Kim, Gwan-Ha;Kim, Kyoung-Tae;Kim, Chang-Il;Kim, Dong-Pyo;Lee, Cheol-In;Kim, Tae-Hyung
Proceedings of the KIEE Conference
/
2004.11a
/
pp.187-190
/
2004
In this work, we investigated etching characteristics and mechanism of BST thin films using $Cl_2$/Ar, $CF_4/Cl_2$/Ar and $BCl_3/Cl_2$/Ar gas mixtures using inductively coupled plasma (ICP) system. A chemically assisted physical etch of BST was experimentally confirmed by ICP under various gas mixtures. The etch rate of the BST thin films had a maximum value at 20 $BCl_3$ and 10% $CF_4$ gas concentration, and decreased with further addition of $BCl_3$ or $CF_4$ gas, because $BaCl_x$, $SrCl_x$, $BaF_x$ and $SrF_x$ compounds have higher melting and boiling points. The maximum etch rate of the BST thin films was 57nm/min at the 30% $Cl_2(Cl_2+Ar)$. The characteristics of the plasma were analyzed by using OES and Langmuir probe.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.16
no.6
/
pp.449-453
/
2003
Ferroelectric YMnO$_3$ thin films were etched with Ar/Cl$_2$ and CF$_4$/Cl$_2$ inductively coupled plasma (ICP). The maximum etch rate of YMnO$_3$ thin film was 300 $\AA$/min at a Ar/Cl$_2$ gas mixing ratio of 2/8, a RF power of 800 W, a DE bias of 200 V, a chamber pressure of 15 mTorr, and a substrate temperature of 30 $^{\circ}C$. From the X-ray photoelectron spectroscopy (XPS) analysis, yttrium etched by chemical reactions with Cl radicals assisted by Ar ion bombardments in Ar/Cl$_2$ plasma. In CF$_4$/Cl$_2$ plasma, yttrium are remained on the etched surface of YMnO$_3$ and formed of nonvolatile YF$_{x}$ compounds manganese etched effectively by chemical reactions with Cl and F radicals. From the X-ray diffraction (XRD) analysis, the (0004) diffraction peak intensity of the YMnO$_3$ thin film etched in Ar/Cl$_2$ plasma shows lower value than that in CF$_4$/Cl$_2$ plasma. It indicates that the crystallinty of YMnO$_3$ thin film is more easily damaged by the Ar ion bombardment than the changes of stoichiometry due to nonvolatile etch by-products.s.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.14
no.7
/
pp.551-556
/
2001
In this work, the recovery of etching damage in the etched PZT thin film with $O_2$ annealing has been studied. The PZT thin films were etched as a function of Cl$_2$/Ar and additive CF$_4$ into Cl$_2$(80%) /Ar(20%). the etch rates of PZT thin films were 1600$\AA$/min at Cl$_2$(80%)/Ar(20%) and 1970 $\AA$/min at 30% additive Cf$_4$ into Cl$_2$(80%)/Ar(20%). In order to recover the characteristics of etched PZT thin films, the etched PZT thin films were annealed in $O_2$ atmosphere at various temperatures. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ annealing process. The improvement of ferroelectric behavior is consistent with the increase of the (100) and (200) PZT phase revealed by x-ray diffraction (XRD). From x-ray photoelectron spectroscopy (XPS) analysis, intensities of Pb-O, Zr-O and Ti-O peak increase and the chemical residue peak is reduced by $O_2$ annealing. From the atomic force microscopy (AFM) images. it shows that the surface morphology of re-annealed PZT thin films after etching is improved.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2001.11b
/
pp.21-25
/
2001
In this study, recovery of plasma etching· damage in PZT thin film with additive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of $Cl_2/CF_4$ with addition of Ar and $O_2$ with inductively induced plasma. The etch rates of PZT thin films were 1450 $\AA$/min at 30% additive Ar into $(Cl_2(80%)+CF_4 (20%))$ and 1100 $\AA$/min at 10% additive $O_2$ into $C(Cl_2(80%)+CF_4(20%))$. In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in at $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x-ray photoelectron spectroscopy (XPS) analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of $Ti_xO_y$ is recovered by $O_2$ recombination during rapid thermal annealing process.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2001.11a
/
pp.21-25
/
2001
In this study, recovery of plasma etching damage in PZT thin film with additive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of Cl$_2$/CF$_4$ with addition of Ar and $O_2$ with inductively induced plasma. The etch rates of PZT thin films were 1450$\AA$/min at 30% additive Ar into (Cl$_2$(80%)+CF$_4$ (20%)) and 1100$\AA$/min at 10% additive $O_2$ into C(Cl$_2$(80%)+CF$_4$ (20%)). In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in at $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x-ray photoelectron spectroscopy (XPS) analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of Ti$_{x}$O$_{y}$ is recovered by $O_2$ recombination during rapid thermal annealing process.s.s.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.15
no.4
/
pp.314-318
/
2002
The etching behaviors of the ferroelectric $YMnO_3$ thin films were studied by an inductively coupled plasma (ICP). The maximum etch rate of $YMnO_3$ thin film is 300 ${\AA}/min$ at Ar/$Cl_2$of 2/8, RF power of 800W, dc bias voltage of 200V, chamber pressure of 15mTorr and substrate temperature of $30^{\circ}C$. Addition of $CF_4$ gas decrease the etch rate of $YMnO_3$ thin film. From the results of XPS analysis, nonvolatile $YF_x$ compounds were found on the surface of $YMnO_3$ thin film which is etched in Ar/$Cl_2$/CF$_4$plasma. The etch profile of YMnO$_3$film is improved by addition of $CF_4$ gas into the Ar/$Cl_2$ plasma. These results suggest that YF$_{x}$ compound acts as a sidewall passivants which reduce the sticking coefficient of chlorine on $YMnO_3$.
Kim, In-Pyo;Park, Jae-Hwa;Kim, Kyoung-Tae;Kim, Chang-Il;Jang, Eui-Goo;Eom, Joon-Chul
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2002.11a
/
pp.159-162
/
2002
Ferroelectric $YMnO_{3}$ thin films were etched with $Ar/Cl_{2}$ and $CF_{4}/Cl_{2}$ inductivly coupled plasma (ICP). The maximum etch rate of $YMnO_{3}$ thin film was $300{\AA}/min$ at a $Ar/Cl_{2}$ gas mixing ratio of 2/8, a RF power of 800 W, a dc bias of 200 V, a chamber pressure of 15 mTorr, and a substrate temperature of ${30^{\circ}C}$. From the X-ray photoelectron spectroscopy (XPS) analysis , yttrium not only etched by chemical reactions with Cl radicals, but also assisted by Ar ion bombardments in $Ar/Cl_{2}$ plasma. In $CF_{4}/Cl_{2}$ plasma, yttrium are remained on the etched surface of $YMnO_{3}$ and formed of nonvolatile YFx compounds Manganese etched effectively by chemical reactions with Cl and F radicals. From the X-ray diffraction (XRD) analysis, the (0004) diffraction peak intensity of the $YMnO_{3}$ thin film etched in $Ar/Cl_{2}$ plasma shows lower value than that in $CF_{4}/Cl_{2}$ plasma. It is indicates that the crystallinty of $YMnO_{3}$ thin film is more easily damaged by the Ar ion bombardment than the changes of stoichiometry due to nonvolatile etch by-products.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2001.11a
/
pp.213-216
/
2001
Etching behaviors of ferroelectric YMn $O_3$ thin films were studied by an inductively coupled plasma (ICP). Etch characteristic on ferroelectric YMn $O_3$ thin film have been investigated in terms of etch rate, selectivity and etch profile. The maximum etch rate of YMn $O_3$ thin film is 300 $\AA$/min at Ar/C $l_2$ of 2/8, RF power of 800W, dc bias voltage of 200V, chamber pressure of 15mTorr and substrate temperature of 3$0^{\circ}C$. Addition of C $F_4$ gas decrease the etch rate of YMn $O_3$ thin film. From the results of XPS analysis, Y $F_{X}$ compunds were found on the surface of YMn $O_3$ thin film which is etched in Ar/C1/C $F_4$ plasma. The etch profile of YMn $O_3$ film is improved by addition of C $F_4$ gas into the Ar/C $l_2$ plasma. These results suggest that fluoride yttrium acts as a sidewall passivants which reduce the sticking coefficient of chlorine on YMn $O_3$.>.
Transactions on Electrical and Electronic Materials
/
v.4
no.2
/
pp.29-34
/
2003
Ferroelectric YMnO$_3$ thin films were etched with Ar/C1$_2$ and CF$_4$/C1$_2$ Plasma. The maximum etch rate of YMnO$_3$ thin film was 300 $\AA$/min at a Cl$_2$/Ar gas mixing ratio of 8/2, an RF power of 800 W, a do bias of-200 V, a chamber pressure of 15 mTorr, and a substrate temperature of 3$0^{\circ}C$. From the X-ray photoelectron spectroscopy (XPS) analysis, yttrium was not only etched by chemical reactions with Cl atoms, but also assisted by Ar ion bombardments in Ar/C1$_2$ plasma. In CF$_4$/C1$_2$ plasma, yttrium formed nonvolatile YF$_{x}$ compounds and remained on and the etched surface of YMnO$_3$. Manganese etched effectively by forming volatile MnCl$_{x}$ and MnF$_{y}$. From the X-ray diffraction (XRD) analysis, the (0004) diffraction peak intensity of the YMnO$_3$ thin film etched in Ar/Cl$_2$ plasma shows lower than that in CF$_4$/Cl$_2$ plasma. It indicates that the crystallinty of the YMnO$_3$ thin film is more easily damaged by the Af ion bombardment than the changes of stoichiometry due to nonvolatile etch by-products.cts.s.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.15
no.4
/
pp.319-324
/
2002
In this study, the reduce of plasma etching damage in PZT thin film with addictive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of $Cl_2/CF_4$ with addition of Ar and $O_2$ with inductively coupled plasma. The etch rates of PZT thin films were 1450 ${\AA}/min$ at 30% additive Ar and 1100 ${\AA}/min$ at 10% auditive $O_2$ into $Cl_2/CF_4$ gas mixing ratio of 8/2. In order to reduce plasma damage of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures at $O_2$ atmosphere. From the hysteresis curries, the ferroelectric properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed PZT films is consistent wish the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x ray photoelectron spectroscopy (XPS) analysis, the intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of $Ti_xO_y$ is recovered by $O_2$ recombination during rapid thermal annealing process.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.