Crystallographic Relationships of (Ba, Sr) $TiO_3$Thin Film Prepared by Metal-Organic Chemical Vapor Deposition on (111) Textured Pt Electrode

  • Yoo, Dong-Chul;Lee, Jeong-Yong
    • 한국세라믹학회지
    • /
    • 제37권11호
    • /
    • pp.1126-1129
    • /
    • 2000
  • The crystallographic orientations of $Ba_{0.6}$S $r_{0.4}$Ti $O_3$(BST) thin film deposited by a metal-organic chemical vapor deposition on (111) textured Pt electrode were studied with a transmission electron microscopy. The fully crystallized BST thin film (50nm) has (100) and (110) preferred orientations. A high resolution transmission electron microscopy study has revealed the crystallographic orientation relationships between BST thin film and Pt electrode. These relationships explained the preferred orientation of BST film on (111) textured Pt electrode. With these results, we could represent the atomic arrangement at the BST/Pt interface.e.e.

  • PDF

$BaTiO_3$계 세라믹의 $Al_{2}O_{3}$ 첨가에 따른 유전 특성 (Dielectric properties of $BaTiO_3$ system Ceramics Doped with $Al_{2}O_{3}$)

  • 허영식;이원섭;이성갑
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.402-405
    • /
    • 2001
  • $(Ba_{0.6-x}Sr_{0.4}Ca_{x})TiO_{3}$ (x=0.10, 0.15, 0.20) ceramics were fabricated by the mixed-oxide method and their stuctural and dielectric properties were investigated with variation of composition ratio and an amount of $Al_{2}O_{3}$ (0.5, 1.0, 1.5. 2.0, 3.0 wt%) doping content. As a result of the X-ray diffraction BSCT specimens showed dense and homogeneous structure without presence of the second phase. The sintered density was decreased with increase an $Al_{2}O_{3}$ doping content. The Curie temperature and relative dielectric constant at room temperature were decreased with increasing an amount of $Al_{2}O_{3}$ doping content. The dielectric loss is minimum for BSCT doped with 1.5wt% $Al_{2}O_{3}$ content. The tunability was decreased with increasing an Ca content and is about 4.2% for BSCT(50/40/10) doped with 2.0wt% $Al_{2}O_{3}$ content.

  • PDF

BaTiO$_3$계 세라믹의 $Al_2$O$_3$ 첨가에 따른 유전 특성 (Dielectric properties of BaTiO$_3$ system Ceramics Doped with $Al_2$O$_3$)

  • 허영식;이원섭;이성갑
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.402-405
    • /
    • 2001
  • (Ba$\_$0.6-x/Sr$\_$0.4/Ca$\_$x/)TiO$_3$(x=0.10, 0.15, 0.20) ceramics were fabricated by the mixed-oxide method and their structural and dielectric properties were investigated with variation of composition ratio and an amount of Al$_2$O$_3$(0.5, 1.0, 1.5, 2.0, 3.0 wt%) doping content. As a result of the X-ray diffraction BSCT specimens showed dense and homogeneous structure without presence of the second phase. The sintered density was decreased with increase an Al$_2$O$_3$ doping content. The Curie temperature and relative dielectric constant at room temperature were decreased with increasing an amount of Al$_2$O$_3$ doping content. The dielectric loss is minimum for BSCT doped with 1.5wt% Al$_2$O$_3$ content. The tunability was decreased with increasing an Ca content and is about 4.2% for BSCT(50/40/10) doped with 2.0wt% Al$_2$O$_3$ content.

  • PDF

BST 세라믹 저온소결에 $Li_2CO_3$와 ZnBO가 미치는 영향 (Effective of $Li_2CO_3$ and ZnBO for low temperature sintered $(Ba_{0.5},Sr_{0.5})TiO_3$ ceramics)

  • 김세호;유희욱;구상모;하재근;이영희;고중혁
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.297-297
    • /
    • 2007
  • The $(B_{0.5},Sr_{0.5})TiO_3$ ceramics, which added with low sintering materials $Li_2CO_3$ and ZnBO, was investigated for LTCC(low temperature co-fired ceramic) applications. To compare sintering temperature of $(B_{0.5},Sr_{0.5})TiO_3$ respectively, we added 1, 2, 3, 4, and 5wt% of $Li_2CO_3$ and ZnBO to $(B_{0.5},Sr_{0.5})TiO_3$. For confirming the sintering temperature, the respective specimens were sintered from $750^{\circ}C$ to $1200^{\circ}C$ by $50^{\circ}C$. The case of $Li_2CO_3$ greatly lowered the sintering temperature of $(B_{0.5},Sr_{0.5})TiO_3$ ($1350^{\circ}C$) below $900^{\circ}C$. The addition of ZnBO improved the loss tangent of $(B_{0.5},Sr_{0.5})TiO_3$. The crystalline structure of $LiCO_3$ doped $(B_{0.5},Sr_{0.5})TiO_3$ and ZnBO doped $(B_{0.5},Sr_{0.5})TiO_3$ was analyzed with the X-ray diffraction (XRD) analysis. The dielectric permittivity and loss tangent of $Li_2CO_3$ doped BST and ZnBO doped BST were measured with the HP 4284A precision. From the electrical characterization, we respectively obtained the dielectric permittivity 1361, loss tangent $6.94{\times}10^{-3}$ at $Li_2CO_3$ doped $(B_{0.5},Sr_{0.5})TiO_3$ (3wt%) and the dielectric constant 1180, loss tangent $3.70{\times}10^{-3}$ at ZnBO doped $(B_{0.5},Sr_{0.5})TiO_3$(5wt%).

  • PDF

Microstructural Investigation of $Ba_{0.7}Sr_{0.3}TiO_3$ (BST) Thin Films on Various Electrodes and Buffers

  • Seokmin Hong;Rhim, Sung-Min;Heungjin Bak;Ilsin An;Kim, Ok-Kyung
    • The Korean Journal of Ceramics
    • /
    • 제6권4호
    • /
    • pp.333-338
    • /
    • 2000
  • $Ba_{0.7}Sr_{0.3}TiO_3$(BST) thin films were deposited simultaneously on various electrodes and buffers by the sputtering technique. When the substrate temperature was varied, the BST thin film on each electrode showed good crystallinity above $550^{\circ}C$ as revealed by X-ray diffraction measurements. The surface morphology, determined by atomic force microscopy, indicated that the roughness of BST thin films on $RuO_2$was substrate dependent. However, BST thin films on Ru electrodes are smoother and showed no substrate dependence, probably because the precursor surface diffusion length was greater than the sinusoidal perturbations of the wavelength.

  • PDF

Tunable Properties of Ferroelectric Thick Films With MgO Added on (BaSr)TiO3

  • Kim, In-Sung;Song, Jae-Sung;Jeong, Soon-Jong;Jeon, So-Hyun;Chung, Jun-Ki;Kim, Won-Jeong
    • Journal of Electrical Engineering and Technology
    • /
    • 제2권3호
    • /
    • pp.391-395
    • /
    • 2007
  • MgO enhanced $(Ba_{0.6}Sr_{0.4})$ $TiO_3$ thick films have been fabricated by a tape casting and firing method for tunable devices on the microwave frequency band. In order to improve ferroelectric properties, the composite thick films enhanced with MgO on BST have been asymmetrically annealed by a focused halogen beam method. Dielectric constants of composite thick films are changed from 1050 to 1300 at 100 kHz after 60 s and 150 s annealing by the focused halogen beam. Even though no prominent changes were previously observed from the thick films before and after annealing in terms of chemical composition and surface morphology, it is clear that the average particle size of the thick films calculated by Scherrer's formula were increased by annealing. Furthermore, a strong correlation between particle size and dielectric constant of the composite thick films has been observed; dielectric constant increases with increased particle size. This has been attributed to the increased volume of ferroelectric domain due to increased particle sizes. As a result, the tuning range was improved by halogen beam annealing.

$Li_2CO_3$가 첨가된 $(Ba_{1-X}Sr_x)TiO_3$의 저온소결 특성에 관한 연구 (Low Temperature Sintering Properties of $(Ba_{1-X}Sr_x)TiO_3$ Ceramics Added $Li_2CO_3$)

  • 전소현;김인성;송재성;민복기;윤존도
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.303-304
    • /
    • 2005
  • Add $Li_2CO_3$ to $(Ba_{0.6}Sr_{0.4})$ $TiO_3$ powder to lower sitering temperature in this research, made thick film by tape casting method. Investigated about sitering temperature and physical properties that added $Li_2CO_3$ Even if lower sitering temperature about $200^{\circ}C$ adding $Li_2CO_3$ 10wt.%, density was near to 5.7$g/cm^3$ that is theoretical values, and crystal structure examined as perobeuseukaiteu senior after sintering.

  • PDF

Structural and electrical properties of Ba(Sr,Ti)O3/K(Ta,Nb)O3 multilayer thin film for the application of electro-caloric devices

  • Kwon, Min-Su;Lee, Sung-Gap;Kim, Kyeong-Min;Choi, Seungkeun
    • Journal of Ceramic Processing Research
    • /
    • 제20권6호
    • /
    • pp.603-608
    • /
    • 2019
  • In this study, the multilayered thin films of (Ba,Sr)TiO3/K(Ta,Nb)O3 were fabricated by the sol-gel and spin coating methods, and their structural and electrical properties were investigated. The specimen showed polycrystalline X-ray diffraction (XRD) characteristics with a tetragonal structure. The average grain size and film thickness for one coating were about 30~40nm and 60nm, respectively. The phase transition temperature of specimen was lower than 10 ℃. The dielectric constant and loss at 20 ℃ of the specimen coated six times were 1,231 and 0.69, respectively. The rate of change in dielectric constant at an applied direct current (DC) voltage of the six times coated thin films was 17.3%/V. The electrocaloric effect was the highest around the temperature at which the remanent polarization rapidly changed. When an electric field of 660kV/cm was applied to the triply coated thin films, the highest electrocaloric property of 4.41 ℃ was observed.

X-Band Phased Array Antenna Using Ferroelectric $(Ba,Sr)TiO_3$ Coplanar Waveguide Phase Shifter

  • Moon, Seung-Eon;Ryu, Han-Cheol;Kwak, Min-Hwan;Kim, Young-Tae;Lee, Su-Jae;Kang, Kwang-Yong
    • ETRI Journal
    • /
    • 제27권6호
    • /
    • pp.677-684
    • /
    • 2005
  • A phased array antenna was fabricated using four-element ferroelectric phase shifters with a coplanar waveguide (CPW) transmission line structure based on a $Ba_{0.6}Sr_{0.4}TiO_3(BST)/MgO$ structure. Epitaxial BST films were deposited on MgO (001) substrates by pulsed laser deposition. To attain the large differential phase shift and small losses for a ferroelectric CPW phase shifter, an impedance-matching-part adding technique between the effective transmission line and connecting cable was used. The return loss and insertion loss for this techniqueadapted BST CPW device were improved with respect to those for a normal BST CPW device. For an X-band phased array antenna system consisting of ferroelectric BST CPW phase shifters, power divider, dc block, patch antenna, and programmed dc power, the steering beam could be tilted by $15^{\circ}$ in either direction.

  • PDF

졸겔법에 의해 제작된 강유전체 BST막의 기계.화학적인 연마 특성 (Chemical Mechanical Polishing (CMP) Characteristics of BST Ferroelectric Film by Sol-Gel Method)

  • 서용진;박성우
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제53권3호
    • /
    • pp.128-132
    • /
    • 2004
  • The perovskite ferroelectric materials of the PZT, SBT and BST series will attract much attention for application to ULSI devices. Among these materials, the BST ($Ba_0.6$$Sr_0.4$/$TiO_3$) is widely considered the most promising for use as an insulator in the capacitors of DRAMS beyond 1 Gbit and high density FRAMS. Especially, BST thin films have a good thermal-chemical stability, insulating effect and variety of Phases. However, BST thin films have problems of the aging effect and mismatch between the BST thin film and electrode. Also, due to the high defect density and surface roughness at grain boundarys and in the grains, which degrades the device performances. In order to overcome these weakness, we first applied the chemical mechanical polishing (CMP) process to the polishing of ferroelectric film in order to obtain a good planarity of electrode/ferroelectric film interface. BST ferroelectric film was fabricated by the sol-gel method. And then, we compared the surface characteristics before and after CMP process of BST films. We expect that our results will be useful promise of global planarization for FRAM application in the near future.