Luminescence properties of Eu- and Mn-activated $BaMgP_2O_7$ as a potential red phosphor for white emission

  • Kim, Yong-Kwang;Choi, Sung-Ho;Jung, Ha-Kyun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.581-584
    • /
    • 2008
  • $BaMgP_2O_7$:Eu,Mn phosphors for white emission were synthesized and their luminescent properties were investigated under UV excitation. The phosphor emits two colors: a blue band by $Eu^{2+}$ and a red band by $Mn^{2+}$. Due to the efficient energy transfer from $Eu^{2+}$ to $Mn^{2+}$, the red emission positioned at 615 nm is greatly enhanced with increasing $Mn^{2+}$ content up to 17.5 mol%.

  • PDF

참조기 천연색소의 분리 및 판별법에 관한 연구 (Studies on the Separation and Discrimination of the Natural Yellow Pigment on Croaker)

  • 김희연;홍기형;홍진환;김동술;한상배;이은주;이정성;강길진;정형욱;송경희;박종석;권용관;장영미;신일식;이창국;박희열;하상철;조재선;박혜경
    • 한국식품과학회지
    • /
    • 제34권5호
    • /
    • pp.762-769
    • /
    • 2002
  • 참조기 추출색소를 컬럼크로마토그래피를 행하여 정제하고 UV-vis spectrophotometry를 행하여 최대 흡수파장을 검색한 결과는 모든 획분의 최대 흡수파장은 $480\;nm{\sim}420\;nm$ 사이에 공통적으로 3개의 최대흡수대역을 나타냈다. 이는 carotenoid의 일반적인 특성과 일치하였으며 파장의 대역도 유사하여 carotenoid계 색소로 추정되었다. 또한 획분 간에 파장의 대역이 큰 차이 없이 유사한 것은 구조가 비슷한 이성체이기 때문으로 추정된다. 이동상 A인 0.1 mol 암모늄아세테이트 용액 메탄올(50 : 50 v/v)과 이동상 B인 메탄올 : 메틸렌클로라이드(90 : 10 v/v)를 이용하고 처음 2분간 10%의 이동상 A로부터 시작하여 60분 동안 이동상 B로 점차 조성을 변화시켜 최종적으로 이동상 B가 되게 gradient mode 조건으로 한 이동상에서 PDA-HPLC를 이용하여 참조기 추출색소를 분석한 chromatogram은 각각 RT값이 27.54, 28.48, 29.40, 29.72. 30.06, 35.61에서 총 6개의 peak가 검출되었다. 이때의 검출파장은 약 $380{\sim}490\;nm$ 사이의 파장이었으며, RT값이 30.06와 35.61 사이에 한 개의 peak가 보였으나 그 양이 너무 적어 peak로 인식되지 않았다. 그러나 이는 UV-vis spectrophotometry를 이용한 추출색소의 최대 흡광도 대역과 거의 일치하여 색소의 조성은 총 7개의 성분인 것으로 사료된다. 본 실험의 결과 참조기 추출색소의 분석을 위한 최적파장은 450 nm인 것으로 사료된다. 이동상 B인 메탄올 : 메틸렌클로라이드(90 : 10 v/v)을 이용하여 isocratic made로 한 이동상의 조건으로 PDA-HPLC를 이용하여 참조기 추출색소를 분석한 chromatogram은 각각 RT값이 3.27, 7.69, 20.92에서 총 3개의 peak가 검출되었고, 이때의 검출파장은 약 $380{\sim}490\;nm$ 사이의 파장으로서 gradient mode로 한 이동상의 조건과 일치하였다. 또한 RT값이 3.27의 peak에서 가장 많은 색소가 검출되었다. 그러나 gradient mode로 한 이동상의 조건에서 7개의 peak가 검출되었고 isocratic mode로 한 이동상의 조건에서는 3개의 peak가 검출된 것으로 보아 정성적으로는 gradient mode로 한 이동상의 조건이 더 적합한 것으로 사료된다. 또한, PDA-HPLC를 이용한 참조기와 수조기의 색소성분을 비교한 결과, 수조기와 참조기에서 검출되는 peak중 각각의 3개의 peak는 유사한 RT값을 보였으나, 참조기 및 수조기의 각각 1개의 peak는 서로 다른 RT값을 보였으며 참조기 성분의 peak중 RT = 31.02는 수조기 성분에서는 발견되지 않아, 이 성분은 참조기 성분과 연관성이 클 것으로 사료된다.

역상 고속 액체크로마토그래피를 이용한 인삼 사포닌의 분석 (Determination of Ginseng Saponins by Reversed-Phase High Performance Liquid Chromatography)

  • 정승일;김천석;이노운;최강주;이용구;김일광
    • 분석과학
    • /
    • 제11권6호
    • /
    • pp.436-439
    • /
    • 1998
  • 인삼 사포닌을 역상 고속 액체크로마토그래피 방법을 이용하여 여러 종류의 컬럼으로 분석하였다. 최적 조건은 Novapak $C_{18}$ ODS 역상 칼럼($3.9mm{\times}150mm$, $5{\mu}m$), $CH_3CN/H_2O$ 이성분 이동상 용액과 기울기 제어장치, 그리고 1.5 mL/min의 용매 흐름속도였으며, UV 검출기(203 nm)를 사용하였다. 인삼의 주성분인 ginsenoside $Rb_1$, $Rb_2$, Rc, Rd, Re, Rf 그리고 $Rg_1$ 7종을 50분 안에 양호하게 분리하였다. 각 성분에 대한 검량선은 직선성이 좋았으며, 회귀계수는 0.98~0.99이었다.

  • PDF

원자층 증착법으로 성장한 HfO2 박막의 제조 (Preparation of Hafnium Oxide Thin Films grown by Atomic Layer Deposition)

  • 김희철;김민완;김형수;김혁종;손우근;정봉교;김석환;이상우;최병호
    • 한국재료학회지
    • /
    • 제15권4호
    • /
    • pp.275-280
    • /
    • 2005
  • The growth of hafnium oxide thin films by atomic layer deposition was investigated in the temperature range of $175-350^{\circ}C$ using $Hf[N(CH_3)_2]_4\;and\;O_2$ as precursors. A self-limiting growth of $0.6\AA/cycle$ was achieved at the substrate temperature of $240-280^{\circ}C$. The films were amorphous and very smooth (0.76-0.80 nm) as examined by X-ray diffractometer and atomic force microscopy, respectively. X-ray photoelectron spectroscopy analysis showed that the films grown at $300^{\circ}C$ was almost stoichiometric. Electrical measurements performed on $MoW/HfO_2$(20 nm)/Si MOS structures exhibited high dielectric constant$(\~17)$ and a remarkably low leakage current density of at an applied field of $1.5-6.2\times10^{-7}A/cm^2$ MV/cm, probably due to the stoichiometry of the films.

A 60-GHz LTCC SiP with Low-Power CMOS OOK Modulator and Demodulator

  • Byeon, Chul-Woo;Lee, Jae-Jin;Kim, Hong-Yi;Song, In-Sang;Cho, Seong-Jun;Eun, Ki-Chan;Lee, Chae-Jun;Park, Chul-Soon
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • 제11권4호
    • /
    • pp.229-237
    • /
    • 2011
  • In this paper, a 60 GHz LTCC SiP with low-power CMOS OOK modulator and demodulator is presented. The 60 GHz modulator is designed in a 90-nm CMOS process. The modulator uses a current reuse technique and only consumes 14.4-mW of DC power in the on-state. The measured data rate is up to 2 Gb/s. The 60 GHz OOK demodulator is designed in a 130nm CMOS process. The demodulator consists of a gain boosting detector and a baseband amplifier, and it recovers up to 5 Gb/s while consuming low DC power of 14.7 mW. The fabricated 60 GHz modulator and demodulator are fully integrated in an LTCC SiP with 1 by 2 patch antenna. With the LTCC SiP, 648 Mb/s wireless video transmission was successfully demonstrated at wireless distance of 20-cm.

Fabrication of Piezoelectric Micro Bending Actuators Using Sol-Gel Thick PZT films

  • Park, Joon-Shik;Yang, Seong-Jun;Park, Kwang-Bum;Yoon, Dae-Won;Park, Hyo-Derk;Kang, Sung-Goon;Lee, Nak-Kyu;Na, Kyoung-Hoan
    • 반도체디스플레이기술학회지
    • /
    • 제3권3호
    • /
    • pp.1-4
    • /
    • 2004
  • Fabrication and electrical and mechanical properties of piezoelectric micro bending actuators (PMBA) using sol-gel-multi-coated thick PZT films and MEMS processes were investigated. PMBA could be used for design and fabrication of micro fluidic devices, for example, micro-pumps, micro dispensers, and so on. PMBA were fabricated using 2 um thick PZT films on Pt (350 nm)/$SiO_2$ (500 nm)/Si ($300\mu\textrm{m}$) substrates and MEMS processes. 7 types of PMBA were fabricated with areas of silicon diaphragms, PZT films and top electrodes. When the sizes of silicon diaphragms, PZT films and Pt top electrodes were reduced from 3000$\times$$1389\mu\textrm{m}$, 4000$\times$$1000\mu\textrm{m}$ and 4000$\times$$900\mu\textrm{m}$ down to 14%, 14% and 11 % of them, respectively, the center displacements of PMBA were decreased from 0.68 um to 0.10 um at 5 Hz and 12 Vpp. So, PMBA with large areas showed larger displacements than PMBA with small areas and experimental results were also good agreement with the plate and shell theory.

  • PDF

Characterization and Genomic Analysis of Novel Bacteriophage ΦCS01 Targeting Cronobacter sakazakii

  • Kim, Gyeong-Hwuii;Kim, Jaegon;Kim, Ki-Hwan;Lee, Jin-Sun;Lee, Na-Gyeong;Lim, Tae-Hyun;Yoon, Sung-Sik
    • Journal of Microbiology and Biotechnology
    • /
    • 제29권5호
    • /
    • pp.696-703
    • /
    • 2019
  • Cronobacter sakazakii is an opportunistic pathogen causing serious infections in neonates. In this study, a bacteriophage ${\Phi}CS01$, which infects C. sakazakii, was isolated from swine feces and its morphology, growth parameters, and genomic analysis were investigated. Transmission electron microscopy revealed that ${\Phi}CS01$ has a spherical head and is 65.74 nm in diameter with a 98.75 nm contracted tail, suggesting that it belongs to the family Myoviridae. The major viral proteins are approximately 71 kDa and 64 kDa in size. The latent period of ${\Phi}CS01$ was shown to be 60 min, and the burst size was 90.7 pfu (plaque-forming units)/infected cell. Bacteriophage ${\Phi}CS01$ was stable at $4-60^{\circ}C$ for 1 h and lost infectivity after 1 h of heating at $70^{\circ}C$. Infectivity remained unaffected at pH 4-9 for 2 h, while the bacteriophage was inactivated at pH <3 or >10. The double-stranded ${\Phi}CS01$ DNA genome consists of 48,195 base pairs, with 75 predicted open reading frames. Phylogenetic analysis is closely related to that of the previously reported C. sakazakii phage ESP2949-1. The newly isolated ${\Phi}CS01$ shows infectivity in the host bacterium C. sakazakii, indicating that it may be a promising alternative to antibacterial agents for the removal of C. sakazakii from powdered infant formulas.

Photoluminescence and cathodoluminescence properties of Tb-activated calcium zirconate phosphor

  • Lee, Dae-Won;Oh, Jae-Suk;Jung, Ha-Kyun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
    • /
    • pp.1523-1525
    • /
    • 2005
  • $CaZrO_3:Tb$ as a new green-emitting phosphor, has been synthesized by solid state reaction. Photoluminescence and cathodoluminescence properties for the phosphor with a Perovskite structure were investigated. The $CaZrO_3:Tb$ phosphor, which has several emission peaks due to energy transfer from $^5D_4$ to $^7F_J(J=6,5,4,3)$ of $Tb^{3+}$ ion, exhibited strong green luminescence with the main emission peak centered at 545 nm. Optimum Tb concentration was 0.02mol%.

  • PDF

Luminescence of $Eu^{3+}-doped\;GdCa_4B_3O_{10}$ phosphor under UV and VUV irradiation

  • Oh, Jae-Suk;Kwak, Chung-Heop;Jung, Ha-Kyun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2006년도 6th International Meeting on Information Display
    • /
    • pp.1355-1359
    • /
    • 2006
  • Due to its efficient red emission, $Eu^{3+}$ ion has been doped in various host materials. $GdCa_4B_3O_{10}:Eu^{3+}$ phosphor for red emission has been prepared by solid state reaction. Photoluminescence properties for the phosphor under UV and VUV excitation were investigated. The $GdCa_4B_3O_{10}:Eu^{3+}$ phosphor under both excitation conditions shows typical red emission spectrum centered at 611 nm with several weak peaks due to energy transfer from $^5D_O\;to\;^7F_J(J=1,2,3,4)$ of $Eu^{3+}$ ion. On the other hand, the activator content exhibiting the concentration quenching under UV and VUV irradiation is 10 mole% and 2.5 mole%, respectively.

  • PDF

Experimental Investigation of a High-repetition-rate Pr3+:YLF Laser with Single-frequency Oscillation

  • Dai, Weicheng;Jin, Long;Dong, Yuan;Jin, Guangyong
    • Current Optics and Photonics
    • /
    • 제5권6호
    • /
    • pp.721-729
    • /
    • 2021
  • We demonstrate a Pr3+:YLF 639.7-nm laser with single-frequency output based on the Q-switched pre-lase technology, pumped by a fiber-coupled GaN blue laser diode. The pre-lase technology is realized by the step-type loss of the acousto-optical Q-switched device. The conclusions of the theoretical research are verified experimentally. The mode-suppression ratio was 44 dB at the single-frequency laser output. Detection by interferometer verified the realization of the stable single-frequency laser. In addition, the emission spectrum had a linewidth of 139.9 MHz, measured by Fabry-Perot interferometer. The single-frequency laser's single-peak power was over 19.7 W with 98.8-ns pulse duration, obtained under an absorption power of 1.74 W.