A Case Study on the Assessment of Damaged Cause for the Damaged Reinforced Concrete Pier

  • Chai, Won-Kyu;Kim, Kwang-Il;Son, Young-Hyun
    • International Journal of Safety
    • /
    • v.10 no.1
    • /
    • pp.16-21
    • /
    • 2011
  • In this thesis, appearance inspection, compressive strength of concrete test, arrangement of bar inspection, survey, and bearing stress analysis were performed on a damaged coping of reinforced concrete pier to investigate the damage cause. According to the performed a series of inspections, it was found that the coping of pier was damaged during PSC (Pre-stressed Concrete) beam construction. In this thesis, the repair method for damaged pier was studied. The repair procedure used in this thesis was follows : chipping for damaged part, clean by high-pressure, installation of wire mesh, coating of surface hardening, construction of section restoration material, copula grinding, and prevent coating for far-infrared radiation.

  • PDF

A Study on the Quality Control of 80MPa UHPC according to the Measurement Method of Compressive Strength (압축강도 측정방법에 따른 80MPa급 UHPC의 품질관리에 관한 연구)

  • Koo, Hyun-Chul;Moo, Ji-Hun;Lee, Hak-ju;Park, Min-Sang;Choi, Sung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.05a
    • /
    • pp.176-177
    • /
    • 2019
  • Recently, efforts are made to apply 200MPa levels of ultra-high strength concrete to structures exceeding 40MPa.. Ultra-high strength concrete has been steadily researched in Korea as well as abroad, and now it is equipped with 200MPa ultra-high strength concrete mixing technology. Because ultra-high strength concrete has a higher range of compressive strength than ordinary concrete, it is difficult to accurately measure the compressive strength of UHPC concrete with existing compressive strength measuring equipment and can be less reliable. In this study, the compressive strength of the SC80 was measured according to the test method to compare the compressive strength of the SC80 by applying various methods of measurement of compressive strength. The compressive strength test method measured the compressive strength according to the size of the specimen, the grinding method, and the capacity of the UTM equipment.

  • PDF

Mechanical and durability properties of concrete incorporating glass and plastic waste

  • Abdelli, Houssam Eddine;Mokrani, Larbi;Kennouche, Salim;Aguiar, J.L. Barroso de
    • Advances in concrete construction
    • /
    • v.11 no.2
    • /
    • pp.173-181
    • /
    • 2021
  • The main objective of this work is to contribute to the valorization of plastic and glass waste in the improvement of concrete properties. Waste glass after grinding was used as a partial replacement of the cement with a percentage of 15%. The plastic waste was cut and introduced as fibers with 1% by the total volume of the mixture. Mechanical and durability tests were conducted for various mixtures of concrete as compressive and flexural strengths, water absorption, ultrasonic pulse velocity, and acid attack. Also, other in-depth analyses were performed on samples of each variant such as X-ray diffraction (XRD), thermogravimetric analysis (DSC-TGA), and scanning electron microscope (SEM). The results show that the addition of glass powder or plastic fibers or a combination of both in concrete improved in the compression and flexural strengths in the long term. The highest compressive strength was obtained in the mix which combines the two wastes about 26.72% of increase compared to the control concrete. The flexural strength increased in the mixture containing the glass powder. Therefore, the mixture with two wastes exhibits better resistance to aggressive sulfuric acid attack, and incorporating glass powder improves the ultrasonic pulse velocity.

A Fundamental Study for Developing Design Forms Application in Building Constructions (건축물에 적용할 수 있는 문양거푸집 개발을 위한 기초적 연구)

  • 임현준;김광기;김병천;김우재;정재욱;정상진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.1053-1058
    • /
    • 2001
  • Contemporary architecture calls for a wide range of surface textures and treatments. A surface compatible with the architect's design may vary from a glass-smooth finish to one requiring special sculptured ornamentation. These surfaces require many different types of form sheathing and lining. Chemical retarders applied to the form surface make It possible to remove surface mortar and expose the aggregate after forms have been removed. Variation in finish may also be achieved by grinding, chiseling, hammering, and sandblasting after the concrete has set. Precast panels as forms or liners may provide the desired surface finish; sometimes a combination several of these techniques is used.

  • PDF

An Experimental Study on the Strength Development of Fly-Ash Mortar by Using the Activator and Curing Temperature change. (자극제 사용 및 양생온도 변화에 의한 플라이애쉬 모르타르의 강도발현에 관한 실험적 연구)

  • 배수환;최광윤;정재동;최영화
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.11a
    • /
    • pp.277-280
    • /
    • 2003
  • The purpose of this study is for the active use of the fly ash, which is a by-product of the combustion pulverizes coal thermal power plants, to compensate for the lack of landfill and for conservation of energy, by using fly ash as the supplementary cementitious material, and to prove its possibility as the related products of the cement. First of all, we examined strength development of Micro grinding fly ash by elevating its fineness and using $Na_{2}SO_{4}$ as an activator to elevate pozzolanic reaction of fly ash. Following fly ash replacement ratio and curing temperature we hope to prove its properties to suggest its possibility in the concrete and cement industry. In case of water curing, the more fineness and higher annexing of activator is, the higher strength is, and the higher curing temperature is the more pozzolanic reaction happens.

  • PDF

A Comparative Study on the Quality of Recycled Aggregate for Concrete by Grinding and Peeling and Milling (파·분쇄기와 박리 및 마쇄기 접목에 따른 콘크리트용 순환골재의 품질 비교 연구)

  • Choi, Won-Young;Jeon, Chan-Soo;Kim, Ji-Hoon
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2018.05a
    • /
    • pp.261-262
    • /
    • 2018
  • In this study, the quality of recycled aggregate for concrete was investigated as the number of recycled aggregate crushing cycles, grinder and crusher, peeling and crushing. First, the quality of density, absorption ratio and solid content was improved as the separation distance decreased and the number of crushing increased, depending on the number of crushing of recycled aggregate and the distance between mantle and cone cave. The quality of density, absorption ratio and solid content was improved as the wire mesh used in striking plate and the number of hammers increased, depending on the type of striking plate and the number of hammers.

  • PDF

A Numerical Method for Macro-fiber Distribution and Orientation In Hardened Concrete Components

  • Li, Mao;Kim, Jin-man;Choi, Hong-Beom
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.11a
    • /
    • pp.85-86
    • /
    • 2017
  • Fiber reinforced concrete as a construction material has been widely used. Fibers, as the reinforced component, the physical properties and the distribution influence the engineering properties of the composite. To illustrate the engineering properties, fiber distribution and orientation are necessary. Steel fibers can be easily captured by X-ray, but it is difficult them to express being numerical because they don't show as perfect circular shape on the grinding face. To get the more exact information for this, the numerical method for the orientation and distribution of fibers have to be more elaborately. This paper presents a possible method which makes the calculate for orientation possible.

  • PDF

Optimal Abrasion Conditions for Separating Aggregate and Cement paste for Using Waste Concrete Fine Powder as Decarbonization Raw Material (폐콘크리트 미분말을 탈탄산 원료로 사용하기 위한 골재와 시멘트페이스트 분리의 최적 마쇄 조건 분석)

  • Ha-Seog Kim;Min-Chul Lee
    • Land and Housing Review
    • /
    • v.14 no.4
    • /
    • pp.121-129
    • /
    • 2023
  • In this study, we attempted to reduce CO2 generated during manufacturing by replacing limestone (CaCO3), a carbonate mineral used to produce cement clinker, with a decarbonated raw material to which CO2 is not bound. The raw material for decarbonization was cement paste attached to waste concrete, among various industrial by-products. Waste concrete has cement paste adhered to the aggregate, which cannot be separated efficiently by general crushing and grinding methods. Peeling and grinding methods effectively remove only the cement paste without damaging the original aggregate. The abrasion time, steel ball type, and steel ball ratio were selected as effective factors for Abrasion. An optimal abrasion experiment was conducted to produce waste concrete fine powder containing decarbonated CaO as a cement clinker raw material through an experimental design method. The experiment revealed that the optimal conditions for producing waste concrete fine powder were an abrasion time of 7 minutes, a steel ball size for pulverization of 8 mm, and a steel ball ratio for pulverization of 0.6.

An Experimental Study on the Effect of Concrete Surface Treatment Methods on the Bond Strength of Metal Spray Coating (콘크리트 표면처리 방법이 콘크리트 표면 금속용사 피막의 부착강도에 미치는 영향에 관한 실험적 연구)

  • Park, Jin-Ho;Kim, Sang-Yeol;Lee, Han-Seung
    • Journal of the Architectural Institute of Korea Structure & Construction
    • /
    • v.36 no.1
    • /
    • pp.147-154
    • /
    • 2020
  • The exterior finishing of reinforced concrete buildings is one of the important factors to prevent durability and prevent natural environment or disaster such as temperature, snow, wind, rain from the outside as well as external design of buildings. Finishing methods can be divided into wet and dry methods. The wet method using paint is relatively easy to construct, but it requires repair and reinforcement every 1 to 5 years and requires a lot of LCC for maintenance. Finishing method using panel has good durability, but it is difficult to install and expensive. Therefore, in this paper, we evaluate the bond strength for the application of the metal spray method in order to overcome the problems of existing methods. Experimental results show that the sandblast + surface roughness agent(S-R(Y)) has a roughness of 41.16 ㎛ and the bond strength is about 3.19 MPa, which is the highest bond strength. In addition, the grinding + surface roughness agent(G-R(Y)) application showed roughness of about 36.59 ㎛ and secured the bond strength performance of 2.94 MPa.

Evaluation on Workability and Compressive Strength Development of Concrete Using Modified Fly-Ash by Vibration Grinding (진동분쇄를 사용한 개질 플라이애시 콘크리트의 유동성 및 압축강도 발현 평가)

  • Ahn, Tae-Ho;Yang, Keun-Hyeok;Jeon, Young-Su
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.1
    • /
    • pp.66-74
    • /
    • 2021
  • The objective of this study is to evaluate the practical application potential and limitations of the modified fly ash(MFA) by vibration grinding as a partial replacement of ordinary portland cement(OPC). The test parameters investigated were the replacement level of fly ash(FA) and FA for OPC, varying from 10% to 40%, and curing temperatures of 5, 20, and 40℃. The various characteristics(including slump, air content, bleeding, setting time, compressive strength development, and hydration products) of MFA concrete were measured and then compared with those of the concrete with conventional FA. Test resul ts showed that the MFA prefers to FA in reducing the bl eeding of fresh concrete and enhancing the compressive strength gain at an early age. The compressive strength ratios between MFA and FA concrete specimens at an age of 1 day were 135%, 146%, and 111% at the curing temperatures of 5, 20, and 40℃, respectively. The corresponding ratios at an age of 28 days were approximately 110%, regardless of the curing temperatures. The X-ray diffraction analysis also revealed less calcium hydroxide products in MFA pastes than in FA pastes.