. Since the main difference of those epitaxial BST films was the lattice constant of the interlayers, we were very successful in controlling the stress of the BST films. BST films under small tensile stress showed larger dielectric constant than that without stress as well as those under compressive stress. Stress relaxation was investigated using epitaxial BST films with various thicknesses grown on different interlayers. For BST films grown on $Ba_{0.7}$S $r_{0.3}$Ti $O_3$ interlayers, the critical thickness was about 600 nm. On the other hand, the critical thickness of single-layer BST film was less than 100 nm.00 nm.m.m.m.

  • PDF

Properties of MTiO3 (M = Sr, Ba) and PbM'O3(M'= Ti, Zr) Superlattice Thin Films Fabricated by Laser Ablation

  • Lim, T.M.;Park, J.Y.;Han, J.S.;Hwang, P.G.;Lee, K.H.;Jung, K.W.;Jung, D.
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권1호
    • /
    • pp.201-204
    • /
    • 2009
  • $BaTiO_3/SrTiO_3$ and $PbTiO_3/PbZrO_3$ superlattice thin films were fabricated on $Pt/Ti/SiO_2/Si$ substrate by the pulsed laser deposition process. The morphologies and physical properties of deposited films were characterized by using X-ray diffractometer, HR-SEM, and Impedance Analyzer. XRD data and SEM images of the films indicate that each layer was well deposited alternatively in the superlattice structure. The dielectric constant of $BaTiO_3/SrTiO_3$ superlattice thin film was higher than that of individual $BaTiO_3$ or $SrTiO_3$ film. Same result was obtained in the $PbTiO_3/PbZrO_3$system. The dielectric constant of a superlattice film was getting higher as the number of layer is increased.

ULSI DRAM의 capacitor 절연막용 BST(Barium Strontium Titanate)박막의 제작과 특성에 관한 연구 (Preparation and properties of BST (Barium Strontium Titanate) thin films for the capacitor dielectrics of ULSI DRAM's)

  • 류정선;강성준;윤영섭
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제9권4호
    • /
    • pp.336-343
    • /
    • 1996
  • We have studied the preparation and the properties of $Ba_{1-x}$Sr$_{x}$TiO$_{3}$(BST) thin films by using the sol-gel method. Through the comparison of the effects of various solvents and additives in making solutions, we establish the production method of the stable solution which generates the high quality of BST film. We also set up the heat-treatment conditions for depositing the BST thin film through the TGA and XRD analyses. Through the comparison of the surface conditions of BST films deposited on Pt/Ta/SiO$_{2}$/Si and Pt/Ti/SiO$_{2}$/Si substrates, we find that Ta is more efficient diffusion barrier of Si than Ti so that Ta layer prevents the formation of hillocks. We fabricate the planar type capacitor and measure the dielectric properties of the BST thin film deposited on the Pt/Ta/SiO$_{2}$/Si substrate. Dielectric constant and dielectric loss tangent at 1V, 10kHz, and leakage current density at 3V of the BST thin film are 339, 0.052 and 13.3.mu.A/cm$^{2}$, respectively.ely.

  • PDF