Effect of Pb dopped on BiSrCaCuO system (BiSrCaCuO계의 Pb첨가 효과)

  • Han, Tae-Heui;Park, Sung-Jin;Hwang, Jong-Sun;Kim, Dong-Pil;Han, Byoung-Sung
    • Proceedings of the KIEE Conference
    • /
    • 1991.11a
    • /
    • pp.269-273
    • /
    • 1991
  • High Tc oxide superconductor with a Tc above 100 K has been successfully prepared by solid state reaction method in added-Pb BiSrCaCuO system. As compared with 123 compound, the formation reaction of the high Tc requires long time heat treatment. It is due to the transformation from the low Tc phase to high Tc phase. The sintering just below the melting point of the calcined powder mixture is effective on the formation of the high Tc phase in BiSrCaCuO system to be added with Pb. The growth of the high Tc superconducting phase has a thin plate shape, which is characterized by the c parameter of 37${\AA}$. The formation kinetics is also investigated in the samples with different Bi/Pb ratio and the 30% Pb addition is most preferable for the formation of the high Tc phase. The formation of the high Tc phases is delayed by the excessive addition of Pb. The lattice parameter(c) of the unit cell(both the low and high Tc phases) is increased with increase of Pb.

  • PDF

Preparation of High Tc Superconductor Powders by Emulsion Drying Method (Emulsion 건조방법에 의한 고온초전도체 분말제조)

  • Eom, Woo-Sik;Kim, Ho-Gi
    • Korean Journal of Materials Research
    • /
    • v.1 no.2
    • /
    • pp.71-76
    • /
    • 1991
  • The superconducting powders in $YBa_2Cu_3O_{7-x}$ and Bi-Pb-Sr-Ca-Cu-O system were easily prepared from water in oil type emulsion by loading each cation into the aqueous phase. In $YBa_2Cu_3O_{7-x}$ system, the superconducting orthorhombic phase was formed by calcining at $750^{\circ}C$ for 10h in $O_2$. The size of the superconducting phase powders was submicron. The density of the sintered specimen using this powders was about 95% of the theoretical density and the resistance sharply decreases at about 90K, In Bi-Pb-Sr-Ca-Cu-O system the low Tc phase($(Bi, Pb)_2Sr_2Ca_1Cu_2O_y$) was formed by calcining at $800^{\circ}C$ for 10h in a low oxygen partial pressure of 1/20 atm The shape of clacined powder is thin plate of which size is about $2\mu\textrm{m}$ and thickness is smaller than $\mu\textrm{m}$. It was observed that the high Tc phase ($(Bi, Pb)_2Sr_2Ca_2Cu_3O_y$) was formed by sintering at $850^{\circ}C$ for 30h in oxygen pressure of 1/20 atm without intermediary grinding. The above sintered sample exhibited superconductivity with a Tc(zero)=105K.

  • PDF

Influence of firing conditions after sintering treatment on superconducting characteristics of Bi(Pb)SrCaCuO system (소결 후 열처리 조건이 Bi(Pb)SrCaCuO계 초전도 특성에 미치는 영향)

  • 박용필;이성우;이준웅
    • Electrical & Electronic Materials
    • /
    • v.4 no.4
    • /
    • pp.293-303
    • /
    • 1991
  • 소결 후 냉각 및 Annealing이 Bi(Pb)SrCaCuO계 초전도체의 특성에 미치는 영향에 대해 연구하였다. 소결 후 시편을 500[.deg.C]에서 5[hr] Annealing함으로써 1)미세조직이 치밀화 되었으며 고온상의 체적비가 증가하였다. 2)임계온도 및 전류밀도 특성이 향상되었다.

  • PDF

A study on the superconducting properties of Bi-Pb-Sr-Ca-Cu-O superconducting wire with cooling conditions. (냉각 조건에 의한 Bi-Pb-Sr-Ca-Cu-O 초전도 선재의 특성 연구)

  • Kim, Min-Ki;Choi, Hyo-Sang;Choi, Sung-Hyan;Park, Sung-Jin;Han, Byoung-Sung
    • Proceedings of the KIEE Conference
    • /
    • 1993.11a
    • /
    • pp.213-215
    • /
    • 1993
  • Silver-sheathed Bi-Pb-Sr-Ca-Cu-O wires by the powder-in-tube method were preparated to study on the superconducting properties with cooling conditions. Superconducting wires were cooled down in the furnace, air and liquid $N_2$ after sintering at $840^{\circ}C$. Critical current density of sample cooled in the furnace is $5.1{\times}10^3\;A/cm^2$ at 77K, zero magnetic field and Jc of sample cooled in the air is very low. 2223 high-Tc superconducting phase of sample cooled in the air was distroyed. Therefore, we knew that superconducting wire need to cool slowly to get the high critical current density.

  • PDF

Magnetic Suspension Effect of BiPbSrCaCuO Superconductor (Bi계 초전도체의 Magnetic Suspension)

  • Lee, Sang-Heon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.101-103
    • /
    • 2001
  • Suspension effect has been studied by using superconductor of BiPbSrCaCuO ceramics containing $Ag_{2}O$ It has been cleared that $Ag_{2}O$ acts as pinning center which plays an important role to the suspension effect. Magnetic repulsive force which affects a superconductor located in magnetic flux from toroidal magnet has been investigated. It has been concluded that the suspension effect arises from the interaction between the pinning effect and the diamagnetic effect.

  • PDF

A Study on the Superconducting prperties of Bi system bulk (Bi system bulk의 superconducting properties)

  • Lee, Sang-Heon
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.59 no.2
    • /
    • pp.352-354
    • /
    • 2010
  • The effects of Au addition on the structure and the superconducting properties of Bi system bulk have been investigated. Au exists in the metalic form in above materials. It does not affect the formation and structure of the BiSrCaCuO(2223) phase. The superconducting transition temperature Tc does not change for $Bi_{1.7}Pb_{0.3}Sr_2Ca_2Cu_3O$ composite However Au doping can make the grains smaller. Metallic Au can make gathers on the grains boundary and lead to the increment of critical transport current density. The current density of $Bi_{1.7}Pb_{0.3}Sr_2Ca_2Cu_3Au_{0.5}O$ was 1000A/$cm^2$ at liquid nitrogen temperature.

Composite Effect of Ag and Au in the $Bi_{1.84}\;Pb_{0.34}\;Sr_{1.91}\;Ca_{2.03}\;Cu_{3.06}\;O_{10+\delta}$(110K Phase) High-Tc Superconductor (Ag와 Au가 혼합된 $Bi_{1.84}\;Pb_{0.34}\;Sr_{1.91}\;Ca_{2.03}\;Cu_{3.06}\;O_{10+\delta}$ 산화물 고온초전도체의 초전도특성)

  • 이민수
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.52 no.6
    • /
    • pp.241-248
    • /
    • 2003
  • $Bi_{1.84}Pb_{0.34}Sr_{1.91}Ca_{2.03}Cu_{3.06}O_{10+\delta}$ high $T_{c}$ superconductors containing Ag as an additive were fabricated by a solid-state reaction method. The superconducting properties, such as the structural characteristics, the critical temperatures, the grain size and the image of mapping on the surface were investigated. Samples with Ag and Au of 50 wt% each were sintered at various temperature(820~$850^{\circ}C$). The structural characteristics, the microstructure of surface and the critical temperature with respect to the each samples were analyzed by XRD and SEM, EDS and four-prove methode respectively. The critical temperature showed the result which the Ag additive samples are higher than Au additive samples. The microstructure of the surface showed the tendency which the Ag additive samples become more minuteness than Au additive samples.

A Study on Fabrication of $Bi_{2}Sr_{2}Ca_{2}Cu_{3}O_{x}$ Superconductor Thick Films on Cu Substrates (동피복 Bi2223 초전도후막 합성에 관한 연구)

  • 한상철;성태현;한영희;이준성;안재원
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07a
    • /
    • pp.478-481
    • /
    • 2002
  • We carried out the experiments for fabricating $Bi_{2}Sr_{2}Ca_{2}Cu_{3}O_{x}$(Bi2223) superconductor thick films on Cu tapes. Cu-free (Bi,Pb)-Sr-Ca-0 powder mixtures were screen- printed on Cu tapes and heat-treated at 840-$860^{\circ}C$ for several minutes in air. Surface microstructures and phases of films were analyzed by XRD and optical microscope. The electric properties of superconducting films were examined by the four probe method. At heat-treatment temperature, the printing layers were in a partially molten state by liquid reaction between CuO in the oxidized copper tape and the precursors which were printed on Cu tapes. During the heat-treatment procedure, it is thought that Bi2223 superconducting particles nucleate at interfaces between Bi2212 phase and liquid.

  • PDF

Development of BiPbAgSrCaCuO Superconductor used diffusion of dual layer and The growth mechanism process of superconducting phase (이중층 시료에서 확산을 이용한 BiPbAgSrCaCuO 초전도체 개발 및 초전도상 성장기구)

  • Choi, S.H.;Gang, H.G.;Yu, H.S.;Yu, J.J.;Choi, M.H.;Kim, M.K.;Choi, H.S.;Han, T.H.;Park, S.J.;Hwang, J.S.;Han, B.S.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1993.05a
    • /
    • pp.22-27
    • /
    • 1993
  • we prepared 70K new BiPbAgSrCaCuO superconductor used diffusion of dual layer which composed of SrCaCuO and BiPbAgCuO compound. This method is used permeation and diffusion on partial melting point of BiPbAgCuO compound. Samples were analyzed by means of X-ray diffraction analysis, Thermal analysis, critical temperature and scanning electron microscopy. It was found that the best results were obtained for spread volume (A:B=1:0.6) and sintring time 210hours.

  • PDF

Effect of Mg Additive in the Bi1.84Pb0.34Sr1.91Ca2.03Cu3.06O10+δ(110 K phase) Superconductors (Bi1.84Pb0.34Sr1.91Ca2.03Cu3.06O10+δ(110 K 상)산화물 고온초전도체에 Mg 첨가에 따른 영향)

  • 이민수
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.6
    • /
    • pp.522-531
    • /
    • 2003
  • Samples with the nominal composition, B $i_{1.84}$P $b_{0.34}$S $r_{1.91}$C $a_{2.03}$C $u_{3.06}$ $O_{10+{\delta}}$ high- $T_{c}$ superconductors containing MgO as an additive were fabricated by a solid-state reaction method. Samples with MgO of 5~30 wt% each were sintered at 820~86$0^{\circ}C$ for 24 hours. The structural characteristics, critical temperature, grain size and image of mapping with respect to MgO contents were analyzed by XRD(X-Ray Diffraction), SEM(Scanning Electron Microscope) and EDS(Energy dispersive X-ray spectrometer) respectively. As MgO contents increased, intensity of MgO Peaks and ratio of Bi-2212 phase in superconductors intensified and the proportion of the phase transition from Bi-2223 to Bi-2212 was increased.