• Title/Summary/Keyword: 철근 파단

Search Result 59, Processing Time 0.02 seconds

Development Length Effects of High Strength Headed Bar (고강도 확대머리 이형철근의 정착길이 효과에 관한 실험적 연구)

  • Moon, Jeong-Ho;Oh, Young-Hun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.5
    • /
    • pp.75-82
    • /
    • 2015
  • An experimental study has been carried out to examine development length effects for high strength headed deformed bars. Current design codes limit the specified yield strength of headed bars to 400 MPa. Such the limit is due to the lack of experimental studies on headed bars made of high strength materials. Thus a test program was planed with headed bars with the yield strength of 600 MPa. The threaded head type with head shapes of round plate and circular cone was selected in this study. The experimental variables were development length, number of bars, and head shape. Specimens were classified into L-type and S-type depending on the development length. The development length of L-type was computed according to the design code without considering the limit. S-type specimens had shorter development lengths than the L-type. Further classification was made depending on the shape of heads. A-types have the head shape of round plate and B-types have the shape of circular cone. Three L-type specimens were fabricated with the variable of number of bars (1, 2, and 3). Four specimens for each of SA and SB types were made with development lengths of 50%, 45%, 40%, and 35% compared with L-type. Pullout tests was carried out with 11 specimens. The test results were compared with computed strengths with the design code equations (Appendix II). Based the current studies, it can be said that high strength headed deformed bars used in this study be able to provide such strengths computed with the current design code without considering the yield strength limit.

Generalized Lateral Load-Displacement Relationship of Reinforced Concrete Shear Walls (철근콘크리트 전단벽의 횡하중-횡변위 관계의 일반화)

  • Mun, Ju-Hyun;Yang, Keun-Hyeok
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.2
    • /
    • pp.159-169
    • /
    • 2014
  • This study generalizes the lateral load-displacement relationship of reinforced concrete shear walls from the section analysis for moment-curvature response to straightforwardly evaluate the flexural capacity and ductility of such members. Moment and curvature at different selected points including the first flexural crack, yielding of tensile reinforcing bar, maximum strength, 80% of the maximum strength at descending branch, and fracture of tensile reinforcing bar are calculated based on the strain compatibility and equilibrium of internal forces. The strain at extreme compressive fiber to determine the curvature at the descending branch is formulated as a function of reduction factor of maximum stress of concrete and volumetric index of lateral reinforcement using the stress-strain model of confined concrete proposed by Razvi and Saatcioglu. The moment prediction models are simply formulated as a function of tensile reinforcement index, vertical reinforcement index, and axial load index from an extensive parametric study. Lateral displacement is calculated by using the moment area method of idealized curvature distribution along the wall height. The generalized lateral load-displacement relationship is in good agreement with test result, even at the descending branch after ultimate strength of shear walls.

Evaluation of Ductility Capacity of Reinforced Concrete Bridge Columns Subject to Cyclic Loading Using Flexibility-Based Fiber Element Method (유연도법 섬유요소모델에 의한 반복하중을 받는 철근콘크리트 교각의 연성능력 평가)

  • 고현무;조근희;조호현
    • Journal of the Earthquake Engineering Society of Korea
    • /
    • v.6 no.3
    • /
    • pp.11-21
    • /
    • 2002
  • The evaluation of displacement ductility is performed by direct method through tracking the inelastic hysteretic behavior of RC bridge columns subject to cyclic loading using a flexibility-based fiber element mode. To reasonably track the inelastic behavior until the RC bridge column reaches its ultimate state, the average stress-average strain relations and joint elements, which agree well with experiments, are modified and applied considering the tension stiffening behavior and discontinuous displacement between the column and its base. In addition the evaluation of displacement ductility is performed by a direct method easily applicable to numerical analysis. Locations for the integration points, values for the post-crushing concrete strength and low-cycle fatigue failure of longitudinal reinforcement that affect the calculation of yielding and ultimate displacements are proposed for the application to flexibility-based fiber element model. Since less than 10% of error occurs during the displacement ductility analysis, the yielding and ultimate displacements evaluated by the applied analysis method and model appear to be valid.

The Study of Longitudinal Joint with Tensile Grip Connection in Highway Bridges (교축방향 인장이음에 관한 연구)

  • Seo, Seung-Tag
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.9 no.2
    • /
    • pp.155-160
    • /
    • 2006
  • 합성상판을 시공하는 경우 교축방향에 분할된 저강판을 접합 일체화해야 한다. 본 논문에서는 강 콘크리트 합성상판을 대상으로 3종류의 배력철근 방향 이음구조를 제안하며, 보 공시체에 의한 정적 정점피로 실험한다. 그 결과 보의 피로실험 결과 저강판 혹은 고력볼트가 피로파단 하였으며, 3차원 FEM해석에 이음부의 휨 강성도 및 피로강도에 대해서 해석적으로 검토된다.

  • PDF

Tensile Test for Lap Welded Joints of Rebars(SD400) (일반철근(SD400) 용접 겹침이음 인장실험)

  • Park, Won-Tae;Chun, Kyoung-Sik
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.5
    • /
    • pp.570-576
    • /
    • 2018
  • In reinforced concrete structures, the joints of ordinary rebars are usually lap joints, which are bound by binding wires with rebars, and mechanical joints by couplers. In domestic design standards (concrete design code), welded lap joints are restricted for ordinary rebars, but overseas standards allow welded lap joints of ordinary rebars through pre-heating. This study investigated the domestic and international standards/criteria and evaluated the fracture strength by performing the tensile test on the lap welded joint of SD400 grade rebars, which is used the most in the construction sites. The weld length of the specimen for weld lap joints is based on the minimum weld length (8d) given in the KS standard (KS B ISO 17660-1). According to AWS D1.4, the preheating temperature was set to $150^{\circ}C$ for D19 and below, and $260^{\circ}C$ for D22 and above. In the test results, the tensile strength of rebars with welded lap joints exceeded the required strength (125% of the yield strength) according to the concrete design code. To analyze the effect of preheating, the tensile strength of the welded rebars after preheating was not significantly different from that of the welded rebars without preheating. The carbon equivalent content (Ceq) of the rebars used in the test was 0.45% or less. Under AWS D1.4, no preheating is required if the carbon equivalent is less than 0.45%. All specimens with a welded lap length of 8d failed by a bar fracture. The effect of preheating was confirmed to be insignificant due to the low carbon equivalent of the rebar.

A Study on the Flexural Minimum Reinforcement for Prevention of Brittle Failure Specified in KCI and EN Codes (유럽과 국내기준에 규정된 취성파괴 방지를 위한 휨 최소철근량 고찰)

  • Park, Sung-Jae;Kang, Tae-Sung;Moon, Do-Young
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.2
    • /
    • pp.211-218
    • /
    • 2014
  • In the design of reinforced rectangular concrete beam structure, the minimum amount of flexural reinforcement is required to avoid brittle failure. KCI code is based on concept of ultimate strength and usually used as a model code. But bridge design code enacted by Ministry of land, transportation and maritime affairs in 2012 is based on concept of limit state and similar to Euro code EN 1992-2. This means that the minimum reinforcement presented in both design codes has different origination and safety margin. When rectangular concrete beams with minimum reinforcement are designed according to EN and KCI codes, the amount of minimum reinforcement specified in EN code is only 76% of that in KCI code. This makes the design engineers to be confused. In this study, flexural tests were conducted on nine beams with the two different minimum reinforcement specified in KCI and EN design codes. In results, the measured ratios of nominal strength to crack strength from the test were about 25% greater than those evaluated from the equations presented in KCI and EN codes. The EN beams having only 76% of the minimum reinforcement for the KCI beams were fractured by rupture of steel reinforcement but in ductile manner. It is confirmed that the minimum reinforcement concrete beams designed according to both codes have enough safety margin in flexural capacity and moreover in ductility.

Anchorage Strength of High Strength Headed Bar Embedded Vertically on SFRC Members (SFRC 부재에 수직 배근된 고강도 확대머리철근의 정착강도)

  • Lee, Chang-Yong;Kim, Seung-Hun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.1
    • /
    • pp.148-156
    • /
    • 2020
  • The paper is a summary of the results of the basic pullout test which is conducted to evaluate the anchorage capacity of high strength headed bars that is mechanical anchored vertically on steel fiber reinforced concrete members. The main experimental parameters are volume fraction of steel fiber, concrete strength, anchorage length, yield strength of headed bars, and shear reinforcement bar. Both sides of covering depth of the specimen are planned to double the diameter of the headed bars. The hinged point is placed at the position of each 1.5𝑙dt and 0.7𝑙dt around the headed bars, and the headed bars are drawn directly. As a result of pullout test experiment, concrete fracture and steel tensile rupture appear by experimental parameters. The compressive strength of concrete is 2.7~5.4% higher than that of steel fiber with the same parameters, while the pullout strength is 20.9~63.1% higher than that of steel fiber without the same parameters, which is evaluated to contribute greatly to the improvement of the anchorage capacity. The reinforcements of shear reinforcements parallel to the headed bars increased 1.7~7.7% pullout strength for steel fiber reinforced concrete, but the effect on the improvement of the anchorage capacity was not significant considering the increase in concrete strength. As with the details of this experiment, it is believed that the design formula for the anchorage length of KCI2017and KCI2012 are suitable for the mechanical development design of SD600 head bar that is perpendicular to the steel fiber reinforced concrete members.

An Experimental Study on the Flexural Behavior of RC Beams Strengthened with Near-Surface-Mounted CFRP Strips (표면매입 탄소섬유판으로 보강된 철근콘크리트 부재의 휨 거동에 관한 실험연구)

  • Lim, Dong-Hwan
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.12 no.6
    • /
    • pp.89-96
    • /
    • 2008
  • The purpose of this study is to investigate the flexural strengthening effectiveness for the beams reinforced with NSM CFRP strips. To accomplish this objective, concrete T beams were made and tested. From this study, it is found that the flexural stiffness and strength of the beams reinforced with NSM strips were significantly improved compared to the beams without CFRP strip. The maximum increase of flexural strength was 247%. Failure of the beam reinforced with NSM was initiated by a part of separation of NSM strips along the longitudinal direction, and the second failure of strips was investigated. After the first rupture of the NSM strips, the load dropped suddenly and the second rupture was succeeded. This result shows that a perfect composite reaction with NSM strips and concrete is possible in the beam reinforced with NSM CFRP strips the NSM strips and Near surface mounted(NSM) is one of the most recent and promising strengthening techniques for reinforced concrete structures.

Development of Non-Shrink Mortar Grouting Type Splice Sleeve (무수축 모르타르 충진형 슬리브 개발)

  • Lee, Young-Ho;Song, Jae-Joon;Cho, Jae-Young;Kim, Do-Hak
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.11 no.2
    • /
    • pp.67-73
    • /
    • 2011
  • This study aims to develop an economical precast hollow concrete column with high constructability which consists of only splice sleeve and general reinforcing bar without using PC tendons in order to reduce the construction period and cost. With this purpose, this study performed the finite element analysis and tension test by using some variables such as length of sleeve, diameter of rebar and curing method for suggesting a grouting type splice sleeve which is a new type joint rebar and developing an optimized splice sleeve. As a result, the analysis on the tension performance of splice sleeve did not show any destruction caused by pull-out in reinforcing bar but it only occurred destruction of tension bar or bolt shear rupture from the mechanical defect of sleeve. Therefore, the experiment showed high performance in tension of the suggested splice sleeve and verified the application of precast hollow concrete column.

Strengthening Effect of Reinforced Concrete Beams Strengthened with NSM CFRP Reinforcements and Various Reinforcement Details (다양한 보강상세를 갖는 CFRP로 표면매립 보강된 철근콘크리트 보의 보강효과)

  • Jung, Woo-Tai;Park, Young-Hwan;Park, Jong-Sup;Kim, Chul-Young
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.6
    • /
    • pp.781-790
    • /
    • 2011
  • This paper contains the experimental results on strengthening effect of RC beams strengthened with NSM CFRP reinforcement and various strengthening details. A total of 14 beams have been tested to analyze strengthening effects of NSMR with various reinforcement details. Variables were cross-sectional shape of CFRP reinforcements, strengthening areas, grooves the number and location etc. Test results revealed that failure modes of NSMR showed two types. One was bond failure at interface between concrete and filler and the other was CFRP rupture. Also, failure mode of specimens with two grooves occurred premature bond failure because of superposition of failure surfaces at concrete around grooves. failure mode of MI specimens considered the equivalent section have changed bond failure to CFRP rupture and CFRP efficiency has improved 83% to 100%.