• 제목/요약/키워드: Casting Technique

검색결과 277건 처리시간 0.027초

치과보철영역에 레이저 이용을 위한 이론적 고찰 (A study of introduction for using Laser in dental prosthesis)

  • 박명호;배봉진;이화식
    • 대한치과기공학회지
    • /
    • 제30권1호
    • /
    • pp.131-139
    • /
    • 2008
  • It's very important to find the most appropriate adhesion technique available, taking into consideration factors such as biocompatibility, non-corrosiveness, mechanical stability, etc. Laser welding is the best choice you can make because from a mechanical viewpoint, a laser welded surface has better particle structure than does a casted particle structure. Furthermore, it requires no additional material and the same metal alloy which is used when casting can be used. Therefore, the resulting mixture will consist of a single alloy, instead of utilizing different alloy combinations. Another benefit is the low economic cost. The most beneficial aspects of laser welding is that it is biologicallly friendlly, doesn't require soldering, can fuse different metal alloys together, and can weld on heat-sensitive spots(E.g. around resin or ceramic). A consistent strong pulse is possible. This technique is capable of welding on master models and creates accurate welds. It is capable of due to its stronger, non-corrosive microscope, which allows 25times magnification during the soldering process. This is possible because of its high stability from the tiny particle structure.

  • PDF

레이저선택용융기술에 의해 제작된 금속 코어의 변연 적합도 분석 (An analysis of marginal adaptation of metal cores fabricated by selective laser sintering)

  • 김원수;김기백
    • 대한치과기공학회지
    • /
    • 제38권4호
    • /
    • pp.305-311
    • /
    • 2016
  • Purpose: The purpose of this study were to analysis of marginal adaptation of metal cores fabricated by selective laser sintering. Methods: Main model was prepared and ten stone models were fabricated. Ten single metal cores were fabricated by selective laser sintering(SLS group) and another ten single metal cores using lost wax technique and casting method were manufactured(CAST group). The marginal adaptation of metal cores were analysis using by the silicone replica technique. Silicone replicas were sectioned two times. The marginal adaptations were measured using by digital microscope. Statistical analyses was performed with independent t-test(${\bullet}{\cdot}=0.05$). Results: Means of marginal adaptations were 90.3 ${\ss}{\uparrow}$ for SLS group and 65.1 ${\ss}{\uparrow}$ for CAST group. Two groups were statistically significant differences (p < 0.05). Conclusion: Marginal adaptation of metal cores fabricated by selective laser sintering were ranged within the clinical recommendation.

제강공정에서 수소의 거동 (Hydrogen Behavior in the Steelmaking Process)

  • 심상철;조중욱;황상택;김광천
    • 대한금속재료학회지
    • /
    • 제46권10호
    • /
    • pp.662-671
    • /
    • 2008
  • The behavior of hydrogen in the steel making process was investigated. The relation between the composition of ladle slag and hydrogen concentration in molten steel was considered. The hydrogen distribution ratio between ladle slag and molten steel was increased with increasing basicity of the slag; it was about 20 when the basicity of slag was 15. Hydroxyl capacity measured from the hydrogen distribution ratio between slag and the molten steel was comparatively corresponding to the value of hydroxyl capacity measured by the equilibrium reaction of slag and $H_2O$ gas. However, it is considerably different from the value calculated by regular solution model. The influence of hydrogen on a sticking type breakout is considered. The effect of hydrogen and $H_2O$ gas on the crystallization behavior of mold powder was investigated by DHTT (Dual hot thermocouple technique). As a result, it was proved that mold powder could be crystallized by $H_2O$ gas in the atmosphere. Therefore, it is concluded that $H_2O$ gas in the atmosphere can be a possible cause of the sticking type breakout that occasionally occurs in the continuous casting process.

치과용 3D 프린터를 활용해 제작된 레진 단일치관보철의 변연적합 평가 (An evaluation of marginal fit of resin single crown manufactured using a dental 3D printer)

  • 김기백
    • 대한치과기공학회지
    • /
    • 제44권4호
    • /
    • pp.126-131
    • /
    • 2022
  • Purpose: The purpose of this study is to evaluate the quality of dental fixed prostheses fabricated by 3DP (three-dimensional printing). Methods: Ten main models were prepared for the study. Ten specimens were printed by 3DP (3DP group). Ten specimens were fabricated by the lost wax technique and casting method to complete the control group (LWC group). The marginal fit was measured for 20 specimens. The measurement of marginal fit was performed using the silicon replica technique. Finally, the marginal fit of 10 specimens from each group was calculated. An independent sample t-test was run to see if the calculated averages for the two groups were mutually significant (α=0.05). Results: According to the experimental results, the mean marginal fit of the 3DP group was 71.9 ㎛, and the LWC group was 55.3 ㎛. The means of the two groups were found to be significantly different (p<0.001) in the results of the independent sample t-test. Conclusion: The marginal fit of fixed dental prostheses produced by 3DP technology was examined with values greater than those fabricated by traditional technology. However, as it appeared to be a value within the range of clinically acceptable range recommended by numerous studies, it was determined that clinical application would be feasible.

모사 슬러리 용액에서 정전류 분극을 활용한 고크롬 주철 부식 시험 (Corrosion Tests for High Chromium Cast Iron Using Galvanostatic Polarization Technique in a Simulating Slurry Solution)

  • 바산자프 오취개럴;이준섭;이예진;오준석;이재현
    • Corrosion Science and Technology
    • /
    • 제22권4호
    • /
    • pp.252-256
    • /
    • 2023
  • The galvanostatic polarization technique was used to accelerate corrosion in high chromium cast iron (HCCI) immersed in a simulated slurry solution of 0.1 mol dm-3 H2SO4, 0.05 mol dm-3 HCl, and 10 wt% SiC. The HCCI contained 27 wt% of Cr and 2.8 wt% of C, and its microstructure mainly comprised austenitic and carbide phases. A two-electrode system using a dense carbon rod and the HCCI sample was employed for the galvanostatic polarization by applying an anodic current for 24 hours. The corrosion rate increased upon applying the anodic current, but the increase was not significant, particularly for current densities higher than 10 µA cm-2. Following polarization, the corrosion morphology revealed that the anodic current accelerated surface corrosion in the HCCI; however while the depth of the corroded area increased, the increase was not substantial. The propagation behavior of the anodic current and its impact on corrosion were further discussed.

금강하구 퇴적변화 및 통행지장에 관한 후측모의 (Hind-casting Simulation of Sedimentation Changes and Passage Hindrance In Keum River Estuary)

  • 서승원
    • 한국해안해양공학회지
    • /
    • 제16권4
    • /
    • pp.224-232
    • /
    • 2004
  • 지난 20여년간 다양한 공사가 시행된 금강하구에서 퇴적으로 인한 수로매몰을 분석하기 위하여 1988년부터 2000년까지 매 2년 간격으로 7가지 경우에 대해 단계별로 수치수동역학모형을 적용한 후측실험이 실시되어 바닥마찰응력의 변화와 상관된 퇴적율 평가가 실시되었다. 금강하구둑 건설로 최대마찰응력장이 약 $1-2N/m^2$ 에서 $0.2-0.6N/m^2$크게 줄어들고, 특히 1994년 금강하구둑의 수문 폐쇄 이후에 장항수로에서는 해저마찰응력이 한계마찰응력으로 제시된 $0.4N/m^2$ 이하로 급감하면서 퇴적환경으로 전이되고 있는 것으로 분석되었다. 하구둑건설은 금강 상류로 전파되는 조석에너지를 차단함으로써 조석수동역학의 급격한 변화를 초래하고 하구둑 전면에 퇴적환경이 급속도로 진행되는 직접적인 원인을 제공하고 있는 것으로 추론되었다. 소형어선의 통행지장을 겪는 장항수로의 매몰평가는 평균대조 조석을 적용하여 분석한 결과 기존에 비해 20% 이상 통행지장을 받는 것으로 평가되었다.

다중 임계치를 적용한 웨이브릿 기반 디지털 워터마킹 기법 (Wavelet-based Digital watermarking Using Multiple threshold)

  • 김재원;남재열
    • 정보처리학회논문지B
    • /
    • 제10B권4호
    • /
    • pp.419-428
    • /
    • 2003
  • 디지털 멀티미디어 데이터에 대한 소유권 문제가 근래에 중요한 문제로 대두되면서 이를 효율적으로 보호할 수 있는 기술적 해결책으로 디지털 워터마킹에 대한 연구가 활발히 진행되어져 왔다. 본 연구에서는 디지털 영상 데이터에 대해 다양한 공격에 강인한 웨이브릿 기반 워터마킹 알고리즘을 제안한다. 웨이브릿 변환을 이용하여 워터마킹된 영상의 변화를 감지 못하도록 하면서 시각적으로 중요한 영역에 워터마크를 삽입하여 일반적인 영상 신호 처리에 강인한 워터마킹 방법을 제시한다. 웨이브릿 변환된 계수의 레벨과 각 부대역별 특성을 고려하고, 영상의 복잡도를 반영한 다중 임계치를 적용하여 원본영상과 워터마킹된 영상이 시각적으로 차이가 없도록 가우시안 랜덤 수열(Gaussian Random Sequence)을 워터마크로 삽입한다. 제안된 알고리즘의 성능을 여러 영상에 대하여 실험해 본 결과 워터마크가 삽입된 영상이 시각적으로 전혀 구별할 수 없을 정도의 비가시도를 보이면서 다양한 공격, 즉 JPEG 손실압축, 필터링, 잡음첨가, 리샘플링, 크로핑 등에 대하여 우수한 워터마크 검출결과와 강인함을 보였다.

Manufacturing Techniques of Ancient Metal Buddha Statues from Archaeological Sites in Bagan, Myanmar

  • Lee, Jae Sung;Win, Yee Yee;Lee, Bonnie;Yu, Jae Eun
    • 보존과학회지
    • /
    • 제35권4호
    • /
    • pp.309-316
    • /
    • 2019
  • This study intends to identify manufacturing techniques, including casting and alloy composition, of nine metal Buddha statues excavated from archaeological sites in Bagan, Myanmar. Two Buddha statues from Pyu city state(2nd to 9th century) contain Cu-Sn alloy(including <1 wt% Fe), with different relatively high percentages of Sn(16 wt% and 25 wt%) identified from each Buddha statue, and no Pb detected. Five Buddha statues from the Bagan dynasty contain various alloy ratios of Cu-Sn(including <1 wt% Pb), Cu-Sn-Pb, and Cu-Sn-Zn-Pb. All Buddha statues appear to be fabricated by casting, as there is no evidence of other heat treatments. The silver Buddha statue manufactured in the 18th century includes >1% Cu besides silver with no additional metallic components identified. The bronze Buddha statue manufactured in the Konbaung dynasty(18th century) is of Cu-Sn-Pb alloy. The Buddha statues of Pyu was alloy of Cu-Sn without Pb including ahigh percentage of The Buddha statues of both the Bagan and Konbaung dynasties are comprised of ternary Cu-Sn-Pb alloys, with a heterogeneous distribution of lead and tin. Some of Buddha statues of the Bagan dynasty have similar alloy ratios as those of Pyu, suggesting that similar manufacturing techniques were used.

Eco-friendly Fabrication Process of Al-Ti-C Grain Refiner

  • Cho, Hoon;Kim, Bong-Hwan
    • 한국주조공학회지
    • /
    • 제30권4호
    • /
    • pp.147-150
    • /
    • 2010
  • 알루미늄 합금의 미세조직 개량을 위한 목적으로 사용되는 Al-Ti-B 합금계의 미세화제는 재활용 과정에서 붕소(B)의 농축(Agglomeration) 문제 및 Zr, Si, Cr 등을 함유하는 합금에서 미세화 효과가 급격히 감소하는 Poisoning effect 등이 지적되어 왔다. 최근에는 이를 대체할 수 있는 Al-Ti-C 합금계의 미세화제에 대한 연구가 활발한데 이는 TiC가 용탕 내에서 ${\alpha}$-Al의 핵생성처로 직접 작용하는 점에 착안한 것이다. 한편, 이들 Al-Ti-B, Al-Ti-C 계의 미세화제는 그 제조공정에서 $K_2TiF_6$를 이용함에 따라 불소함유 유해가스를 배출하여 환경 문제를 야기하고, 이를 포집/정화하기 위한 추가설비를 요구하게 된다. 따라서 대기 환경 오염 및 경제성 측면에서 유리한 미세화제의 친환경 제조기술에 대한 개발이 필요한 시점이다. 본 연구에서는 $K_2TiF_6$를 사용하지 않고 용탕 내의 자발적 반응을 이용하여 환경 및 경제적 측면에서 유리한 Al-Ti-C 미세화제를 개발하고자 하였다. A3003 합금을 대상소재로 하여 개발된 Al-Ti-C 미세화제와 상용 Al-Ti-B 미세화제의 미세화 도달시간 및 fading 발생 등을 비교하였다. 본 연구를 통하여 개발된 Al-8.6Ti-0.025C 미세화제는 상용 Al-Ti-B 미세화제 보다 적은 첨가량에도 유사한 미세화 성능을 나타내었으며 용탕 유지시간 100분까지도 fading이 발생하지 않는 것을 확인하였다.

당뇨병성 족부 궤양에서 고 농도 은($Ag^+$) 도포 포말 드레싱을 이용한 전 접촉 석고 붕대 치료 결과 (The Result of Total Contact Cast with High Concentrate Silver ($Ag^+$) Coated Foam Dressing in Diabetic Foot Ulcers)

  • 김재영;최재혁;이경태;양기원;김진수;이재준
    • 대한족부족관절학회지
    • /
    • 제10권2호
    • /
    • pp.250-254
    • /
    • 2006
  • Purpose: The treatment of diabetic foot ulcers with total contact cast has been reported to be associated with numerous undesirable complications. This study shows that our technique of total contact casting that incorporates high concentration silver coated foam dressing. Materials and Methods: Forty-four diabetic foot ulcers were treated with total contact cast along with high concentration silver coated foam dressing. Complication and healing rates were evaluated. Results: Eighty five percent of the ulcers healed within 6 weeks with an overall complication rate of 7%. There were only two cases (5%) of infection and no recurrent ulceration and no another site new pressure ulcer in our study. Conclusion: Total contact casting incorporates high concentration silver coated foam dressing resulted in fewer complications rate and healing rate that is comparable to other studies.

  • PDF