Properties Analysis for Small Elements Added Shadow Mask Materials

  • Kim, Ku-Hak;Kim, Chung-Ho;Kim, Dong-Soo;Kim, One-Seek
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2002.08a
    • /
    • pp.1053-1055
    • /
    • 2002
  • Recently CRT is getting large-sized, Flatness and High Fine Pitched in the meantime the raw material for shadow mask is in rapid progress of thinness, Low Thermal Expansion and high strength.Until now we have used AK(Aluminum Killed) & Invar(Fe-Ni alloy) materials for main raw material of shadow mask component. However recently Nb and Co addition and Nb+Co addition, which has advantage of Low Thermal Expansion and High Strength. has been developed as well as applying in mass production as CRT's trend has become more flat and fine pitch. Among of them, Co addition has been mass production as forming type (Flat CRT) with the beneficial effect of low thermal expansion & high strength for the first time. Since then Nb+Co addition has been used in mass production by the request of much higher strength of shadow mask component. In case of Nb addition, It's thermal expansion coefficient is a little lower than normal Invar and a little higher than Co addition, meanwhile Its Mechanical property is almost similar to Co Addition. The used samples of this experiment are 36%Ni + Fe, 32%Ni + 5%Co + Fe, 32%Ni + 5%Co + 0.3%Nb + Fe, 32%Ni + 0.3%Nb + Fe with heat treatment temperature of 600$^{\circ}C$, 650$^{\circ}C$, 700$^{\circ}C$, 750$^{\circ}C$, 800$^{\circ}C$, 850$^{\circ}C$, 900$^{\circ}C$ respectively under the condition of 15min holding time. After heat treatment, we have observed the change of mechanical property with addition of small elements through mechanical property investigation and metal structure observation as well as transition of thermal expansion coefficient by measuring of thermal expansion coefficient at 850$^{\circ}C$. In conclusion, 5%Co addition indicates that its thermal expansion coefficient is very similar under the condition of at 850$^{\circ}C$ for 15min 's heat treatment. From the experimental result it is suggested that Co addition is mostly suitable for Doming property and Nb addition is mostly suitable for Drop property.

  • PDF

Micro Structure and Surface Characteristics of NiCr Thin films Prepared by DC Magnetron Sputter according to Annealing Conditions (DC 마그네트론 스퍼터링 NiCr 박막의 열처리 조건에 따른 미세구조 및 표면특성)

  • Kwon, Yong;Kim, Nam-Hoon;Choi, Dong-You;Lee, Woo-Sun;Seo, Yong-Jin;Park, Jin-Seong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.6
    • /
    • pp.554-559
    • /
    • 2005
  • Ni/Cr thin film is very interesting material as thin film resistors, filaments, and humidity sensors because their relatively large resistivity, more resistant to oxidation and a low temperature coefficient of resistance (TCR). These interesting properties of Ni/Cr thin films are dependent upon the preparation conditions including the deposition environment and subsequent annealing treatments. Ni/Cr thin films of 250 nm were deposited by DC magnetron sputtering on $Al_2O_3/Si$ substrate with 2-inch Ni/Cr (80/20) alloy target at room temperature for 45 minutes. Annealing treatments were performed at $400^{\circ}C,\;500^{\circ}C,\;and\;600^{\circ}C$ for 6 hours in air or $H_2$ ambient, respectively. The clear crystal boundaries without crystal growth and the densification were accomplished when the pores were disappeared in air ambient. Most of surface was oxidic including NiO, $Ni_2O_3$ and $Cr_xO_y$(x=1,2, y=2,3) after annealing in air ambient. The crystal growth in $H_2$ ambient was formed and stabilized by combination with each other due to the suppression of oxidized substance on film surface. Most oxidic Ni was restored when the oxidic Cr was present due to its stability in high-temperature $H_2$ ambient.

Electrospray and Thermal Treatment Process for Enhancing Surface Roughness of Fecralloy Coating Layer on a Large Sized Substrate (대면적 Fecralloy 코팅층의 표면 거침도 극대화를 위한 정전분무 및 열처리 공정 연구)

  • Lee, Hye Moon;Koo, Hye Young;Yang, Sangsun;Park, Dahee;Jung, Sooho;Yun, Jung-Yeul
    • Journal of Powder Materials
    • /
    • v.24 no.1
    • /
    • pp.46-52
    • /
    • 2017
  • Fecralloy coating layer with large surface area is suitable for use as a filter media for efficient removal of hot gaseous pollutants exhausted from combustion processes. For uniform preparation of a Fecralloy coating layer with large surface area and strong adhesion to substrate, electrospray coating and thermal treatment processes are experimentally optimized in this study. A nano-colloidal solution with 0.05 wt% Fecralloy nanoparticles is successfully prepared. Optimized electrospraying conditions are experimentally discovered to prepare a uniform coating layer of Fecralloy nano-colloidal solution on a substrate. Drying the electrospray coated Fecralloy nano-colloidal solution layer at $120^{\circ}C$ and subsequent heating at $600^{\circ}C$ are the best post-treatment for enhancing the adhesion force and surface roughness of the Fecralloy coating layer on a substrate. An electrospray coating system, consisting of several multi-groove nozzles, is also experimentally confirmed as a reasonable device for uniform coating of Fecralloy nano-colloid on a large area substrate.

A Study on the Stress Relief Cracking of HSLA-100 and HY-100 steels (HSLA-100강 및 HY-100강의 응력제거처리 균열에 관한 연구)

  • 박태원;심인옥;김영우;강정윤
    • Journal of Welding and Joining
    • /
    • v.14 no.3
    • /
    • pp.48-57
    • /
    • 1996
  • A study was made to examine the characteristics of base metal and stress relief cracking(SRC) of heat affected zone(HAZ) for HY-100 and Cu-bearing HSLA-100 steels. The Gleeble thermal/mechanical simulator was used to simulate the SRC/HAZ. The details of mechanical properties of base plate and SRC tested specimens were studied by impact test, optical microscopy and scanning electron microscopy. The specimens were aged at $650^{\circ}C$ for HSLA-100 steel and at $660^{\circ}C$ for HY-100 steel and thermal cycled from $1350^{\circ}C$ to $25^{\circ}C$ with a cooling time of $\Delta$t_${800^{circ}C/500^{circ}C}$=21sec. corresponds to the heat input of 30kJ/cm. The thermal cycled specimens were stressed to a predetermined level of 248~600MPa and then reheated to the stress relief temperatures of $570~620^{\circ}C$. The time to failure$(t_f)$ at a given stress level was used as a measure of SRC susceptibility. The strength, elongation and impact toughness of base plate were greater in HSLA-100 steel than in HY-100 steel. The time to failure was decreased with increasing temperature and/or stress. HSLA-100 steel was more susceptible to stress relief cracking than HY-100 steel under same conditions. It is thought to be resulted from the precipitation of $\varepsilon$-Cu phase by dynamic self diffusion of solute atoms. By the precipitation of $\varepsilon$-Cu phase, the differential strengthening of grain interior relative to grain boundary may be greater in the Cu-bearing HSLA-100 steel than in HY-100 steel. Therefore, greater strain concentration at grain boundary of HSLA-100 steel results in the increased SRC susceptibility. The activation energies for SRC of HSLA-100 steel are 103.9kcal/mal for 387MPa and 87.6kcal/mol for 437MPa and that of HY-100 steel is 129.2kcal/mol for 437MPa.

  • PDF

Evaluation for Weld Residual Stress and Operating Stress around Weld Region of the CRDM Nozzle in Reactor Vessel Upper Head (원자로 압력용기 상부헤드 CRDM 노즐 용접부의 용접잔류응력 및 운전응력 평가)

  • Lee, Kyoung-Soo;Lee, Sung-Ho;Bae, Hong-Yeol
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.10
    • /
    • pp.1235-1239
    • /
    • 2012
  • Primary water stress corrosion cracking (PWSCC) has been observed around the weld region of control rod drive mechanism (CRDM) nozzles in nuclear power plants overseas. The weld has a J-shaped groove and it connects the CRDM nozzle with the reactor vessel upper head (RVUH). It is a dissimilar metal weld (DMW), because the CRDM is made of alloy 600 and the RVUH is made of carbon steel. In this study, finite element analysis (FEA) was performed to estimate the stress condition around the weld region. Generally, it is known that a high tensile region is more susceptible to PWSCC. FEA was performed as for the condition of welding, hydrostatic test and normal operation successively to observe how the residual stress changes due to plant condition. The FEA results show that a high tensile stress region is formed around the weld starting point on the inner surface and around the weld stop point on the outer surface.

Characteristics of Tensile Deformation and Shape Recovery with Transformation Temperature Change in a Ni-Ti Alloy Wire (Ni-Ti계 합금 선재의 변태온도 변화에 따른 인장변형 및 회복 특성)

  • Choi, Y.G.;Kim, M.S.;Cho, W.S.;Jang, W.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.21 no.6
    • /
    • pp.307-313
    • /
    • 2008
  • The tensile deformation and shape recovery behaviors were studied in Ni-Ti shape memory wires showing different transformation characteristics by annealing at $200{\sim}600^{\circ}C$. Both R phase ${\rightarrow}$ B19' martensitic transformation at lower temperature and B2 ${\rightarrow}$ R phase transformation at higher temperature occurred in the shape memory wires annealed at $200{\sim}500^{\circ}C$. Transformation temperature and heat flow of B19' martensite increase but those of R phase main almost constant even with increasing annealing temperature. In the case of wires annealed and then cooled to $20^{\circ}C$, plateau on stress-strain curves in tensile testing can be observed due to the collapse of R phase variants and the formation of deformation-induced B19' martensite. In the case of wires annealed and then cooled to $-196^{\circ}C$, however, plateau on stress-strain curves does not appear and stress increases steadily with increasing tensile deformation. Comparing shape recovery rate with cooling temperature after annealing, shape recovery rate of the wire cooled to $20^{\circ}C$ is higher than that of the wire cooled to $-196^{\circ}C$ after annealing, and maximum shape recovery rate of 95% appears in the wire annealed at $400^{\circ}C$ and then cooled to $20^{\circ}C$. $R_s$ and $R_f$ temperatures measured during shape recovery tests are higher than $A_s$ and $A_f$ temperatures measured by DSC tests even at the same annealing temperature.

Design and Preliminary Performance Test for 5kWt Dish Solar Collector ($5kW_t$급 접시형 태양열 집열기의 설계 및 예비 성능실험)

  • Seo, Joo-Hyun;Ma, Dae-Sung;Kim, Yong;Seo, Tae-Beom;Han, Gui-Young
    • Journal of the Korean Solar Energy Society
    • /
    • v.27 no.4
    • /
    • pp.113-120
    • /
    • 2007
  • The 5kWt dish solar collector is designed and the preliminary performance test for this is carried out. The diameter of the parabolic dish is 3.2 m, and its focal length is 2 m. It consists of 10 small reflectors which have their own curvatures, and the effective reflecting area is $5.9\;m^2$, and the rim angle of the dish is $43.85^{\circ}$. The reflectivity of reflectors is 0.95, and the thermal capacity of the system is about 5 kW thermal. The aperture diameter of the cylindrical-shape receiver which is made of stainless steel is 100 mm, and the height is 210 mm. A quartz window is installed at the receiver aperture to minimize the convective heat loss and prevent air leakage. In order to increase the heat transfer area, porous materials (nickel-alloy) are inserted into the receiver. Air flows into the upper part of the receiver which is the opposite side of the aperture. After the air flows through the inside of the receiver, that goes out of the receiver through 3 exits which are located near the aperture. The volumetric flow rates of air are varied from 600 to 1200 L/min. The results show that the system efficiency and receiver efficiency increase as the volume flow rate increases.

Fabrication of Densified W-Ti by Reaction Treatment and Spark Plasma Sintering of WO3-TiH2 Powder Mixtures (WO3-TiH2 혼합분말의 반응처리 및 방전 플라스마 소결에 의한 W-Ti 치밀체 제조)

  • Kang, Hyunji;Kim, Heun Joo;Han, Ju-Yeon;Lee, Yunju;Jeong, Young-Keun;Oh, Sung-Tag
    • Korean Journal of Materials Research
    • /
    • v.28 no.9
    • /
    • pp.511-515
    • /
    • 2018
  • W-10 wt% Ti alloys that have a homogeneous microstructure are prepared by thermal decomposition of $WO_3-TiH_2$ powder mixtures and spark plasma sintering. The reduction and dehydrogenation behavior of $WO_3$ and $TiH_2$ are analyzed by temperature programmed reduction and a thermogravimetric method, respectively. The X-ray diffraction analysis of the powder mixture, heat-treated in an argon atmosphere, shows W- oxides and $TiO_2$ peaks. Conversely, the powder mixtures heated in a hydrogen atmosphere are composed of W, $WO_2$ and $TiO_2$ phases at $600^{\circ}C$ and W and W-rich ${\beta}$ phases at $800^{\circ}C$. The densified specimen by spark plasma sintering at $1500^{\circ}C$ in a vacuum using hydrogen-reduced $WO_3-TiH_2$ powder mixtures shows a Vickers hardness value of 4.6 GPa and a homogeneous microstructure with pure W, ${\beta}$ and Ti phases. The phase evolution dependent on the atmosphere and temperature is explained by the thermal decomposition and reaction behavior of $WO_3$ and $TiH_2$.

Material Integrity Assessment for a Ni Electrodeposit inside a Tube

  • Kim, Dong-Jin;Kim, Myong Jin;Kim, Joung Soo;Kim, Hong Pyo
    • Corrosion Science and Technology
    • /
    • v.6 no.5
    • /
    • pp.233-238
    • /
    • 2007
  • Due to the occasional occurrence of a localizedcorrosion such as a SCC and pitting in steam generator tubing(Alloy 600), leading to a significant economical loss, an effective repair technology is needed. For a successful electrodeposition inside a tube, many processes should be developed. Among these processes, an anode to be installed inside a tube, a degreasing condition to remove any dirt and grease, an activation condition for a surface oxide elimination, a strike layer forming condition which needs to be adhered tightly between an electroforming layer and a parent tube and a condition for an electroforming layer should be established. Through a combination of these various process condition parameters, the desired material properties can be acquired. Among these process parameters, various material properties including a mechanical property and its variation along with the height of the electrodeposit inside a tube as well as its thermal stability and SCC resistance should be assessed for an application in a plant. This work deals with the material properties of the Ni electrodeposits formed inside a tube by using the anode developed in this study such as the current efficiency, hardness, tensile property, thermal stability and SCC behavior of the electrodeposit in a 40wt% NaOH solution at $315^{\circ}C$. It was found that a variation of the material properties within the entire length of the electrodeposit was quite acceptable and the Ni electrodeposit showed an excellent SCC resistance.

Effect of Process Parameters on Friction Stir Welds on AA2219-AA2195 Dissimilar Aluminum Alloys (마찰교반접합의 공정변수가 AA2219-AA2195 이종 알루미늄 접합에 미치는 영향)

  • No, Kookil;Yoo, Joon-Tae;Yoon, Jong-Hoon;Lee, Ho-Sung
    • Korean Journal of Materials Research
    • /
    • v.27 no.6
    • /
    • pp.331-338
    • /
    • 2017
  • This study was carried out to investigate the optimum condition of a friction stir welding process for a joint of AA2219-T87 and AA2195-T8 dissimilar aluminum alloys. These alloys are known to have good cryogenic properties, and as such to be suitable for use in fuel tanks of space vehicles. The welding parameters include the travelling speed, rotation speed and rotation direction of the tool. The experiment was conducted under conditions in which the travelling speed of the tool was 120-300 mm/min and the rotation speed of the tool was 400-800 rpm. To investigate the effect of the rotation direction of the tool, the joining was performed by switching the positions of the two dissimilar alloys. After welding, the microstructure was observed and the micro-hardness were measured; non-destructive evaluation was carried out to perform tensile tests on defect-free specimens. The result was that the microstructure of the weld joint underwent dynamic recrystallization due to sufficient deformation and frictional heat. The travelling speed of the tool had little effect on the properties of the joint, but the properties of the joint varied with the rotation speed of the tool. The conditions for the best joining properties were 600 rpm and 180-240 mm/min when the AA2219-T8 alloy was on the retreating side(RS).