An Experimental Study on Quality Management of Strength in High Strength Mass Concrete Structure Using Thermal Insulation Material (보온재를 사용한 고강도 매스 콘크리트의 품질관리에 관한 연구)

  • Cho, Kyu-Hyun;Back, Min-Soo;Kim, Sung-Sik;Lim, Nam-Gi;Lee, Young-Do
    • Journal of the Korea Institute of Building Construction
    • /
    • v.4 no.2
    • /
    • pp.113-118
    • /
    • 2004
  • This study is a basic experiment on quality management of the compression strength of high strength concrete, aiming. at quality management of high strength mass concrete by giving the temperature hysteresis of the mass test pieces to managerial test pieces. Different from ordinary concrete, high strength concrete generally shows the temperature high rising caused by hydration heat inside the concrete. It is known that, in mass concrete, thermal stress occurs due to the difference in temperature between the inside and the outside, which causes a significant difference in compression strength between structure beams and managerial test pieces. It is also reported that there is a large difference between the compression strength of cylindrical managerial test pieces of standard underwater curing and the strength of structure beam concrete. Thus, this study made concrete test pieces in an optimal mix ratio for each strength level, and also created thermal insulation curing box and managerial test pieces. Then it carried out comparative analysis in relation to core strength and suggested equipment and a technique that can control the strength of high strength concrete mass more conveniently and accurately.

Repair of Highway Bridge damaged by Chloride Attack in Marine Environment(2) - Application of Cathodic Protection (해양에 위치한 고속도로교량에 대한 내염보수 공법(2)-전기방식시공결과)

  • Chi, Han-Sang;Han, Bog-Kyu;Cheong, Hai-Moon;Ahn, Tae-Song;Ryu, Jong-Hyun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.786-789
    • /
    • 2004
  • Corrosion of reinforced concrete structures in marine environment is one of the most important mechanism of deterioration. However, conventional rehabilitation techniques in tidal zone, which consist of removing delaminated areas of concrete, cleaning affected steel and patching with portland cements mortar, have proven to be ineffective for marine structures. Also, repairs are often repeated every several years. The purpose of this report is to announce appropriate repair method of highway bridge damaged by chloride attack in marine environment (application of cathodic protection) using FRP and antiwashout underwater mortar.

  • PDF

A Study on the Flexural Behavior of Proposed Spliced PSC-I Type Girder (제안된 Spliced PSC-I형 거더의 휨거동에 관한 연구)

  • 심종성;오홍섭
    • Journal of the Korea Concrete Institute
    • /
    • v.12 no.5
    • /
    • pp.13-23
    • /
    • 2000
  • In this study, an flexural test on half-scale spliced PSC-I girder was conducted to verify the efficiency of the long span spliced girder as suggested by the Korean Highway Design Specification. The experimental results showed that the specimens developed a complex failure mode due to flexural-compression and torsional stress. The cracking moment of each girder was higher the experiment than was calulated by the ACI and the ultimate strength were the almost same. To estimate the safety and the structural efficiency of the spliced girder, the proposed Yielding Resistance Index(YRI) and ductility index by American Concrete Institutes were used based on the energy concept. The proposed YRI defined the ratio of crack resisting energy and the total energy calculated from load-displacement relationship. Based on the analysis of YRI and ductility index, the flexural behavior of the spliced girder was found to be efficient. Through the experimental results, the structural behavior of proposed spliced PSC I-type girder for long span bridge was found to be more efficient than the exsisting PSC I-type girders.

An Experimental Study on the Compressive Strength of Cement Mortar mixing Anion Exchange Resin (음이온교환수지 혼입 시멘트 모르타르의 압축강도에 관한 실험적 연구)

  • Jeong, Do-Hyun;Lee, Yun-Su;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2018.05a
    • /
    • pp.54-55
    • /
    • 2018
  • Reinforced concrete is a building material that is generally used in modern society. Securing the performance of reinforced concrete is directly connected to the durability and longevity of the building. One of the major factors that deteriorate the durability of concrete is harmful ion. Recently, the quality and improvement method of reinforced concrete for penetration of harmful ion has been studied. In this study, the bead type ion exchange resin is substituted for 0%, 3%, and 6% of the fine aggregate volume in the mortar. The speciments underwent underwater curing and were checked for compressive strengths of 3 days and 28 days. From the results of compressive strength, it can be seen that the higher the substitution ratio of the ion exchange resin, the lower the early strength and long-term strength development, especially the early strength development.

  • PDF

An Experimental Study about Behavior of a Repaired Underwater Structure with an Epoxy Fiber Panel and Polymer Mortar (에폭시 섬유판넬과 폴리머 모르타르로 단면보수된 수중구조물의 거동에 관한 실험적 연구)

  • Hong, Sung-Nam;Park, Jun-Myoung;You, Chung-Jun;Han, Kyoung-Bong;Park, Sun-Kyu
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.13 no.1 s.53
    • /
    • pp.69-77
    • /
    • 2009
  • An underwater structure is made to put with serious damage state by special environmental factors. If this damage phenomena persist, as for the structure, it is generated a structural serious problem because of the corrosion of a reinforcing bar and the loss of the concrete cut end. Repair work of an underwater structure is very harder than repair work in land, and it is actual that certification about a maintenance effect is uncertain. And the existing repair method is applied to a structure damaged with you without verification of a repair effect by a foreign reward and experience. In this study, a repair method about an underwater structure was proposed and observed a behavior characteristic and interface failure of an specimens. and comparison analyzed an effect of a proposed maintenance method.

Mechanical Properties of Permeable Polymer Concrete for Permeability Pavement with Recycled Aggregate and Fiber Volume Fraction (재생골재 및 섬유 혼입률에 따른 포장용 투수성 폴리머 콘크리트의 역학적 특성)

  • Sung, Chan-Yong;Kim, Young-Ik
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.52 no.1
    • /
    • pp.69-77
    • /
    • 2010
  • Research on permeable pavement like asphalt and concrete pavement with porous structure has been increasing due to environmental and functional need such as reduction of run off and flood, and increase and purification of underwater resource. This study was performed to evaluate permeability, strengths and durability of permeable polymer concrete (PPC) using recycled aggregate that is obtained from waste concrete. Also, 6mm length of polypropylene fiber was used to increase toughness and interlocking between aggregate and aggregate surrounded by binder. In the test results, regardless of kinds of aggregates and fiber contents, the compressive strength and permeability coefficient of all types of PPC showed the higher than the criterion of porous concrete that is used in permeable pavement in Korea. Also, strengths of PPC with increase polypropylene fiber volume fraction showed slightly increased tendency due to increase binder with increase of fiber volume fraction. The weight reduction ratios for PPC after 300 cycles of freezing and thawing were in the range of 1.6~3.8 % and 2.2~5.6 %, respectively. The weight change ratio was very low regardless of the fiber volume fraction and aggregates. The weight reduction ratios of PPC with fiber and aggregate were in the range of 1.3~2.7 % and 2.2~3.2 % after 13 weeks and was very low regardless of the fiber volume fraction and aggregates.

The Properties of Underwater-Hardening Epoxy Mortar Used the Rapidly Cooled Steel Slag (RCSS) (급냉 제강슬래그를 사용한 수중 경화형 에폭시 모르타르의 특성)

  • Kim, Jin-Man;Kwak, Eun-Gu;Bae, Kee-Sun
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.5
    • /
    • pp.549-555
    • /
    • 2007
  • Although blast furnace slag has been widely used in concrete as a cementitious admixture or aggregate for many years, the slowly cooled steel slag is not used in concrete but mainly in road. Its use in concrete operates problem such as the lack of volume stability due to high free CaO content, which can be potentially hazardous in concrete. However, the rapidly cooled steel slag by atomization has a low free CaO content, a high density, and a spherical shape, so it is expected to use in concrete so much. This paper is to understand the probability that the rapid cooled steel slag can replace the silica sand used as aggregate in the epoxy mortar. We did the experimental study on the properties of the epoxy mortar having various replacement proportion of rapidly cooled steel slag. This study shown that increasing content of the rapidly cooled steel slag in epoxy mortar lead to increase largely the passing time of nozzle by O-lot, compressive strength and flexural strength. However except the flow is almost same level. So we understand that the rapidly cooled steel slag has positive effect on increasing of properties in epoxy mortar.

Experimental Study on Evaluation of Abrasion Resistance of Concrete Irrigation Facilities (콘크리트 수리구조물의 수중마모저항성 평가기술에 관한 실험적 연구)

  • Kim, Meyongwon
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.60 no.3
    • /
    • pp.123-133
    • /
    • 2018
  • The purpose of this paper is to propose an experimental method to evaluate the resistance of abrasion about 24 MPa, 27 MPa, and 30 MPa compressive strength. These strength are used in the design and construction of concrete hydraulic structures in Korea. The mixing ratios of the ready mixed concrete strengths were investigated countrywide and set the representative mixture proportion ratios of the nine mixed types of OPC, FA and BFS. After making and curing the test specimens, the underwater abrasion test was performed. ASTM C 1138 International Standard was used to fabricate the test equipment, and the surface abrasion resistance of the specimen was tested using the test equipment. In the case of OPC, the 30% abrasion resistance improvement effect was observed at 72 hours as the water-binder ratio decreased. That was reason the coated cement bond strength of the specimen was strong. In the case of BFS and FA, it was improved by 9.9% and 3.8%, respectively, at 72 hours as the water-binder ratio decreased. It was due to the characteristics of the latent hydraulic and pozzolanic reactions. Generally, the relative abrasion resistance of concrete can be evaluated at 24 hours. However, in case of low strength (under 24 MPa), the surface mortar layer wears much faster at the first 12 hours, so it can be considered to evaluate the relative abrasion loss rate at this point.

Study on the Long age Strength Properties of Antiwashout Underwater Concrete (수중불분리성 콘크리트의 장기강도 특성에 관한 연구)

  • 박세인;이동화;김종수;김명수
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.04a
    • /
    • pp.113-117
    • /
    • 2000
  • The objective of this study is to find the long-age strength property and the compressive strength of age which is used as the specified concrete strength. The W/W ratio (45%, 50%, 55%, 60%) fine aggregate of useful river sand or blended sand(river sane : sea sand=1:1) were chosen as the experimental parameters. the experimental results show that pH(it means the material segregation resistance) & suspension were increased larger, so W/C become larger, and slump flow was increased as W/C increased (except W/C=60%), air-contents were decreased as W/C became increase and all of this results are satisfied with the under of 40%. The compressive strength ( a case use only river sand as fine aggregate) is showed less than the case of blended asnd. Because the unit weight of the blended sand is more heavy than the unit weigh of the river sand. The results of the case which haven been used only river sand, and the case have been used blended sand), both case have considered W/C. So it's possible to use the compressive strength of age 28 day like the case of plain concrete.

  • PDF

Mix Design of Polymer Grouting Mortar for Prepacked Concrete Using Polymer Dispersions (폴리머 디스퍼션을 이용한 프리팩트 콘크리트용 주입 모르타르의 배합에 관한 연구)

  • Jo, Young-Kug;Kim, Wan-Ki
    • Journal of the Korea Institute of Building Construction
    • /
    • v.8 no.5
    • /
    • pp.85-91
    • /
    • 2008
  • Prepacked concrete has recently been used in the special constructions fields such as underwater concrete work, heavy-weight concrete work, underground structure work, partial repair works for damaged reinforced concrete structures. and polymer-modified mortars have been employed as grouting mortars for the prepacked concrete. The purpose of this study is to recommend the optimum mix design of polymer-modified grouting mortars for prepacked concrete. Polymer-modified mortars using SBR and EVA emulsions as admixture of grouting mortars for prepacked concrete are prepared with various mix proportions such as sand-binder ratio, fly ash replacement ratio, polymer-binder ratio. and tested for flowability, viscosity of grouting mortars, bleeding ratio, expansion ratio, flexural and compressive strengths of grouting mortars and compressive and tensile strengths of prepacked concretes. From the test results, it is apparent that polymer-modified mortars can be produced as grouting mortars when proper mix design is chosen. We can design the mix proportions of high strength mortars for prepacked concrete according to the control of mix design factors such as type of polymer, polymer-binder ratio, sand-binder ratio and fly ash replacement ratio. Water-binder ratio of plain mortars for a constant flowability value are in the ranges of 43% to 50%. SBR-modified mortar has a little water-binder ratios compared to those of plain mortar, however, EVA-modified mortar needs a high water-binder ratio due to a high viscosity of polymer dispersion. The expansion and bleeding ratios of grouting mortars are also controlled in the proper value ranges. Polymer-modified grouting mortars have good flexural. compressive and tensile strengths, are not affected with various properties with increasing fly ash replacement to cement and binder-sand ratio. In this study, SBR-modified grouting mortar with a polymer-binder ratio of 10% or less, a fly ash replacement of 10% to cement and a sand-binder ratio of 1.5 is recommended as a grouting mortar for prepacked concrete.