Axial Behavior of Concrete Cylinders Confined with FRP Wires (FRP 와이어 보강 콘크리트 공시체의 압축거동)

  • Cho, Baiksoon;Lee, Jong-Han;Choi, Eunsoo
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.33 no.5
    • /
    • pp.1765-1775
    • /
    • 2013
  • The application of FRP wire as a mean of improving strength and ductility capacity of concrete cylinders under axial compressive load through confinement is investigated experimentally in this study. An experimental investigation involves axial compressive test of three confining amounts of FRP wire and three concrete compressive strengths. The effectiveness of FRP wire confinement on the concrete microstructure were examined by evaluating the internal concrete damage using axial, circumferential, and volumetric strains. The axial stress-strain relations of FRP wire confined concrete showed bilinear behavior with transition region. It showed strain-hardening behavior in the post-cracking region. The load carrying capacity was linearly increased with increasing of the amount of FRP wire. The ultimate strength of the 35 MPa specimen confined with 3 layer of FRP wire was increased by 286% compared to control one. When the concrete were effectively confined with FRP wire, horizontal cracks were formed by shearing. It was developed from sudden expansion of the concrete due to confinement ruptures at one side while the FRP wire was still working in hindering expansion of concrete at the other side of the crack. The FRP wire failure strains obtained from FRP wire confined concrete tests were 55~90%, average 69.5%, of the FRP wire ultimate uniaxial tensile strain. It was as high as any other FRP confined method. The magnitude of FRP wire failure strain was related to the FRP wire effectiveness.

Evaluation of Plastic Collapse Behavior for Multiple Cracked Structures (다중균열 구조물의 소성붕괴거동 평가)

  • Moon, Seong-In;Chang, Yoon-Suk;Kim, Young-Jin;Lee, Jin-Ho;Song, Myung-Ho;Choi, Young-Hwan;Hwang, Seong-Sik
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.28 no.11
    • /
    • pp.1813-1821
    • /
    • 2004
  • Until now, the 40% of wall thickness criterion, which is generally used for the plugging of steam generator tubes, has been applied only to a single cracked geometry. In the previous study by the authors, a total number of 9 local failure prediction models were introduced to estimate the coalescence load of two collinear through-wall cracks and, then, the reaction force model and plastic zone contact model were selected as the optimum ones. The objective of this study is to estimate the coalescence load of two collinear through-wall cracks in steam generator tube by using the optimum local failure prediction models. In order to investigate the applicability of the optimum local failure prediction models, a series of plastic collapse tests and corresponding finite element analyses for two collinear through-wall cracks in steam generator tube were carried out. Thereby, the applicability of the optimum local failure prediction models was verified and, finally, a coalescence evaluation diagram which can be used to determine whether the adjacent cracks detected by NDE coalesce or not has been developed.

A study on the fatigue crack growth of mild steel weldments using flux cored wire $CO_2$ welding (국산 Flux-Cored Wire를 이용한 반자동용접이음새에서의 피로파괴 특성)

  • 엄동석
    • Journal of Welding and Joining
    • /
    • v.7 no.1
    • /
    • pp.42-50
    • /
    • 1989
  • The application of fracture mechanics is being increased gradually to assess the safety of welded structures containing crack. Fatigue crack propagation behavior and elastic-plastic fracture toughness J$_{IC}$ of home made flux cored wire(1.22mm) CO$_{2}$ weldments was discussed. Especially fatigue crack propagation test was carried out by .DELTA.K control instead of load control and elastic-plastic fracture toughness J$_{IC}$ was obtained by ASTM-R curve method on C.T.specimen in transverse direction of weldments. The results obtained are as follows; (1) Weld metal presented an almost complete similarity to base metal on fatigue crack propagation rate in transverse direction. (2) Weld metal was more than base metal on J$_{IC}$ value in transverse direction. (3) F.C.W. CO$_{2}$ weldments had an excellent characteristic of fatigue crack propagation rate and J$_{IC}$ in less than 50kg/mm$^{2}$ steel grade, this would result from that weld metal had good static strength.trength.

  • PDF

Evaluation for Rock Cleavage Using Distribution of Microcrack Lengths and Spacings (1) (미세균열의 길이 및 간격 분포를 이용한 결의 평가(1))

  • Park, Deok-Won
    • The Journal of the Petrological Society of Korea
    • /
    • v.26 no.1
    • /
    • pp.45-54
    • /
    • 2017
  • The characteristics of the rock cleavage in Jurassic Geochang granite were analysed using the distribution of microcrack lengths and spacings. The phases of distribution of the above lengths and spacings were derived from the enlarged photomicrographs(${\times}6.7$) of the thin section. First, the length and spacing-cumulative diagrams for the six directions of rock cleavages were arranged in increasing order($H2{\rightarrow}R1$) on the density(${\rho}$) of microcrack length. The various parameters were extracted through the combination of the above two types of diagrams. The discrimination factors representing the three quarrying planes and three rock cleavages were acquired through the mutual contrast between the values of parameters. The analysis results of the research are summarized as follows. The evaluation for the six directions of rock cleavages was performed using the parameters such as (1) intersection angle(${\alpha}-{\beta}$) and (2) exponent difference(${\lambda}_S-{\lambda}_L$) between two exponential straight lines related to spacing(${\alpha}$, ${\lambda}_S$) and length(${\beta}$, ${\lambda}_L$). The values of parameters(1 and 2) are in order of H(hardway, (H1 + H2)/2) < G(grain, (G1 + G2)/2) < R(rift, (R1 + R2)/2). On the contrary, the values of the above two parameters for three planes are in order of R < G < H. Meanwhile, the direction of convergence between two exponential straight lines was derived. The above direction is compliant to arrangement of the line os' centering around the line ol. The above two lines converge in the direction of the Y-axis when the line ol and line os' occupy the upper region on the left and the lower region on the right, respectively(R-type). On the contrary, the above two lines converge in the direction of the X-axis when the order of arrangement between line ol and line os' is reversed(H-type). Especially, the positive(+) or negative(-) value of intersection angle(${\alpha}-{\beta}$) is determined by the arrangement of two vertical lines. This type of correlation analysis is useful for evaluating the relative strength of rock cleavage and discriminating three quarrying planes.

Evaluation for Rock Cleavage Using Distribution of Microcrack Lengths (미세균열의 길이 분포를 이용한 결의 평가)

  • Park, Deok-Won
    • The Journal of the Petrological Society of Korea
    • /
    • v.24 no.3
    • /
    • pp.165-180
    • /
    • 2015
  • Jurassic granite from Geochang was analysed with respect to the characteristics of the rock cleavage. The phases of distribution of microcracks were well evidenced from the enlarged photomicrographs(${\times}6.7$) of the thin section. In this study, the length - cumulative frequency diagrams were used for expressing the distribution characteristics of microcrack. The diagrams for the six directions were arranged in the magnitude of density(${\rho}$). These diagrams show an order of H2 < H1 < G2 < G1 < R2 < R1 from the related chart. Among six diagrams, the diagram for hardway 2(H2) occupies the lowermost region on the left. On the contrary, the diagram for rift 1(R1) occupies the uppermost region on the right. Curve patterns of the two diagrams change from uniform to exponential distribution type in accordance with the increased density. The overall distribution characteristics of the diagrams were well evidenced from the magnitude of the exponent(${\lambda}$) and length of line oa related to the exponential straight line. The magnitude of exponent governing the values of slope(${\theta}$) is inversely proportional to the values of microcrack parameters such as number(N), length(L) and density. On the contrary, length of line oa is directly proportional to the values of the above three parameters. Above microcrack parameters related to the order of arrangement of diagrams show an order of hardway(H1 + H2) < grain(G1 + G2) < rift(R1 + R2). The distribution characteristics of progressive variation are found among the six diagrams. The order of arrangement of the diagrams indicates a relative magnitude of the rock cleavage. Meanwhile, the parameters such as slope, exponent, density and length of line oa were arranged in an order of H2 < H1 < G2 < G1 < R2 < R1. The variation curves of a smooth quadratic function are shown from the related chart. From the correlation chart between density and the above parameters, a common regularity following power-law correlation function was derived. Finally, the analysis for the rock cleavage was conducted through the combination between the diagram and microcrack parameter. This type of combination contribute to the progressivity in evaluation for the rock cleavage.

Fracture Behavior and Crack Growth of Concrete by The Nonlinear Fracture Mechanics (비선형 파괴역학에 의한 콘크리트의 파괴거동과 균열성장에 관한 연구)

  • 배주성;나의균
    • Magazine of the Korea Concrete Institute
    • /
    • v.2 no.2
    • /
    • pp.81-92
    • /
    • 1990
  • Concrete, a mixed material, has heterogeniety, anisotrophy and nonlinearity. Therefore, in its 'racture analysis, it is more reasonable to evaluate its fracture toughness by applying the concept of 'racture mechanics rather than the strength concept. Up to the present the concepts of fracture mechanics which were applied to concrete have been divided into two main classes. The one is the concept of linear elastic fracture mechanics and the other is the concept of elastic-plastic fracture mechanics. But it has been pointed out that there are many problems and irrationalities in applying the concept of linear elastic fracture mechanics to concrete. In this study, the J -integral method and the COD method mainly used in the analysis of nonlinear fracture mechanics, were introduced and the three point bending test was carried out for investigating the effects of the variation of the maximum aggregate size and notch depth on the fracture behavior and the crack growth of concrete, and the relationships of fracture energy and crack opening displacement. According to the results of this study the more the maximum aggregate size and the notch depth increased, the more the nonlinearity of load-deflection behavior was remarkable. The increase of the coarse aggregate size created the more ductility of concrete. Thus concrete showed the more stable fracture. As for the path of the crack growth, the more the coarse aggregate size increased, the more it was irregulary deviated from the straight line but it was not almost affected by the variation of the notch depth. Also, the fracture energy increased according as the coarse aggregate size increased and the notch depth decreased.

A method of Determination of Fracture Toughness of Reactor Pressure Vessel Steel by J Integral (J적분을 이용한 원자력 압력용기강의 파괴인성치의 결정)

  • 오세욱;임만배;김진선
    • Journal of Ocean Engineering and Technology
    • /
    • v.9 no.1
    • /
    • pp.111-119
    • /
    • 1995
  • The elastic-plastic fracture toughness($J_{IC}$) and fracture resistance (J-R curve) of SA508-3 alloy steel used for nuclear reactor pressure vessel are investigated by using CT-type specimens. Fracture toughness tests are conducted by unloading compliance method and multiple specimen method at room temperature, -2$0^{\circ}C$ and 20$0^{\circ}C$. The apparent negative crack growth phenomenon which usually arises in partial unloading compliance test is well known. The negative crack growth phenomenon in determining J sub(IC) or J-R cure from partial unloading compliance experiments may be eliminated by the offset technique. In this study, the evaluation of $J_{IC}$ multiple specimen method recommended by the JSME gives the most reliable results by using half-size CT(similar-type) specimens.

  • PDF

Determination of Stress Intensity Factors for Bimaterial Interface Rigid Line Inclusions by Boundary Element Method (경계요소법을 이용한 접합재료 경계면의 직선균열형상의 강체 함유물에 대한 응력세기계수 결정)

  • Lee, Kang-Yong;Kwak, Sung-Gyu
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.176-181
    • /
    • 2000
  • Stress intensity factors for a rigid line inclusion tying along a bimaterial interface are calculated by the boundary element method with the multiregion and double-Point techniques. The formula between the stress intensity factors and the inclusion surface stresses are derived. The numerical values of the stress intensity factors for the bimaterial interface rigid line inclusion in the infinite body are proved to be in good agreement within 3% when compared with the previous exact solutions. In the finite bimaterial systems, the stress intensity factors for the center and edge rigid line inclusions at interface are computed with the variation of the rigid line inclusion length and the shear modulus ratio under the biaxial and uniaxial loading conditions.

  • PDF

Effects of Accelerated Iso-Thermal Aging on Elastic-Plastic Fracture Toughness and Fracture Resistance Curve by Unloading Compliance Method in SA533B Low Alloy Steel (제하 컴플라이언스법에 의한 SA533B강의 $J_1C$ 및 J-R 곡선에 미치는 열시효 영향)

  • 윤한기;차귀준
    • Journal of Ocean Engineering and Technology
    • /
    • v.8 no.2
    • /
    • pp.157-165
    • /
    • 1994
  • Effect of an accelerated iso-thermal aging (375 degree C x 66days, 375 degree C x 200days) on elastic-plastic fracture resistance curve were examined in SA533B low alloy steel. Fracture toughness test are conducted by unloading compliance method at room temperature. But the apparent negative crack growth phenomenon, usually arise in partial unloading compliance test. The phenomenon of negative crack growth may be eliminated by the offset technique. There is no effect of aging on J sub(IC) and dJ/da in iso-thermal aged (375 degree C x 66 days) specimen, but there is very little effect in iso-thermal aged (375 degree C x 200 days) specimen.

  • PDF

Evaluation on fracture toughness of high frequency electric resistance welded steel pipe by unloading compliance method (고주파 전기저항 용접강관의 제하 컴플라이언스법에 의한 파괴인성 평가)

  • 오세욱;윤한기;안광주
    • Journal of Welding and Joining
    • /
    • v.5 no.2
    • /
    • pp.44-52
    • /
    • 1987
  • The fracture toughness, $J_{IC}$ of high frequency electric resistance welded steel pipe for smooth and side-grooved CT specimen was evaluated by unloading compliance method. The crack growth, .${\delta}a$ was obtained from the equation of Donald and Saxena & Hudak, and $J_{IC}$ was determined from the curve of J-${\delta}a$ relations. The crack growth on the experiment using unloading compliance method is underestimated as compared with ${\delta}a$ measured directly by the SEM, so the reliability of $J_{IC}$ from saxena & Hudak equation is large than that from Donald. The $J_{IC}$ value of side-grooved CT Specimen is estimated less than that of smooth, and this is the effect of the side-groove, the shear-lip of crack tip and the reduction of crack tunnelling phenomena.