Effect of Carbon Filler and Ester Type Binder on the Reactivity and Adhesive Properties with PET Film of Conductive Paste (탄소필러와 에스테르계 바인더가 전도성 페이스트의 반응성 및 PET 필름과의 접착특성에 미치는 영향)

  • Shim, Chang Up;Ku, Hyo Sun;Kim, Youn Cheol
    • Applied Chemistry for Engineering
    • /
    • v.33 no.4
    • /
    • pp.381-385
    • /
    • 2022
  • It is very important to secure the adhesion durability between the base film and the conductive paste for the development of a sensor for detecting hazardous chemicals. In this study, an ester binder was used to improve the adhesive properties which can be a problem when applying the sensor to the cross cut 0B or 1B grade. This problem was found while evaluating the adhesive properties by coating the polyaniline/graphene nano plate (GNP) paste on the polyethylene terephthalate (PET) film. When 10 wt% or more of the ester-based binder was added, the cross cut grade to which the sensor can be applied was 3B or higher. It was confirmed that the excessive addition of the binder may affect the electrical properties of the conductive paste and actually decrease the reactivity to sulfuric acid. To improve the electrical property, a carbon black (CB) content was varied resulting in the optimum electrical property observed at 2 wt% of CB.

Improvement in Fatigue Durability of RC Beams Strengthened with Carbon Fiber Sheets (탄소섬유시트로 보강된 RC 보의 피로내구성 향상에 관한 연구)

  • Park, Jeong-Yong;Kim, Seong-Do;Jo, Baik-Soon;Kim, In-Tae;Cheung, Jin-Hwan
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.6
    • /
    • pp.205-212
    • /
    • 2006
  • In recent investigations, reinforced concrete beams strengthened with Carbon Fiber Sheets (CFS) subjected to fatigue loading were reported to be failed at the ends of CFS by its debonding. U-shaped CFS were attached to both ends of the CFS when fatigue tests on strengthened beams were conducted to delay and/or prevent fatigue failures of adhesive interface. The experimental parameters of this study were the usage of anchorage at the ends of CFS, the number of CFS layers, and the applied load levels of 60%~90% of the static ultimate load obtained from the static tests. The failure modes and the load cycle-deflection relations were observed and discussed from the experimental results. Those results also showed that the U-shaped anchoring system changes the fatigue failure modes and influences greatly on the fatigue capacity of the strengthened beams.

Pre-treatment condition and Curing method for Fabrication of Al 7075/CFRP Laminates (Al 7075/CFRP 적층 복합재료 제조를 위한 전처리 조건과 경화방법 연구)

  • 이제헌;김영환
    • Composites Research
    • /
    • v.13 no.4
    • /
    • pp.42-53
    • /
    • 2000
  • A study has been made to establish an optimum condition in the surface treatment and curing method that is important for the fabrication of Al 7075/CFRP laminates. PAA(Phosphoric Acid Anodizing) provided a good adhesive strength and FPL(Sulfuric / Sodium Dichromate Acid Etching) had a similar adhesive strength with PAA. On the other hand, the poor adhesive strength was shown on vapor degrease and CAA(Chromic Acid Anodizing). By using the atomic force microscope(AFM), it was found that the PAA oxide surface obviously had a greater degree of microroughness as compared to vapor degrease, CAA and FPL treated surfaces. These results support the concept of a mechanical interlocking of the adhesive with-in the oxide pores as the predominant adhesion mechanism. In curing methods, the adhesive strength of co-curing method was higher than that of secondary curing method. With respect to stability of specimen shape, the secondary curing method was better than co-curing method. DMA(Dynamic Mechanical Analysis) test revealed $T_g$ in curing times over 60 min is nearly same, so it is estimated they will have similar degree of curing and joint durability in using FM300M adhesive film.

  • PDF

A Study on the Eco-Friendly Durable Pre-Painting for Concrete Structure (콘크리트 구조물의 친환경 내구성 도장에 관한 기초 연구)

  • Jo, Byung Wan;Choi, Ji Sun;Lee, Seong Won
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.2
    • /
    • pp.110-116
    • /
    • 2013
  • A concrete structure has become bigger and higher because of development of construction technology and a change in construction environment. Also it tends to focus on repairing, reinforcement and exterior in harmony with environment for structure maintenance and performance improvement. The research is about eco friendly durable painting applicable to concrete structure using civil and architecture. it purpose to improve external beauties and durable problems due to flexibility by variation of temperature, adhesion of exterior wall, crack and delamination in existing organic and mineral painting. For those problems, we made a eco friendly pre-paint that is made with preliminary treatment mixture as a highly enriched waterproof agent and adhesive increasing agent in preprocessing mixture. Then we performed an experiment on durability of prevention neutralization of concrete, durability abrasion, hiding power, adhesion, temperature resistance and resistance to chemical attack. The result of an experiment shows that hiding power is over 0.96 in standard test, durability abrasion test got higher value 1mg than water paint 75mg and tensile strength is 6 times higher than standard waterproof specification.

High Efficiency Hybrid Ion Exchange Chemical Filter for Removal of Acidic Harmful Gases (산성유해가스 제거를 위한 고효율 음이온교환 복합 폼 화학필터의 제조)

  • Jung, Youn Seo;Kim, In Sik;Hyeon, Seung Mi;Hwang, Taek Sung
    • Applied Chemistry for Engineering
    • /
    • v.28 no.5
    • /
    • pp.539-546
    • /
    • 2017
  • In this study, an outstanding anion exchange chemical filter was prepared for acidic gas removal. Commercial anion exchange resin was attached to polyurethane (PU) foam by using different types of pressure sensitive adhesive (PSA). The water and chemical resistance and also adhesive elongation were investigated. Also, the behavior of HCl and HF adsorption was evaluated as functions of the initial concentration and flow rate. ATE-701, AT-4000C and HCA-1000 showed 900, 1,500% and 2,400% of the elongation, respectively. It was confirmed that the desorption ratio of HCA-1000 was less than 6% and had excellent durability in water and chemical resistance tests. The adsorption occurred faster as the concentration and flow rate of HCl and HF increased. But 100% adsorption equilibrium occurred after 110 minutes, regardless of the concentration and flow rate. In addition, SEM morphology showed that the adhesive was uniformly dispersed, while the porous structure of the ion exchange resin was maintained, and the chemical filter exhibited excellent durability for the adsorption/desorption process.

An Experimental Study on the Adhesion Property of Self Adhesive Rubberized Asphalt Waterproofing Sheet (자착식 고무화 아스팔트 방수시트의 접착특성에 관한 실험적 연구)

  • Jeoung Hyoun-Sang;Kang Hyo-Jin;Song Je-Young;Oh Sang-Keun
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2005.05a
    • /
    • pp.1-4
    • /
    • 2005
  • This study is to examine adhesion the characteristics of self adhesive asphalt to minimize of the construction periods and the environmental problems through the performance estimation of materials to reduce waterproof problem and the long durability maintenance of building structures. This study tested the estimation items of self rubberized adhesive asphalt to examine the sheet discovered the most important problem in the construction site and the connection stability in the sheet joint. Besides, this study examined the material characteristics such as tension property, tear property, temperature dependence, heat resistance, adhesion stability and so on. Test results of the separative items satisfied in the reference figure of connection stability and adhesion stability which could confirm adhesion performances and other items also satisfied in the reference.

  • PDF

THE EFFECT OF THERMOCYCLING ON THE DURABILITY OF DENTIN ADHESIVE SYSTEMS (열순환이 상아질 접착제의 결합 내구성에 미치는 영향)

  • Moon, Young-Hoon;Kim, Jong-Ryul;Choi, Kyung-Kyu;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.3
    • /
    • pp.222-235
    • /
    • 2007
  • The objectives of this study was to evaluate the effect of thermocycling on the ${\mu}TBS$ (microtensile bond strength) to dentin with four different adhesive systems to examine the bonding durability. Freshly extracted $3^{rd}$ molar teeth were exposed occlusal dentin surfaces, and randomly distributed into 8 adhesive groups 3-steps total-etching (Scotchbond Multi-Purpose Plus; SM, All Bond-2; AB), 2-steps total-etching (Single Bond; SB, One Step plus; OS), 2-steps self-etching (Clearfil SE Bond; SE, AdheSE AD) and single-step self-etching systems (Promp L-Pop; PL, Xeno III; XE) Each adhesive system in 8 adhesives groups was applied on prepared dentin surface as an instruction and resin composite (Z250) was placed incrementally and light-cured. The bonded specimens were sectioned with low-speed diamond saw to obtain $1\times1mm$ sticks after 24 hours of storage at $37^{\circ}C$ distilled water and proceeded thermocycling at the pre-determined cycles of 0, 1,000 and 2,000. The ${\mu}TBS$ test was carried out with EZ-tester at 1mm/min. The results of bond strength test were statistically analyzed using one-way ANOVA/ Duncan's test at the a < 0.05 confidence level. Also, the fracture mode of debonded surface and the interface were examined under SEM. The results of this study were as follows ; 1. 3-step total etching adhesives showed stable, but bond strength of 2-step adhesives were decreased as thermocycling stress. 2. SE showed the highest bond strength, but single step adhesives (PL, XE) had the lowest value both before and after thermocycling. 3 Most of adhesives showed adhesive failure. The total-etching systems were prone to adhesive failure and the single-step systems were mixed failure after thermocycling. Within limited results of this study, the bond strength of adhesive system was material specific and the bonding durability was affected by the bonding step/ procedure of adhesive Simplified bonding procedures do not necessarily imply improved bonding performance.

A Study on the Degradation Properties of DGEBA/TETA Epoxy System for Restoration of Ceramics by Temperature (도자기 복원용 DGEBA/TETA Epoxy계 수지의 온도에 의한 열화 특성 연구)

  • Nam, Byeong Jik;Jang, Sung Yoon
    • Journal of Conservation Science
    • /
    • v.31 no.4
    • /
    • pp.373-386
    • /
    • 2015
  • This study identified degradation properties by temperature stress with Araldite$^{(R)}$ AY103-1/HY956 used for ceramics. Tensile and compressive strength of durability increased for 6,480 hours at temperature of $34{\sim}45^{\circ}C$. In stability of external stress and temperature, compressive strength is superior to tensile strength, it requires conservation plans considering strength properties and stress of restoration materials. The tensile shear strength of adhesion properties decreased for 4,320 hours at temperature of $40{\sim}60^{\circ}C$. In ceramics with porosity, environments under isothermal-isohumidity are important because interfacial properties of adherend are concerned with performance variation. Glossiness decreased for 6,480 hours at temperature of $34{\sim}45^{\circ}C$ and color difference increased. Gloss stability was superior and color stability was weak, which requires improvement of optical properties. In artifacts on display in museums, there is concern about temperature rise on restoration materials by lighting therefore, it needs to minimize change in physical properties by exposure environments.

A Fundamental Study on the Attachment Performance of Impervious Waterproof Asphalt Mixture (불투수성 방수아스팔트의 부착성능에 관한 기초적 연구)

  • Kim, Kyeong-Jin;Kim, In-Joong;Kim, Kyong-Tae;Cho, Jae-Hyeong
    • Proceedings of the Korean Society of Disaster Information Conference
    • /
    • 2016.11a
    • /
    • pp.353-356
    • /
    • 2016
  • 불투수성 방수아스팔트는 아스팔트 혼합물이 골재와 골재 사이를 강력하게 부착하며, 골재간의 공간을 메우고, 골재표면을 두껍게 코팅하여 골재 상호간의 강한 접착을 유지시켜주는 열가소성 폴리머를 사용한 포장공법이다. 이러한 불투수성 아스팔트는 기존의 가열식 일반아스팔트 공법에서 문제시 되고 있는 내구성 저하와 잦은 유지보수로 인한 문제점을 해결할 수 있는 공법으로 차세대 고내구성 포장공법으로 주목을 받고 있다. 본 연구는 불투수성 방수아스팔트 혼합물 개발을 위한 연구의 일환으로 상온과 영하 $10^{\circ}C$의 조건하에서 기존 아스팔트수지와 새로운 개념의 불투수성 고분자계 수지의 부착성능 비교 검토하였으며, 아스팔트혼합물의 부착성능도 실험을 통해 비교 하였다. 실험결과 불투수성 아스팔트의 부착성능이 기존 아스팔트에 비해 상온은 물론 저온에서도 뛰어난 성능을 발휘하는 것을 확인 하였다.

  • PDF

THE BONDING DURABILITY OF TOTAL ETCHING ADHESIVES ON DENTIN (산부식형 상아질 접착제의 접착 내구성에 관한 연구)

  • Jung, Mi-Ra;Choi, Gi-Woon;Park, Sang-Hyuk;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.4
    • /
    • pp.365-376
    • /
    • 2007
  • The purpose of this study was to evaluate the effect of different etching times on microtensile bond strength (${\mu}TBS$) to dentin both initial and after thermocycling with 3 different types of total-etching adhesives. Fifty four teeth were divided into 18 groups by etching times (5, 15, 25 sec), adhesives types (Scotchbond Multipurpose (SM), Single Bond (SB), One-Step (OS)) and number of thermocycling (0, 2,000 cycles). Flat dentin surfaces were prepared on mid-coronal dentin of extracted third molars. After exposed fresh dentin surfaces were polished with 600-grit SiC papers, each specimen was acid-etched with 35% phosphoric acid (5, 15, 25 sec) and bonded with 3 different types of total etching adhesives respectively. Then, hybrid composite Z-250 was built up. Half of them were not thermocycled (control group) and the ethers were subjected to 2,000 thermocycle (experimental group). They were sectioned occluso-gingivally into $1.0\;{\times}\;1.0\;mm^2$ composite-dentin beams and tested with universal testing machine at a crosshead speed of 1.0 mm/min. Within limited data of this study, the results were as follows 1. There was no statistically significant difference in ${\mu}TBS$ between the thermocycled and non-thermocycled groups, except for both SM and SB etched for 25 sec. 2. In thermocycled SM and SB groups, bond strength decreased by extended etching time. In total etching systems, adhesive durability for dentin could be affected by type of solvents in adhesive and etching time. Especially, extended etching time may cause deteriorate effects on bond strength when ethanol-based adhesive was used.