COMPARISON OF MARGINAL MICROLEAKAGE BETWEEN LOW AND HIGH FLOWABLE RESINS IN CLASS V CAVITY (5급 와동에서 저유동성과 고유동성 레진의 변연 미세누출 비교)

  • Bae, Sang-Bae;Cho, Young-Gon;Lee, Myeong-Seon
    • Restorative Dentistry and Endodontics
    • /
    • v.34 no.6
    • /
    • pp.477-483
    • /
    • 2009
  • The purpose of this study was to compare the microleakage of low and high viscosity flowable resins in class V cavities applied with 1-step adhesives. Forty Class V cavities were prepared on the cervices of buccal and lingual surfaces of extracted molar teeth and divided into four groups (n=8). Cavities were restored with AQ Bond Plus /Metafil Flo $\alpha$, G-Bond/ UniFil LoFlo Plus (Low flow groups), AQ Bond Plus/Metafil Flo and G-Bond/UniFil Flow (High flow group), respectively. Specimens were immersed in a 2% methylene blue solution for 24 hours, and bisected longitudinally. They were observed microleakages at the enamel and dentinal margins. In conclusion, the low viscosity flowable resins showed lower marginal microleakage than do the high vis cosity flowable resins in class V cavities.

A STUDY ON THE RELATIVE SHEAR BOND STRENGTH OF COMPOSITE RESIN TO COMPOMERS (컴포머에 대한 복합레진의 전단결합강도에 관한 연구)

  • Jeong, Song-Ran;Choi, Nam-Ki;Yang, Kyu-Ho;Kim, Seon-Mi;Song, Ho-Jun
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.32 no.3
    • /
    • pp.509-516
    • /
    • 2005
  • For the purpose of comparing the bond strengths of compomers to composite resin, composite Z250, and two polyacid modified composite resin, Dyract AP and F2000, were selected and investigated using universal testing machine for measuring the shear bond strengths. Additionally, the failure modes were examined by observing the fractured surfaces of each specimen. The following results were obtained. 1. The shear bond strength of Dyract AP to Z250 were higher than those of F2000, but there was no statistically significant difference between group 1 and group 3(p>0.05), and groups using fresh compomers showed higher bond strength than those using aged compomers(p<0.05). 2. After measuring the shear bond strength of each group, it was highest in group 5 and was lowest in group 9(p<0.05). 3. Although there was no statistically significant difference, groups treated with thermocycling showed lower bond strengths than those of non-thermocycling groups. 4. Overall compomer/composite resin failures were adhesive. Cohesive failures occurred mainly in groups using bonding agent. Based on these results, the application of a bonding agent on fresh polyacid-modified resin composite increases the bond strength between polyacid-modified resin composite and composite resin. Additionally, the surface of aged polyacid-modified resin composite has to be roughened mechanically and a bonding agent has to be used in combination with composite resin.

  • PDF

THE INFLUENCE OF $CARISOLV^{TM}$ ON SHEAR BOND STRENGTH OF COMPOSITE RESIN RESTORATIONS ($Carisolv^{TM}$의 사용이 복합레진 수복물의 전단결합강도에 미치는 영향)

  • Kim, Dae-Eop
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.30 no.1
    • /
    • pp.47-53
    • /
    • 2003
  • This study evaluated the influence of chemomechanical caries removal agent $Carisolv^{TM}$(MediTeam, Sweden) for composite resin adhesion to sound human permanent and primary dentin. The buccal/labial surfaces of 80 permanent molars and 80 primary incisors were used. Four types of adhesives and one composite resin were used; AQ Bond(Sun Medical, Japan), Clearfil SE Bond(Kuraray, Japan), Single Bond(3M, USA), Scotchbond Multi-Purpose(3M, USA) and Z100(3M, USA). One drop of $Carisolv^{TM}$(MediTeam, Sweden) was pretreated on the dentin for 0 second(control) and 60 seconds. The specimens were thermocycled for 1,000 times in baths kept 5 degrees C and 55 degrees C with a 30 seconds dwell time. Shear bond strengths were tested and the data was statistically analyzed using one-way ANOVA with subsequent post hoc Scheffe test at p<0.05. $Carisolv^{TM}$ treatment significantly decreased the shear bond strength. Shear bond strength of permanent dentin was significantly higher than that of primary dentin. Clearfil SE Bond treatment groups showed the highest shear bond strength and AQ Bond treatment groups showed the lowest shear bond strength.

  • PDF

DEVELOPMENT OF ANTICARIOGENIC COMPOSITE RESIN (항우식성 복합레진의 가능성)

  • Park, Jeong-Won
    • Restorative Dentistry and Endodontics
    • /
    • v.35 no.2
    • /
    • pp.65-68
    • /
    • 2010
  • Due to the improvement of the composite resin and esthetic desire of the patient, amalgam restoration has been replaced by composite resin. However, still there are many unsolved problems, for example, technique sensitivity, polymerization shrinkage stress and limited mechanical properties. These factors results in fracture of the restoration and secondary caries of the tooth. Also the use of the dental bonding system should be used for the retention of the restoration. In this paper, I want to talk about the present and the future of the remineralizing component released from dental composite resin to overcome the secondary caries and there possibility in the clinical use.

The comparison on micro-tensile bond strengths of variable adhesive systems to Class V cavity (5급 와동에서의 수종 접착 시스템의 결합강도에 관한 비교연구)

  • Kwon, Jung-Mi;Choi, Kyung-Kyu;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.29 no.1
    • /
    • pp.1-12
    • /
    • 2004
  • 이 연구는 발거 소구치에서 5급 와동을 형성하여 접착 시스템 및 와동 위치에 따른 상아질에 대한 접착시스템의 미세 인장결합강도의 차이를 비교, 연구하였다. 접착방법은 resin-modified glass ionomer(Gl), compomer(부식여부에 따라 DE 및 DN군으로 분류), 그리고 상아질 접착제인 Single Bond(SB) 및 Cleayfil SE Bond(SE)와 복합레진(Clearfil AP-X)을 사용한 5개의 실험군으로 분류하였다. 소구치 협측 치경부에 wedge형태의 와동을 형성하고 5종의 접착 시스템을 제조자의 지시에 따라 적용, 충전하여 시편을 제작하여 미세인장결합강도를 측정하고, One-way ANOVA / Duncan's test로 통계분석하였다. SEM 검사는 미세인장결합강도의 시편제작과 동일한 방법으로 시편을 제작한 후 관찰하였다. 실험 결과, 상아질 접착제 및 복합레진(SB, SE)의 미세인장결합강도가 GI보다 높게 나타났고(p<0.05), 치은측이 교합측보다 더 낮게 나타났으며, CI, DE, SE에서 유의성 있게 낮게 나타났다(p<0.05). Compomer에서 conditioning 여부(DN, DE)에 따른 변화는 치은측에서만 유의차 있는 것으로 나타났다. SEM 관찰에서, 교합측의 상아세관은 결합 계면과 평행하게 주행하였고, 치은측에서는 결합계면에 수직으로 주행하는 것으로 관찰되었다.

The effect of denture adhesives on the retention of complete denture (의치 접착제가 총의치의 유지력에 미치는 영향에 관한 연구)

  • Yoon, Yu-Mi;Choi, Yu-Sung;Lee, Joon-Seok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.2
    • /
    • pp.87-93
    • /
    • 2010
  • Purpose: The purpose of this study was to compare the retention of the two denture adhesives with a silicone edentulous model and a resin denture base in vitro study. Material and methods: The experimental groups were used two denture adhesives and classified into 5 subgroups each. Subgroups were divided by the number of times the saliva sprayed. The control group was used synthetic saliva only. Dislodging tensile strengths were applied to the resin denture base using Instron in 3 directions ; vertical, lateral, and anterior-posterior. Results: The retention of two denture adhesives was increased significantly than saliva alone (P <.05). In each denture adhesives, the retention of saliva sprayed first was decreased than denture adhesive alone, but it didn't have significant differences. Whenever saliva sprayed repeated, the retention was decreased significantly than saliva sprayed first (P <.05). In each denture adhesives, vertical retentive force was highest than lateral and anterior-posterior retentive forces, and anterior-posterior retentive force was higher than lateral retentive force. This results were significantly different (P < .05). Significant differences of the retentive ability among two denture adhesives were not observed. Conclusion: From the results, use of the denture adhesives resulted in improved retentive ability of denture. Especially retentive force was highest in vertical direction.

THE CHANCE OF ADAPTABILITY CHANCE IN ADHESIVE SYSTEMS TO DENTIN SUBSTRTE ACCORDING TO STORAGE TIME (상아질 접착 후 저장기간에 따른 접착제의 접착력 변화)

  • Cho, Young-Gon;Ban, Il-Hwan;Yu, Mi-Kyung
    • Restorative Dentistry and Endodontics
    • /
    • v.30 no.3
    • /
    • pp.204-214
    • /
    • 2005
  • This study compared the microtensile bond strength (${\mu}$TBS) and microscopic change of two 2-step and two 1-step self-etching adhesives to dentin according to storage times in distilled water. Occlusal dentin was exposed in 48 human molars. They were divided to four groups by different adhesives: SE Bond group (Clearfil SE Bond), AdheSE group (AdheSE). Adper group (Adper Prompt L-Pop), and Xeno group (Xeno III) . Each group was stored in 37$^{\circ}C$ distilled water for 1, 15, and 30 days. Resin-bonded specimens were sectioned into beams and subjected to ${\mu}$TBS testing with a crosshead speed of 1 mm/minute. For SEM observation, one specimen was selected and sectioned in each group after each stroage time. Resin-dentin interface was observed under FE-SEM. In all storage times, mean ${\mu}$TBS of SE group was significantly higher than those of other groups (p < 0.05). There was no significant difference between mean ${\mu}$TBS of SE group and AdheSE group among all storage times, but significant difference between 1- and 30-day storage in mean y${\mu}$TBS of Adper group and Xeno group (p > 0.05). For 1-and 15-day storage, all groups showed the close adaptation between resin-dentin interfaces. For 30-day storage, resin-dentin interfaces showed wide gap in Adper group and separate pattern in Xeno III group.