검색결과 97건 처리시간 0.031초

균일침전법을 이용항 Hydroxyapatite 분말의 제조 및 가열변화 (Synthesis of Hydroxyapatite Powders by Homogeneous Precipitation Method and Their Thermal Changes)

  • 이진호;박훈;김창은
    • 한국세라믹학회지
    • /
    • 제33권1호
    • /
    • pp.7-16
    • /
    • 1996
  • ${CO_3}^{2-}$ containing whisker-like hydroxyapatite powders were synthesized byhomogeneous precipitation method using urea, Dicalcium phosphate anhdrate[DCPA; $CaHPO_4$] and octacalcium phosphate [OCP; $Ca_8H_2(PO_4_)6\cdot5H_20$]were obtained as precursors and they transformed to high crystalline hydroxyapatites at pH 5.62, and 6.54 respectively. According to the condition of the final pH in the solutions for the solution products and urea contents OCP was remained. When the solution product of $Ca^{2-}$ and ${PO_4}^{3-}$ was $1.5\times 10^4$[$mM^2$] and the content of urea was 0.25 mol.$dm^{-3}$ well crystallized whisker-like hydroxyapatite tens of micrometer in length was obtained. By heat treatment DCPA and OCP were decomposed into $\beta$-tricalcium phosphate [$\beta$-TCP ; $\beta$-$Ca_3{PO_4}_2$] and $\beta$-dicalcium phosphate [$\beta$-DCP ;$\beta$-$Ca_2P_2O_4}_2$]. And well-crystallized hydroxyapatite was partially decomposed into $\beta$-TCP at $800^{\circ}C$.

  • PDF

두개결손부 모델에서 배양된 골막유래세포를 이용한 골이식 시 지지체로서 TCP의 효과 (EffeCt of tricalcium phosphate (TCP) as a scaffold during bone grafting using cultured periosteum-derived cells in a rat calvarial defect model)

  • 심경미;김세은;김종춘;배춘식;최석화;강성수
    • 한국방사선학회논문지
    • /
    • 제5권1호
    • /
    • pp.11-18
    • /
    • 2011
  • 다능성 세포를 포함하는 골막은 골모세포와 연골세포로 분화될 수 있다. 그리고 배양된 골막유래세포는 골형성 능력을 가지고 있다. 이 연구의 목적은 골막유래 세포들과 골이식재 간의 상호작용을 평가하는 것이다. Sprague-Dawley 랫드의 두개골 골막에서 세포를 분리한 다음, 배양된 골막유래세포를 beta-tricalcium phosphate (${\beta}$-TCP)와 함께 임계결손부 크기의 두개결손부에 이식하였다. 모든 랫드는 골이식 수술 후 8주째에 희생되었으며, 골이식부의 골형성 능력은 일반방사선, micro CT 및 조직검사를 통해 평가되었다. ${\beta}$-TCP와 함께 이식된 골막유래세포는 골결손부에서 더욱 증가된 석회화작용을 나타내었으며, 골결손부 안쪽 및 가장자리에 골밀도 증가와 신생골이 형성되었다. 특히 골막유래세포는 ${\beta}$-TCP만 단독으로 이식하였을때보다 함께 이식 시 효과적으로 신생골을 형성하였다. 이러한 결과는 배양된 골막유래세포가 골결손부에서 골형성을 증진시킬 수 있는 가능성을 보였다.

수열합성법에 의한 calcium phosphates 분말합성 (Preparation of calcium phosphates by hydrothermal synthesis route)

  • 문성욱;이병우
    • 한국결정성장학회지
    • /
    • 제29권5호
    • /
    • pp.203-207
    • /
    • 2019
  • 인산칼슘(hydroxyapatite(HAp), ${\beta}$-tricalcium phosphate(${\beta}$-TCP) 및 HAp와 ${\beta}$-TCP가 혼합된 2상 인산칼슘(BCP, HA/${\beta}$-TCP))들을 수열합성법을 통해 합성하였다. 여러 수열합성 조건(최고온도 $150^{\circ}C$ 및 pH 12 이하)에서 수산화칼슘($Ca(OH)_2$) 수용액과 인산($H_3PO_4$) 용액을 반응시켜 얻은 침전물을 수열합성에 이용하였다. 초기 전구체 Ca/P 비율을 1.30, 1.50 및 1.67로 조절하였으며 이 조성비와 합성 후 열처리가 분말 및 소결체의 상합성에 미치는 영향에 대해 조사하였다. 초기 전구체 Ca/P 비율을 조절함으로써 분말 및 소결체의 상의 조절이 가능하였다. Ca/P 비율이 1.67일 경우 모든 열처리 온도에서 분말 및 소결체 모두에서 HAp 단일 상이 합성되었다. Ca/P 비율이 1.30과 1.50에서 $900^{\circ}C$ 이상 열처리 할 경우 각각 순수한 ${\beta}$-TCP와 BCP(HAp/${\beta}$-TCP)가 합성되었다. 반응성 높은 미세한 분말을 이용하여 소결함으로써 미세한 입경을 가지며 투광성을 가지는 소결체들을 저온에서 얻을 수 있었다.

Microstructure and Biocompatibility of Porous BCP(HA/β-TCP) Biomaterials Consolidated by SPS Using Space Holder

  • Woo, Kee-Do;Kwak, Seung-Mi;Lee, Tack;Oh, Seong-Tak;Woo, Jeong-Nam
    • 한국재료학회지
    • /
    • 제26권8호
    • /
    • pp.449-453
    • /
    • 2016
  • $HA(hydroxyapatite)/{\beta}-TCP$ (tricalcium phosphate) biomaterial (BCP; biphasic calcium phosphate) is widely used as bone cement or scaffolds material due to its superior biocompatibility. Furthermore, $NH_4HCO_3$ as a space holder (SH) has been used to evaluate feasibility assessment of porous structured BCP as bone scaffolds. In this study, using a spark plasma sintering (SPS) process at 393K and 1373K under 20MPa load, porous $HA/{\beta}-TCP$ biomaterials were successfully fabricated using $HA/{\beta}-TCP$ powders with 10~30 wt% SH, TiH2 as a foaming agent, and MgO powder as a binder. The effect of SH content on the pore size and distribution of the BCP biomaterial was observed by scanning electron microscopy (SEM) and a microfocus X-ray computer tomography system (SMX-225CT). The microstructure observations revealed that the volume fraction of the pores increased with increasing SH content and that rough pores were successfully fabricated by adding SH. Accordingly, the cell viabilities of BCP biomaterials were improved with increasing SH content. And, good biological properties were shown after assessment using Hanks balanced salt solution (HBSS).

In Vitro Reaction for Calcium Phosphate Ceramics

  • Ioku, Koji;Toya, Hiroyuki;Fujimori, Hirotaka;Goto, Seishi
    • The Korean Journal of Ceramics
    • /
    • 제6권3호
    • /
    • pp.214-218
    • /
    • 2000
  • Hydroxyapatite (HA) and $\beta$-tricalcium phosphate ($\beta$-TCP) are bio-compatible materials with bones and teeth. HA has been widely applied as bone substitutes because of chemical stability in vivo, while $\beta$-TCP has higher resorbability than HA when the material is implanted in a bone defect. In the present study, both HA and $\beta$-TCP porous ceramics were soaked in the simulated body fluid in order to investigate the reaction between the materials and the fluid. After the soaking test, carbonate hydroxyapatite was formed on HA surface at 1 week, and then the amount of precipitates increased with increasing period of the soaking test. While $\beta$-TCP was not dissolved in the fluid, carbonate hydroxyaopatite was also formed on $\beta$-TCP surface after 12 weeks, and the amount of precipitates was less than that on HA. In vitro behavior of HA was similar to that in vivo, but in vitro behavior of $\beta$-TCP was not similar to that in vivo.

  • PDF

The BMPs expression and histomorphometric study of ${\beta}-TCP$ / rhBMP-2 Grafting on the rabbit cranial bone defects

  • Lim, Byung-Sup;Jeon, Jae-Yoon;Park, Chang-Joo;Im, Jae-Jung;Hwang, Kyung-Gyun;Shim, Kwang-Sup
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제34권1호
    • /
    • pp.49-58
    • /
    • 2008
  • Objective: The Purpose of the study was to investigate the bone morphogenic protein expression of rhBMP-2(recombinant human bone morphogenic protein-2) as singnaling molecule and ${\beta}-TCP$(Tricalcium phosphate) as a bone substitute and carrier medium of rhBMP-2. Materials and Methods: 16 rabbits divided into 2 group of each 8 rabbit. Two standardized bone defect, round bilateral defect was made in the cranium of the 8 rabbit of first group, and was grafted with $150{\sim}500{\mu}m$ diameter ${\beta}-TCP$ 0.25g in one side, which was soaked with rhBMP-2, and autogenous bone was grafted on another side as a positive control. Second group of 8 rabbit, only ${\beta}-TCP$ was grafted with same size and same manner. After 2, 4, 8, and 12 weeks, specimen was taken for microscopic immunohiostochemical and histomorphometric analysis. Result: Grafting ${\beta}-TCP$ with rhBMP show the early formation of the bone regenerative factor (BMP-4) and more quantity of new bone formation than only use of ${\beta}-TCP$ (8,12 week), even show less new bone formation than autogenous bone. Conclusion : The experimental study result that ${\beta}-TCP$ graft combination with rhBMP-2 as a delivery system is an effective with osteoinductive capacity and biodegradable properties, so that provide clinical availibility of composite use in reconstruction of bony defect.

SPS로 제조된 HA/β-TCP 복합재의 기공의 크기와 분포에 미치는 지지체 량의 영향 (Effect of Space Holder Content on Pore Size and Distribution in HA/β-TCP Composites Consolidated by SPS)

  • 이택;우기도;강동수;이해철;장준호
    • 한국재료학회지
    • /
    • 제25권4호
    • /
    • pp.165-170
    • /
    • 2015
  • Ceramics biomaterials are useful as implant materials in orthopedic surgery. In this study, porous HA(hydroxyapatite)/${\beta}$-TCP(tricalcium phosphate) composite biomaterials were successfully fabricated using HA/${\beta}$-TCP powders with 10-30 wt% $NH_4HCO_3$ as a space holder(SH) and $TiH_2$ as a foaming agent, and MgO powder as a binder. The HA/${\beta}$-TCP powders were consolidated by spark plasma sintering(SPS) process at $1000^{\circ}C$ under 20 MPa conditions. The effect of SH content on the pore size and distribution of the HA/${\beta}$-TCP composite was observed by scanning electron microscopy(SEM) and a microfocus X-ray computer tomography system(SMX-225CT). These microstructure observations revealed that the volume fraction of the pores increased with increasing SH content. The pore size of the HA/${\beta}$-TCP composites is about $400-500{\mu}m$. The relative density of the porous HA/${\beta}$-TCP composite increased with decreasing SH content. The porous HA/${\beta}$-TCP composite fabricated with 30%SH exhibited an elastic modulus similar to that of cortical bone; however, the compression strength of this composite is higher than that of cortical bone.

달걀껍질의 재 사용에 의해 제조 된 생체용 Calcium Phosphate 분말의 상변화 거동 및 미세구조 변화에 관한 연구 (Phase Developments and Microstructure Changes of Calcium Phosphate Powders Synthesized by Recycling Eggshell)

  • 이상진;김주원
    • 한국분말재료학회지
    • /
    • 제11권5호
    • /
    • pp.391-398
    • /
    • 2004
  • Calcium phosphate powders were successfully synthesized by using re-cycled eggshell and phosphoric acid. The crystallization behavior and powder morphologies of the synthesized powders were dependent on the starting condition of the eggshell, the mixing ratio and method of the eggshell and phosphoric acid, and calcination temperature. In general, $\beta$-tricalcium phosphate was stably synthesized at about $900^{\circ}C$ for 1h at each proper mixing ratio. And, the synthesized powders showed the similar microstructures to the morphology of original eggshell with uniform particle sizes. In this study, the calcium phosphate powders were synthesized with eggshell in various processing method. And their unique microstructures obtained from the eggshell were also. observed. The crystalline developments and microstructures of the synthesized powders were examined by X-ray diffractometer and scanning electron microscopy.

후처리공정에 따른 고상반응 β-TCP/HAp 복합분체의 미세구조 변화 (Microstructure Evolution of Solid State Reacted HAp/β-TCP Composite Powders by Post-Treatment Processing)

  • 박영민;양태영;박상희;윤석영;박홍채
    • 한국세라믹학회지
    • /
    • 제41권8호
    • /
    • pp.582-587
    • /
    • 2004
  • 수산화아파타이트(HAp) 및 P-인산3칼슘($\beta$-TCP)으로 구성되는 2상 인산칼슘염(BCP)을 고상반응법으로 합성하고, 이를 상압 및 autoclave를 이용한 고압에서 수열반응 시킴으로써 응집입자의 미세화를 시도하였다. 이 과정에서 일어나는 결정 상 및 화학조성, 구성상의 상대적인 양, 비표면적, 미세구조의 변화에 미치는 공정조건의 영향을 XRD, FT-IR, 질소흡착에 의한 BET법, SEM을 이용하여 검토하였다.