HE-CVD법에 의한 Diamond/WC-Co 박막합성 (The Synthesis of Diamond/WC-Co Thin Film by HE-CVD)

  • 이기선;서성만;신동욱;김동선
    • 한국자원리싸이클링학회:학술대회논문집
    • /
    • 한국자원리싸이클링학회 2003년도 추계정기총회 및 국제심포지엄
    • /
    • pp.185-189
    • /
    • 2003
  • The effect of surface roughness of the substrate on HF-CVD diamond coating was researched. The surface roughness was changed variously by electro-chemical etching conditions. The etching process acted to remove the metallic cobalt from the WC-Co. Diamond nucleation density was higher in etched the substrate. Therefore, the etching process was effective in both Co-removal and higher surface roughness, leading to the improving the diamond nucleation and deposition.

  • PDF

a-plane 사파이어기판에 증착된 Polycrystalline Diamond 박막의 특성 (Characteristics of a Polycrystalline Diamond Thin Film Deposited on a-plane Sapphire Substrate)

  • 싱얀탄;장태환;권진욱;김태규
    • 한국표면공학회지
    • /
    • 제53권3호
    • /
    • pp.109-115
    • /
    • 2020
  • In this study, polycrystalline diamond was synthesized by chemical vapor deposition (CVD). Diamond films were deposited on a-plane sapphire substrates while changing the concentration of methane for hydrogen (CH4/H2), and the concentrations of methane were 0.25, 0.5, 1, 2, 3 and 4 vol%, respectively. Crystallinity and nucleation density according to changes in methane concentration were investigated. At this time, the discharge power, vacuum pressure, and deposition time were kept constant. In order to deposit polycrystalline diamond, the sapphire substrate was etched with sulfuric acid and hydrogen peroxide (ratio 3:7), and the sapphire surface was polished for 30 minutes with 100 nm-sized nanodiamond particles. The deposited diamond thin film was analyzed by a scanning electron microscope (SEM), a Raman spectra, Atomic force microscope (AFM) and an X-ray diffractometer (XRD). By controlling the ratio of methane to hydrogen and performing appropriate pre-treatment conditions, a polycrystalline diamond thin film having excellent crystallinity and nucleation density was obtained.

다이아몬드 박막기술 (Diamond Thin Film Technology)

  • 이지화
    • 공업화학
    • /
    • 제1권1호
    • /
    • pp.11-22
    • /
    • 1990
  • 다이아몬드가 준안정상태로 존재하는 조건(저압 및 저온) 하에서 화학증착시키는 방법이 80년대에 개발되어 새로운 다이아몬드 코팅기술로 등장하고 있다. 여기서는 여러가지 CVD 방법을 장단점과 함께 소개하였다. 다이아몬드 박막의 성장에 관련된 반응기구와 수소원자의 역할을 논하였으며, 또 장래의 연구분야와 응용을 전망하였다.

  • PDF

마이크로웨이브 플라즈마 CVD에 의한 나노결정질 다이아몬드 박막 성장 시 DC 바이어스 효과 (Effect of DC Bias on the Growth of Nanocrystalline Diamond Films by Microwave Plasma CVD)

  • 김인섭;강찬형
    • 한국표면공학회지
    • /
    • 제46권1호
    • /
    • pp.29-35
    • /
    • 2013
  • The effect of DC bias on the growth of nanocrystalline diamond films on silicon substrate by microwave plasma chemical vapor deposition has been studied varying the substrate temperature (400, 500, 600, and $700^{\circ}C$), deposition time (0.5, 1, and 2h), and bias voltage (-50, -100, -150, and -200 V) at the microwave power of 1.2 kW, working pressure of 110 torr, and gas ratio of Ar/1%$CH_4$. In the case of low negative bias voltages (-50 and -100 V), the diamond particles were observed to grow to thin film slower than the case without bias. Applying the moderate DC bias is believed to induce the bombardment of energetic carbon and argon ions on the substrate to result in etching the surfaces of growing diamond particles or film. In the case of higher negative voltages (-150 and -200 V), the growth rate of diamond film increased with the increasing DC bias. Applying the higher DC bias increased the number of nucleation sites, and, subsequently, enhanced the film growth rate. Under the -150 V bias, the height (h) of diamond films exhibited an $h=k{\sqrt{t}}$ relationship with deposition time (t), where the growth rate constant (k) showed an Arrhenius relationship with the activation energy of 7.19 kcal/mol. The rate determining step is believed to be the surface diffusion of activated carbon species, but the more subtle theoretical treatment is required for the more precise interpretation.

고주파 플라즈마 CVD 다이아몬드 박막의 합성시 첨가된 산소의 효과 (The effect of oxygen in RF PACVD diamond thin film)

  • 김대일;이상희;이병수;박종관;박상현;김보열;우호환;이덕출
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.786-788
    • /
    • 1998
  • Synthetic diamond films were deposited on pretreated silicon substrate in activated gas phase using RF plasma-assisted CVD. We investigated the influence of $O_2$ gas on facets of diamond crystal. In $H_2-CH_4-O_2$ gas mixture, the increase of oxygen concentration lead to well-faceted diamond particles and increasing crystallinity of diamond films. The deposited diamond films were analyzed by SEM, XRD, Raman spectroscopy.

  • PDF

플라즈마 CVD 법을 이용한 대면적 균일한 비정질 탄소 막 증착 (Large-area Uniform Deposition of Amorphous Hydrogenated Carbon Films using a Plasma CVD Method)

  • 윤상민;양성채
    • 한국전기전자재료학회논문지
    • /
    • 제22권5호
    • /
    • pp.411-414
    • /
    • 2009
  • It has been investigated for the film uniformity and deposition rate of a-C:H films on glass substrate and polymeric materials in the presence of the modulated crossed magnetic field. We used Plasma CVD, i.e, using a crossed electromagnetic field, for uniform depositing thin film. The optimum discharge condition has been discussed for the gas pressure, the magnetic flux density and the distance between substrate and electrodes, As a result, it is found that the optimum discharge conditions are $CH_4$ concentration $CH_4$=10 %, modulated magnetic flux density B=48 Gauss, pressure P=100 mTorr, discharge power supply voltage V=l kV under these experimental conditions. By using these experimental condition, it is possible to prepare the most uniform film extends over about 160 mm of the film width. In this study, we deposited a-C:H thin film on glass substrate, and have a plan that using this condition, study depositing a-C:H thin film on polymeric substrate in next studies.

고주파 플라즈마 CVD에 의한 $\textrm{H}_2$-$\textrm{CH}_4$ 계로부터 다이아몬드 박막의 합성 (Synthesis of Diamond Thin Film by RF PACVD from $\textrm{H}_2$-$\textrm{CH}_4$ Mixed Gas)

  • 임헌찬
    • 전자공학회논문지T
    • /
    • 제36T권3호
    • /
    • pp.13-18
    • /
    • 1999
  • 다이아몬드 박막은 RF PACVD법에 의해 수소와 메탄으로부터 실리콘 웨이퍼 상에 성장되어졌다. 박막 성장 전에 표면의 핵생성 밀도를 증가시키기 위하여 1㎛의 다이아몬드 페이스트로 기계적 흡집을 내어 사용하였다. 메탄 농도를 변화시켜 제작한 박막에 대한 평가는 XRD, SEM 및 Raman Spectroscopy에 의해 이루어졌다. 성장된 박막의 결정성은 메탄 농도가 낮을수록 증가되었다.

  • PDF

Charged Cluster Model as a New Paradigm of Crystal Growth

  • Nong-M. Hwang;In-D. Jeon;Kim, Doh-Y.
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 2000년도 Proceedings of 2000 International Nano Crystals/Ceramics Forum and International Symposium on Intermaterials
    • /
    • pp.87-125
    • /
    • 2000
  • A new paradigm of crystal growth was suggested in a charged cluster model, where charged clusters of nanometer size are suspended in the gas phase in most thin film processes and are a major flux for thin film growth. The existence of these hypothetical clusters was experimentally confirmed in the diamond and silicon CVD processes as well as in gold and tungsten evaporation. These results imply new insights as to the low pressure diamond synthesis without hydrogen, epitaxial growth, selective deposition and fabrication of quantum dots, nanometer-sized powders and nanowires or nanotubes. Based on this concept, we produced such quantum dot structures of carbon, silicon, gold and tungsten. Charged clusters land preferably on conducting substrates over on insulating substrates, resulting in selective deposition. if the behavior of selective deposition is properly controlled, charged clusters can make highly anisotropic growth, leading to nanowires or nanotubes.

  • PDF

ZnO/나노결정다이아몬드 적층 박막 SAW 필터 (SAW Filter Made of ZnO/Nanocrystalline Diamond Thin Films)

  • 정두영;강찬형
    • 한국표면공학회지
    • /
    • 제42권5호
    • /
    • pp.216-219
    • /
    • 2009
  • A surface acoustic wave (SAW) filter structure was fabricated employing $4{\mu}m$ thick nanocrystalline diamond (NCD) and $2.2{\mu}m$ thick ZnO films on Si wafer. The NCD film was deposited in an $Ar/CH_4$ gas mixture by microwave plasma chemical vapor deposition method. The ZnO film was formed over the NCD film in an RF magnetron sputter using ZnO target and $Ar/O_2$ gas. On the top of the two layers, copper film was deposited by the RF sputter and inter digital transducer (IDT) electrode pattern (line/space : $1.5/1.5{\mu}m$) was defined by the photolithography including a lift-off etching process. The fabricated SAW filter exhibited the center frequency of 1.66 GHz and the phase velocity of 9,960 m/s, which demonstrated that a giga Hertz SAW filter can be realized by utilizing the nanocrystalline diamond thin film.