• 제목/요약/키워드: $Al_2O_3$- composites

검색결과 450건 처리시간 0.027초

탄소섬유강화 질화규소 세라믹스의 마찰마모 특성 (Sliding Wear Properties of Carbon Fiber Reinforced $Si_3N_4$ Ceramics)

  • 박이현;윤한기;김부안;박원조
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.347-351
    • /
    • 2004
  • [ $Si_3N_4$ ] composites have been extensively studied for engineering ceramics, because it has excellent room and high temperature strength, wear resistance properties, good resistance to oxidation, and good thermal and chemical stability. In the present work, carbon short fiber reinforced $Si_3N_4$ ceramics were fabricated by hot press method in $N_2$ atmosphere at $1800^{\circ}C$ using $Al_2O_3\;and\;Y_2O_3$ as sintering additives. Content of carbon short fiber was $0\%,\;0.1\%\;and\;0.3\%$. The composites were evaluated in terms of density, flexural strength and elastic modulus through the 3-point bending test at room temperature. Also, The wear behavior was determined by the pin on disk wear tester using silicon nitride ball. Experimental density and flexural strength decreased with increasing content of carbon fiber. But specific modulus increased with increasing content of carbon fiber. In addition, friction coefficient and specific wear loss decreased with increasing content of carbon short fiber by reason of interfacial defects between matrix and fiber.

  • PDF

액상소결법에 의한 탄화규소 제조시 소결조제와 온도의 영향 (Influence of Sintering Additives and Temperature on Fabrication of LPS-SiC)

  • 정헌채;윤한기
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.266-270
    • /
    • 2004
  • SiC materials have been extensively studied for high temperature components in advanced energy system and advanced gas turbine because it has excellent high temperature strength, low coefficient of thermal expansion, good resistance to oxidation and good thermal and chemical stability etc. However, the brittle characteristics of SiC such as low fracture toughness and low strain-to fracture still impose a severe limitation on practical applications of SiC materials. For these reasons, SiC/SiC composites can be considered as a promising for various structural materials, because of their good fracture toughness compared with monolithic SiC ceramics. But, high temperature and pressure lead to the degradation of the reinforcing jiber during the hot pressing. Therefore, reduction of sintering temperature and pressure is key requirements for the fabrication of SiC/SiC composites by hot pressing method. In the present work, monolithic Liquid Phase Sintered SiC (LPS-SiC) was fabricated by hot pressing method in Ar atmosphere at $1800^{\circ}C$ under 20MPa using $Al_2O_3,\;Y_2O_3\;and\;SiO_2$ as sintering additives in order to low sintering temperature and sintering pressure. The starting powder was high purity $\beta-SiC$ nano-powder with all average particle size of 30mm. The characterization of LPS-SiC was investigated by means of SEM and three point bending test. Base on the composition of sintering additives-, microstructure- and mechanical property correlation, tire compositions of sintering additives are discussed.

  • PDF

소결온도 및 SiO2 첨가량에 따른 탄화규소의 마모 특성 (Wear Characteristics of SiC by Sintered Temperature and SiO2 Contents)

  • 박성호;박원조;윤한기
    • 대한기계학회논문집A
    • /
    • 제32권11호
    • /
    • pp.1003-1009
    • /
    • 2008
  • In this study, liquid phase sintered SiC (LPS-SiC) materials were made by hot pressing method. The particle size of nano-SiC powder was 30nm. Alumina ($Al_2O_3$), yttria ($Y_2O_3$) and silica ($SiO_2$) were used for sintering additives. To investigate effects of $SiO_2$, ratios of $SiO_2$ contents were changed by five kinds. Materials have been sintered for 1 hour at $1760^{\circ}C$, $1780^{\circ}C$ and $1800^{\circ}C$ under the pressure of 20MPa. The system of sintering additives which affects a property of sintering as well as the influence depending on compositions of sintering additives were investigated by measurement of density, mechanical properties such as flexural strength, vickers hardness and sliding wear resistance were investigated to make sure of the optimum condition which is about matrix of $SiC_f$/SiC composites. The abrasion test condition apply to load of 20N at 100RPM for 20min. Sintered density, flexural strength of fabricated LPS-SiC increased with increasing the sintering temperature. And in case of LPS-SiC with low $SiO_2$, sliding wear resistance has very excellent. Monolithic SiC $1800^{\circ}C$ sintering temperatures and 3wt% have excellent wear resistance.

리튬이온 배터리용 정극재료(正極材料)의 기술동향(技術動向) (Technology Trends of Cathode Active Materials for Lithium Ion Battery)

  • 황용길;길상철;김종헌
    • 자원리싸이클링
    • /
    • 제21권5호
    • /
    • pp.79-87
    • /
    • 2012
  • 리튬이온전지의 대형화와 범용화에 따라 경제성과 안정성 관점에서 정극재료의 개발은 중요한 과제로 대두되고 있다. 18650 원통형 전지의 에너지 밀도는 발매 초기인 1991년 230Wh/l에서 2005년 2배 이상의 500Wh/l로 증가하였으며, 제품 대부분의 에너지용량은 450~500 Wh/l, 150~190Wh/kg이고 안전성, 제조비 절감 및 장 수명을 중점적으로 개발하고 있다. $LiCoO_2$ 정극활물질 중의 Co가 고가이므로 Co 사용량을 줄이면서 에너지 용량을 향상시키기 위하여 $LiMn_2O_4$, $LiCo_{1/3}N_{i1/3}Mn_{1/3}O_2$, $LiNi_{0.8}Co_{0.15}Al_{0.05}O_2$, $LiFePO_4$-C복합체 (167 mA/g)등이 개발되고 있다. 전동자전거용 전지는 출력밀도 500 Wh/kg, 전동공구용 1,500Wh/kg, EV나 PHEV용으로는 4,000~5,000Wh/kg의 대용량 출력밀도를 요구하고 있으므로 배터리 소재의 성능을 향상시키려고 많은 연구가 진행되고 있다. 최근 Graphene-sulfur 복합체정극활물질 600 Ah/kg, 2차전지용 분자클러스터(molecular cluster) 320 Ah/kg 등의 새로운 정극활물질이 연구 개발되고 있으므로 실용화가 기대된다.

Ceramic Matrix Composites의 내산화 코팅이 초고온 산화 특성에 미치는 영향

  • 전민광;유연우;남욱희;변응선
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.134-134
    • /
    • 2016
  • CMC(Ceramic Matrix Composites)는 $1500^{\circ}C$ 이상의 고온에서 내열성, 내산화성, 내식성이 우수하여, 초음속 비행체, 가스터빈 엔진 및 원자로용 초고온 부품 등에 수요가 증가하고 있다. 하지만 이러한 특성은 비산소 환경에 국한되는 것으로 약 $400^{\circ}C$ 이상의 산화 분위기에는 탄소섬유가 산화되는 문제로 인하여 적용의 한계를 가지고 있다. 따라서 CMC의 적용범위 확대를 위하여 내산화 코팅으로 CMC의 초고온 산화특성을 개선하는 것이 필수적이며, 장시간 초고온 산화환경 분위기에서 사용되기 위하여 안정적인 코팅기술이 최근 기술개발의 핵심현안으로 부각되고 있다. 본 연구에서는 pack cementation 공정을 이용하여 내산화성이 우수한 SiC 코팅층을 제조하였다. Pack cementation 공정에 사용된 코팅 분말은 57wt.% SiC, 30wt.% Si, 3wt.% B, 10wt.% Al2O3의 비율로 혼합된 것이다. 실험은 3D 직조된 CMC 모재를 혼합분말 내에 침적한 후, Ar 분위기에서 $1600^{\circ}C$, 4~12시간 반응시켜 수 마이크론 두께의 SiC 코팅층을 형성하였다. 더 우수한 산화 특성을 부여하기 위하여 pack 처리된 CMC 표면에 초고온 세라믹인 TaC 소재를 진공플라즈마 코팅 공정으로 적층시켰다. 제조된 코팅층을 SEM, XRD를 이용하여 미세구조 및 결정구조를 분석하였으며, pack cementation에 따른 내산화 특성을 비교 분석하고자 $2000^{\circ}C$에서 산화 실험을 진행하였다. 산화 실험 이후 미세구조 및 결정구조 분석으로 산화거동을 규명하고자 하였다.

  • PDF

섬유/입자 혼합금속복합재료의 인장거동 (Tensile Behavior of Fiber/Particle Hybrid Metal Matrix Composites)

  • 정성욱;정창규;한경섭
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2002년도 추계학술발표대회 논문집
    • /
    • pp.139-142
    • /
    • 2002
  • This study presents a mathematical model predicting the stress-strain behavior of fiber reinforced (FMMCs) and fiber/particle reinforced metal matrix composites (F/P MMCs). MMCs were fabricated by squeeze casting method using Al2O3 short fiber and particle as reinforcement, and A356 aluminum alloy as matrix. The fiber/particle ratios of F/P MMCs were 2:1, 1:1, 1:2 with the total reinforcement volume fraction of 20 vol.%, and the FMMCs were reinforced with 10 vol,%, 15 vol. %, 20 vol. % of fibers. Tensile tests were conducted and compared with predictions which were derived using laminate analogy theory and multi-failure model of reinforcements. Results show that the tensile strength of FMMCs with 10 vol.% of fiber was well matched with prediction, and as the fiber volume increases, predictions become larger than experimental results. The difference between the prediction and experiment is considered to be a result of matrix allowance of fiber damage in tensile loading. As the fiber volume fraction in FMMCs increases, the fiber damage increases and so that the tensile strength is reduced. The strength of F/P MMCs approaches more closely to the prediction than FMMCs reinforced with 20 vol.% of fibers because F/P MMCs contains small quantity of fibers and thus has a positive effect in fiber strengthening.

  • PDF

치과 임플란트용 지르코니아-알루미나 복합체의 생 가공 및 경 가공 특성 (Green and Hard Machining Characteristics of Zirconia-alumina Composites for Dental Implant)

  • 임형봉;당동욱;이기주;조원승
    • 한국세라믹학회지
    • /
    • 제48권2호
    • /
    • pp.152-159
    • /
    • 2011
  • The green and hard machining characteristics of dental ceramics are of great interest to dental industry. The green bodies of TZP/$Al_2O_3$ composites were prepared by the cold isostatic pressing, and machined on the CNC lathe using PCD (polycrystalline diamond) insert under various machining conditions. With increasing nose radius of PCD insert, surface roughness initially increased due to increased cutting resistance, but decreased by the onset of sliding fracture. The lowest surface roughness was obtained at spindle speed of 1,300 rpm and lowest feed rate. Hard bodies were prepared by pressureless sintering the machined green bodies at several temperatures. The grinding test for sintered hard body was conducted using electroplated diamond bur with different grit sizes. During grinding, grain pull out in the composite was occurred due to thermal expansion mismatch between the alumina and zirconia. The strength of the composite decreased with alumina contents, due to increased surface roughness and high monoclinic phase transformed during grinding process. The final polished samples represented high strength by the elimination of a phase transformation layer.

Analysis of Surface Tracking of Micro and Nano Size Alumina Filled Silicone Rubber for High Voltage AC Transmission

  • Loganathan, N.;Chandrasekar, S.
    • Journal of Electrical Engineering and Technology
    • /
    • 제8권2호
    • /
    • pp.345-353
    • /
    • 2013
  • This paper discusses the experimental results in an effort to understand the tracking and erosion resistance of the micro and nano size $Al_2O_3$ filled silicone rubber (SIR) material which has been studied under the AC voltages, with ammonium chloride as a contaminant, as per IEC 60587 test procedures. The characteristic changes in the tracking resistance of the micro and nano size filled specimens were analyzed through leakage current measurement and the eroded masses were used to evaluate the relative erosion and tracking resistance of the composites. The fundamental, third and fifth harmonic of the leakage current during the tracking study were analyzed using moving average current technique. It was observed that the harmonic components of leakage current show good correlation with the tracking and erosion resistance of the material. The thermogravimetry-derivative thermo gravimetric (TG-DTG) studies were performed to understand the thermal degradation of the composites. The physical and chemical studies were carried out by using scanning electron microscope (SEM), Energy Dispersive X-ray analysis (EDAX) and Fourier Transform Infra-red (FTIR) Spectroscopy. The obtained result indicated that the performance of nano filled SIR was better than the micro filled SIR material when the % wt. of filler increased.

Effect of Additive Amount on Microstructure and Fracture Toughness of SiC-TiC Composites

  • Min-Jin Kim;Young-Wook Kim;Wonjoong Kim;Hun-Jin Lim;Duk-Ho Cho
    • The Korean Journal of Ceramics
    • /
    • 제6권2호
    • /
    • pp.91-95
    • /
    • 2000
  • Powder mixtures of $\beta$-SiC-TiC in a weight ratio of 2:1 containing 5-20 wt% additives ($Al_2O_3$-$Y_2O_3$) were liquid-phase sintered at $1830^{\circ}C$ for 1h by hot-pressing and subsequently annealed at $1950^{\circ}C$ for 6h to enhance grain growth. The annealed specimens revealed a microstructure of \"in situ-toughened composite\" as a result of the $\beta$longrightarrow$\alpha$ phase transformation of SiC during annealing. The increase of the content of additives accelerated the growth of elongated $\alpha$-SiC grains with higher aspect ratio and improved fracture toughness. The fracture toughness of SiC-TiC composite containing 20 wt% additive was 6.2 MPa.$m^{1/2}$.2}$.

  • PDF

온도 상승에 따른 혼합금속복합재료의 건식 마찰특성 평가 (Evaluation of Dry Tribological Characteristics of Hybrid Metal Matrix Composites with Temperature Rising)

  • 왕일기;알리 모하마드 압사;송정일
    • Composites Research
    • /
    • 제23권2호
    • /
    • pp.10-16
    • /
    • 2010
  • 가압주조법으로 제조된 알루미나 섬유와 SiC 입자 혼합금속복합재료의 마찰특성을 조사하였다. 핀 형태의 마모 시험편은 전체 부피비 20%에 섬유와 입자의 서로 다른 비를 갖고 있다. 혼합금속복합재료의 윤활마모시험은 핀과 디스크 타입의 마모시험기를 사용하여 수행되었는데, 상온과 고온 $100^{\circ}C$$150^{\circ}C$.에서의 건식마찰특성을 각각 수행하였다. 마모면의 미시분석은 주사전자현미경(SEM)으로 조사하여 마찰특성과 마모거동을 분석하였다. 시험 결과 마모저항은 상온에서는 섬유와 같은 방향인 (PR) 방향에서는 SiC입자의 증가에 따라 향상되었다. 고온에서는 섬유와 수직한 방향(N)의 마모특성은 PR방향의 섬유가 마모면으로 전체적으로 쉽게 뽑히기 때문에 PR방향의 금속보합재료의 마모특성보다 우수하였다. 한편 마찰계수는 온도증가에 따라 감소하였다.