Degradation of a nano-thick Au/Pt bilayered catalytic layer with an electrolyte in dye sensitized solar cells (염료감응태양전지의 Au/Pt 이중 촉매층의 전해질과의 반응에 따른 열화)

  • Noh, Yunyoung;Song, Ohsung
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.15 no.6
    • /
    • pp.4013-4018
    • /
    • 2014
  • A 0.45 $cm^2$ DSSC device with a glass/FTO/blocking layer/$TiO_2$/N719(dye)/electrolyte/50 nm-Pt/50 nm-Au/FTO/glass was prepared to examine the stability of the Au/Pt bilayered counter electrode (CE) with electrolyte and the energy conversion efficiency (ECE) of dye-sensitized solar cells (DSSCs). For comparison, a 100 nm-thick Pt only CE DSSC was also prepared using the same method. The photovoltaic properties, such as the short circuit current density ($J_{sc}$), open circuit voltage ($V_{oc}$), fill factor (FF), and ECE, were checked using a solar simulator and potentiostat with time after assembling the DSSC. The microstructure of the Au/Pt bilayer was examined by optical microscopy after 0~25 minutes. The ECE of the Pt only CE-employed DSSC was 4.60 %, which did not show time dependence. On the other hand, for the Au/Pt CE DSSC, the ECEs after 0, 5 and 15 minutes were 5.28 %, 3.64 % and 2.09 %, respectively. The corrosion areas of the Au/Pt CE determined by optical microscopy after 0, 5, and 25 minutes were 0, 21.92 and 34.06 %. These results confirmed that the ECE and catalytic activity of Au/Pt CE decreased drastically with time. Therefore, a Au/Pt CE-employed DSSC may be superior to the Pt only CE-employed one immediately after integration of the device, but it would degrade drastically with time.

Adsorption Characteristics of Non-degradable Eosin Y Dye by Carbon Nano Tubes (Carbon Nano Tubes에 의한 난분해성 염료 Eosin Y의 흡착 특성)

  • Lee, Min-Gyu;Yun, Jong-Won;Suh, Jung-Ho
    • Korean Chemical Engineering Research
    • /
    • v.55 no.6
    • /
    • pp.771-777
    • /
    • 2017
  • Adsorption characteristics of Eosin Y dye by carbon nano tubes (CNTs) were examined through batch experiments. CNTs used in the study had specific surface area of $106.9m^2/g$, porosity volume of $1.806cm^3/g$, and porosity diameter of $163.2{\AA}$, respectively. Adsorption experiments were carried out as function of contact time, initial solution pH (2~10), dye concentration (100, 150 and 200 mg/L), adsorbent dose (0.05~1.0 g) and temperature (293, 313 and 333 K). The adsorption was favoured at lower pHs and temperatures. Adsorption data were well described by the Langmuir model. The adsorption process followed the pseudo-second order kinetic model. The adsorption capacity decreased with increase in temperature. The results of the intraparticle diffusion model suggested that film diffusion and particle diffusion were simultaneously occured during the adsorption process. Thermodynamic studies suggested the spontaneous and endothermic nature of adsorption of Eosin Y dye onto CNTs.

Degradation of Reactive Black 5 by potassium ferrate(VI) (페레이트를 활용한 아조 염료 Reactive Black 5 분해 연구)

  • Minh Hoang Nguyen;Il-kyu Kim
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.38 no.1
    • /
    • pp.17-27
    • /
    • 2024
  • This paper aims to study the degradation process for refractory azo dye namely Reactive Black 5(RB5) by potassium ferrate(VI) synthesized using the wet oxidation method. The process of degradation of azo dyes by Ferrate was studied with several parameters such as pH, different Ferrate(VI) dosage, different azo dye initial concentration, and temperature. A second-order reaction was observed in all degradation processes for RB5 having the highest degradation efficiency. The highest kapp value of RB5 degradation was 190.49 M-1s-1. In the pH experiments, the neutral condition has been identified as the optimum condition for the degradation of RB5 with 63.2% of dye removal. The efficiency of degradation also depends on the amount of ferrate(VI) available in the reactor. Degradation efficiency increased with an increase in Potassium Ferrate(VI) dosage or a decrease of RB5 initial concentration. The temperature has been reported as one of the most important parameters. From the results, increasing the temperature(up to 45℃) will increase the degradation efficiency of azo dye by Ferrate(VI) and if the temperature exceeds 45℃, the degradation efficiency will be decreased.

The Dyeing Properties of Woody Fiber Regenerated from Waste MDF by Reactive Dyes (반응성염료에 의한 폐MDF 재생 목질섬유의 염색특성)

  • Ju, Seon-Gyeong;Roh, JeongKwan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.2
    • /
    • pp.163-177
    • /
    • 2019
  • This study aims to review the relations between the dyeing conditions (i.e., dye concentration, addition amounts of salt and alkali, and dyeing temperature) and dyeing properties and color fastness to light for identifying the optimal dyeing conditions when dyed regenerated woody fibers were obtained through the defibration of waste medium density fiberboard (MDF) using reactive Red H-E3B (Bis-monochlorotriazine (MCT)/MCT type) and reactive Red RB133% (Bis-MCT/Vinyl sulphone type). The dyeing yield (K/S) obtained using two types of reactive dyes increased as the dye concentration increased by 1-10% (on the weight of fiber (OWF)). In addition, the K/S of H-E3B was higher than that of RB133% irrespective of the dye concentration. The color difference of H-E3B after ultraviolet (UV) radiation was lower than that of RB133%, denoting good resistance to discoloration by UV. As the amount of sodium sulfate increased, the color difference and K/S also increased, and the adequate salt content was determined to be 50-70 g/L. Further, the color difference and K/S significantly increased only the addition of 2 g/L of sodium carbonate; however, almost no difference was observed when more than 2 g/L of sodium carbonate was added. The addition amount of sodium carbonate was adequate 5-10 g/L to dyeing the fiber and the pH at this addition level was 10. The dyeing yield of H-E3B increased when the dyeing temperature increased; however, it subsequently decreased after the dyeing temperature became $80^{\circ}C$. The dyeing yield of RB133% was almost the same up to $60-70^{\circ}C$ but declined subsequently. Thus, the adequate temperatures were $80^{\circ}C$ and $60^{\circ}C$ for H-E3B and RB133%, respectively. If the waste MDF woody fiber was dyed under the aforementioned optimal conditions, dyed regenerated woody fiber can be obtained having the following colors: 1.5 to 2.0R with the H-E3B dye and 9.6 to 10.0 PR with RB133%.

Adsorption Kinetics and Thermodynamics of Brilliant Blue FCF Dye onto Coconut Shell Based Activated Carbon (야자계 활성탄에 의한 Brilliant Blue FCF 염료의 흡착 동력학 및 열역학에 관한 연구)

  • Lee, Jong Jib
    • Korean Chemical Engineering Research
    • /
    • v.53 no.3
    • /
    • pp.309-314
    • /
    • 2015
  • Adsorption of brilliant blue FCF dye from aqueous solution using coconut shell based activated carbon was investigated. Batch experiments were carried out as function of adsorbent dose, initial concentration, contact time and temperature. The equilibrium adsorption data were analyzed by Langmuir and Freundlich model. The results indicate that Freundlich model provides the best correlation of the experimental data. Base on the estimated Freundlich constant (1/n=0.129~0.212), this process could be employed as effective treatment method. Adsorption kinetics experimental data were modeled using the pseudo-first-order and pseudo-second-order kinetic equation. It was shown that pseudo-second-order kinetic equation could best describe the adsorption kinetics. Base on the negative Gibbs free energy value (-4.81~-10.33 kJ/mol) and positive enthalpy value (+78.59 kJ/mol) indicate that the adsorption is spontaneous and endothermic process.

Competitive Adsorption of Two Basic Dyes RB5 and GB4 on a Local Clay (점토에 대한 2개 염기성 염료 RB5와 GB4의 경쟁 흡착)

  • Elaziouti, A.;Derriche, Z.;Bouberka, Z.;Laouedj, N.
    • Journal of the Korean Chemical Society
    • /
    • v.54 no.1
    • /
    • pp.110-114
    • /
    • 2010
  • The equilibrium of adsorption of basics dyes RB 5 and BG 4 from a single dyes in the mixtures on the sodium-exchanged clay of the Maghnia (Algeria) was studied. The maximum adsorption capacities of BR5 and BG4 in single dyes were 465.13 and 469.90 mg/g respectively. In the simultaneous adsorption of BR5 and BG4 from mixture solutions, three different initials concentrations ratios R (R=$C_{(BR5)}/C_{(BG4)}$) were tested: 2.5/1, 1/1 and 1/2.5 using ADMI method. The isotherms adsorptions of dyes from the mixtures are characteristics of competition phenomenon. A very strong interaction between BR5 and BG4 for the active sites of adsorption of surface of clay is obtained for R = 1/1. The ratio R' (R'=$Qe_{(mixture)}/Qe_{(single)}$) of the adsorption capacity of BR5 and BG4 in the mixture were reduced by factor of 0.86, 0.74 and 0.84 for the initials concentrations ratios R (R=$C_{(BR5)}/C_{(BG4)}$) of 2.5/1, 1/1 and 1/2.5 respectively. The variation of the ratio of the adsorption capacity R‘ of BR5 and BG4 in the mixture solutions with initial concentration ratios R indicates that BR5 dye is slightly favourable in the competition adsorption than BG4. Langmuir and Freundlich models fit very well with adsorption behaviour of single dyes as well as the dyes in mixture solutions.

Synthesis, Fastness and Spectral Properties of Some New Azo Pyrazole and Pyrazolotriazole Derivatives (Pyrazole과 Pyrazolotriazole 유도체의 합성 및 특성 연구)

  • Rizk, Hala F.;El-Badawi, Mahmoud A.;Ibrahim, Seham A.;El-Borai, Mohamed A.
    • Journal of the Korean Chemical Society
    • /
    • v.54 no.6
    • /
    • pp.737-743
    • /
    • 2010
  • Coupling of 5-amino-1,3-diaryl-pyrazoles 1a-c with diazonium salts of different aryl amines gave a series of novel 1,3-diaryl-5-amino-4-arylazopyrazoles 3a-l. Such compounds could be also obtained by reaction of 5-amino-1,3-diaryl-4-nitroso- 1H-pyrazoles 2a-c with different aryl amines in alkaline medium. Oxidation of azo derivatives 3a-l with cupric acetate, in dimethyl formamide and stream of air, gave 2,4,6-triaryl-2,4-dihydropyrazolo [4,3-d]-1,2,3-triazoles 4a-l. and the fluorescence properties of the cyclic triazoles were studied. Diazotization of 5-amino-1,3-diaryl-1H-pyrazoles 1a-c by sodium nitrite in ortho-phosphoric acid followed by coupling with some aryl amines gave o-aminoazo compounds 5a-f. Cyclisation of compounds 5a-f in pyridine and cupric acetate gave the corresponding triazoles 6a-f. The coupling of compounds 6a-f with different aryl diazonium salts gave compounds 7a-j. The synthesized dyes were applied to polyesters as disperse dyes and the fastness properties were evaluated.

Optimization of Hybrid Process of(Chemical Coagulation, Fenton Oxidation and Ceramic Membrane Filtration) for the Treatment of Reactive Dye Solutions (반응성 염료폐수 처리를 위한 화학응집, 펜톤산화, 세라믹 분리막 복합공정의 최적화)

  • Yang, Jeong-Mok;Park, Chul-Hwan;Lee, Byung-Hwan;Kim, Tak-Hyun;Lee, Jin-Won;Kim, Sang-Yong
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.28 no.3
    • /
    • pp.257-264
    • /
    • 2006
  • This study investigated the effects of hybrid process(chemical coagulation, Fenton oxidation and ceramic UF(ultrafiltration)) on COD and color removals of commercial reactive dyestuffs. In the case of chemical coagulation, the optimal concentrations of $Fe^{3+}$ coagulant for COD and color removals of RB49(reactive blue 49) and RY84(reactive yellow 84) were determined according to the different coagulant dose at the optimal pH. They were 2.78 mM(pH 7) in RB49 and 1.85 mM(pH 6) in RY84, respectively. In the case of Fenton oxidation, the optimal concentrations of $Fe^{3+}\;and\;H_2O_2$ were obtained. Optimal $[Fe^{2+}]:[H_2O_2]$ molar ratio of COD and color removals of RB49 and RY84 were 4.41:5.73 mM and 1.15:0.81 mM, respectively. In the case of ceramic UF, the flux and rejection of supernatant after Fenton oxidation were investigated. After ceramic UF for 9 hr, the average flux of RB49 and RY84 solutions were $53.4L/m^2hr\;and\;67.4L/m^2hr$ at 1 bar, respectively. In addition, the permeate flux increased and the average flux recovery were 98.5-99.9%(RB49) and 91.0-97.3%(RY84) according to adopting off-line cleaning(5% $H_2SO_4$). Finally, COD and color removals were 91.6-95.7% and 99.8% by hybrid process, respectively.

Thermodynamic Analysis on the Hydrolysis Reaction of Vinylsulfonyl Reactive Dyes (VS계 반응염료 가수분해반응의 열역학적 해석)

  • Gwon, Hyeok-Seong;Jeon, Yeong-Sil;Nam, Seong-U;Kim, In-Hoe
    • Proceedings of the Korean Society of Dyers and Finishers Conference
    • /
    • 2008.04a
    • /
    • pp.74-76
    • /
    • 2008
  • The hydrolyses of ten VS dyes were examined at 40$^{\circ}C$, 50$^{\circ}C$, and 60$^{\circ}C$ and the kinetic parameters were estimated. The values of free energy, enthalpy and entropy of hydrolysis and reaction with cellulose for VS dyes were calculated. The linear relationship exist between the enthalpy and entropy. The structure and entropy of VS dyes gave a effect on the dimerization for VS reactive dyes. The VS dyes have small value of entropy were formed dimer. It was confirmed that no dimer form for m-substituted VS dyes. There were similarities among various reactions including homo- and mixed dimerization.

  • PDF

산화물 전극을 이용한 Rhodamine B의 탈색

  • Park, Yeong-Sik;Kim, Dong-Seok
    • Proceedings of the Korean Environmental Sciences Society Conference
    • /
    • 2007.05a
    • /
    • pp.370-374
    • /
    • 2007
  • 난분해성 유기물 처리에 적절한 불용성 전극을 선정하고 성능을 평가하기 위하여 1-3 성분계 전극을 이용하여 양이온 염료인 Rhodamine B (RhB)의 전기분해 처리에서 다음의 결론을 얻었다. 1) 반응 2분 후 RhB 농도를 고찰한 결과 RhB 농도감소는 Ru-Sn-Ti/Ti ${\fallingdotseq}$ Ru-Sn-Sb/Ti > Ir-Sn-Sb/Ti > Sn-Sb/Ti > Ru/Ti > Ir/Ti > Pt/Ti의 순서로 나타나 3성분계 > 2성분계 > 1성분계 전극의 순서로 나타났다. Ru를 사용한 전극이 Ir을 사용한 전극보다 1성분계와 3성분계 모두 성능이 우수한 것으로 나타났다. 기존 전극으로 가장 많이 사용되고 있는 Pt 전극의 성능은 가장 떨어지는 것으로 나타났다. 2) RhB 초기 농도감소 속도는 전극 간격이 좁은 것이 유리한 것으로 나타났으나 최종 농도는 비슷하였다. 전극 간격이 좁을수록 전력 면에서 유리한 것으로 나타났다. 면적이 큰 전극이 초기 반응이 빠르고 나타났고 최종농도도 약간 낮은 것으로 나타났으나 차이는 크지 않았다. 면적이 좁은 경우 반응면적이 적지만 전류밀도가 높기 때문에 성능의 차이는 크지 않으나 면적이 적은 전극의 경우 요구 전력량이 높기 때문에 적절한 크기의 전극이 필요한 것으로 사료되었다.