Atomic layer etching (ALE) is a promising technique with atomic-level thickness controllability and high selectivity based on self-limiting surface reactions. ALE is performed by sequential exposure of the film surface to reactants, which results in surface modification and release of volatile species. Among the various ALE methods, thermal ALE involves a thermally activated reaction by employing gas species to release the modified surface without using energetic species, such as accelerated ions and neutral beams. In this study, the basic principle and surface reaction mechanisms of thermal ALE?processes, including "fluorination-ligand exchange reaction", "conversion-etch reaction", "conversion-fluorination reaction", "oxidation-fluorination reaction", "oxidation-ligand exchange reaction", and "oxidation-conversion-fluorination reaction" are described. In addition, the reported thermal ALE processes for the removal of various oxides, metals, and nitrides are presented.
본 연구에서는 중성빔을 이용한 Atomic Layer Etching(ALET) system을 이용하여 $ZrO_2$의 atomic layer etching mechanism에 대하여 연구하였다. Ar neutral beam irradiation dose와 $BCl_3$ gas pressure의 변화에 따라 $ZrO_2$ etch rate와 RMS roughness를 관찰했을 때, Ar neutral beam irradiation dose이 $1.485{\times}10^{16}atoms/cm^2{\bullet}cycle$ 이상이고 $BCl_3$ gas pressure가 0.15mTorr 이상 일 때 $ZrO_2$ etch rate은 $1.07\;{\AA}/cycle$의 일정한 값에서 유지됨을 확인하였다. 그리고 ALET와 ICP Etcher을 통해 $ZnO_2$를 각각 식각하여 physically or chemically damage를 비교한 결과, ALET가 기존의 ICP Etcher system보다 $ZrO_2$ 식각공정에 대해 적은 damage를 받는 것을 ARXPS를 통해 관찰 하였다.
Contact Pattern을 Plasma Etching을 통해 Pattering 공정을 진행함에 있어서 Plasma 내에 존재하는 High Energy Ion 들의 Bombardment 에 의해, Contact Bottom 의 Silicon Lattice Atom 들은 Physical 한 Damage를 받아 Electron 의 흐름을 방해하게 되어, Resistance를 증가시키게 된다. 또한 Etchant 로 사용되는 Fluorine 과 Chlorine Atom 들은, Contact Bottom 에 Contamination 으로 작용하게 되어, 후속 Contact 공정을 진행하면서 증착되는 Ti 나 Co Layer 와 Si 이 반응하는 것을 방해하여 Ohmic Contact을 형성하기 위한 Silicide Layer를 형성하지 못하도록 만든다. High Aspect Ratio Contact (HARC) Etching 을 진행하면서 Contact Profile을 Vertical 하게 형성하기 위하여 Bias Power를 증가하여 사용하게 되는데, 이로부터 Contact Bottom에서 발생하는 Etchant 로 인한 Damage 는 더욱 더 증가하게 된다. 이 Damage Layer를 추가적인 Secondary Damage 없이 제거하기 위하여 본 연구에서는 원자층 식각방법(Atomic Layer Etching Technique)을 사용하였다. 실험에 사용된 원자층 식각방법을 이용하여, Damage 가 발생한 Si Layer를 Secondary Damage 없이 효과적으로 Control 하여 제거할 수 있음을 확인하였으며, 30 nm Deep Contact Bottom 에서 Damage 가 제거될 수 있음을 확인하였다. XPS 와 Depth SIMS Data를 이용하여 상기 실험 결과를 확인하였으며, SEM Profile 분석을 통하여, Damage 제거 결과 및 Profile 변화 여부를 확인하였으며, 4 Point Prove 결과를 통하여 결과적으로 Resistance 가 개선되는 결과를 얻을 수 있었다.
Kim, Yong-Soo;Jeon, Sang-Hwan;Yim, Byung-Joo;Lee, Hyo-Cheol;Jung, Jong-Heon;Kim, Kye-Nam
한국방사성폐기물학회:학술대회논문집
/
한국방사성폐기물학회 2004년도 학술논문집
/
pp.32-42
/
2004
Recently, plasma surface-cleaning or surface-etching techniques have been focused in respect of the decontamination of spent or used nuclear parts and equipment. In this study the removal rate of metallic cobalt surface is experimentally investigated via its surface etching rate with a $CF_4-o_2$mixed gas plasma. Experimental results reveal that a mixed etchant gas with about 80% $CF_4$-20% $O_2$ (molar) gives the highest reaction rate and the rate reaches 0.06 ${\mu}m$/min at $380^{\circ}C$ and ion-assisted etching dramatically enhances the surface reaction rate. With a negative 300 V DC bias voltage applied to the substrate, the surface reaction initiation temperature lowers and the rate increases about 20 times at $350^{\circ}C$ and up to 0.43 ${\mu}m$/min at $380^{\circ}C$, respectively. Surface morphology analysis confirms the etching rate measurements. Auger spectrum analysis clearly shows the adsorption of fluorine atoms on the reacted surface. From the current experimental findings and the results discussed in previous studies, mechanistic understanding of the surface reaction, fluorination and/or fluoro-carbonylation reaction, is provided.
플라즈마 건식 식각 기술은 반도체 식각공정에서 효과적으로 이용되고 있으며, 반도체 소자의 크기가 줄어듬에 따라 미세하고 정확하게 식각 깊이를 제어할 수 있는 원자층 식각 기술이 개발되었다. 3-5족 반도체 소자의 Interface Passivation Layer 로 이용되는 $Al_2O_3$ 와 BeO 의 원자층 식각을 하였으며, 각각의 원자층 식각 조건과 식각 후의 표면 거칠기 변화에 대한 영향을 확인 할 수 있었다.
Area selective atomic layer deposition (AS-ALD) is a bottom-up nanopattern fabrication method that can grow the ALD films only on the desired substrate areas without using photolithography and etching processes. Particularly, AS-ALD has attracted great attention in the semiconductor manufacturing process due to its advantage in reducing edge placement error by fabricating self-aligned patterns. In this paper, the basic principles and characteristics of AS-ALD are described. In addition, various approaches for achieving AS-ALD with excellent selectivity were comprehensively reviewed. Finally, the technology development to overcome the selectivity limit of AS-ALD was introduced along with future prospects.
Since the first report on ferroelectricity in Si-doped hafnia (HfO2), this emerging ferroelectrics have been considered promising for the next-generation semiconductor devices with their characteristic nonvolatile data storage. The robust ferroelectricity in the sub-10-nm thickness regime has been proven by numerous research groups. However, extending their scalability below the 5 nm thickness with low temperature processes compatible with the back-end-of-line technology. In this review, therefore, the current status, technical issues, and their potential solutions of atomic layer deposition (ALD) of HfO2-based ferroelectrics are comprehensively reviewed. Several technical issues in the physical scaling of the ferroelectric thin films and potential solutions including advanced ALD techniques including discrete feeding ALD, atomic layer etching, and area selective ALD are introduced.
트랜지스터 응용 등에 관한 연구가 활발해 지면서 에너지 밴드갭이 0 eV에 가까운 그래핀 이외의 밴드 갭 조절이 가능한 MoS2 (molybdenum disulfide), BN (boron nitride), Bi2Te3 (bismuth telluride), WS2 (tungsten disulfide) 등과 같은 이차원 Transition Metal DiChalcogenides (TMDC) 물질이 반도체 물질로 각광받고 있다. 특히 MoS2의 경우 단결정 덩어리 상태에서는 약 1.3 eV의 밴드갭을 가지나 두께가 줄어들어 두 층일 경우에는 약 1.65 eV, 단일층이 되면 약 1.9 eV의 밴드갭을 가져 박막 층수에 따라 에너지 밴드갭 조절이 가능한 것으로 알려져있다. 하지만 두께 조절이 가능하면서 대면적, 고품질을 가지는 MoS2 박막 합성은 아직 제한적이라 할 수 있으며 새로운 방법 및 물질에 대한 연구가 지속적으로 이루어 지고 있다. 따라서 본 연구에서는 다양한 층수를 지니는 MoS2 합성을 위해 나노 두께의 MoS2 박막을 CF4 plasma 를 이용하여 layer etching 진행하고 CF4 plasma 100초 etching 진행한 2 layer 두께의 MoS2를 기준으로 H2S plasma를 이용하여 treatment 진행하였다. 물리적, 화학적 분석은 Raman spectroscopy, XPS(X-ray Photoelectron Spectroscopy), AFM (Atomic Force Microscopy) 등을 이용해 진행하였고 이를 통해 MoS2 layer 감소 및 damage recovery 등을 확인하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.