• 제목/요약/키워드: 3점 굽힘

검색결과 165건 처리시간 0.026초

다층 구조 폼 코아 샌드위치 복합재의 기계적 거동 연구 (Mechanical behaviors of multi-layered foam core sandwich composite)

  • 오진오;윤성호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.381-382
    • /
    • 2006
  • The mechanical behaviors of multi-layered foam core sandwich composite were investigated through a 3-point bending test. The sandwich specimens were obtained from sandwich panel consisting of aluminum faces and urethane foam core. Three types of sandwich specimens such as a single structure, a double structure and a triple structure were considered. The span of sandwich specimens were varied from 170mm to 350mm. According to the results, the flexural and shear properties of multi-layered sandwich composite were found to be higher than those of single-layered sandwich composite.

  • PDF

분말고속도공구강 JYPS-23에서 열처리조건에 따른 3점 굽힘피로특성 (Three Point Bending Fatigue Property with Heat Treatment Condition in a Powder Metallurgical High Speed Steel JYPS-23)

  • 홍성현;배종수;김용진
    • 한국분말재료학회지
    • /
    • 제7권3호
    • /
    • pp.131-136
    • /
    • 2000
  • The effect of tempering temperature on the three point bending fatigue behavior of a P/M high speed steel JYPS-23 (1.28% C, 4.20% Cr, 6.40% W, 5.00% Mo, 3.10% V, bal. Fe) was investigated. The number of cycles to failure of the specimen austenitized at $1175^{\circ}C$ drastically increased with increasing tempering temperature. As tempering temperature increased from 500 to $620^{\circ}C$, the volume fraction and average size of carbides (MC or M6C) did not significantly changed, while hardness decreased drastically. The reduced hardness is due to the softening of matrix, which increased the resistance of the fatigue crack propagation. For a practical application, powder compacting test were also conducted with the P/M high speed steel punches tempered at 500, 580, and $620^{\circ}C$. The number of compacting cycles to failure of the punches also increased with increasing tempering temperature.

  • PDF

세라믹/금속접합재의 고온 열사이클에 따른 잔류응력분포 및 굽힘강도 특성 (Characteristics of bending strength and residual stress distribution on high thermal cycle of ceramic and metal joint)

  • 박영철;허선철;부명환;김현수;강재욱
    • 대한기계학회논문집A
    • /
    • 제21권10호
    • /
    • pp.1541-1550
    • /
    • 1997
  • Since the ceramic/metal joint material is made at a high temperature, the residual stress develops when it is cooled from bonding temperature to room temperature due to remarkable difference of thermal expansion coefficient between ceramic and metal. As residual stress at ceramic/metal joints influences the strength of joints, it is important to estimate residual stress quantitatively. In this study, it is attempted to estimate joint residual stress of Si$_3$N$_4$STS304 joints quantitatively and to compare the strength of joints. The difference of residual stress is measured when repeated thermal cycl is loaded, under the conditions of the practical use of the ceramic/metal joint. The residual stress increases at 1 cycle of thermal load but decreases in 3 cycles to 10 cycles of thermal load. And 4-point bending test is performed to examine the influence of residual stress on fracture strength. As a result, it is known that the stress of joint decreases as the number of thermal cycle increases.

가동 철심형 용접기와 정현파를 출력하는 디지털 용접기의 3점식 굽힘시험을 이용한 용접성 비교 분석 (Comparative analysis of weldability using a three-point bending test of a movable iron core welder and a digital welder that outputs a sine wave)

  • 김종식;이광호;주이환;고종철;윤경열
    • 문화기술의 융합
    • /
    • 제9권1호
    • /
    • pp.605-611
    • /
    • 2023
  • 본 연구에서는 자연환경에 영향을 주는 에너지를 절감하기 위해 피복아크용접에서 가동철심형 용접기와 전력사용량이 적은 디지털 용접기(인버터 방식)를 비교하여 전력 사용은 적으며 용접성은 동일한 조건을 갖춰야 하는 부분을 확인하고자 한다. 가동철심형 용접기는 정현파를 출력하는 교류를 사용하며 디지털 용접기 또한 정현파 교류를 발생시켜 동일 조건을 갖추고 전력사용량은 적으며 같은 용접성을 갖추어야 한다. 다만 용접성은 다양하게 검증할 수 있으나 국가기술자격 용접 분야의 자격시험으로 한정하여 분석하고자 한다.

SMC 압축성형재의 기계적 물성 및 특성에 관한 연구 (A Study on Material Characterization and Mechanical Properties of SMC Compression Molding Parts)

  • 김기택;임용택
    • 대한기계학회논문집
    • /
    • 제18권9호
    • /
    • pp.2396-2403
    • /
    • 1994
  • An experimental study on material characterization and mechanical properties of SMC(Sheet Molding Compounds) compression method parts was carried out. Simple compression test using grease oil as a lubricant was carried out to characterize flow stress of SMC at elevated temperatures. Two different mold temperatures, $130^{\circ}C{\;}and{\;}150^{\circ}C$ and two different mold speeds, 15, 45 mm/min were used for preparing the specimen of SMC compression molded parts. Surface roughness, tensile, and 3-point bending tests were used to determine the effects of molding temperatures and speeds on mechanical properties of compression molded SMC parts. Orientation and distribution of glass fiber in the compression molded SMC parts were also investigated by photographing the burnt flat specimen and taking SEM(Scanning Electron Microscope) of cross-sectional T-specimen.

미세입자 분사마모 표면처리가 Fiber-Reinforced Composite 포스트의 굴곡 강도에 미치는 영향 (Influence of airborne-particle abrasion on flexural strength of fiber-reinforced composite post)

  • 심은주;김진우;조경모;박세희
    • 구강회복응용과학지
    • /
    • 제32권1호
    • /
    • pp.24-31
    • /
    • 2016
  • 목적: 미세입자 분사마모 표면처리가 Fiber-Reinforced Composite (FRC) 포스트의 굴곡강도에 미치는 영향을 평가하는 것이다. 연구 재료 및 방법: 두 종류의 FRC 포스트 (DT Light Post, Size 2, Bisco Inc. / RelyX Fiber Post, Size 3, 3M ESPE)를 사용하여 표면처리에 따라 6개의 그룹으로 무작위 분류하였다. 표면처리를 위해 $30{\mu}m$ Rocatec Soft와 $50{\mu}m$ aluminum oxide를 사용하였다. 표면처리 후 편평한 5 mm 부분을 만능시험기로 3점 굽힘시험을 시행하여 FRC 포스트의 굴곡강도와 굴곡계수를 측정하고 통계분석하였다. 결과: FRC포스트의 미세입자 분사마모 표면처리가 FRC포스트의 굴곡강도와 굴곡계수에는 영향을 미치지 않음을 알 수 있었다. 결론: 임상가들이 FRC포스트에 대하여 미세입자 분사마모 표면처리를 하여도 포스트의 굴곡강도와 굴곡계수에는 영향을 미치지 않으면서 접착강도를 높일 수 있을 근거 중의 하나가 될 수 있을 것이다.

강화 섬유의 분산도가 SiCf/SiC 복합소재의 기계적 강도에 미치는 영향 (Effect of Fiber Dispersion on Mechanical Strength of SiCf/SiC Composites)

  • 최지범;김수현;이슬희;한인섭;방형준;김세영;성영훈
    • Composites Research
    • /
    • 제36권3호
    • /
    • pp.180-185
    • /
    • 2023
  • 본 논문에서는 스프레딩된 SiC 섬유를 적용해 SiCf/SiC를 제조하였을 경우, 섬유의 분산도가 복합소재의 내부구조 및 기계적 강도에 어떠한 영향을 주는지를 연구하였다. Spread SiC 섬유를 적용한 시편의 섬유 체적비는 non-spread 시편 대비 9%p 감소하였으며, 수지 슬러리가 섬유 사이로 더 원활히 함침되어 기지내 기공도 거의 발견되지 않았다. 각 시편의 섬유 분산도를 비교하기 위해, 복합소재 내 섬유간 이격거리를 수치화하고 평가하는 방법을 제안하였다. 그 결과 spread 시편의 섬유간 중심거리는 non-spread 시편 대비 2.23 ㎛ 증가하였으며, 섬유 표면 사이 거리는 42.6%로 대폭 증가하였다. 3점 굽힘시험을 통해 spread 시편의 굽힘강도가 non-spread 시편 대비 49.3% 가량 높으며, 시험 데이터의 편차도 더 균일함을 확인하였다. 따라서 복합소재 기지내 SiC 섬유의 분산도 향상이 SiCf/SiC의 균일한 기지상 치밀화와 기계적 강도 증가에 매우 큰 영향을 미친다는 점을 알 수 있다.

고주파 열처리된 SAE1055 강의 피로거동 및 이의 확률론적 평가 (Probabilistic Analysis of Fatigue Behavior of Induction Hardened Steel)

  • 이선호;이승표;강기원
    • 대한기계학회논문집A
    • /
    • 제37권3호
    • /
    • pp.429-436
    • /
    • 2013
  • 본 논문에서는 고주파 열처리된 SAE1055 베어링강의 경도에 따른 피로 거동 및 이의 확률론적 평가를 수행하였다. 이를 위하여 경도 수준에 따른 5 종류의 시험편(A : 원재료, B : HV390-전경화, C : HV510-전경화, D : HV700-전경화 및 E : HV-700 표면경화)를 준비하였다. 피로시험은 4 점 회전굽힘 피로시험기를 이용하여 응력비 R=-1 의 조건하에서 수행하였다. 그 결과, SAE1055 강의 피로 거동은 경도에 따라 크게 변화하였으나 HV510 수준이상에서는 피로한도의 증가는 관찰되지 않았다. 또한 피로 파손기구에 대한 경도의 영향을 평가하기 위하여 SEM(scanning electron microscope)을 이용한 파면 관찰을 수행하였다. 피로수명의 통계적 특성은 P-S-N(probabilistic S-N) 곡선을 이용하여 평가되었으며 이에 대한 경도의 영향은 잔류치 해석(residue analysis)을 통하여 수행하였다.

유한변형과 굽힘효과가 고려된 3차원 보-기둥요소에 의한 공간구조물의 분기좌굴해석 (A Bifurcation Analysis of Space Structures by Using 3D Beam-Column Element Considering Finite Deformations and Bowing Effect)

  • 이경수;한상을
    • 한국전산구조공학회논문집
    • /
    • 제22권4호
    • /
    • pp.307-314
    • /
    • 2009
  • 본 논문은 기하학적 비선형성을 가진 보존적 단일 하중 매개변수의 탄성 상태 공간구조의 탄성 분기 좌굴해석을 위한 공간프레임의 정식화, 분기경로 추적을 위한 pin-pointing 및 분기경로 전환알고리즘을 기술하고 있다. 복잡한 좌굴 후 거동특성을 파악하기 위한 본 연구의 공간프레임요소는 오일러리안 좌표계에 의한 유한회전이론으로 강체변형을 계산하였고, 굽힘효과가 고려된 보-기둥식을 적용하여 적은 개수의 요소의 사용으로도 정해를 얻을 수 있도록 하였으며, 후좌굴해석과 같은 고도의 비선형해석을 수행하기 위해 기하강성행렬의 모멘트에 대한 영향을 고려하였다. 분기좌굴에 의한 좌굴후 평형상태인 주경로와 분기경로의 pin-pointing 알고리즘으로 특이점을 계산하였으며, 고유치 및 고유모드를 이용한 본 연구의 수치알고리즘에 의해 분기경로를 추적하였다. 분기좌굴 해석예제로 평면프레임, 평면아치 및 공간돔에 대한 분기좌굴 해석을 수행하여 본문에서 제시한 수치해석법의 정확성 및 적용성을 검증한다.

빙해항행선박의 선수부 형상과 쇄빙능력에 관한 연구 (A Study on Bow Hull Form and Icebreaking Capability of Icebreaking Vessels)

  • 최경식;손창배;팽은경
    • 대한조선학회논문집
    • /
    • 제29권4호
    • /
    • pp.87-97
    • /
    • 1992
  • 극지방의 천연자원의 수송에 필수적인 빙해항행선박은 금후 우리나라의 조선산업이 지향해야 할 기술집약형 선박중 하나로서 국제경쟁에 대비하여 독자적인 연구가 요구되는 분야이다. 본 연구는 빙해항행선박 기본설계의 중요한 인자인 선수부 형상과 평탄빙에서의 쇄빙능력 사이의 상관관계를 밝히는데 목적이 있다. 통상 평탄빙(level ice)에서 선박의 전진속도를 3-4 knots로 볼 때, 탄성으로 취급되는 얼음의 재료특성을 고려하여, 파괴시킬 수 있는 얼음의 최대두께와 파괴된 얼음의 특성길이를 수치적으로 추정하는데 주안점을 두고 있다. 본 연구에서는 빙해항행 선박이 평탄빙에서 연속쇄빙을 하고 있는 상황을 탄성지지기반 위에 놓인 유한 길이의 쐐기보에 작용한 충격하중의 문제로 가정하고 굽힘모멘트에 의해 어떤 위치에서 발생한 최대인장응력이 얼음의 굽힘파괴강도에 도달한다면 그 부분에서 파단이 일어날 가능성이 가장 높다고 판단한다.

  • PDF