  • During the past several years, significant advances have occurred in the utilization of osseointegrated implants for the treatment of partially edentulous patients. One of the biggest purposes for treating of these patients is the high demand for improved esthetics, especially in the anterior region. For this esthetics, the new trend in dental implants is the immediate placement and immediate superstructure fabrication. The refined surgical technique, the skillful soft tissue management, and the proper prosthetic coordination are the main factors to achieve natural looking of implant supported prosthesis. The customized provisional restoration and the customized impression coping are recommended for the optimal peri-implant soft tissue contour. The basic concept of Frialit 2 system was the immediate replacement of a tooth with root-analog fixture after extraction. This system guarantees an ideal result in function and esthetics. The ceramic abutment system offers improved quality in the respect of esthetics, fitness, translucency, and biocompatibility. In this clinical report, the final restoration made with IPS Empress 2 crown on the CeraBase abutmen of Frialit 2 system allowed the reproduction of the natural vitality of tooth and adjacent gingiva.

An Experimental Study of Marginal Distortion Related to Heat treatment and Surface Treatment in Metal Copings for Metal-Ceramic Restorations (금속.도재수복물용 금속의 열처리 및 표면처리에 따른 변형에 관한 연구)

  • Kim, Uoong-Chul
    • Journal of Technologic Dentistry
    • /
    • v.14 no.1
    • /
    • pp.45-54
    • /
    • 1992
  • The purpose of this study was to observe the change of marginal distortion related to heat treatment and surface treatment in. Thirty copings were made on the self-curing resin dies and twenty coping among them were treated by heat and surface grinding. All copings were adapted on the respective dies and then were invested into the plastic boxes with tray resin. Both copiong and die invested in tray resin were cut through labio-lingually by a separating disc. This cross-cutting surface was ground and polished. Specimens were mounted on a light microscope and photographed. Marginal discrepancies were measured on photographes by a scale. The obtained results could be summarized in the followings : 1. In all metal copings, the distortion of cervical margin was shown after heat treatment and surface treatment. 2. There were no statistically significant differences in marginal fitness between shoulder and deep chamfer. 3. There were no statistically significant differences in marginal fitness between labial margin and lingual margin in one die. 4. In case of the copings which were not treated with preheating and were treated with surface grinding, the marginal distortion shows a tendency to increase.

  • PDF

Reestablishing the occlusal plane in full mouth rehabilitation patient, using Shilla system (전악수복환자에서 Shilla system을 이용한 교합평면 재구성 증례)

  • Yang, Min-Soo;Vang, Mong-Sook;Park, Sang-Won;Lim, Hyun-Phil;Yun, Kwi-Dug;Yang, Hong-So
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.1
    • /
    • pp.33-38
    • /
    • 2013
  • Occlusal plane is a sagittal expression of dental arch form, and it composes the shape of occlusion, which is one of the most important elements of Maxillo-oral system. In this case, vertical, horizontal coordinates of bionic-median-sagittal plane was produced in articulator, and to achieve relation of left and right position of upper, lower teeth and deficits in alveola, Shilla system was used to reconstruct occlusal plane. In this case, a 41 year-old male patient visited for fracture of 10 unit metal-ceramic fixed partial denture of upper anterior teeth and for overall treatment. Clinical, radiographical, model examination was held, full mouth rehabilitation was achieved by placing dental implant. Maxillo-oral relation was recorded using Gothic arch Tracer complex and were mounted. And for the next step, we estimated original occlusal plane using Shilla system. After analysis we produced diagnosis wax pattern. On the basis of this, radiography stent was manufactured and dental implant was placed, and temporary prosthesis was made by using diagnosis wax pattern. Cross mounting and anterior guiding table were performed in order to reproduce temporary restoration morphology and bite pattern, followed by final restoration made of all ceramic crown with zirconia coping. As stated above, appropriately esthetic and functional results can be seen in using Shilla system in diagnosis and treatment procedure of full mouth rehabilitation patient.

Influence of porcelain re-firing on the formation of surface bubble and on the change in shade of metal-ceramic crown exposed to artificial saliva (인공타액에 노출되었던 금속도재관의 재소성이 색조와 표면기포 형성에 미치는 영향에 관한 연구)

  • Park, Ji-Hyun;Yeo, In-Sung;Kim, Sung-Hun;Han, Jung-Suk;Lee, Jai-Bong;Yang, Jae-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.2
    • /
    • pp.161-167
    • /
    • 2011
  • Purpose: The purpose of this study was to evaluate the influence of porcelain re-firing on the formation of surface bubble and on the change in shade of metal-ceramic crown exposed to artificial saliva. Materials and methods: Thirty disk-shaped specimens were made in 10 mm diameter with 0.5 mm metal core thickness and 1 mm ceramic thickness. A spectroradiometer was used to determine the CIE Lab coordinates. The number and size of surface bubble were observed with a stereomicroscope. After the exposure to artificial saliva for 7 days, re-firing was performed at glazing temperature. After re-firing, the CIE Lab were calculated, and the number and size of surface bubble were observed again. The change in shade was expressed with ${\Delta}E$. Statistical analysis was done with paired t-test for the change in the number of surface bubble and student t-test for the change in the size of surface bubble (${\alpha$}=0.05). Results: Shade difference was calculated 2.14 ${\Delta}E$ units. The mean number of surface bubble was $1.33{\pm}1.49$ before re-firing, $3.27{\pm}2.90$ after re-firing. After re-firing, the number of surface bubble was significantly increased (P<.05). The mean size of surface bubble was $81.97{\pm}32.03\;{\mu}m$ before re-firing, $142.94{\pm}47.40\;{\mu}m$ after re-firing. After re-firing, the size of surface bubble was significantly increased (P<.05). Conclusion: Shade change after re-firing was perceptible (${\Delta}E$ < 2.0) and clinically acceptable (${\Delta}E$ < 3.7). The number and size of surface bubble was significantly increased after re-firing. Further investigation to decrease the surface bubble on the extra oral repair of metal-ceramic crown, will be needed in future study.

The effect of resin cements and primer on retentive force of zirconia copings bonded to zirconia abutments with insufficient retention

  • Kim, Seung-Mi;Yoon, Ji-Young;Lee, Myung-Hyun;Oh, Nam-Sik
    • The Journal of Advanced Prosthodontics
    • /
    • v.5 no.2
    • /
    • pp.198-203
    • /
    • 2013
  • PURPOSE. The purpose of this study was to investigate the effect of resin cements and primer on the retentive force of zirconia copings bonded to zirconia abutments with insufficient retention. MATERIALS AND METHODS. Zirconia blocks (Lava, 3M ESPE, St. Paul, MN, USA) were obtained and forty sets of zirconia abutments and copings were fabricated using CAD/CAM technology. They were grouped into 4 categories as follows, depending on the types of resin cements used, and whether the primer is applied or not:Panavia F2.0 (P), Panavia F2.0 using Primer (PRIME Plus, Bisco Inc, Schaumburg, IL, USA) (PZ), Superbond C&B (S), and Superbond C&B using Primer (SZ). For each of the groups, the cementation was conducted. The specimens were kept in sterilized water ($37^{\circ}C$) for 24 hours. Retentive forces were tested and measured, and a statistical analysis was carried out. The nature of failure was recorded. RESULTS. The means and standard deviations of retentive force in Newton for each group were $265.15{\pm}35.04$ N (P), $318.21{\pm}22.24$ N (PZ), $445.13{\pm}78.54$ N (S) and $508.21{\pm}79.48$ N (SZ). Superbond C&B groups (S & SZ) showed significantly higher retentive force than Panavia F2.0 groups (P & PZ). In Panavia F2.0 groups, the use of primer was found to contribute to the increase of retentive force. On the other hand, in Superbond C&B groups, the use of primer did not influence the retention forces. Adhesive failure was observed in all groups. CONCLUSION. This study suggests that cementation of the zirconia abutments and zirconia copings with Superbond C&B have a higher retentive force than Panavia F2.0. When using Panavia F2.0, the use of primer increases the retentive force.

Fracture load and marginal fitness of zirconia ceramic coping by design and coloration (유색 및 백색 지르코니아 세라믹 코핑의 코핑 디자인에 따른 파절 하중과 변연 적합성)

  • Shin, Mee-Ran;Kim, Min-Jeong;Oh, Sang-Chun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.4
    • /
    • pp.406-415
    • /
    • 2009
  • Purpose: The purpose of this study was to compare the marginal fitness and fracture load of the zirconia copings according to the design with different thickness and coloration. Material and methods: The evaluation was based on 80 zirconia copings. Zirconia copings were fabricated in design with different thicknesses using CAD/CAM system (Everset, KAVO dental GmbH, Biberach, Germany). The designs of copings were divided into four groups. The first group consisted of copings with uniform thickness of 0.3 mm. The thickness in the second group was 0.3 mm on the buccal surface and 0.6 mm on the lingual surface. The third group consisted of coping with uniform thickness of 0.6 mm. The thickness in the fourth group was 0.6 mm on the buccal surface and 1mm on the lingual surface. Each group consisted of 10 colored and 10 uncolored copings. Half of the copings (40) processed with a milling system according to the specific design were sent to be given a color (A3) through saturation in special dye by a manufacturing company. Just after sintering, the marginal discrepancies of copings were measured on the buccal, lingual, mesial and distal surfaces of metal die, under a Video Microscope System (sv-35, Sometech, Seoul, Korea) at a magnification of $\times$ 100. It was remeasured after the adjusting of the inner surface. Next, all copings were luted to the metal dies using reinforced cement {GC FujiCEM (GC Corp. Tokyo, Japan)} and mounted on the testing jig in a Universal Testing Machine (Instron 4467, Norwood, MA, USA). The results were analyzed statistically using the one-way ANOVA test. Results: The obtained results were as follow: 1. The measured value of marginal discrepancy right after sintering was the greatest in the contraction of the buccal area in all groups, except for group I2. 2. There was no significant difference of marginal fitness among the groups in the colored zirconia group (P<.05). 3. When the marginal fitness among the groups in the uncolored zirconia group was considered, group II2 had the smallest marginal discrepancy. 4. When the colored and uncolored groups with the same design were compared, there was a significant difference between I1 and II1 groups. In group 2, 3, and 4, the uncolored zirconia had the greatest marginal fitness (P<.05). 5. After adjustment of inner surface, there was no significant difference in the marginal fitness in all groups when color and design of the zirconia coping were compared. 6. The fracture load of CAD/CAM zirconia copings showed significant difference in group 1, 2, 3, and 4. I4 and II4 had the strongest fracture load. 7. When groups with different color and same design were compared, all colored groups showed greater fracture load (P>.05), with no significance. Conclusion: There was difference in the marginal fitness according to the design and coloration of zirconia copings right after sintering, but it was decided that the copings may well be used clinically if the inner surface are adjusted. The copings should be thick enough for the reinforcement of fracture strength. But considering the esthetics of the visible surfaces (labial and buccal surface), the thickness of copings may be a little thin, without giving any significant effect on the fracture strength. This type of design may be considered when giving priority to preservation of tooth or esthetics.

Comparative evaluation of marginal and internal fit of metal copings fabricated by various CAD/CAM methods (다양한 CAD/CAM 방식으로 제작한 금속하부구조물 간의 변연 및 내면 적합도 비교 연구)

  • Jeong, Seung-Jin;Cho, Hye-Won;Jung, Ji-Hye;Kim, Jeong-Mi;Kim, Yu-Lee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.3
    • /
    • pp.211-218
    • /
    • 2019
  • Purpose: The purpose of the present study was to compare the accuracy of four different metal copings fabricated by CAD/CAM technology and to evaluate clinical effectiveness. Materials and methods: Composite resin tooth of the maxillary central incisor was prepared for a metal ceramic crown and duplicated metal die was fabricated. Then scan the metal die for 12 times to obtain STL files using a confocal microscopy type oral scanner. Metal copings with a thickness of 0.5 mm and a cement space of $50{\mu}m$ were designed on a CAD program. The Co-Cr metal copings were fabricated by the following four methods: Wax pattern milling & Casting (WM), Resin pattern 3D Printing & casting (RP), Milling & Sintering (MS), Selective laser melting (SLM). Silicone replica technique was used to measure marginal and internal discrepancies. The data was statistically analyzed with One-way analysis of variance and appropriate post hoc test (Scheffe test) (${\alpha}=.05$). Results: Mean marginal discrepancy was significantly smaller in the Group WM ($27.66{\pm}9.85{\mu}m$) and Group MS ($28.88{\pm}10.13{\mu}m$) than in the Group RP ($38.09{\pm}11.14{\mu}m$). Mean cervical discrepancy was significantly smaller in the Group MS than in the Group RP. Mean axial discrepancy was significantly smaller in the Group WM and Group MS then in the Group RP and Group SLM. Mean incisal discrepancies was significantly smaller in the Group RP than in all other groups. Conclusion: The marginal and axial discrepancies of the Co-Cr coping fabricated by the Wax pattern milling and Milling/Sintering method were better than those of the other groups. The marginal, cervical and axial fit of Co-Cr copings in all groups are within a clinically acceptable range.

Comparison of the Marginal and Internal Fit on the Cast and CAD-CAM Cores (주조에 의한 Core와 CAD-CAM에 의한 Core의 적합도 비교평가)

  • Han, Man-So;Kim, Ki-Baek
    • Journal of dental hygiene science
    • /
    • v.12 no.4
    • /
    • pp.368-374
    • /
    • 2012
  • Dental CAD (computer-aided design)/CAM (computer-aided manufacturing) systems facilitate the use of zirconia core for all-ceramic crown. The purpose of this study was to evaluate the marginal and internal fit of zirconia core fabricated using a dental CAD/CAM system and to compare the fit of metal cores by a conventional method. Ten identical cases of single coping study models (abutment of teeth 11) were manufactured and scanned. Ten zirconia cores were fabricated using dental CAD/CAM system. An experienced dental technician fabricated 10 samples of metal cores for the control group using the lost wax technique. Marginal and internal fit was measured by the silicone replica technique. Fit was measured with magnification of 160 using a digital Microscope. Margin, rounded chamfer, axial wall and incisal fits were measured for comparison. T-test of independent sample for statistical analysis was executed with SPSS 12.0 for Windows (SPSS Inc., Chicago, IL, USA) (${\alpha}$=0.05). The mean (SD) for marginal, rounded chamfer, axial wall and incisal were: $97.0\;(25.3){\mu}m$, $104.0\;(22.0){\mu}m$, $59.6\;(21.4){\mu}m$ and $124.8\;(33.3){\mu}m$ for the zirconia core group, and $785.2\;(18.4){\mu}m$, $83.8\;(15.1){\mu}m$, $42.7\;(9.6){\mu}m$ and $83.4\;(14.4){\mu}m$ for the metal core group. T-test showed significant differences between groups for margin (p<.001), rounded chamfer (p<.001), axial wall (p<.001) and incisal (p<.001). But zirconia core group observed that the marginal and internal fit values in the present study were within clinically acceptable range.