• 제목/요약/키워드: wellbore integrity

검색결과 5건 처리시간 0.025초

Rock Permeability Estimation from Hydraulic Injection Tests in a Sealed Borehole Interval

  • Quach, Nghiep Q.;Jo, Yeonguk;Chang, Chandong
    • 지질공학
    • /
    • 제28권1호
    • /
    • pp.1-9
    • /
    • 2018
  • We propose a borehole test technique to estimate permeability of rocks in borehole. The borehole tests are hydraulic injection tests such as leak-off test and hydraulic fracturing tests, which are originally conducted for stress or casing integrity assessment and not for permeability measurement. We use one-dimensional radial diffusion equation to interpret fluid injection test results in terms of permeability. We apply this technique to a leak-off test conducted at a depth of 700 m in a wellbore, where rock formation is mudstone. The estimated permeability is at an order of $10^{-16}m^2$, which is somewhat high but within the range reported for mudstones previously. Quantitative rick assessment suggests that an accurate measurement of open hole section length is important to improve reliability of results. More data may be needed to ensure the reliability of this technique. If validated, however, this technique can provide cost-effective estimation of in situ permeability without conducting independent permeability tests in borehole.

Formation of Hydroxyapatite in Portland Cement Paste

  • Chung, Chul-Woo;Lee, Jae-Yong;Kim, Ji-Hyun
    • 한국건축시공학회지
    • /
    • 제14권1호
    • /
    • pp.68-75
    • /
    • 2014
  • In order to increase the integrity of the wellbore which is used to prevent the leakage of supercritical $CO_2$, it is necessary to develop a concrete that is strongly resistant to carbonation. In an environment where the concentration of $CO_2$ is exceptionally high, $Ca^{2+}$ ion concentration in pore solution of Portland cement concrete will drop significantly due to the rapid consumption of calcium hydroxide, which decreases the stability of the calcium silicate hydrate. In this research, calcium phosphates were used to modify Portland cement system in order to produce hydroxyapatite, a hydration product that is strongly resistant to carbonation under such an environment. According to the experimental results, calcium phosphates reacted with Portland cement to form hydroxyapatite. The formation of hydroxyapatite was verified using X-ray diffraction analyses with selective extraction techniques. When using dicalcium phosphate dihydrate and tricalcium phosphate, the 28-day compressive strength was lower than that of plain cement paste. However, the specimen with monocalcium phosphate monohydrate showed equivalent strength to that of plain cement paste.

Field trial of expandable profile liners in a deep sidetrack well section and optimizable schemes approach for future challenges

  • Zhao, Le;Tu, Yulin;Xie, Heping;Gao, Mingzhong;Liu, Fei
    • Steel and Composite Structures
    • /
    • 제44권2호
    • /
    • pp.271-281
    • /
    • 2022
  • This study discusses challenges of running expandable profile liners (EPLs) to isolate trouble zones in directional section of a deep well, and summary the expandable profile liner technology (EPLT) field trial experience. Technically, the trial result reveals that it is feasible to apply the EPLT solving lost-circulation control problem and wellbore instability in the deep directional section. Propose schemes for optimizing the EPLT operation procedure to break through the existing bottleneck of EPLT in the deep directional section. Better-performing transition joints are developed to improve EPL string reliability in high borehole curvature section. High-performing and reliable expanders reduce the number of trips, offer excellent mechanical shaping efficiency, simplify the EPLT operation procedure. Application of the expansion and repair integrated tool could minimize the risk of insufficient expansion and increase the operational length of the EPL string. The new welding process and integrated automatic welding equipment improve the welding quality and EPL string structural integrity. These optimization schemes and recent new advancements in EPLT can bring significant economic benefits and promote the application of EPLT to meet future challenges.

초임계 CO2 - 시멘트 반응 전후의 투수율 및 강도 변화 (Permeability and Strength of Cements Exposed to Supercritical CO2 for Varying Periods)

  • 이희권;김기덕;김태희;김교원
    • 지질공학
    • /
    • 제26권1호
    • /
    • pp.117-128
    • /
    • 2016
  • 시멘트(KS-1 보통 포틀랜드와, Class G)을 이용하여, 시멘트-초임계CO2 반응실험과 반응 전/후 시료의 절대투수율 및 강도를 측정하였다. 시멘트 시료는 W/S (Water/Solid)와 fly ash 첨가량을 조절하여 제작하였다. 반응 전 시료의 투수율은 0.009~0.025 mD, 초임계CO2와 100일간 반응 한 시료의 투수율은 0.11~0.29 mD의 범위로 각각 측정되었다. 반응 후 시료의 투수율이 높게 측정된 이유는, 반응 시료들이 겪은 응력해방으로 인해 균열이 발생하였기 때문이다. 그러나 측정된 투수율은 대부분의 시료에서 API가 추천하는 최대허용 투수율(=0.2 mD)보다 낮다. 초임CO2에 의한 시멘트 변질은 시료 전체가 아닌 시료의 가장자리에서 일정 두께로 시료의 내부로 발생하였다. 반응영역의 비커스 경도 값이 비반응영역의 것보다 훨씬 높게 측정되었다. 또한 대부분의 시료에서 반응영역 내에서 경도값이 증가한 후 감소하는 현상이 관찰 되었다. 경도값의 증가는 탄산화로 인한 밀도증가, 공극률 감소, 그리고 경도값 감소는 낮은 강도를 갖는 비정질 규산염수화물의 생성이 원인이다.

국내 대구경 시추공 굴진 중 Extended Leak-Off Test 수행 사례 보고 (Report on Extended Leak-Off Test Conducted During Drilling Large Diameter Borehole)

  • 조영욱;송윤호;박세혁;김명선;박인화;이창현
    • 터널과지하공간
    • /
    • 제32권5호
    • /
    • pp.285-297
    • /
    • 2022
  • 본 고에서는 한반도 동남권에 분포하는 주요 단층대에 대한 장기 거동 및 미소진동 관찰을 목적으로 하는 시추공 기반 심부 복합지구물리 모니터링 시스템 구축의 일환으로 수행된 대구경 시추공 굴착 현장에서 이루어진 Extended Leak-Off Test (XLOT)에 대한 내용 및 결과를 보고한다. 다양한 시추공 센서 설치를 위한 모니터링공의 굴착은 ~1 km 깊이에서 최종 구경 200 mm 이상을 확보하는 것을 목표로 하여, 중간 깊이까지 12" 구경의 시추공 굴진 및 케이싱 설치, 이후 최종 심도까지 7-7/8" 구경의 시추공을 굴진하는 것으로 설계되었다. 현장 여건에 맞추어 약 504 m 깊이까지 12" 구경의 시추공이 굴착되었으며, API 규격의 8-5/8" 케이싱을 설치하고 배면과 암반 간의 틈새(annulus)에 대한 세멘팅 작업을 수행하였다. 이후 하부 구간 굴진(7-7/8")에 앞서 세멘팅 건정성 확인 및 암반 응력 측정 등을 목적으로 XLOT를 수행하였다. 약 4 m 길이의 나공 구간(open hole)을 확보하고, 상부에 설치된 케이싱을 이용해 물을 주입하여 시험 심도의 암반을 가압하였다. XLOT 수행 과정에서 주입 유량에 따른 시험 구간 내 압력 변화 양상을 실시간 모니터링 하였으며, 이 자료들을 일부 활용하여 현장 시추공 조건에서의 암반 투수율을 해석하였다.