Investigation of Maximum Strength and Effective Bonding Length at the Interface Between Structure and GFRP Material Under Freeze-thaw Cycles and Applied Different Bonding Materials (동결융해 및 부착재료 변화에 따른 GFRP-구조물 경계면의 최대 부착강도 및 유효부착길이 평가)

  • Choi, Hyun Kyu;Jung, Woo Young;Ahn, Mi Kyoung
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.15 no.2
    • /
    • pp.107-115
    • /
    • 2011
  • This research studies the behavior of the FRP-concrete interface subjected to two environmental substances. Frist is to investigate the behavior by the application of different bonding materials at the interface between FRP and concrete, second is to understand a long-term performance at the interface by Freeze-thaw actions. The parameters considered in this research are the maximum bonding strength and the effective bonding length at the FRP-concrete interface. In the first experimental phase, three types of specimens are fabricated and tested considering the number of applied bonding materials and the Freeze-thaw tests are performed to evaluate the behavior of the interface in the cycle range of 0 to 300 cycles. Finally, it is known that there is a 5~7% difference of the effective bonding length between applied bonding materials and the values for the maximum stress and the effective length under Freeze-thaw action are varied randomly as the freeze-thaw cycle is increased even though initial reduction of their capacities are occurred.

Pull-out Bond Characteristics of Reinforced Concrete Members (철근콘크리트 부재의 뽐힘 부착특성 연구)

  • 오병환
    • Magazine of the Korea Concrete Institute
    • /
    • v.4 no.3
    • /
    • pp.113-121
    • /
    • 1992
  • 본 논문에서는 철근콘크리트 부재의 뽐힘부착거동을 규명하기 위하여 일련의 포괄적인 실험 및 이론 연구를 수행하였다. 실험의 주요변수는 콘크리트의 압축강도, 철근간격 및 덮개, 그리고 철근의 부착길이 등을 선정하였다. 본 연구결과 철근 콘크리트의 부착강도는 뿐만아니라 부착길이, 철근의 덮개 등에 따라 큰 영향을 받는 것으로 나타났으며, 본 연구에서는 이들의 영향을 정량적으로 도출하였다. 또한, 본 연구에서는 철근콘크리트의 부착강도식을 새롭게 제안하였으며, 부착응력-슬립관계식도 유도하여 제시하였다.

Analytical Model for Transfer Bond Performance of Prestressing Strands (PS 강선의 정착부착성능에 관한 해석 모델)

  • 유승룡
    • Magazine of the Korea Concrete Institute
    • /
    • v.6 no.4
    • /
    • pp.92-101
    • /
    • 1994
  • A new analytical model is proposed to better understand the transfer bond performance in a prestressed pretensioned concrete beam. The transfer length is divided into an elastic and a plas tic zones in this model. The bond stress is assumed t.o increase proportionally with the slip t.o the lirnit of maximum bond stress within the elastic zone and remains at a constant maximum value wthin the plastic zone. Four main stress patterns: bond stress, slip, steel stress, and concrete stress distributions within the transfer length are obtained precisely. The total transfer length al\ulcornerd free-end slip obtained here give a close comparison to the test results by Cousins et al.

Experimental Study on Interfacial Bond Stress between Aramid FRP Strips and Steel Plates (아라미드 FRP 스트립과 강판 사이의 계면 부착응력에 관한 실험적 연구)

  • Park, Jai Woo;Ryoo, Jae Yong;Choi, Sung Mo
    • Journal of Korean Society of Steel Construction
    • /
    • v.27 no.4
    • /
    • pp.359-370
    • /
    • 2015
  • This paper presents the experimental results for the interfacial bond behaviour between AFRP strip and steel members. The objective of this paper is to examine the interfacial behavior and to evaluate the interfacial bond stress between Aramid FRP strips and steel plates. The test variables were bond length and AFRP thickness. 18 specimens were fabricated and one-face shear type bond tests were conducted in this study. There were two types of failure mode which were debonding and delamination between AFRP strip and steel plates. From the test, the load was increased with the increasing of bond length and AFRP thickness, which was observed that maximum increase of 63 and 86% were also achieved in load with the increasing of bond length and AFRP thickness, respectively. Finally, bond and slip characteristics had the elastic bond-slip model and it was observed that bond strength and fracture energy were not affected by bond length and AFRP thickness.

Inverstigation of Maximum Strength and Effective Bonding Length at the Interface between Concrete and FRP Materials under Freeze-thaw Cycles and Applied Different Bonding Materials (동결융해 및 부착재료 변화에 따른 FRP-Concrete 경계면의 최대 부착강도 및 유효부착길이 평가)

  • Kim, Sung-Hoon;Jung, Woo-Young;Choi, Hyun-Kyu
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.435-436
    • /
    • 2010
  • This research presents two important factors; first, the advanced design equation of effective bonding length at the interface between concrete and FRP materials is proposed when different bonding materials are applied and secondly maximum bonding strength between concrete-FRP bonding surface is evaluated under Freeze-thaw cycles.

  • PDF

An Evaluation of Lap Splice Length of Epoxy Coated Reinforcements Using Beam-End Test (보-단부 시험을 이용한 에폭시 도막 철근의 겹침 이음길이 평가)

  • Kim, Jee-Sang;Kang, Won Hyeak
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.2
    • /
    • pp.175-182
    • /
    • 2020
  • The application of epoxy coated reinforcements is increased as a means to prevent a corrosion of reinforcements embedded in reinforced concrete structures, However, epoxy coating may reduce the bond capacity between concrete and reinforcement, which results a longer development length and lap splice length. This paper aims to the possibility of modification in lap splice length from reduction of basic development length which was confirmed using a direct pull out test. Total 36 beam specimens were tested to compare the lap splice properties of normal and epoxy coated reinforcements with beam-end test for various lap lengths and diameters of reinforcements. According to the results on failure modes, deformations, and crack widths of this experiments, the modification factor of 1.2 should be used, though the direct bond capacity is assured through direct pull out test.

Bond Strength of Near Surface-Mounted FRP Plate in RC Member (콘크리트 내에 표면매입 보강된 FRP 판의 부착강도)

  • Seo, Soo-Yeon
    • Journal of the Korea Concrete Institute
    • /
    • v.24 no.4
    • /
    • pp.415-422
    • /
    • 2012
  • This paper analyzed seventy eight previous test results to evaluate bond strength of Near Surface-Mounted (NSM) FRP and prediction formulas previously proposed by researchers. The results showed that the most reliable bond strength prediction was the one proposed by Seracino, who considered the shape coefficient (ratio of width-thickness) and stiffness of FRP. However, the equation tended to underestimate the bond strength, especially serious when FRP bond length was relatively short, because the equation did not consider the effect of bond length. Based on the analysis of previous test results, the relation between bond length and bond strength and the group effect due to close proximity of FRPs were determined. Based on the findings, the Seracino's formula was modified and it's applicability was evaluated. The result showed that the suggested formula can be used effectively to predict the bond strength of NSM FRP.

Bond Strength of Grout-Filled Splice Sleeve Considering Effects of Confinement (구속효과를 고려한 모르타르 충전식 철근이음의 부착강도)

  • Kim, Hyong-Kee;Ahn, Byung-Ik
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.4
    • /
    • pp.615-622
    • /
    • 2003
  • The purpose of this study is to propose the more reasonable equation of bond strength of grout-filled splice sleeve. To accomplish this objective, total 60 full-sized specimens were tested under monotonic loading. The experimental variables are compressive strength of mortar, embedment length and size of reinforcing bars. Following conclusions are obtained; 1) If the adequacy of existing equations which estimate the bond strength of grout-filled splice sleeve are investigated, they underestimate the bond strength of grout-filled splice sleeve by 8-18%. Also the existing equations have a tendency to underestimate with decrease in the embedment length of reinforcing bars. 2) From the test result of bond failure, the equation which estimates the confining pressure of grout-filled splice sleeve was proposed by making multiple regression analyses of which independent variables are embedment length of reinforcing bars and compressive strength of mortar. This equation predicted the measured bond capacity of this test more accurately than existing equations and eliminated the deviation according to the embedment length of reinforcing bars.

Bond Strength of Near Surface-Mounted FRP Plate in Concrete Corresponding to Space and Bond Length (콘크리트에 표면매입 보강된 FRP판의 매입간격과 길이에 따른 부착강도)

  • Seo, Soo-Yeon;Kim, Min-Sik
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.1
    • /
    • pp.37-43
    • /
    • 2013
  • Recently, experimental and analytical researches have been performed in order to find interface failure between FRP plate and concrete in near surface-mounted (NSM) retrofit using FRP plate. As a result, it was found that the bond strength between concrete and NSM FRP plate had a close relationship with shape of FRP, concrete compressive strength and bond length. However, research need is increasing about another factors such as suitable space of FRP plate and group effect. In this study, therefore, a bond test was performed with aforementioned factors and compared with a previous equation to verify its suitability for predicting bond strength of NSM FRP plate. From the test, it was found that the bond strength increased according to the increase of space of NSM FRP plates even if its bond length was same. The splitting failure of concrete governed when space of FRPs was too narrow and it changed to FRP's tensile failure with increase of the space. From the evaluation of test specimens using previous equation, it was found that the bond strength could be predicted properly with consideration of group effect.

Effect of Bond Length and Web Anchorage on Flexural Strength in RC Beams Strengthened with CFRP Plate (부착길이와 복부정착이 CFRP판으로 보강된 RC 보의 휨 보강효과에 미치는 영향)

  • 박상렬
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.5
    • /
    • pp.645-652
    • /
    • 2002
  • This paper presents the flexural behavior and strengthening effect of reinforced concrete beams bonded with carbon FRP plate. Parameters involved in this experimental study were plate bond length and sheet web anchorage length. Test beams were strengthened with FRP plate on the soffit and anchored with FRP sheet on the web. In general, strengthened beams with no web anchorage were failed by concrete cover failure along the longitudinal reinforcement. On the other hand, strengthened beams with web anchorage were finally failed by delamination shear failure within concrete after breaking of CFRP sheet wrapping around web. The ultimate load and deflection of strengthened beams increased with an increased bond length of FRP plate. Also, the ultimate load and deflection increased with an increased anchorage length of FRP sheet. Particularly, the strengthened beams with web anchorage maintained high ultimate load resisting capacity until very large deflection. The shape of strain distribution of CFRP plate along beam was very similar to that of bending moment diagram. Therefore, an assumption of constant shear stress in shear span could be possible in the analysis of delamination shear stress of concrete. In the case of full bond length, the ultimate resisting shear stress provided by concrete and FRP sheet Increased with an increase of web anchorage length. In the resisting shear force, a portion of the shear force was provided by FRP anchorage sheet.