  • We investigated the MoS2 thin film layer by thermolytic deposition and applied it to the silicon solar cells. MoS2 thin films were made by two methods of dipping and spin coating of (NH4)2MoS4 precursor solution. We implemented two types of substrates of microtextured and nano-microtextured 6-in. Si pn junction wafers. The fabricated MoS2 thin film layer was analyzed, and solar cells were fabricated by applying the standard silicon solar cell process. The MoS2 thin film layer of sulfur-deficient form was deposited on the n-type emitter layer, and electrons, which are minority carriers, were well transported at the interface and exhibited photovoltaic solar cell characteristics. The cell efficiencies were achieved at 5% for microtextured wafers and 2.56% for nano-microtextured wafers.

  • PDF

Effect of Saw-Damage Etching Conditions on Flexural Strength in Si Wafers for Silicon Solar Cells (태양전지용 실리콘 기판의 절삭손상 식각 조건에 의한 곡강도 변화)

  • Kang, Byung-Jun;Park, Sung-Eun;Lee, Seung-Hun;Kim, Hyun-Ho;Shin, Bong-Gul;Kwon, Soon-Woo;Byeon, Jai-Won;Yoon, Se-Wang;Kim, Dong-Hwan
    • Korean Journal of Materials Research
    • /
    • v.20 no.11
    • /
    • pp.617-622
    • /
    • 2010
  • We have studied methods to save Si source during the fabrication process of crystalline Si solar cells. One way is to use a thin silicon wafer substrate. As the thickness of the wafers is reduced, mechanical fractures of the substrate increase with the mechanical handling of the thin wafers. It is expected that the mechanical fractures lead to a dropping of yield in the solar cell process. In this study, the mechanical properties of 220-micrometer-solar grade Cz p-type monocrystalline Si wafers were investigated by varying saw-damage etching conditions in order to improve the flexural strength of ultra-thin monocrystalline Si solar cells. Potassium hydroxide (KOH) solution and tetramethyl ammonium hydroxide (TMAH) solution were used as etching solutions. Etching processes were operated with a varying of the ratio of KOH and TMAH solutions in different temperature conditions. After saw-damage etching, wafers were cleaned with a modified RCA cleaning method for ten minutes. Each sample was divided into 42 pieces using an automatic dicing saw machine. The surface morphologies were investigated by scanning electron microscopy and 3D optical microscopy. The thickness distribution was measured by micrometer. The strength distribution was measured with a 4-point-bending tester. As a result, TMAH solution at $90^{\circ}C$ showed the best performance for flexural strength.

A Study on the Bond Strength of BCB-bonded Wafers (BCB 수지로 본딩한 웨이퍼의 본딩 결합력에 관한 연구)

  • Kwon, Yongchai;Seok, Jongwon;Lu, Jian-Qiang;Cale, Timothy;Gutmann, Ronald
    • Korean Chemical Engineering Research
    • /
    • v.45 no.5
    • /
    • pp.479-486
    • /
    • 2007
  • Four point bending is used to study the dependences of bond strength of benzocyclobutene(BCB) bonded wafers and BCB thickness, the use of an adhesion promoter, and the materials being bonded. The bond strength depends linearly on BCB thickness, due to the thickness-dependent contribution of the plastic dissipation energy of the BCB and thickness independence of BCB yield strength. The bond strength increases by about a factor of two with an adhesion promoter for both $2.6{\mu}m$ and $0.4{\mu}m$ thick BCB, because of the formation of covalent bonds between adhesion promoter and the surface of the bonded materials. The bond strength at the interface between a silicon wafer with deposited oxide and BCB is about a factor of three higher than that at the interface between a glass wafer and BCB. This difference in bond strength is attributed to the difference in Si-O bond density at the interfaces. At the interfaces between plasma enhanced chemical vapor deposited (PECVD) oxide coated silicon wafers and BCB, and between thermally grown oxide on silicon wafers and BCB, 12~13 and $15{\sim}16bonds/nm^2$ need to be broken. This corresponds to the observed bond energies, $G_0s$, of 18 and $22J/m^2$, respectively. Maximum 7~8 Si-O $bonds/nm^2$ are needed to explain the $5J/m^2$ at the interfaces between glass wafers and BCB.

Data Qualification of Optical Emission Spectroscopy Spectra in Resist/Nitride/Oxide Etch: Coupon vs. Whole Wafer Etching

  • Kang, Dong-Hyun;Pak, Soo-Kyung;Park, George O.;Hong, Sang-Jeen
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.433-433
    • /
    • 2012
  • As the requirement in patterning geometry continuously shrinks down, the termination of etch process at the exact time became crucial for the success in nano patterning technology. By virtue of real-time optical emission spectroscopy (OES), etch end point detection (EPD) technique continuously develops; however, it also faced with difficulty in low open ratio etching, typically in self aligned contact (SAC) and one cylinder contact (OCS), because of very small amount of optical emission from by-product gas species in the bulk plasma glow discharge. In developing etching process, one may observe that coupon test is being performed. It consumes costs and time for preparing the patterned sample wafers every test in priority, so the coupon wafer test instead of the whole patterned wafer is beneficial for testing and developing etch process condition. We also can observe that etch open area is varied with the number of coupons on a dummy wafer. However, this can be a misleading in OES study. If the coupon wafer test are monitored using OES, we can conjecture the endpoint by experienced method, but considering by data, the materials for residual area by being etched open area are needed to consider. In this research, we compare and analysis the OES data for coupon wafer test results for monitoring about the conditions that the areas except the patterns on the coupon wafers for real-time process monitoring. In this research, we compared two cases, first one is etching the coupon wafers attached on the carrier wafer that is covered by the photoresist, and other case is etching the coupon wafers on the chuck. For comparing the emission intensity, we chose the four chemical species (SiF2, N2, CO, CN), and for comparing the etched profile, measured by scanning electron microscope (SEM). In addition, we adopted the Dynamic Time Warping (DTW) algorithm for analyzing the chose OES data patterns, and analysis the covariance and coefficient for statistical method. After the result, coupon wafers are over-etched for without carrier wafer groups, while with carrier wafer groups are under-etched. And the CN emission intensity has significant difference compare with OES raw data. Based on these results, it necessary to reasonable analysis of the OES data to adopt the pre-data processing and algorithms, and the result will influence the reliability for relation of coupon wafer test and whole wafer test.

  • PDF

A Study on the Fabrication of the Solar Cells using the Recycled Silicon Wafers (Recycled Si Wafer를 이용한 태양전지의 제작과 특성 연구)

  • Choi, Song-Ho;Jeong, Kwang-Jin;Koo, Kyoung-Wan;Cho, Tong-Yul;Chun, Hui-Gon
    • Journal of Sensor Science and Technology
    • /
    • v.9 no.1
    • /
    • pp.70-75
    • /
    • 2000
  • The recycled single crystal silicon wafers have been fabricated into solar cells. It can be a solution for the high cost in materials for solar cells and recycling of materials. So, p-type (100) single crystal silicon wafers with high resistivity of $10-14\;{\Omega}cm$ and the thickness of $650\;{\mu}m$ were used for the fabrication of solar cells. Optimistic conditions of formation of back surface field, surface texturing and anti-reflection coating were studied for getting high efficiency. In addition, thickness variation of solar cell was also studied for increase of efficiency. As a result, the solar cell with efficiency of 10% with a curve fill factor of 0.53 was fabricated with the wafers which have the area of $4\;cm^2$ and thickness of $300\;{\mu}m$. According to above results, recycling possibility of wasted wafers to single crystal silicon solar cells was confirmed.

  • PDF

FRICTION AND WEAR PROPERTIES OF MICRO TEXTURED SURFACES IN BOUNDARY LUBRICATED SLIDING

  • Pettersson, U.;Jacobson, S.
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.10b
    • /
    • pp.207-208
    • /
    • 2002
  • In the present study, the friction and wear properties of boundary lubricated textured surfaces were investigated. The capability of textured surfaces to feed lubricant into the interface of a sliding contact and to isolate wear partices was studied and related to the properties of the textured surfaces. Well-defined surface textures were produced by lithography and anisotropic etching of silicon wafers. Different widths and distributions of parallel groves were manufactured and subsequently the wafers were PVD coated with thin wear resistant TiN or DLC coatings, retaining the substrate texture. The surfaces were evaluated in reciprocating sliding against a ball bearing steel ball under starved or boundary lubricated conditions.