• 제목/요약/키워드: very early strength

검색결과 188건 처리시간 0.022초

터널의 품질관리를 위한 숏크리트 초기강도의 현장강도 시험기술 (Field Testing Methods on Early Shotcrete Strength for Tunnel Quality Control)

  • 홍의준;장석부;이성우;김기림;문상조
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2007년도 춘계학술대회 논문집
    • /
    • pp.468-476
    • /
    • 2007
  • Generally, the strength of the field shotcrete is heavily dependent on the field mixing and spraying conditions so that it is different from the strength of the shotcrete mixed in laboratories. As a support member, the early strength of shotcrete unlike concrete as structural material is very important to the initial stabilization of the excavation face in tunnels. Therefore, the field methods to efficiently test the early strength of shotcrete have been highly required. This paper aimed to verify the pneumatic pin penetration test and the point load test for measuring the early strength of the field shotcrete. Through a series of uniaxial compression, pin penetration, and point load tests for the range of the early shotcrete strength, two equations to estimate reliably the uniaxial compressive strength by the pin penetration and the point load tests were derived. Field tests in working tunnel were carried out in order to estimate the economic efficiency. As a result, pin penetration method was proved to be the most effective method for testing the early strength of the field shotcrete.

  • PDF

칼슐설포알루미네이트를 사용한 모르타르의 초기강도 특성에 관한 연구 (A Study on the Early-Age Strength of Mortar Using Calcium Sulfo Aluminate)

  • 송태협;이세현;서치호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.397-400
    • /
    • 2005
  • This study is a result that, in order to improve the early stage strength of fly ash, the calciumsulfoaluminate in which the generation of ettringite was very active in the early stage was substituted by some amount, and then the effect on the early stage was analyzed. when fly ash was substituted by 30$\%$, the strength dropped by maximum 54 $\%$ in the 3rd day of aging, compared to the cement mixture, but when CSA was substituted by 8 $\%$ in the fly ash amount, the strength improved at the 86 percent level of cement, it is suggested as an economical and effective method to improve the early-stage strength that CSA should be mixed by 8$\%$ compared to the fly ash amount used

  • PDF

현장실험을 통한 VES-LMC 균열발생 원인분석 (Diagnosis of Crack Occurrence of Very-Early Strength Latex-Modified Concretes through Field Tests)

  • 최판길;이봉학
    • 산업기술연구
    • /
    • 제26권A호
    • /
    • pp.139-146
    • /
    • 2006
  • Many concrete bridge decks develop transverse cracking shortly after construction. These cracks accelerate corrosion of reinforcing steel and lead to concrete deterioration, damage to components beneath the deck, unsightly appearance. These cracks shorten the service life and increase maintenance costs of bridge structures. In this study, VES-LMC overlay, which provides the same benefits as a conventional overlay, is designed to cure very quickly. Although the materials for VES overlays are more expensive, the cost is more than offset by the savings on traffic control and work zone safety measures. Otherwise, reaction of hydration occurs very rapidly in beginning step(concrete placing). As a results, thermal cracking can be occur by thermal stress in accordance with hydration-heat The purpose of this study was to estimate diagnosis of crack occurrence of VES-LMC through field tests at early-age.

  • PDF

초속경라텍스개질콘크리트의 초기수축 (Early-Age Shrinkage of Very-Early Strength Latex Modified Concrete)

  • 이정호;최판길;최승식;윤경구
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.269-272
    • /
    • 2004
  • After concrete casts, temperature decent and shrinkage bring volume changes of concrete pavement. Microcracking and cracking in concrete pavement are caused by these volume changes. As a result, durability of concrete pavement is deteriorated. Recently, Very-Early Strength Latex Modified concrete(below:VESLMC) from the beginning of High-Way is used as urgent repair material for bridge deck. The advantage of VESLMC is that compressive and flexural strength at 3 hours age are 4.5MPa and 21MPa respectively. It allows the traffic to open in 3 hours. But, this material has the problem which is early-age shrinkage cracking caused by water self-dissipation with rapid hydration reaction and water evaporation with body dry. Unfortunately, until now, the research about early-age shrinkage of VESLMC leaves something to be desired. Therefore, the purpose of this study is to present the early-age shrinkage of VESLMC respect to latex contents and shrinkage ratio to maximum length change that can help field engineers' skill. Latex contents of 0, 5, 10, 15, $20\%$ in standard of same workability in VESLMC are selected by experimental variables. After initial set, shrinkage value was measured with 10mm LVDT for 3 days. The results of maximum shrinkage ratio were 0.019, 0.017, 0.023, $0.027\%$ respectively.

  • PDF

촉진형 AE감수제를 사용한 콘크리트의 최적공기산정을 위한 조기강도 발현 특성 연구 (A Study on Early-strength Development of Concrete Using Accelerating AE Water Reducing Agents for the Estimation of Optimum Duration)

  • 이주헌;사순헌;지석원;전현규;서치호
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 추계 학술논문 발표대회 논문집
    • /
    • pp.91-94
    • /
    • 2006
  • The way to shorten a construction period is considered to an very important technology development element as reducing the formwork removal periods with promoting strength revelation own concrete. This study executed experiment to review usability of early strength revelation chemical admixture which is judged in ways effective with premature removal of form about concrete. Use of early strength revelation AE water reducin admixture is apperaing so that strength revelation by early hydration promotions is excellent. The results of being applied proposed work process are that compressive strength are appeared more than 5MPa within 16 hours so that removal of vertical form was possible. the concrete compressive strength satisfied with a more than 2/3 of specified concrete strength for removal of horizontal form are appeared in 42 hours of 27 MPa proportioning strength, in 36 hours of 30, 35 MPa proportioning strength so that the 6 days cycle time of concrete structural frame work is cut by 2 days as shortening delayed period in works of removing slab forms. So construction cost reductions and a construction period shortening are judged so that it is possible.

  • PDF

초기재령 콘크리트의 부등건조수축과 자기수축에 관한 연구 (Differential Drying Shrinkage and Autogenous Shrinkage of Concrete at Early Ages)

  • 김진근;이칠성
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회 논문집(I)
    • /
    • pp.309-314
    • /
    • 1998
  • The moisture diffusion and self-desiccation cause the differential drying shrinkage and autogenous shrinkage at early ages, respecitvely. Thus total shrinkage strain includes the differential drying shrinkage and self-desiccation shrinkage. Thus in this study the shrinkage strain was measured at various positions in the exposed concrete and in the sealed concrete the self-desiccation shrinkage was measured. In low-strength concrete, the differential drying shrinkage increases very rapidly, but self-desiccation shrinkage is very small. But high-strength concrete shows the reverse result. And the analytical results for differential drying shrinkage were in good agreement with the test results.

  • PDF

슬립폼 적용을 위한 고강도콘크리트의 조기강도 발현성상에 관한 실험적 연구 (An Experimental Study on Early Strength Development of High-Strength Concrete to Apply Slip-Form)

  • 주지현;여동구;강석표;길배수;남재현;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.355-358
    • /
    • 2000
  • Nowadays, with high-storied and large-sized of structures, high-strength concrete is applied to the various kinds of concrete structure. Among of them, for reduction of completion time, high-strength concrete is applied to the high-storied tower, building which is constructed continuously by the slip-form method and it is expected to be on the increase. In this case, it is very important to grasp development of early-strength to apply the slip-form method. But the strength data prior 1 day is rare. Therefore, to apply slip-form method in field, this study aim is to present basic data for development of early-strength of high-strength concrete, through examining development of strength by different curing temperature, replacement of fly-ash.

  • PDF

마이크로파에 의한 모르터의 조기강조 추정기법에 관한 실험적 연구 (An Experimental Study on the Estimation Technique of Mortar Early Strength by Microwave)

  • 원준연;백민수;이종균;안형준;정상진
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.15-218
    • /
    • 1999
  • Concrete is the most generous, universal main structural material. There is active study for processing quality, stable quality mangement. Especially, strength is basic factor of evaluating stability of concrete building. Regaining required strength and homogeneity is very important to get self-stability in building to evaluate another characteristic. Concrete strength is important to the quality management. But, result of hardened concrete's quality test is hardly reflected to works immediately. When required strength is not enough, it could bring out safe problem, economic and administrative cost. It is pointed out that problems from strength evaluation, so early evaluation of concrete quality is required. From the trend that accelerating high quality concrete development, improving the method of quality test and early evaluation measure is urgent project. Throughout this report, it is suggested the method with use of microwave to evaluate 28-days concrete strength.

  • PDF

초기수화발열이 고강도콘크리트의 자기수축특성에 미치는 영향 (Effect of Hydration Heat Evolution on Autogenous Shrinkage of High Strength Concrete)

  • 정해문;도변박지;하야도륭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.95-100
    • /
    • 2003
  • The shrinkage of high strength/high performance concrete is very important property for the good working of a structure since it very often generates early age cracking due to thermal and autogenous shrinkage. Autogenous shrinkage occurs as a result of internal moisture depletion due to hydration and temperature-induced effects. The level of autogenous shrinkage occurring due to hydration also depends on temperature history at very early age. It is necessary that effect of temperature on autogenous shrinkage is investigated since the stress generated due to autogenous shrinkage is quantified. In this study, Effect of hydration heat evolution on autogenous shrinkage of high strength concretes with W/C=25-40% was investigated.

  • PDF

콘크리트 조기강도 발현방법에 관한 연구 (A Study on Development Method for Early-Strength Concrete)

  • 류종현;전현규
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.681-684
    • /
    • 2008
  • The way to shorten a construction period is considered to an very important technology element as reducing the form work removal periods with promoting strength revelation own concrete. This study presents an experimental study on the development method, material for early strength concrete. The result is as follow : In OPC, the compressive strength has over 5MPa after 26hours at 20$^{\circ}C$ curing and another 36hours at 10$^{\circ}C$ curing. Used with early strength potland cement, the compressive strength has over 5MPa after 15hours at 20$^{\circ}C$ curing temperature and another 30hours at 10$^{\circ}C$ curing temperature.

  • PDF