• Title/Summary/Keyword: B4C grain

Search Result 340, Processing Time 0.034 seconds

Mechanical properties of $B_4C$ ceramics fabricated by a spark plasma sintering process (방전플라즈마 소결법을 이용한 고밀도 탄화 붕소 제조 및 기계적 특성)

  • Kim, Kyoung-Hun;Chae, Jae-Hong;Park, Joo-Seok;Kim, Dae-Keun;Shim, Kwang-Bo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.3
    • /
    • pp.128-132
    • /
    • 2007
  • [ $B_4C$ ] ceramics were fabricated by spark plasma sintering process and their sintering behavior, microstructure and mechanical properties were evaluated. Relative density of $B_4C$ ceramics were obtained by spark plasma sintering method reached as high as 99% at lower temperature than conventional sintering method, in addition, without any sintering additives. The mechanical properties of $B_4C$ ceramics was improved by a methanol washing process which can be removed $B_2O_3$ phase from a $B_4C$ powder surface. This improvement results ken the formation of homogeneous microstructure because the grain coarsening was suppressed by the elimination of $B_2O_3$ phase. Particularly, fracture toughness of the sintered specimen using a methanol washed powder improved over 30% compared with the specimen using an as-received commercial powder.

Coercivity Enhancement of Sintered Nd-Fe-B Magnets by Grain Boundary Diffusion with DyH3 Nanoparticles

  • Liu, W.Q.;Chang, C.;Yue, M.;Yang, J.S.;Zhang, D.T.;Liu, Y.Q.;Zhang, J.X.;Yi, X.F.;Chen, J.W.
    • Journal of Magnetics
    • /
    • v.18 no.4
    • /
    • pp.400-404
    • /
    • 2013
  • Grain boundary diffusion technique with $DyH_3$ nanoparticles was applied to fabricate Dy-less sintered Nd-Fe-B permanent magnets with high coercivity. The magnetic properties and microstructure of magnets were systematically studied. The coercivity and remanence of grain boundary diffusion magnet were improved by 60% and reduced by 7% compared with those of the original magnet, respectively. Meanwhile, both the remanence temperature coefficient (${\alpha}$) and the coercivity temperature coefficient (${\beta}$) of the magnets were improved after diffusion treatment. Investigation shows that Dy is preferentially enriched as (Nd, Dy)$_2Fe_{14}B$ phase in the surface region of the $Nd_2Fe_{14}B$ matrix grains indicated by the remarkable enhancement of the magneto-crystalline anisotropy field of the magnet. As a result, the magnet diffused with a small amount of Dy nanoparticles possesses enhanced coercivity without remarkably sacrificing its magnetization.

High-Temperature Fracture Strength of a CVD-SiC Coating Layer for TRISO Nuclear Fuel Particles by a Micro-Tensile Test

  • Lee, Hyun Min;Park, Kwi-Il;Park, Ji-Yeon;Kim, Weon-Ju;Kim, Do Kyung
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.6
    • /
    • pp.441-448
    • /
    • 2015
  • Silicon carbide (SiC) coatings for tri-isotropic (TRISO) nuclear fuel particles were fabricated using a chemical vapor deposition (CVD) process onto graphite. A micro-tensile-testing system was developed for the mechanical characterization of SiC coatings at high temperatures. The fracture strength of the SiC coatings was characterized by the developed micro-tensile test in the range of $25^{\circ}C$ to $1000^{\circ}C$. Two types of CVD-SiC films were prepared for the micro-tensile test. SiC-A exhibited a large grain size (0.4 ~ 0.6 m) and the [111] preferred orientation, while SiC-B had a small grain size (0.2 ~ 0.3 mm) and the [220] preferred orientation. Free silicon (Si) was co-deposited onto SiC-B, and stacking faults also existed in the SiC-B structure. The fracture strengths of the CVD-SiC coatings, as measured by the high-temperature micro-tensile test, decreased with the testing temperature. The high-temperature fracture strengths of CVD-SiC coatings were related to the microstructure and defects of the CVD-SiC coatings.

Magnetic properties of high performance NdFeB perpendicular thin film (고성능 NdFeB 수직 박막자석의 자기적 특성)

  • 김만중;양재호;김윤배;김택기
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.802-805
    • /
    • 2000
  • Anistropic [Ta/NdFeB/Ta] thin film was sputtered on heated Si substrate by Nd$\_$17/Fe$\_$74/B$\_$9/ target. The grain size of the films increased according to the increase of substrate temperature, and the film deposited at 650$^{\circ}C$ showed optimum coercivity. 4$\pi$M$\_$r/, $\_$i/H$\_$c/ and (BH)$\_$max/ measured perpendicular to the film plane of thin film deposited at 650$^{\circ}C$ are 12.3 kG, 9.9 kOe and 37 MGOe, respectivly.

  • PDF

Densification and Properties of ZrB2-based Ceramics for Ultra-high Temperature Applications (초고온용 ZrB2-계 세라믹스의 치밀화와 물성)

  • Kim, Seong-Won;Kim, Hyung-Tae;Kim, Kyung-Ja;Seo, Won-Seon
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.29 no.3
    • /
    • pp.273-278
    • /
    • 2012
  • $ZrB_2$ has a melting temperature of $3245^{\circ}C$ and a low density of $6.1\;g/cm^3$, which makes this a candidate for application to ultra-high temperature over $2000^{\circ}C$. Beside these properties, $ZrB_2$ has excellent resistance to thermal shock and oxidation compared with other non-oxide engineering ceramics. This paper reviewed briefly 2 research examples, which are related to densification and properties of $ZrB_2$-based ceramics for ultra-high temperature applications. In the first section, the effect of $B_4C$ addition on the densification and properties of $ZrB_2$-based ceramics is shown. $ZrB_2$-20 vol.% SiC system was selected as a basic composition and $B_4C$ or C was added to this system in some extents. With sintered bodies, densification behavior and hightemperature (up to $1400^{\circ}C$) properties such as bending strength and hardness are examined. In the second section, the effect of the SiC size on the microstructures and physical properties is shown. $ZrB_2$-SiC ceramics are fabricated by using various SiC sources in order to investigate the grain-growth inhibition and the mechanical/thermal properties of $ZrB_2$-SiC.

The Effects of Nitrogen on Microstructure and Magnetic Properties of Nanocrystalline Fe-Nb-B-N Thin Films (나노결정구조 Fe-Nb-B-N 박막의 미세구조 및 자기적 특성)

  • 박진영;서수정;노태환;김광윤;김종열;김희중
    • Journal of the Korean Magnetics Society
    • /
    • v.7 no.5
    • /
    • pp.250-257
    • /
    • 1997
  • The microstructure and magnetic properties of Fe-Nb-B-N thin film alloys, which produced by rf magnetron sputtering method in $Ar+N_2$ mixed gas atmosphere, were investigated. The $Fe_{70}Nb_{14}B_{11}N_5$ films, annealed at 59$0^{\circ}C$, exhibit soft magnetic properties: $4{\pi}M_s=16.5kG$ , $H_c=0.13Oe$ and ${\mu}_{eff}$ (1~10 MHz)=5, 000. The frequency stability of the Fe-Nb-B-N films has also been found to be good up to 10 MHz. The Fe-Nb-B-N thin film alloys annealed at 59$0^{\circ}C$ consist of three phase; fine crystalline $\alpha$-Fe phase with grain size of about 5~10 nm, Nb-B rich amorphous phase and Nb-nitride precipitates with the size of less than 3 nm. Annealed Fe-Nb-B films have two phases; $\alpha$-Fe grains with the size of about 10 nm and Nb-B rich amorphous phase. The addition of N decreased $\alpha$-Fe grain size due to the precipitation of NbN. The good magnetic properties of the Fe-Nb-B-N film alloys are due to fine $\alpha$-Fe grains resulting from the precipitation of NbN.

  • PDF

A Study on Cu(B)/Ti/SiO2/Si Structure for Application to Advanced Manufacturing Process (차세대 공정에 적용 가능한 Cu(B)/Ti/SiO2/Si 구조 연구)

  • Lee Seob;Lee Jaegab
    • Korean Journal of Materials Research
    • /
    • v.14 no.4
    • /
    • pp.246-250
    • /
    • 2004
  • We have investigated the effects of boron added to Cu film on the Cu-Ti reaction and microstructural evolution of Cu(B) alloy film during annealing of Cu(B)/Ti/$SiO_2$/Si structure. The result were compared with those of Cu(B)/$SiO_2$ structure to identify the effects of Ti glue layers on the Boron behavior and the result grain growth of Cu(B) alloy. The vacuum annealing of Cu(B)/Ti/$SiO_2$ multilayer structure allowed the diffusion of B to the Ti surface and forming $TiB_2$ compounds at the interface. The formed $TiB_2$ can act as a excellent diffusion barrier against Cu-Ti interdiffusion up to $800^{\circ}C$. Also, the resistivity was decreased to $2.3\mu$$\Omega$-cm after annealing at $800^{\circ}C$. In addition, the presence of Ti underlayer promoted the growth Cu(l11)-oriented grains and allowed for normal growth of Cu(B) film. This is in contrast with abnormal growth of randomly oriented Cu grains occurring in Cu(B)/$SiO_2$ upon annealing. The Cu(B)/Ti/$SiO_2$ structure can be implemented as an advanced metallization because it exhibits the low resistivity, high thermal stability and excellent diffusion barrier property.

Some effects of rice weevil (Sitophilus oryzae L.) on the moisture contents of polished rice (쌀바구미(Sitophilus oryzae Linne)의 현미함수량에 미치는 영향)

  • HYUN Jai Sun
    • Korean journal of applied entomology
    • /
    • v.1
    • /
    • pp.20-25
    • /
    • 1962
  • A. The increases moisture contents of grain at R.H $75\%,\; and\; 28^{\circ}C$ 1) The moisture contents of polished rice were $0.4\%,\; 1 \%,\; 3.3\%$ higher than control after 4weeks in which had been infested with 100, 200, 500 individuals of weevil at the beginning. respectively. 2) The greatest moisture contents of polished rice was $16.26\%$ for 500 individual infested grain and the lowest one was $14.86\%$ for the 100 individual weevil infested grain after 4 weeks. 3) The increases in moisture contents of grain were proportionally greater with the size of the weevil population. B. Changes in moisture contents of polished rice at the three levels of cylinder which contain 3kgs of grain and 1000 weevils were infested at the beginning of the experiment. 1) The moisture contents of the grain at all the levels of the cylinder which was not infested with weevil, were consistantly decreased in 12 weeks. 2) The moisture contents of the grain at all the levels of the cylenders which had been infested with 1000 weevils at the beginning of the experiment, were increased except top lovel, that were $15.6\%$ for middle, $41.55\%$ for the bottom levels after 12 weeks. 3) The moisture contents of the grain were greater toward bottom in both weevil infested grain and in control. 4) The moisture content increase might be caused by the respiration of the weevils and deterioration of the grain by microorganisms. 5) There were no tendency to confine the weevils at any definite levels, but as the deterioration of the grain goes on, the weevil moved to top levels of cylinders. 5) The decreases in moisture contents of the grain at the top levels of the cylinders might be caused by diffusion of water to the environment. 7) The differences in temperature at three levels of the cylinder from enviroment were little or negative in control but were greater and positive. and the bottom were higher than top in experimental cylinders. 8) The increases of temperature might be caused by the respiration of the weevil and microorganisms.

  • PDF

Development of a Cost-Effective Process for the Fabrication of Single Grain $YBa_2Cu_3O_{7-y}$ Bulk Superconductors (단결정 $YBa_2Cu_3O_{7-y}$ 벌크 초전도체 제조를 위한 경제적 공정의 개발)

  • Park, Soon-Dong;Kim, Kwang-Mo;Jun, Byung-Hyuk;Han, Young-Hee;Kim, Chan-Joong
    • Progress in Superconductivity
    • /
    • v.13 no.2
    • /
    • pp.133-138
    • /
    • 2011
  • To reduce the processing cost of the single grain REBCO (RE: Rare-earth elements) bulk superconductors, a cost-effective process should be developed. One possible way of developing the cost-effective process is the use of low-cost precursor powders. In this study, the single grain YBCO superconductors were fabricated using a home made powder. $YBa_2Cu_3O_{7-y}$ (Y123) powders were synthesized at $850-900^{\circ}C$ in air by the powder calcination method with repeated crushing and heat treatment steps. The processing parameters for the fabrication of single grain Y123 bulk superconductors, $T_{max}$ (maximum temperature), $T_p$ (peritectic temperature) and a cooling rate through $T_p$ were optimized. To enhance the flux pinning capacity of the single grain Y123 samples, $Y_2BaCuO_5$ (Y211) particles were dispersed in the Y123 matrix by adding $Y_2O_3$ powder to the calcined Y123 powder. Applying the optimized processing condition, the single grain Y123 superconductors with $T_c=91\;K$ and $J_c=1.5{\times}10^4\;A/cm^2$ at 2 T were successfully fabricated using a home made powder. The levitation forces and trapped magnetic field at 77 K measured using a Nd-B-Fe permanent magnet of 5300 G were 47 N and 3000 G, respectively, which are comparable to those obtained for the samples fabricated using a commercial grade Y123 powders.

The Effect of Carbide Size on the Mechanical Properties of AISI E 52100 Steel (AISI E 52100 강(鋼)의 기계적(機械的) 성질(性質)에 미치는 탄화물(炭化物) 크기의 영향(影響))

  • Cho, K.R.;Kim, B.W.;Nam, T.W.;Lee, B.K.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.3 no.4
    • /
    • pp.10-22
    • /
    • 1990
  • A study has been investigated on the effect of mechanical properties (tension strength, rotary bending fatigue strength, wear resistance, hardness) according to the carbide particle size variation by the treatment of 1) quenching tempering, and 2) quenching, subzero treatment and tempering. The material used in this investigation was a typical bearing steel, high C high Cr, AISI E 52100. The result obtained in this study were as follows : (1) Finer the carbide particle size increasing the hardness and retained austenite in same quenching condition. (2) Finer the carbide particle size reduced the tension and rotary bending fatigue which were resulted from austenite grain growth and carbide precipitation on grain boundry that induced by carbide refine heat treatment. (3) Finer the carbide particel size increasing the wear resistance which were resulted by uniform distribution of carbide and increased hardness induced by microstructural uniform hardenability of matrix. (4) When the carbide particles were refinded, subzero treatment is effective only wear resistance and hardness.

  • PDF