Needle-like $\alpha-Fe_{2}O_{3}$ particles as precursor for magnetic recording media were prepared directly from amorphous ferric hydroxide in the aqueous solution by hydrothermal reaction. Ellipsoidal or rectangular $\alpha-Fe_{2}O_{3}$ particles were formed in the range of pH 10.75~11.75. The length and acicularity of $\alpha-Fe_{2}O_{3}$ particles were decreased gradually with increasing of citric acid concentration. The formation of needle-like $\alpha-Fe_{2}O_{3}$ particles was inhibited above citric acid concentration of $1.5{\times}10^{-4}\;mol$. We can synthesize $\alpha-Fe_{2}O_{3}$ particles with the most superior acicularity at $140^{\circ}C$ and can not expect a good needle-like particles above $220^{\circ}C$.
A study on the characteristics of ${\alpha}$-particle track on cellulose nitrate film was carried out with a particular emphasis on the dependence of track diameter upon chemical etching condition. The track diameters etched in KOH solution appeared to be, on average, three times larger than those etched in NaOH under the same etching condition. The relationship between the track diameters and both etching time and the energy of incident ${\alpha}$-particles was also investigated. It is shown that the particle fluence rate is fairly independent of etching time as far as the condition of irradiation remains unchanged.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.28
no.2
/
pp.69-73
/
2018
Crystal growth of ${\alpha}-Fe_2O_3$ nanosized particles of 80~90 nm in size, which were hydrothermally prepared from 0.03 M $FeCl_3$ solution at $100^{\circ}C$, was investigated in Pb-containing and Pb-free frit. By heating ${\alpha}-Fe_2O_3$ nanosized particles in two frits at $800^{\circ}C$, the average diameter of particles in frits was increased to 200~210 nm and 150~160 nm, respectively, and the crystal growth due to the aggregation and sintering of several ${\alpha}-Fe_2O_3$ particles was observed. Formation ratios of larger particles over 100 nm in diameter were 54 % in Pb-free frit and 85 % in Pb-containing frit. After heating ${\alpha}-Fe_2O_3$ particles in frits at $800^{\circ}C$, 7~9 nm in average diameter of pores were formed in particles. Theses pores were derived from the porous structure of original ${\alpha}-Fe_2O_3$ particles and confined in particles during sintering.
$\alpha$-D-mannosyl fullerene[$C_{60}$]-functionalized gold nanoparticle films were selfassembled using the layer-by-layer method on the reactive of glass slides functionlized with 3-aminopropyltrimethoxysilane. The functionalized glass slides were alternately soaked in the solutions containing $\alpha$-D-mannosyl fullerene[$C_{60}$] and 4-aminothiophenoxide/hexanethiolate-protected gold nanoparticles. $\alpha$-D-mannosyl fullerene[$C_{60}$]-functionalized gold nanoparticle films have grown up to 5 layers depending on the immersion time. The self-assembled nanoparticle films were characterized using UV-vis spectroscopy showed that the surface plasmon band of gold at 530 nm gradually became more evident as successive layers were added to the films.
A method of detecting charged particles in an allyl diglycol carbonate material (PN-3) which is available, amorphous, optically clear and thermoset plastic in which nuclear particle tracks could be revealed by etching in hot NaOH solutions, has been investigated. It has been applied to the study of alpha particle tracks over an energy range of 3.17~5.49 MeV which has been obtained after having passed through several sheets of polycarbonate. The dose equivalent rate of the alpha source was calculated and the spark chamber was used in order to measure the range of alpha particles after having passed through different number of absorbers. The etching characteristics and the detection response of PN-3 have been studied as a funcion of lengths of etched tracks against the parameters of energies and of the track etching rate(V$_{T}$). The investigation of the etching process for alpha particles in the PN-3 provided the most interesting results.s.
Iron oxide (hematite, $\alpha$-${Fe}_{2}{O}_{3}$) particles were prepared directly from aqueous solution using a crystal growth controller. Paticles properties and reaction mechanisum of products as a function of basicity, formation process and mechanism of needle-lkie hematite were investigated. hexagonal hermatite particles were formed in teh range below pH 9.0, ellipsoidal or rectangular hematite particles in the range of pH 10.75-11.75 respectively. In the range above pH 12.50, acicular $\alpha$-FeOOH was formed. Basicity of product solution produced in the range of pH 10.7511.75 was increased slightly as compared with basicity of reastants due to hydroxly ion(OH-) formed by dissociation crystal growth controller. Citric acid which is acted as a crystal growth controller was adsorbed in the form of itrate anion(R-COO-) on the ferric hydroxide and exerted important role on the formation to the needle-like $\alpha$-${Fe}_{2}{O}_{3}$ particles in this reaction system.
Proceedings of the Korea Association of Crystal Growth Conference
/
1997.10a
/
pp.21-25
/
1997
우수한 세라믹스 제조를 위해서는 작은 입자지름, 좁은 입도분포, 구형의 입자형태, dopant와 matrix가 균일한 고용체를 갖고, 응집입자가 없으며 고순도인 원료 분말의 제조가 선행되어야 한다. 이를 위하여 본 연구에서는 수열 합성법을 이용하여$\alpha$-Al$_2$O$_3$, $\alpha$-SiO$_2$, PZT, PSZT, BTO등의 미세분말을 제조하는 공정에서 반응온도, 광화제의 양과 종류, 반응시간, 출발물질의 양과 종류, 전처리공정, 교반공정 등이 평균입자지름과 결정성 및 입도분포에 미치는 영향을 조사하였다. 그결과 미세분말의 종류에 관계없이 반응온도, 반응시간, 성장기질의 농도, 종자결정의 농도 등이 증가할수록 평균입경은 커지며, 광화제의 농도가 증가할수록 평균 입자지름이 작아지고, 광화제의 농도가 종자결정의 농도가 증가할수록 입도분포가 좁아짐을 알 수 있었다. 특히 $\alpha$-SiO$_2$에 대해 수열합성실험으로부터 평균입자지름과 수열합성의 조업변수간의 특성방정식을 얻었다.
In this study, core-crosslinked amphiphilic polymer (CCAP) nanoparticles prepared using a reactive amphiphilic polymer precursor (RARP) were used for preparing some valuable compounds encapsulated polymer nanoparticles with high payload through nanoprecipitation process. Various solvents (acetone, ethanol, and THF) having different polarity and CCAP nanoparticles prepared using different amphiphilicity were used for the preparation of ${\alpha}$-tocopherol encapsulated polymer nanoparticles to investigate their effects on the encapsulation efficiency, payload, nanoparticle size, and stability. CCAP dissolved in hydrophobic solvent, THF, could form ${\alpha}$-tocopherol encapsulated polymer nanoparticles dispersed in water with the high payload of ${\alpha}$-tocopherol and encapsulation efficiency. Because of their physically and chemically robust nano-structure originated from crosslinking of the hydrophobic core, CCAP nanoparticles could encapsulate ${\alpha}$-tocopherol with the high payload (33 wt%) and encapsulation efficiency (97%), and form 70 nm-sized stable nanoparticles in water.
Porous nanofibers comprising hollow ${\alpha}-Fe_2O_3$ nanospheres were prepared by applying both template method and Kirkendall diffusion effect to electrospinning process. During heat-treatment processes, the solid Fe nano-metals formed by initial heat-treatment in the carbon matrix were converted into the hollow structured ${\alpha}-Fe_2O_3$ nanospheres. In particular, PS nanobeads added in the spinning solution were decomposed and formed numerous channels in the composite, which served as a good pathway for Kirkendall diffusion gas. The resulting porous nanofibers comprising hollow ${\alpha}-Fe_2O_3$ nanospheres were applied as an anode material for lithium-ion batteries. The discharge capacities of the nanofibers for the 30th cycle at a high current density of $1.0A\;g^{-1}$ was $776mA\;h\;g^{-1}$. The good lithium ion storage property was attributed to the synergetic effects of the hollow ${\alpha}-Fe_2O_3$ nanospheres and the interstitial nanovoids between the nanospheres. The synthetic method proposed in this study could be applied to the preparation of porous nanofibers comprising hollow nanospheres with various composition for various applications, including energy storage.
The present paper reports the effect of precursor alumina particle size on pore structure and single gas permeation properties of tubular ${\alpha}$-alumina supports, prepared by a combined process of slip casting and sintering. Pore diameter of as-prepared ${\alpha}$-alumina support was highly dependent on precursor ${\alpha}$-alumina particle size. Although, increase in the precursor particle size increases the pore diameter, but the porosity of ${\alpha}$-alumina support mainly control by sintering temperature. Sintering studies reveal that as sintering temperature increased porosity of support decreased. Single gas permeance results indicate that permence is proportional to the square of pore diameter and linearly to porosity. These dependencies revealed that gas permeation trough as-prepared ${\alpha}$-alumina support was governed by viscous flow mechanism. The present announces that precursor ${\alpha}$-alumina particle size and sintering temperature are key parameters to control gas permeantion properties of ${\alpha}$-alumina supports.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.