In this paper, $Al_2O_3$ film deposited by thermal atomic layer deposition (ALD) with diluted $NH_4OH$ instead of $H_2O$ was suggested for passivation layer and anti-reflection (AR) coating of the p-type crystalline Si (c-Si) solar cell application. It was confirmed that the deposition rate and refractive index of $Al_2O_3$ film was proportional to the $NH_4OH$ concentration. $Al_2O_3$ film deposited with 5 % $NH_4OH$ has the greatest negative fixed oxide charge density ($Q_f$), which can be explained by aluminum vacancies ($V_{Al}$) or oxygen interstitials ($O_i$) under O-rich condition. $Al_2O_3$ film deposited with $NH_4OH$ 5 % condition also shows lower interface trap density ($D_{it}$) distribution than those of other conditions. At $NH_4OH$ 5 % condition, moreover, $Al_2O_3$ film shows the highest excess carrier lifetime (${\tau}_{PCD}$) and the lowest surface recombination velocity ($S_{eff}$), which are linked with its passivation properties. The proposed $Al_2O_3$ film deposited with diluted $NH_4OH$ is very promising for passivation layer and AR coating of the p-type c-Si solar cell.
Understanding of effects of changes in the particle size of the matrix material on the mullite whisker growth during the production of porous mullite is crucial for better design of new porous ceramics materials in different applications. Commercially, raw materials such as Al2O3/SiO2 and Al(OH)3/SiO2 are used as starting materials, while AlF3 is added to fabricate porous mullite through reaction sintering process. When Al2O3 is used as a starting material, a porous microstructure can be identified, but a more developed needle shaped microstructure is identified in the specimen using Al(OH)3, which has excellent reactivity. The specimen using Al2O3/SiO2 composite powder does not undergo mulliteization even at 1,400 ℃, but the specimen using the Al(OH)3/SiO2 composite powder had already formed complete mullite whiskers from the particle size specimen milled for 3 h at 1,100 ℃. As a result, the change in sintering temperature does not significantly affect formation of microstructures. As the particle size of the matrix materials, Al2O3 and Al(OH)3, decreases, the porosity tends to decrease. In the case of the Al(OH)3/SiO2 composite powder, the highest porosity obtained is 75 % when the particle size passes through a milling time of 3 h. The smaller the particle size of Al(OH)3 is and the more the long/short ratio of the mullite whisker phase decreases, the higher the density becomes.
The overall objective of this research was to find out the role of rapid mixing conditions in the species of hydrolyzed Al(III) formed by different Al(III) coagulants. When an Al(III) salt is added to water, monomers, polymers, or solid precipitates may form. Different Al(III) coagulants (alum and PACl) show to have different Al species distribution over a rapid mixing condition. During the rapid mixing period, for alum, formation of dissolved Al(III) (monomer and polymer) increases, but for PACl, precipitates of $Al(OH)_{3(s)}$. increases rapidly. Also, for alum, higher mixing speed favoured Al(III) polymers formation over precipitates of $Al(OH)_{3(s)}$ but for PACl, higher mixing speed formed more precipitates of $Al(OH)_{3(s)}$. At A/D and sweep condition, both $Al(OH)_{3(s)}$ and dissolved Al(III) (monomer and polymer) exist, concurrent reactions by both mechanism appear to cause simultaneous precipitation.
Lee Hong-rim;Lee Young-Woo;Lee Jung-Won;Kang Jong-Bong
Korean Journal of Materials Research
/
v.15
no.10
/
pp.644-651
/
2005
The thermal analysis of $Al(OH)_3-SiO_2-AIF_3$ system was done. The thermal behaviors of components and the effect of moisture on the formation of mullite were investigated via TG-DTA and XRD analysis. The mixture of $Al(OH)_3,\;SiO_2,\;AIF_3$showed two endothermic peaks with drastic weight loss and one exothermic peak. Fluorotopaz was formed at $800^{\circ}C$ and turned into mullite completely at $1100^{\circ}C$. But the mixture $Al_2O_3$ of or dehydrated $Al(OH)_3$ and $SiO_2$ could not form mullite even at $1200^{\circ}C$ in which the crystalline phases were $\alpha-Al_2O_3$ ana cristobalite. It was found that the synthesized mullite was aciculate shaped single crystalline whisker.
Aoolphane was treated with 30% Hydrochloric acid at $18^{\circ}C$ for two hows with stirring in order to obtain the insoluble form of SiO2 gel and to extract quantitatively both $Al_2O_3$as and $Fe_2O_3AlCl_3{\cdot}6H_2O Fe$ and $Cl_3{\cdot}6H_2O$ forms, respectively, at the same time. $SiO_2$ gel was filtered and to the filterate Ammonia was added to precipitate $Al(OH)_3[Fe(OH)_3 Contaminated ]$ The precipitate was separated by filteration and the filterate was recovered as the form of $NH_4Cl$. The precipitate was treated with 200g (NaOH)/l Concentration of NaOH a little excessively to the equivalent at $65~70^{\circ}C$ as $Fe(OH)_3$ formed was insoluble, it was filtered of and to the filterate containing $NaAl(OH)_4(OH_2)_2$Carbon dioxide gas was bubbled at $50^{\circ}C~90^{\circ}C$ to obtain the precipitate with excellent filterability and crystallinity. The product was certified to be Dawsonite $(NaAl(OH)_2CO_3)$ by X-Ray diffraction analysis at below $40^{\circ}C$, when $CO_2$ gas was bubbled into the relatively lower concentration of $NaAl(OH)_4(OH_2)_2$ solution, the precipitate of very fine particles was formed, which was hard to filter and with the Composition of $\alpha-Al_2O_3-H_2O$ (Boehmite).
Mullite whiskers were synthesized by a vapor-solid reaction with $Al(OH)_3-SiO_2-AlF_3$. The heat treatment temperature did not affect the shape of mullite whisker but the composition change resulted in different sizes. The first one was $30-50{\mu}m$ in size with the aspect ratio of 60 and above, and the second one was $600{\mu}m$ and below in size with the aspect ratio of 15 and below. The $Al_2O_3$ content in formed mullite whisker was 73.57-80.29 wt%, which is high $Al_2O_3$ content composition. The Young's modulus and the hardness measured by nano-indentation method were 136.7 GPa and 19.81 GPa, respectively.
Seo, Young-Ik;Jeon, Yong-Jin;Lee, Young-Jung;Kim, Dae-Gun;Lee, Kyu-Hwan;Kim, Young-Do
Korean Journal of Materials Research
/
v.20
no.2
/
pp.97-103
/
2010
In this study, a new, relatively simple fabrication method for forming a mesoporous $Al(OH)_3$ film on Al substrates was demonstrated. This method, i.e., alkali surface modification, was simply comprised of dipping the substrate in a $5\times10^{-3}$ M NaOH solution at $80^{\circ}C$ for one minute and then immersing it in boiling water for 30 minutes. After alkali surface modification, a mesoporous $Al(OH)_3$ film was formed on the Al substrate, and its chemical state and crystal structure were confirmed by XPS and TEM. According to the results of the XPS analysis, the flake-like morphology after the alkali surface modification was mainly composed of $Al(OH)_3$, with a small amount of $Al_2O_3$. The mesoporous $Al(OH)_3$ layer was composed of three regions: an amorphousrich region, a region of mixed amorphous and crystal domains, and a crystalline-rich region near the $Al(OH)_3$ layer surface. It was confirmed that the stabilization process in the alkali surface modification strongly influenced the crystallization of the mesoporous $Al(OH)_3$ layer.
Aluminum hydrates were prepared by precipitation method using Al2(SO4)3$.$18H2O as a starting material and NH4OH as precipitation agent. The phases of aluminum hydrate were changed from amorphous aluminum hydrate to pseudo-boehmite of AlOOH form and bayerite, gibbsite, hydragillite and norstrandite of Al(OH)3 form with increasing pH. As pH increased, agglomeration phenomena were reduced. Aluminum hydrates of AlOOH and Al(OH)3 form represented dehydration of structural water near 175$^{\circ}C$ and 385$^{\circ}C$, and 280$^{\circ}C$, respectively. As the ratio of Al(OH)3 to AlOOH increased, specific surface area was reduced.
The surface characteristics of calcined ${\gamma}-Al_2O_3$ particles as well as ${\gamma}-AlO$(OH) sol particles were controlled by aging in the boehmite sol preparation. As a result of the study, the IEPs of ${\gamma}-AlO$(OH) particles were decreased from pH 9.25 to pH 8.70 and those of the calcined ${\gamma}-Al_2O_3$ particles were decreased from pH 9.90 to pH 8.86 by the increase of the aging times. As a result of the acidic and basic characterization of the calcined ${\gamma}-Al_2O_3$ particles by the aging, the amount of acid sites was decreased from 0.1367 mmol/g to 0.0783 mmol/g by the increase of the aging times and Hammett acidity, $H_o$ was showed the acidic strength of 4.8 or above. On the other hand, the amount of basic sites was decreased from 0.4399 mmol/g to 0.3074 mmol/g by the increase of the aging times. Based on these results, we proposed the fact that the aging step in the sol-gel process was an important step to control the surface characterization of ${\gamma}-Al_2O_3$ particles including acidity and basicity.
This study was investigated to the recovery of alumina from the first calcined waste pottery using alkaline sintering. This study was based on calcination result of a commercial ${\alpha}-Al2_O_3$ with NaOH powder. $NaAlO_2$ was formed by calcination of ${\alpha}-Al_2O_3$ with NaOH and conversion of $NaAlO_2$ from ${\alpha}-Al_2O_3$ was 91.4% at calcination condition ; weight ritio of $NaOH/{\alpha}-Al2_O_3$ 1.5, $800^{\circ}C$, and 90min. The first calcined waste porrery from the manufacturing Procedure of H Ltd. was grinded to 170/270mesh by a ball mill and calcined over $500^{\circ}C$ with NaOH powder. The calcined sample was dissolved in $25^{\circ}C$ water and sodiumaluminosilicate solid was formed. After filtration, the contained aluminum was leached out by dissolving sodiumaluminosilicate solid in 1N HCl. We estimated the efficiency of Al extraction from waste pottery by ICP analysis and NaOH was added to the filtrate and then aluminum compound was precipitated with $Al(OH)_3$ and recovered. The investigation was carried out with the variables ; the calcination temperature($500-900^{\circ}C$), the calcination time(30~90min), and the weight ratio of NaOH/waste pottery(0.5~1.5). The treatment efficiency of the waste pottery and the recovery of Al as 97.9%, 91.9% were obtained under the optimum conditions as followed ; the weight ratio of NaOH/waste pottery was 1.5 and the calcination conditions were $900^{\circ}C$ and 60min.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.