Effect of Organic Admixture(Calcium Lignosulfonate) on the Early Hydration Process of Portland Cement(III) (시멘트 초기수화과정에 대한 유기혼화제의 영향(III))

  • 문정연;최상홀
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.1
    • /
    • pp.5-10
    • /
    • 1985
  • The effect of calcium lignosulfonate (CLS) on the early hydration characteristics for clinker minerals was investigated. In the presence of CLS and unsufficient gypsum The hydration of $C_3$A lowered CLS adsorption to form ettrin-gite and the residual CLS in the liquid phase accelerated the solubility of C4AF hydration. As the result unreacted $Fe^{3+}$ in the liquid phase would be precipitated gelatinously on $C_3$ hydrates and the hydration of $C_3$ could be retarded. But by addition of optimum gypsum into the cement with CLS the presence of $Fe^{3+}$ in the liquid phase were lowered and $C_3$ hydration would be normallized.

  • PDF

On the Rapid Hardening Cement (II) (초속경시멘트 제조에 관한 연구(제2보 수화반응))

  • 한기성;최상흘;한상목;서일영
    • Journal of the Korean Ceramic Society
    • /
    • v.12 no.4
    • /
    • pp.3-8
    • /
    • 1975
  • Hydration processes of the rapid hardening cement clinkers, which were synthesized from domestic alunite for major alumina source, limestone, kaolin and fluorite, were investigated by means of x-ray diffraction analysis, thermal analysis and microscopic observation etc. The clinkers were composed mainly of alite, calcium fluroaluminate (C11A7.CaF2) minerals. While the hydratio processes of the clinkers are altered by concentration of SO3 in the paste, calcium aluminate hydrates such as C4AH13, CAH10 and calcium monosulfate hydrate (C3A.CaSO4.12H2O) are formed at first and then some of them are transformed into ettringite(C3A.3CaSO4.32H2O) within 30~60 min. when the concentration of SO3 in the paste are enough. However the formed ettringite are changed slowly into calcium monosulfate hydrate as the concentration of SO3 become lowered, and the paste is hardened with these close-packed minerals. When the content of SO3 in clinker is so enough, calcium sulfoaluminate hydrates are found without any addition of anhydrite or hemi-hydrite.

  • PDF

Synthesis of Cordierite and Preparation of Refractory Setter from Domestic Raw Materials (Cordierite의 합성 및 내화갑제조에 관한 연구)

  • 지응업;최상욱;김광호
    • Journal of the Korean Ceramic Society
    • /
    • v.12 no.4
    • /
    • pp.19-28
    • /
    • 1975
  • In order to obtain the superior refractory setter having better spalling resistance, cordierite was synthesized from domestic raw materials. Raw mixtures were fired between 125$0^{\circ}C$ and 140$0^{\circ}C$, and qualitative determination of crytallization was investigated by x-ray diffraction analysis. The results obtained are as follows; 1) The optimum batch composition of synthesized cordierite is 80.5% of Hadong kaolin (pink), 14% of Kyulsung tromolite talc and 5.5% of magnesia clinker, and the firing temperature is 1375$^{\circ}C$. 2) The composition of the refractory setter which exhibits the best values for the thermal properties is 40% of synthesized cordierite, 30% of kaolin chamotte(contains more than 60% of mullite), and 30% of Japanese clay. 3) The optimum particle size distribution of ternary mixture consists of 50% of coarse articles (3.327-1.168mm), 25% of intermediate particles (1.168-0.208mm) and 25% of fine particles (0.208-0.000mm).

  • PDF

Solidification/stabilization of Hazardous Wastes Using Cementitious Materials(III) (특수시멘트 고형화재를 이용한 지정폐기물의 고형화/안정화(III))

  • Lim, Chae-Yong;Ku, Ki-Dae;Um, Tae-Sun;Lee, Jong-Ryul;Choi, Long;Oh, Byoung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.289-294
    • /
    • 2001
  • This study concerns the cement-solidification/stabilization of the waste with high concentration heavy metals. Compressive strength and leaching test of heavy metals were evaluated for ing types of cements and the effect of the additives of Hauyne clinker and slag were also cussed. Using ordinary portland cement, rapid hardening portland cement and the cement with additives solidification materials, it shows that the strength and stability of concrete is satisfactory and superiority is in the order of rapid hardening portland cement > the cement with additives > nary portland cements.

  • PDF

A Study on Design of High Early Strength Cement and Concrete for Road Way Pavements (신속개방형 콘크리트 도로포장재의 설계를 위한 실험실적 평가 연구)

  • 임채용;엄태선;신국재;이종열;엄주용;조윤호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.295-300
    • /
    • 2001
  • In road pavements, it is known that cement concrete pavement has superior durability, safety in compared with asphalt concrete pavement. But in reparing pavement cement concrete pavement is not usually applied because of the length of time while the road is interrupted when using Ordinary and Rapid-hardening Portland Cement. And Super High Early Strength Cement and Ultra Super High Early Strength Cement are not favorable for ready mixied concrete because of rapid setting time, high slump loss and other restrictions. We aim to develope specific cement and concrete developing 1 day strength of over 300 kg/$cm^{2}$ to open the road within one day and workable time is maintained over 1 hour that can be used as ready mixed concrete. In this study, we Produced cement using rapid-hardening cement, Hauyne clinker, anhydride gypsum and accelerator and studied on its properties. The concrete strength was over 300 kg/$cm^{2}$ at 1 day and 550 kg/$cm^{2}$ at 28 day and workable time was maintained for over 1 hour.

  • PDF

A Study on Evaluation of High Early Strength Concrete as Pavement Overlay Materials for Early Traffic Opening(2) (신속개방형 콘크리트 도로포장재의 설계를 위한 평가 연구(2))

  • 엄태선;임채용;유재상;이종열;엄주용;조윤호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.233-238
    • /
    • 2001
  • In road Pavements, it is known that cement concrete pavement has superior durability, safety compared with asphalt pavement. But in repairing pavement, cement concrete pavement is not usually applied because of the length of time while the road is interrupted when using Ordinary and Rapid-hardening Portland Cement. And Super High Early Strength Cement and Ultra Super High Early Strength Cement are not favorable for ready mixed concrete because of rapid setting time, high slump loss and other restrictions. We aim to develope special cement and concrete developing 1 day strength of over 300 kg/$\textrm{cm}^2$ to open the road within one day and workable time is maintained over 1 hour that can be used as ready mixed concrete. In this study, we produced cement using rapid-hardening cement, Hauyne clinker, anhydride gypsum and accelerator and studied on its properties. The comperssive strength was over 400 kg/$\textrm{cm}^2$ and tensile at 1 day and workable time was maintained for over 1 hour.

  • PDF

Fundamental Properties of Mortar Utilizing Waste Concrete Power (폐콘크리트 분말을 활용한 모르타르의 기초물성에 관한 연구)

  • Choi, Yun-Wang;Moon, Dae-Joong;Kim, Sung-Su;Kim, Ki-Hyung;Moon, Han-Young
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.620-623
    • /
    • 2004
  • Waste concrete powder(WCP) has been estimated with a great value-added material as by-product of waste concrete manufactured to fine and coarse aggregate for concrete, because it is able to utilized for cement clinker and concrete admixture. In the experimental results for this study, chemical composition of WCP was similar to that of cement, and specific gravity of WCPs were 2.46 and 2.48 due to internal micro-void of WCP. Final setting of paste with WCP was delayed, and flow value of mortar with WCP was tendency to reduced in comparison with that of paste and mortar with only ordinary portland cement as replacement ratio of WCP increased. Furthermore, sorptivity of mortar with WCP was increased as replacement ratio of WCP increased. Compressive strength of mortar with $15\%$ WCP was developed about 27MPa at 28days.

  • PDF

A multiscale creep model as basis for simulation of early-age concrete behavior

  • Pichler, Ch.;Lackner, R.
    • Computers and Concrete
    • /
    • v.5 no.4
    • /
    • pp.295-328
    • /
    • 2008
  • A previously published multiscale model for early-age cement-based materials [Pichler, et al.2007. "A multiscale micromechanics model for the autogenous-shrinkage deformation of early-age cement-based materials." Engineering Fracture Mechanics, 74, 34-58] is extended towards upscaling of viscoelastic properties. The obtained model links macroscopic behavior, i.e., creep compliance of concrete samples, to the composition of concrete at finer scales and the (supposedly) intrinsic material properties of distinct phases at these scales. Whereas finer-scale composition (and its history) is accessible through recently developed hydration models for the main clinker phases in ordinary Portland cement (OPC), viscous properties of the creep active constituent at finer scales, i.e., calcium-silicate-hydrates (CSH) are identified from macroscopic creep tests using the proposed multiscale model. The proposed multiscale model is assessed by different concrete creep tests reported in the open literature. Moreover, the model prediction is compared to a commonly used macroscopic creep model, the so-called B3 model.

Solidification of municipal solid waste incineration fly ash by hauyne clinker (Hauyne 클링커에 의한 생활폐기물 소각 비산재의 고화 특성)

  • Han, Gi-Chun;You, Kwang-Suk;Um, Nam-Il;Cho, Kye-Hong;Cho, Hee-Chan;Ahn, Ji-Whan
    • Proceedings of the Korean Institute of Resources Recycling Conference
    • /
    • 2005.10a
    • /
    • pp.355-359
    • /
    • 2005
  • 본 연구에서는 OPC 및 hauyne 클링커의 비산재에 대한 고화특성을 검토하였다. 비산재에 대해 OPC 및 OPC에 hauyne 클링커를 20%까지 대체하였을 때의 압축강도, 길이변화율, 중금속 용출량 등을 조사하였다. 결과로서, hauyne 클링커의 첨가량에 따라 고화체의 압축 강도가 증가하였다. hauyne 클링커의 첨가량은 10%내외가 적합하였으며, 그 이상에서는 길이변화율이 증가하며 팽창하였다. 고화체의 중금속 용출시험결과 모든 배합조건에서 환경기준치이하의 값을 나타내었다.

  • PDF

Studies on Magnesia Production. Production of Magnesium Hydroxide from Bittern and Sea Water (마그네시아 製造에 關한 硏究 간수, 海水로 부터 水酸化마그네슘 製造)

  • Maeng, Jung-Jae;Chang, In-Soon
    • Journal of the Korean Chemical Society
    • /
    • v.9 no.1
    • /
    • pp.49-54
    • /
    • 1965
  • One of the difficult and time consuming problems in the production of magnesia from sea water is a settling rate of magnesium hydroxide. In this experiments, authors attempted to accelerate its settling rate by addition of various sedimenting agents as C.M.C., Separan and Starch, and sought for optimum calcination temperature for domestic dolomite, as alkali source, mole ratio of dolomite milk to bittern. It is observed through experiments that the small amounts of sedimenting agents, C.M.C., Separan, starch, 20 mg/l, 40 mg/l, 400mg/l, respectively increase the settling rate of magnesium hydroxide by 8 times or more. The following conditions resulted in good yield of magnesium hydroxide from sea water with relatively tolerable calcium oxide contaminated for the magnesium clinker. Calcinating temperature, $1,100{\sim}1,200^{\circ}C$, mole ratio of 10% dolomite milk to magnesium salts in sea water or bittern, 1. 2 : 1.