• 제목/요약/키워드: toughness

검색결과 2,679건 처리시간 0.027초

Al 7175 합금의 정적 파괴인성에 미치는 노치반경 영향 (Notch Radius Effect for Static Fracture Toughness of Al 7175 Alloys)

  • 김재훈;김덕회;박성욱;문순일
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2002년도 제18회 학술발표대회 논문초록집
    • /
    • pp.84-87
    • /
    • 2002
  • In this study, intrinsic fracture toughness of Al 7175-T74 is evaluated from the apparent toughness of notched specimen. Modified average stress model is used to establish the relationship to predict the intrinsic fracture toughness from the apparent fracture toughness of a notched-cracked specimen. The modified average stress model is established the relation between notch radius and effective distance calculated by FEM analysis. The results show that fracture toughness decreases with decreasing of notch root radius. The true fracture toughness can be predicted from test results of apparent fracture toughness measured by using notched specimen.

  • PDF

고속철도용 윤축의 정${\cdot}$동적파괴인성 평가 (Static and Dynamic Fracture Toughness of Wheelset for High Speed Train)

  • 권석진
    • 한국철도학회논문집
    • /
    • 제8권3호
    • /
    • pp.210-215
    • /
    • 2005
  • The safety evaluations of railway wheelsets make use of the static fracture toughness obtained in ingot materials. The static fracture toughness of wheelset materials has been extensively studied by experiments, but the dynamic fracture toughness with respect to wheelset materials has not been studied enough yet. It is necessary to evaluate the characteristics of the fracture mechanics depending on each location for a full-scale wheelset for high-speed trains, because the load state for each location of the wheelset while running is different the contact load between the wheel and rail, cyclic stress in the wheel plate, etc. This paper deals with the fracture toughness depend on load rates. The fracture toughness depending on load rate data shows that once the downward curve from quasi-static values was reached, subsequent values showed a slow increase with respect to the impact velocity. This means that dynamic fracture toughness should be considered in the design code of the wheelset material.

에너지 방출률에 의한 접착이음의 계면균열에 대한 파괴인성의 평가 (Evaluation of Fracture Toughness by Energy Release Rate for Interface Crack in Adhesively Bonded Joints)

  • 정남용;이명대;강삼근
    • 대한기계학회논문집A
    • /
    • 제24권9호
    • /
    • pp.2174-2183
    • /
    • 2000
  • In this paper, the evaluation method of interfacial fracture toughness to apply the fracture toughness was investigated in adhesively bonded joints of AI/Ced./A1. Four types of adhesively bonded double-cantilever beam(DCB) joints with the interface crack were prepared for the test of interfacial fracture toughness. The experiments to measure the interfacial fracture toughness were performed under the various mixed-mode conditions. The critical energy release rate, Gc, was obtained by the experimental measurement of compliances. From the experimental results, the interfacial fracture toughness for the mixed-mode specimens is well characterized by the energy release rate, and the method of strength evaluation by the interfacial fracture toughness was discussed in adhesively bonded joints.

항복강도 390 MPa급 가공열처리강 대입열용접 열영향부 충격인성 및 연화현상 (Impact Toughness and Softening of the Heat Affected Zone of High Heat Input Welded 390 MPa Yield Strength Grade TMCP Steel)

  • 방국수;안영호;정홍철
    • 대한금속재료학회지
    • /
    • 제56권11호
    • /
    • pp.796-804
    • /
    • 2018
  • The Charpy impact toughness of the heat affected zone (HAZ) of electro gas welded 390 MPa yield strength grade steel, manufactured by a thermo mechanically controlled process, was investigated. The effects of added Nb on the toughness of the steel and the factors influencing scatter in toughness are discussed in the present work. It was observed that adding Nb to the steel led to the deterioration of HAZ toughness. The presence of soluble Nb in the HAZ increased its hardenability and resulted in a larger amount of low toughness bainitic microstructure. Microstructural observations in the notch root area revealed the significant role of different microstructures in the area. In the presence of a larger amount of bainitic microstructures, the HAZ exhibited a lower Charpy toughness with a larger scatter in toughness. A softened zone with a lower hardness than the base metal was formed in the HAZ. However, theoretical analysis revealed that the presence of the zone might not be a problem in a real welded joint because of the plastic restraint effect enforced by surrounding materials.

FRACTURE TOUGHNESS OF VARIOUS CORE MATERIALS

  • Lee Shin-Won;Lee Sun-Hyung;Yang Jae-Ho;Han Jung-Suk;Lee Jai-Bong
    • 대한치과보철학회지
    • /
    • 제39권6호
    • /
    • pp.682-697
    • /
    • 2001
  • This investigation evaluated the fracture toughness($K_{IC}$) of eight currently available core materials, and relate the fracture toughness value to fractography analysis and surface characteristics using a atomic force microscope (AFM). Single-edge notched (SEN) test specimens (n=10) and compact tension (CT) test specimens (n=10) were prepared conforming to the ASTM Standard E-399 for a high copper amalgam, three composite core materials (Core-Max II, Core Paste, Bisfil Core), two reinforced composite core materials (Ti-Core, Ti-Core Natural), a resin-modified glass ionomer core material (Vitremer), and a conventional glass ionomer core material (Ketac-Molar). The specimens were tested with an Instron Universal Testing Machine. The maximum loads were measured to calculate the fracture toughness ($K_{IC}$). Thereafter, fracture surfaces of SEN specimens of each material were investigated for fractography analysis using scanning electron microscope. And, disc-shaped specimens with 1mm thickness were fabricated for each material and were investigated under AFM for surface morphology analysis. The results were as follows: 1. Bisfil Core showed the highest mean fracture toughness regardless of test methods. 2. For the tooth-colored materials, Ti-Core Natural exhibited the highest fracture toughness. 3. Ketac Molar showed a significantly low fracture toughness when compared with the amalgam and the composite resin core materials(p<0.05). 4. The fracture toughness values obtained with the single-edge notched test, except Ketac Molar, were higher than those obtained in the compact tension test. 5. SEM revealed that the fracture surface of high fracture toughness material was rougher than that of low fracture toughness material. 6. AFM revealed that the surface particles of the composite resins were smaller in size, with a lower surface roughness than the glass ionomer core materials.

  • PDF

Ni-Mo-Cr계 저합금강의 천이온도영역에서의 파괴인성에 미치는 Ni 및 Cr 함량의 영향 (Effects of Ni and Cr Contents on the Fracture Toughness of Ni-Mo-Cr Low Alloy Steels in the Transition Temperature Region)

  • 이기형;박상규;김민철;이봉상;위당문
    • 대한금속재료학회지
    • /
    • 제47권9호
    • /
    • pp.533-541
    • /
    • 2009
  • Materials used for a reactor pressure vessel(RPV) are required high strength and toughness, which determine the safety margin and life of a reactor. Ni-Mo-Cr low alloy steel shows better mechanical properties than existing RPV steels due to higher Ni and Cr contents compared to the existing RPV steels. The present study focuses on effects of Ni, Cr contents on the cleavage fracture toughness of Ni-Mo-Cr low alloy steels in the transition temperature region. The fracture toughness was characterized by a 3-point bend test of precracked Charpy V-notch(PCVN) specimens based on ASTM E1921-08. The test results indicated that the fracture toughness was considerably improved with an increase of Ni and Cr contents. Especially, control of Cr content was more effective in improving fracture toughness than manipulating Ni content, though Charpy impact toughness was changed more extensively by adjusting Ni content. These differences between changes in the fracture toughness and that in the impact toughness were derived from microstructural features, such as martensite lath size and carbide precipitation behavior.

입열량에 따른 FCAW용접부 파괴인성에 미치는 미세조직의 영향 (Evaluation of Fracture Toughness and Microstructure on FCA Weldment According to Heat Input)

  • 신용택;강성원;김명현
    • Journal of Welding and Joining
    • /
    • 제26권3호
    • /
    • pp.51-60
    • /
    • 2008
  • This paper is to evaluate fracture characteristics of API 2W Gr.50 TMCP steel weldment typically applied for offshore structures, with the focus on the influence of heat input arising from flux cored arc welding. Based on the results and insights developed from this study, it is found that the toughness for both CTOD and impact exhibits a tendency to decrease as the weld heat input increases. The reheated zone of weldmetal exhibit lower hardness than solidified zone and microstructure that are liable to affect the toughness are acicular ferrite and martensite-austenite constituents (M-A). In particular, M-A is a more effective micro-phase for CTOD toughness than impact toughness.

Determination of fracture toughness in concretes containing siliceous fly ash during mode III loading

  • Golewski, Grzegorz Ludwik
    • Structural Engineering and Mechanics
    • /
    • 제62권1호
    • /
    • pp.1-9
    • /
    • 2017
  • This paper describes laboratory tests carried out to evaluate the influence of class F fly ash (FA) on fracture toughness of plain concretes, specified at the third model fracture. Composites with the additives of: 0%, 20% and 30% siliceous FA were analysed. Fracture toughness tests were performed on axial torsional machine MTS 809 Axial/Torsional Test System, using the cylindrical specimens with dimensions of 150/300 mm, having an initial circumferential notch made in the half-height of cylinders. The studies examined effect of FA additive on the critical stress intensity factor $K_{IIIc}$. In order to determine the fracture toughness $K_{IIIc}$ a special device was manufactured.The analysis of the results revealed that a 20% FA additive causes increase in $K_{IIIc}$, while a 30% FA additive causes decrease in fracture toughness. Furthermore, it was observed that the results obtained during fracture toughness tests are convergent with the values of the compression strength tests.

고인성 비조질강 샤시부품 개발 (Development of Chassis Parts Using High Toughness Micro-alloyed Steel)

  • 이시엽;김혁
    • 한국자동차공학회논문집
    • /
    • 제20권3호
    • /
    • pp.1-6
    • /
    • 2012
  • This paper developed the chassis part as micro-alloyed steel with high toughness. The performance of micro-alloy steels are superior to similar heat treated steels. The strengthening effects of vanadium make micro-alloyed steels particularly suited for high-strength-steel applications. The disadvantages are that ductility and toughness are not as good as quenched and tempered (Q&T) steels. Precipitation hardening increases strength but may contribute to brittleness. Toughness can be improved by reducing carbon content and titanium additions. dispersed titanium nitrides (TiN) formed by titanium additions effectively prevents grain coarsening. Grain refinement increases strength but also improves toughness. For the chassis parts using high toughness micro-alloy steel, it had proven superior to a plain steel forging by static strength test and endurance test.

하중속도가 탄소섬유/에폭시 적층복합재의 층간분리인성에 미치는 영향 (Loading rate effect on the delamination toughness of carbon/epoxy composites)

  • 하성록;이경엽;김현주;정동호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.593-597
    • /
    • 2005
  • It is generally accepted that fracture toughness of fiber-reinforced polymer composites is affected by loading rate in an atmospheric presure condition. For a present study, the loading rate effect on the fracture toughness of fiber-reinforced laminated composites in the hydrostatic pressure condition was investigated. For this purpose, fracture tests have been conducted using carbon/epoxy composites applying three steps of the strain rate at 270 MPa hydrostatic pressure condition. The loading rates applied were 0.05%/sec, 0.25%/sec, and 0.55%/sec. Fracture toughness was determined from the work factor approach as a function of applied loading rate. The result showed that fracture toughness decreased as the loading rate increased. Specifically, the fracture toughness decreased 12% as the loading rate increased from 0.05%/sec to 0.55%/sec.

  • PDF