• Title/Summary/Keyword: 전부도재관

Search Result 74, Processing Time 0.024 seconds

Esthetic improvement in patient with deep bite using porcelain laminate veneers and a full veneer crown (과개교합 환자에서 도재 라미네이트 비니어와 전부도재관을 이용한 심미수복 증례)

  • Yoon, Jong-Sang;Shin, Soo-Yeon;Lee, Jonghyuk
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.30 no.2
    • /
    • pp.192-198
    • /
    • 2014
  • This case is a porcelain laminate veneer (PLV) and all-ceramic crown treatment case on a female patient in her thirties who visited for esthetic improvement. The patient's chief complaint was protrusive and uneven anterior teeth, and she wanted minimum tooth reduction. The patient was in skeletal class II deep bite. Considering this, check bite method was used for mounting on articulator during diagnostic wax-up. Tooth reduction was done using mock-up base on diagnostic wax-up, and the amount of deletion was checked by index. For the accordance of shade, PLVs were restored in prior to all ceramic crown. After using all-ceramic crown, satisfactory esthetic improvement was obtained.

The effect of repeated firings on the color of zirconia-based all-ceramic system (반복 소성이 지르코니아 전부도재관의 색조에 미치는 영향)

  • Jang, Jung-Eun;Kim, Mu-Hyon;Yun, Mi-Jung;Jeong, Chang-Mo;Jeon, Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.1
    • /
    • pp.73-79
    • /
    • 2011
  • Purpose: The aim of this study was to evaluate the effect of repeated firings on the color of zirconia restoration with different shading method. Materials and methods: Three different types of zirconia frameworks (adding metallic pigments to the initial zirconia powder before sintering (Group NM), dipping the milled frameworks in dissolved coloring agents (Group KI), or application of liner material to the sintered white frameworks (Group KW) were used to support A3 shade dentin porcelain. Repeated firings (3, 5, or 7) were performed, color differences among ceramic specimens were measured using a colorimeter. Repeated measurements analysis of variance (ANOVA) was used to analyze the data for significant difference. The Tukey Honestly Significant Different (HSD) test was used to perform multiple comparisons (${\alpha}$ = .05). Results: 1. $L^*a^*b^*$ values of the ceramic systems were affected by the number of firings (1, 3, 5 or 7 firings) (P < .001) and shading methods (P < .001). 2. As the number of firings increased, the $L^*$ (for all groups) and $a^*$ value (for KW and NM groups) decreased and the $b^*$ value(for all groups) increased. 3. The mean color differences caused by repeated firings were perceptible (${\Delta}E$ > 1) for group KW and KI fired after 3 times, except for group NM fired after 7 times. 4. In order of decreasing ${\Delta}E$ value fired after 7 times, the values were group KI(${\Delta}E$ = 2.26) > group KW (${\Delta}E$ = 1.47) > group NM (${\Delta}E$ = 1.08) (P < .001). Conclusion: Repeated firings influenced the color of the zirconium-oxide all-ceramic specimens with different shading methods.

A Study on the Shear Bond Strength of Veneering Ceramics to the Lithium Disilicate (IPS e.max CAD) Core (Lithium Disilicate (IPS e.max CAD) 코어와 전장 도재 사이의 전단결합강도에 관한 연구)

  • Kim, Ki-Baek;Kim, Jae-Hong
    • Journal of dental hygiene science
    • /
    • v.13 no.3
    • /
    • pp.290-295
    • /
    • 2013
  • The purpose of this study was to investigate the shear bond strength between various commercial all-ceramic system core and veneering ceramics, and evaluate the clinical stability by comparing the conventional metal ceramic system. The test samples were divided into three groups: Ni-Cr alloy (metal bond), yttria-stabilized, tetragonal zirconia polycrystal (Y-TZP) (zirconia bond), lithium disilicate (lithium disilicate bond). The veneering porcelain recommended by the manufacturer for each type of material was fired to the core. After firing, the specimens were subjected to shear force in a universal testing machine. Load was applied at a crosshead speed of 0.50 mm/min until failure. Average shear strengths (mega pascal) were analyzed with a one-way analysis of variance and the Tukey test (${\alpha}$=0.05). The mean shear bond strength${\pm}$SD in MPa was $44.79{\pm}2.31$ in the Ni-Cr alloy group, $28.32{\pm}4.41$ in the Y-TZP group, $15.91{\pm}1.39$ in the Lithium disilicate group. The ANOVA showed a significant difference among groups (p<0.05). None of the all-ceramic system core and veneering ceramics could attain the high bond strength values of the metal ceramic combination.

Esthetic Rehabilitation of Anterior Dentition by All Ceramic Crowns Using IPS e.max CAD : A Case of Tetracycline Discoloration (전치부 전부도재관을 이용한 테트라싸이클린 착색의 심미보철 회복 증례 (IPS e.max CAD 블록의 이용))

  • Kim, Jae-Hong;Cho, Young-kyu;Kim, Hae-Young
    • Journal of dental hygiene science
    • /
    • v.11 no.4
    • /
    • pp.299-303
    • /
    • 2011
  • The purpose of this case report was to present an example of an esthetic and functional rehabilitation of anterior teeth with tetracycline discoloration and minor morphological abnormality of a 39-year old female. A chairside computer-aided design/computer-aided manufacturing (CAD/CAM) system with CEREC AC was applied for the prosthetic procedure and all ceramic crowns made with lithum disilicate (IPS e.max CAD) restored the esthetic and functional features of sixteen anterior teeth successfully.

A Study on improvements in manufatured technique of all Ceramic Crown (전부도재관 기법 개선에 관한 연구)

  • Shin, Moo-Hak;Kim, Yeon-Soo;Choi, Un-Jea;Chung, Hee-Sun
    • Journal of Technologic Dentistry
    • /
    • v.23 no.2
    • /
    • pp.9-15
    • /
    • 2002
  • A new kind of 'All Ceramic Crown' could be manufactured by making improvements in the manufacturing technique for the current 'All Ceramic Crown' which does not use a special ceramic but rather a general one as a substitute. If we use the manufacturing technique for the 'All Ceramic Crown', metal coping and core are not produced. The effects of the new manufacturing technique for the 'All Ceramic Crown' are as follows: First. We do not need to use new material or special machinery or tools. Second. We can use general machinery and tools. Third. Using the basic 'All Ceramic Technique', we anticipate improvement in learning in our students. Forth. We can save effort, materials and time. Fifth. The technique also has advantages for esthetic 'temporary crown'.

  • PDF

FRACTURE STRENGTH OF ZIRCONIA MONOLITHIC CROWNS AND METAL-CERAMIC CROWNS AFTER CYCLIC LOADING AND THERMOCYCLING (지르코니아 단일구조 전부도재관과 금속도재관의 파절강도 비교)

  • Lee, Sang-Min;Jeong, Hee-Chan;Jeon, Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.1
    • /
    • pp.12-20
    • /
    • 2007
  • Purpose: The purpose of this study was to compare the fracture strength of the zirconia monolithic all-ceramic crowns according to the thickness (0.5mm, 0.8mm, 1.1mm) and metal-ceramic crowns (1.0mm, 1.5mm) Material and method: Twelve crowns for each of 3 zirconia crown groups were fabricated using CAD/CAM system (Kavo, Germany) and twelve crowns for each of 2 metal-ceramic crown groups were made by the conventional method. All crowns were luted to the metal dies using resin cement. Half of the specimens were exposed to thermocycling ($5-55^{\circ}C$, 1 Hz) and cyclic loading (300,000 cycles, 50N). Subsequently, all crowns were mounted on the testing jig in a universal testing machine. The load was directed at the center of crown with perpendicular to the long axis of each specimen until catastrophic failure occurred. Analysis of variance and Tukey multiple comparison test (P<.05) were used for statistical analysis of all groups, and paired t-test (P<.05) was followed for statistical comparison between each groups' fracture load before and after cyclic loading. Results: 1. The fracture strength of the zirconia monolithic crowns and the metal-ceramic crown increased as thickness increased (P<.05). 2. The cyclic loading and thermocycling significantly decreased the fracture strength of the zirconia monolithic crowns (P<.05). 3. The standard deviation of fracture strength of the zirconia monolithic crowns was very low. Conclusion: The fracture strength of the zirconia monolithic crowns for the posterior area tends to be higher with thickness increased and 0.8mm or over in thickness is recommended to have similar or over the fracture strength of metal-ceramic crowns.

Maxillary anterior all ceramic restoration using digital impression and CAD/CAM (디지털 인상채득 및 CAD/CAM을 이용한 상악 전치부 보철물 제작과 기존 방식 보철물과의 임상적 비교)

  • Pyo, Se-Wook;Park, Young-Bum;Kim, Jee-Hwan;Moon, Hong-Suk;Lee, Keun-Woo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.3
    • /
    • pp.263-269
    • /
    • 2011
  • The digital impression technique has been developed for more precise restorations and convenient procedures in prosthodontic treatment compared to the conventional impression technique. Along with the utilization of CAD/CAM, the introduction of digital impression technique actualizes the digitalization of dental treatments. This case is to compare two different prostheses introducing each procedure in detail; one from CAD/CAM after taking digital impression and the other from the conventional technique. A 22-year-old female visited the clinic with the chief complaint of correction of discoloration and shape on maxillary right central incisor. Due to the trauma 8 years ago, the tooth was endodontically treated with post and resin core. The treatment was planned and the procedures were conducted under the patient's consent to treat the tooth with all ceramic crowns in two different ways for comparison. In conclusion, both prostheses presented clinically acceptable results with comparing the internal fitness of two all ceramic crowns. The prosthesis from digital impression, however, showed more errors in respect of internal fitness.

Comparative study in fracture strength of zirconia cores fabricated with three different CAD/CAM systems (3종의 CAD/CAM 시스템에서 지르코니아 코어의 파절 강도에 관한 비교 연구)

  • Shin, Eon-Sick;Lee, Young-Soo;Park, Won-Hee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.1
    • /
    • pp.22-30
    • /
    • 2008
  • Purpose: The purpose of this study is to compare three different CAD/CAM systems through the fracture strength of zirconia core and to evaluate the clinical availability of each system. Material and methods: The following three groups of 30 maxillary mesial incisor core for all-ceramics(each group 10) were fabricated as follows: group 1. $Adens^{(R)}$ CAD/CAM system, group 2. $Cerasys^{(R)}$ CAD/CAM system, group 3. 3M $Lava^{(R)}$ CAD/CAM system. All specimens were manufactured consistently thickness 0.5mm and relief $40{\mu}m$. Specimens were subjected to compressive loading on the lingual area by Z250/$SN5S^{(R)}$. Each group's mean and standard deviation were calculated and Kruskal Waillis test, Wilcoxon Rank Sum test were utilized to find out the relationship among the groups. Results: The results were as follows: 1. The mean fracture strength of $Adens^{(R)}$ system was $615.89{\pm}156.1N$, the $Cerasys^{(R)}$ system was $863.98{\pm}151.5N$, and the 3M $Lava^{(R)}$ system was $1143.1{\pm}286.6N$. 2. The fracture strength of the systems showed the significant statistical differences in order of 3M $Lava^{(R)}$ system, $Cerasys^{(R)}$ system, $Adens^{(R)}$ system. Conclusion: In this study, in spite of the differences among the groups, every group showed clinically useful results. It is necessary to study further clinical experiments on a long term basis.