Development and Performance Evaluation of Liquid-type Chemical Additive for Warm-Mix Asphalt (중온화 액상형 화학첨가제 개발과 이를 적용한 중온 아스팔트의 성능 평가)

  • Baek, Cheolmin;Yang, Sunglin;Hwang, Sungdo
    • International Journal of Highway Engineering
    • /
    • v.15 no.4
    • /
    • pp.107-116
    • /
    • 2013
  • PURPOSES: The liquid-type chemical warm-mix asphalt (WMA) additive has been developed. This study evaluates the basic properties of the additive and the mechanical properties of WMA asphalt and mixture manufactured by using the newly developed chemical additive. METHODS: First, the newly developed WMA additive was applied to the original asphalt by various composition of additive components and dosage ratio of additive. These WMA asphalt binders were evaluated in terms of penetration, softening point, rotational viscosity, and PG grade. Based on the binder test results, one best candidate was chosen to apply to the mixture and then the mechanical properties of WMA mixture were evaluated for moisture susceptibility, dynamic modulus, and rutting and fatigue resistance. RESULTS : According to the binder test, WMA asphalt binders showed the similar properties to the original asphalt binder except the penetraion index of WMA additive was a little higher than original binder. From the Superpave mix design, the optimum asphalt content and volumetric properties of WMA mixture were almost the same with those of hot mix asphalt (HMA) mixture even though the production and compaction temperatures were $30^{\circ}C$ lower for the WMA mixture. From the first set of performance evaluation, it was found that the WMA mixture would have some problem in moisture susceptibility. The additive was modified to improve the resistance to moisture and the second set of performance evaluation showed that the WMA mixture with modified chemical additive would have the similar performance to HMA mixture. CONCLUSIONS : Based on the various laboratory tests, it was concluded that the newly developed chemical WMA additve could be successfully used to produce the WMA mixture with the comparable performance to the HMA mixture. These laboratory evaluations should be confirmed by applying this additive to the field and monitoring the long-term performance of the pavement, which are scheduled in the near future.

Evaluation for Application of Warm-mix Asphalt Concrete for Rural Road Pavement (농촌 도로 포장용 준고온 아스팔트 콘크리트 적용 평가)

  • Lee, Sungjin;Kim, Kwang W.;Kim, Sungun
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.63 no.2
    • /
    • pp.41-50
    • /
    • 2021
  • The asphalt pavement industry has introduced the warm-mix asphalt (WMA) as a mean of energy saving and environmentally safe technology, because the WMA mixture can be mixed and compacted at 30℃ lower than conventional hot-mix asphalt (HMA) at 160℃ or higher. The implementation of WMA can be a good option for paving operations for rural road in remote place, not only due to energy saving and environmental issues, but also lower working temperature. Using WMA technology, the cooled-down asphalt mixture can be still compacted to meet the quality requirement in narrow winding rural road in remote places. Therefore, this study is designed to evaluate engineering properties of WMA binders and concretes, which were prepared for rural road pavement. The objective of the study was to evaluate and suggest proper fundamental properties level of the WMA concrete for rural road pavement. The kinematic viscosity test result indicated that the WMA binders used in this study were effective for compaction at lower temperature, i.e., at 115℃, compared to the HMA binder. According to strength property analyses, it was found that the WMA concrete was acceptable for rural road pavement even though it was compacted at 30℃ lower level. Since the deformation strength (SD) of 3.2 MPa was found to satisfy rutting and cracking resistance minimum guidelines, this value was suggested as a minimum SD value for rural road pavement, considering lack of maintenance program for rural area.

Variation of Flexural Strength of Warm-mix Asphalt Concretes Due to Differential Thermal Contraction at Low Temperatures (저온하에서 시차열 수축에 의한 WMA 콘크리트의 휨강도 변화)

  • Choi, Jung-Soon;Kim, Sung-Un;Kim, Kwang-Woo
    • International Journal of Highway Engineering
    • /
    • v.14 no.4
    • /
    • pp.63-72
    • /
    • 2012
  • PURPOSES : Hot-mix asphalt(HMA) concretes show a trend of strength increase at low temperature due to binder stiffness increase, but strength decrease below a ceratin low temperature. This is due to the differential thermal contraction(DTC) which is induced by a significant difference in coefficients of thermal contraction between aggregate and asphalt which is coated around the aggregate. This DTC damage is well known to occur in HMA concrete, but is not yet investigated in warm-mix asphalt(WMA) concretes. METHODS : To evaluate DTC damage on WMA in this study, the flexural strength($S_f$) of WMA concretes, which were produced at $30{\sim}40^{\circ}C$ lower temperature, was evaluated in comparison with that of HMA at -5, -15 and $-25^{\circ}C$. RESULTS : Most of WMA and HMA mixtures showed flexural strength increase down to $-15^{\circ}C$ and decrease below $-15^{\circ}C$. this type of strength reduction below $-15^{\circ}C$ can e explained as the effect of differential thermal contraction that is a consequence of the large difference in coefficients of thermal contraction between aggregate and asphalt. the property reduction of WMA is similar the result of previous works dealt with HMA mixtures. CONCLUSIONS : Even though there is some differences by materials used, the WMA concretes showed a significantly lower DTC damage than HMA concrete at low temperature at ${\alpha}$=0.05 level.

Properties of SBS-modified Warm-mix Asphalt Binders (SBS 개질 준고온 아스팔트 바인더의 특성)

  • Kim, Sung Un;Lee, Sung Jin;Youn, Yeo;Kim, Kwang Woo
    • International Journal of Highway Engineering
    • /
    • v.16 no.2
    • /
    • pp.19-24
    • /
    • 2014
  • PURPOSES : The study objective was to evaluate rheology and physical properties of SBS-modified warm-mix asphalt (WMA) binders in comparison with hot-mix asphalt (HMA) binders. METHODS : Four different SBS polymers were used to prepare polymer-modified asphalt (PMA) binders, and three different warm-mix additives (WAD) were used to prepare a total of 12 WMA PMA binders. The kinematic viscosity was measured at 115, $135^{\circ}C$. The PG was determined using DSR and BBR. The pass/fail (P/F) temperatures for high and low PG grading were evaluated for HMA PMA and WMA PMA binders. RESULTS : PG 76-22 binders could be prepared by modifying the base binder (PG 64-22) using 4.5 wt% of SBS. The kinematic viscosity (KV) of SBS PMA was increased by 3 times higher than that of base asphalt. The SBS PMA with WAD showed 10% lower KV than that of the normal SBS PMA at $115^{\circ}C$ The high P/F temperatures showed almost no difference between HMA PMA and WMA PMA binders. The high P/F temperature showed very high correlations with KV ($R^2$ > 0.97). The result of SBS modification caused increase of low P/F temperature by $2.7^{\circ}C$ on average. CONCLUSIONS : Since the PMA with WAD showed 10% lower KV than normal (HMA) PMA at $115^{\circ}C$, reducing PMA mixture temperature down to a WMA level was possible in this study. The higher KV binders showed the higher P/F temperature. There was almost no change in high P/F temperature due to the use of WAD. The SBS PMA, showing an increased low P/F temperature, might show somewhat poorer performance at low-temperature, even though the lower PG grade was staying at the same level, i.e., $-22^{\circ}C$.

Evaluation of Fatigue Resistance of Selected Warm-mix Asphalt Concrete (준고온 아스팔트 콘크리트 피로저항성 평가)

  • Kim, Sungun;Lee, Sung-Jin;Kim, Kwang W.
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.62 no.3
    • /
    • pp.29-38
    • /
    • 2020
  • Since some warm-mix asphalt (WMA) concretes were known to show poorer rut resistance than the hot-mix asphalt (HMA) concretes, many studies were performed in efforts of improving its performance at high temperature. The reason is assumed to be due to the moisture remaining in aggregates dried at lower temperature. Therefore, not only the rut resistance, the crack resistance of WMA concrete was also in question. In this study, fatigue life of WMA concrete was evaluated in comparison with HMA using 3-point bending (3PB) beam test. The asphalt mixtures were prepared based on Korean mix-design guide using a 13 mm dense-graded aggregate and 6 binders; two HMA binders and four WMA binders. By 3PB fatigue test, normal (unmodified) and polymer-modified WMA concretes were evaluated in comparison with normal and polymer-modified HMA concretes at a low temperature (-5℃). The results showed that most of WMA concretes showed longer fatigue lives than HMA concretes, even though the same PG binders were used for HMA and WMA. This result indicates that the WMA concretes have stronger resistance against fatigue cracking than HMA at the low temperature, and this result is in contrast to the high-temperature performance test.

Characterization of Flame-Retardant Foam Asphalt (난연성 폼아스팔트 특성에 관한 연구)

  • Hong, Young-Keun
    • Elastomers and Composites
    • /
    • v.47 no.3
    • /
    • pp.246-253
    • /
    • 2012
  • This study was carried out to prepare a type of warm mix asphalt. Through urethane foam and emulsion asphalt preparation techniques a protocol of asphalt foam was made. Then three kinds of flame retardant agents were added in there to alleviate the inherent susceptability of asphalt and foam material to flame and thus flame retardant asphalt foam was made. The internal structure of form asphalt was composed of open cell. The higher the NCO% brought the larger the cell and the stronger also. Asphalt increased the strength of the foam. Among the flame retardant agents employed tritorylphosphate was the most effective.

Performance Evaluation of RAP and WMA Mixtures Located in MN/Road Test Cells through Air Voids Analyses (MN/Road 시험포장 구간내의 공기량 측정 및 결과값 분석을 통한 RAP 및 저온 아스팔트(WMA) 혼합물의 특성 평가)

  • Moon, Ki Hoon;Falchetto, Augusto Cannone;Jeong, Jin Hoon
    • International Journal of Highway Engineering
    • /
    • v.16 no.4
    • /
    • pp.63-74
    • /
    • 2014
  • PURPOSES: This research is to evaluate the mechanical performance of different types of Hot Mix Asphalt (HMA) pavement cells prepared for MN/Road field testing section through an extensive experimental analysis of air voids and simple statistical evaluation tools (i.e. hypothesis test). METHODS: An extensive experimental work was performed to measure air voids in 82 asphalt mixture cores (238 samples in total) obtained from nine different types of road cell located in MN/Road testing field. In order to numerically and quantitatively address the differences in air voids among the different test Cells built in MN/Road, a simple statistical test method (i.e. t-test) with 5% significance was used. RESULTS: Similar trends in air voids content were found among the mixtures including conventional HMA, Reclaimed Asphalt Pavement (RAP) and Warm Mix Asphalt (WMA) combined with taconite aggregate this provides support to the use of RAP and WMA technology in the constructions of asphalt pavement. However, in case of acid modified HMA mixtures, significant differences in air void content were observed between on the wheel path and between wheel path location, which implies negative performances in rutting and thermal cracking resistances. Conclusions : It can be concluded that use of RAP and WMA technology in the construction of conventional asphalt pavement and the use of PPA (Poly Phosphoric Acid) in combinations with SBS (Styrene Butadiene Styrene) in asphalt binder production provide satisfactory performance and, therefore, are highly recommended.

A Study on Characteristic of Warm Mix Asphalt (중온형 아스팔트 콘크리트 특성연구)

  • Jo, Shin-Haeng;Jun, Soon-Je;Jeun, Jun-Young;Ryu, Deug-Hyun
    • 한국방재학회:학술대회논문집
    • /
    • 2008.02a
    • /
    • pp.313-316
    • /
    • 2008
  • Temperature reduction in the manufacturing of asphalt mixtures is highly desirable from a number of aspects. Reduced fumes and emissions, and reduced energy consumption, are important environmental reasons to continue pursuing the goal of temperature reduction. There are important construction and performance advantages as well. For instance, improved workability results in better compaction; lower production and placement temperatures may improve prospects for cold weather paving; and lower temperatures will result in less binder aging and possibly better cracking resistance. The performance of WMA is not to be satisfied though there are various advantages. Therefore, more research is needed on a number of issues