Preparation of Ultrafine Mullite Powder from Metal Alkoxides (금속 알콕사이드로부터 Mullite 초미분체의 제조)

  • Yim, Going;Yim, Chai-Suk;Kim, Young-Ho
    • Korean Journal of Materials Research
    • /
    • v.16 no.12
    • /
    • pp.719-724
    • /
    • 2006
  • Ultrafine mullite powder was prepared from aluminium-secbutoxide and tetraethyl orthosilicate(TEOS) in the molar $Al_2O_3/SiO_2$=3/2. Sol-gel method by partial hydrolysis technique, as it were, first, TEOS was partially hydrolysized and then mixed with Al-secbutoxide for complete hydrolysis was used. X-ray diffraction, infrared spectroscopy and transmission electron microscopy, etc. confirmed that the mullite powder prepared by this method is in the stoichiometric $Al_2O_3/SiO_2$ ratio. Al-Si spinel was formed at $980^{\circ}C$ and ultrafine mullite powder with about 20 nm particle size was obtained above $1,200^{\circ}C$. Also mullite powders calcined at $1,600^{\circ}C$ had a stoichiometric composition, $3Al_2O_3{\cdot}2SiO_2$ and the lattice constants of the mullite powders calcined above $1,200^{\circ}C$ were almost coincided with theoretical values.

Enzymatic Synthesis of Fructose-based Sugar Fatty Acid Ester Using Methyl Fructoside (메틸프룩토시드를 이용한 과당계열 당 지방산 에스테르의 효소적 합성)

  • 허주형;김해성
    • KSBB Journal
    • /
    • v.13 no.6
    • /
    • pp.706-717
    • /
    • 1998
  • Enzymatic synthesis of fructose-based sugar fatty acid esters, such as methyl fructoside oleic acid mono and diester, was investigated using methyl fructoside as a sugar starting material. For the production of methyl fructoside fatty acid monoester by solvent process, 2-methyl 2-propanol was found to be a god reaction medium resulting a higher yield and productivity due to its high sugar solubility. The yield and productivity of methyl fructoside oleic acid monoester were 70% and 12.6g/L-hr, respectively, when molar ratio of methyl fructoside, initial concentration of methyl fructoside, enzyme(Novozym 435) content, and reaction temperature were 3:1, 200g/L, 1%(w/v), and $60^{\circ}C$, respectively. Methyl fructoside oleic acid diester was prepared by lipase-catalyzed diacylation of methyl fructoside and oleic acid in the solvent-free process. Maximum yield of 98% and productivity of 140g/L-hr were achieved when molar ratio(methyl fructoside and oleic acid) of 1:2 enzyme content of 10%(w/v) and reaction temperature of $70^{\circ}C$ were applied for the operating conditions under a reduced pressure of 20∼200 mmHg.

  • PDF

Reduction of NOx by CO on the Lanthanoid Perovskite-type Catalysts for Hot Gas Cleanup (고온 배가스 처리용 Lanthanoid계 Perovskite 형 촉매상에서 CO에 의한 NOx의 환원)

  • Lee, Jea-Keun;Lee, Jae-Hee;Lim, Jun-Heok
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.22 no.1
    • /
    • pp.169-178
    • /
    • 2000
  • Perovskite oxide catalysts doped on porous alumina beads are prepared in a citric acid solution. To investigate the applicability of the catalysts to the hot gas cleanup, a series of experiments on the reduction characteristics of $NO_x$ by CO as a reducing agent are carried out in a packed bed reactor containing the catalysts. Parameters tested are the operating temperature and $CO/NO_x$ molar ratio. It is found that mixed complex oxides of $La_{0.5}Sr_{0.5}CoO_3$, $SrAl_{12}O_{19}$ and $LaAl_{11}O_{18}$ are uniformly distributed on the alumina beads. The conversion efficiency of $NO_x$ by CO sharply increases with the operating temperature up to $700^{\circ}C$ and then approaches 100% when $CO/NO_x$ molar ratio is greater than 1.0. The conversion efficiency of $NO_x$ is maintained by over 98% during a continuous operation for 23 hours at $800^{\circ}C$ and space velocity of $10700hr^{-1}$.

  • PDF

Treatment of Phenol Contaminated Soil Using Sulfidated Zero-Valent Iron as a Persulfate Activator for Advanced Oxidation Process (황화영가철 기반의 과황산 고도산화공정을 이용한 페놀 오염토양 처리)

  • Hyuk Sung Chung;Nguyen Quoc Bien;Jae Young Choi;Inseong Hwang
    • Journal of Soil and Groundwater Environment
    • /
    • v.28 no.1
    • /
    • pp.15-24
    • /
    • 2023
  • A persulfate(PS)/sulfidated microscale zero-valent iron(S-mZVI) system was tested for treating a soil contaminated with phenol. Sulfidation of bare mZVI was conducted using a mechanochemical process utilizing a ball mill in order to improve persulfate activation capacity and stability of unmodified mZVI. The synthesized S-mZVI performed markedly better than the bare mZVI in activating PS. The optimum molar ratio of sulfur to mZVI was around 0.12. In the soil slurry experiments, a very rapid and complete removal of phenol was observed at the optimum molar ratios of PS to S-mZVI of 2:1 and PS to phenol of 16:1. The phenol removal efficiencies decreased as the water content of the slurries decreased. This was believed to be due to increased soil oxidant demand as the amount of soil was increased as relative to the water content. To evaluate the field applicability of the process, slurry experiments adopting high soil contents were carried out that simulated in-situ soil mixing conditions. These experiments resulted in substantially compromised degradation efficiencies of 54.3% and 43.8% within 4 hours. The current study generally shows that the PS/S-mZVI process has a potential to be developed into a remediation technology for soils contaminated with organics.

Characterization of Synthesized WS$_2$ Solid Lubricant (합성 WS$_2$ 고체윤활제의 특성 분석)

  • 신동우;윤대현;최인혁;김인섭
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1997.10a
    • /
    • pp.211-216
    • /
    • 1997
  • The tungsten disulfide (WS$_2$) solid lubricant was synthesized by two different reaction processes, and the chemical and physical characteristics of synthesized WS$_2$ powder were analyzed in terms of the average particle size, morphology, crystalline phase. The solid WO$_3$ powder with the average size of 0.2 $\mu$m was reacted with CS$_2$ gas flowed with N$_2$ or 96% N$_2$ + 4% H$_2$ forming gas for 36 h and 24 h at 900$\circ$C respectively. In the case of vapour phase transport method, the 3.5 wt% iodine was added as a vapour transport reagent into the composition of tungsten and sulfur powders maintaining a constant molar ratio of W : S = 1 : 2.2. The mixture was then heat treated at 850$\circ$C for 2 weeks in vacuum The reaction product obtained showed the average size of 12 $\mu$m and the hexagonal plate shape of typical solid lubricant with 2H-WS$_2$ crystalline phase.

  • PDF

Synthesis of zeolite from power plant fly ash (화력발전소 비산회를 이용한 제올라이트합성)

  • 김재환;연익준;김광렬
    • Journal of environmental and Sanitary engineering
    • /
    • v.12 no.1
    • /
    • pp.49-58
    • /
    • 1997
  • A study on the synthesis of zeolite from bituminous coal ESP fly ash as a raw material, which was emitted from the power plant, was carried out to reduce environmental problems and reuse of the industrial wastes. Bituminous coal fly ash was used as the source of silica and alumina. Zeolite was synthesized by hydrothermal reaction in aqueous NaOH solution with sodium aluminate as additive. The objective of this study is to elucidate the effect of several experimental variables on the synthesis of zeolite. The effects of preroasting temperature, mixing speed, leaching alkalinity, and molar ratio of Na$_{2}$O/SiO$_{2}$ and SiO$_{2}$/Al$_{2}$O of the products were investigated. The synthesized zeolite was proved to be NaA, which is known as 4A type, by comparing with SEM images, and X-ray diffraction analysis. And also we know that the transformation of zeolite A take places into other types of zeolites, i.e. Hydroxysodalite, zeolite P, with the variation of leaching alkalinity.

  • PDF

Studies on Synthesis of Magnesium Carbonate. I. Factorial Analysis on the Preparation of Exrta-light Magnesium Carbonate (탄산마그네슘의 제조연구 I 경질탄산마그네슘의 제조조건)

  • Rhee, Gye-Joo;Song, Churl;Sung, Nak-Won;Ahn, Yung-Pil
    • YAKHAK HOEJI
    • /
    • v.15 no.1
    • /
    • pp.24-31
    • /
    • 1971
  • Optimum reaction conditions for the preparation of extra-light magnesium carbonate from bittern by the reaction with sodium carbonate solution was found to be as follows: reaction temperature 33.deg. molar ratio(Mg$^{+2}/CO$^{2-}_{3}$)0.8, reaction time 14 minutes, drying temperature 99.deg. and bittern concentration 17%. While Korean pharmacopeia regulates the bulkiness above 12 mililiters per gm., our experimental result shows above 45 mililiters. Electron microscopic shapes were compared with products prepared under various reaction conditions, and it was found that there exists lighter the powder the more pillar crystalline, the heavier the powder the more amorphous and the intermediate was mixture of them.

  • PDF

Synthesis of Biodiesel from Soybean Oil Using Lewis Acidic Ionic Liquids Containing Metal Chloride Salts (금속염화물을 첨가한 루이스산 이온성 액체 촉매를 이용한 대두유로부터 바이오디젤 합성)

  • Choi, Jae Hyung;Park, Yong Beom;Lee, Suk Hee;Cheon, Jae Kee;Choi, Jae Wook;Woo, Hee Chul
    • Korean Chemical Engineering Research
    • /
    • v.48 no.5
    • /
    • pp.643-648
    • /
    • 2010
  • Production of biodiesel from soybean oil catalyzed by Lewis acidic ionic liquids(ILs) containing metal chloride salts was investigated in this study. Metal chloride salts, such as $SnCl_2$, $ZnCl_2$, $AlCl_3$, $FeCl_3$ and CuCl, were screened for oil transesterification in the range of 363-423 K. Among these metal chlorides, tin chloride showed particularly high catalytic property for the oil transesterification. Similarly, among these Lewis acidic ionic liquid catalysts, $[Me_3NC_2H_4OH]Cl-2SnCl_2$ resulted in a high fatty acid methyl esters(FAMEs) content of 91.1% under the following reaction conditions: 403 K, 14 h, and a molar ratio of 1:12:0.9 (oil:methanol:catalyst). Unlike the pure tin chloride catalysts, Lewis acidic ILs containing tin chloride $[Me_3NC_2H_4OH]Cl-2SnCl_2$ catalyst could be recycled up to five times without any significant loss of activity by separating from the FAMEs with simple decantation. The Lewis acidity and high moisture-stability of this catalyst appeared to be responsible for the excellent catalytic performance. The effects of reaction time and the molar ratio of methanol/catalyst to oil on the FAMEs production were also studied in this work.

Fabrication of 1 ㎛ Thickness Lead Zirconium Titanate Films Using Poly(N-vinylpyrrolidone) Added Sol-gel Method

  • Oh, Seung-Min;Kang, Min-Gyu;Do, Young-Ho;Kang, Chong-Yun;Yoon, Seok-Jin;Nahm, Sahn
    • Transactions on Electrical and Electronic Materials
    • /
    • v.12 no.5
    • /
    • pp.222-225
    • /
    • 2011
  • Lead zirconate titanate (PZT) films were fabricated on Pt/Ti/$SiO_2$/Si substrate by the sol-gel method using a sol containing poly(N-vinylpyrrolidone) (PVP). PVP in alkoxide solutions can suppress the condensation reaction in gel films during heat treatment, and increase the viscosity of alkoxide solutions. Single-phase PZT films as thick as 1 ${\mu}m$ were deposited by repetitive coating with successive third-step heat treatments at 150$^{\circ}C$, 350$^{\circ}C$ and 650$^{\circ}C$. After heat treatment, the films were crack free, and optically transparent. As a result, we demonstrated a PZT film with a PVP molar ratio of 0.5, which has a permittivity of 734, a dielectric loss of 0.042, a $P_r$ of 40.5 ${\mu}C/cm^2$ and an $E_c$ of 156 kV/cm.

Physico-Chemical and Rheological Properties of a Bioflocculant BF-56 from Bacillus sp. A56

  • Suh, Hyun-Hyo;Moon, Seong-Hoon;Seo, Weon-Taek;Kim, Kyung-Kab;Jeon, Gee-Ill;Park, Hyun-Geoun;Park, Yong-Il
    • Journal of Microbiology and Biotechnology
    • /
    • v.12 no.2
    • /
    • pp.209-216
    • /
    • 2002
  • Bacillus sp. A56 was studied, because of its high flocculating activity. The flocculating substance produced by this strain was purified by ethanol precipitation, cetylpyridinium chloride (CPC) precipitation, and gel permeation chromatography (GPC). The FT-IR spectrum of the purified bioflocculant, designated as BF-56, showed typical characteristics of polysaccharides. The non-sugar substituents, and sugar components of BF-56 containing glucose, fucose, glucuronic acid, and galactose in an approximate molar ratio of 2.76:1.10:1:0.12, suggested that it was a novel bioflocculant with an estimated molecular mass of over $7{\times}10^3$ kDa. Rheological analysis of BF-56 revealed that it was a pseudoplastic that had higher apparent viscosity rate at dilute concentrations than those of zooglan. The solution of bioflocculant BF-56 exhibited non-Newtonian characteristics and it was compatible to high concentrations of salts such as KCl, NaCl, $CaCl_2,\;or\;FeCl_3.$ The present results suggested strong possibility of bioflocculant BF-56 to be fully applicable to industries such as wastewater treatment.