• 제목/요약/키워드: thermal vacuum evaporation

검색결과 168건 처리시간 0.034초

석영 기판 위에 집속 이온빔 기술에 의해 형성된 비정질 게르마늄 박막 미세 패턴의 편광 및 복굴절 특성 (Characteristics of Polarization and Birefringence for Submicron a-Ge Thin Film on Quartz Substrate Formed by Focused-Ion-Beam)

  • 신경;김진우;박정일;이현용;정홍배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.617-620
    • /
    • 1999
  • In this study, the polarization e(fecal and the birefringence effect of amorphous germanium (a-Ge) thin films were investigated by using linearly polarized He-Ne laser beam. The a-7e thin films were deposited on the quarts substrate by plasma enhanced chemical vapor deposition (PECVD) and thermal vacuum evaporation In order to obtain the optimum grating arrays, inorganci resists such as Si$_3$N$_4$ and a-Se$_{75}$ Ge$_{25}$ , were prepared with the optimized thickness by Monte Carlo (MC) simulation. As the results of MC simulation, the thickness ofa-Se$_{75}$ Ge$_{25}$ resist was determined with Z$_{min}$ of 360$\AA$ . The resists were exposed to Ga$^{+}$-FIB with accelerating energies of 50 keV, developed by wet etching, and a-Ge thin film was etched by reactive ion-etching (RIE). Finally, we were obtained grating arrays which grating width and linewidth are 0.8${\mu}{\textrm}{m}$, respectively and we studied the polarization and birefringence effect in transmission grating array made of high refractive amorphous material, and the applicability as waveplates and polarizers in optical device.e.e.

  • PDF

An Organic Electrophosphorescent Device Driven by All-Organic Thin-Film Transistor using Polymeric Gate Insulator

  • Pyo, S.W.;Shim, J.H.;Kim, Y.K.
    • Journal of Information Display
    • /
    • 제4권2호
    • /
    • pp.1-6
    • /
    • 2003
  • In this paper, we demonstrate that the organic electrophosphorescent device is driven by the organic thin film transistor with spin-coated photoacryl gate insulator. It was found that electrical output characteristics in our organic thin film transistors using the staggered-inverted top-contact structure showed the non-saturated slope in the saturation region and the sub-threshold nonlinearity in the triode region, where we obtained the maximum power luminance that was about 90 $cd/m^2$. Field effect mobility, threshold voltage, and on-off current ratio in 0.45 ${\mu}m$ thick gate dielectric layer were 0.17 $cm^2/Vs$, -7 V, and $10^6$ , respectively. In order to form polyimide as a gate insulator, vapor deposition polymerization process was also introduced instead of spin-coating process, where polyimide film was co-deposited by high-vacuum thermal evaporation from 4,4'-oxydiphthalic anhydride (ODPA) and 4,4'-oxydianiline (ODA) and cured at 150${\sqsubset}$for 1hr. It was also found that field effect mobility, threshold voltage, on-off current ratio, and sub-threshold slope with 0.45 ${\mu}m$ thick gate dielectric films were 0.134 $cm^2/Vs$, -7 V, and $10^6$ A/A, and 1 V/decade, respectively.

상보형 전기변색소자용 $V_2O_5$박막의 대향전극 특성 (Characterization of $V_2O_5$ thin films as a counter electrode for complementary electrochromic devices)

  • 조봉희;김영호
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제9권7호
    • /
    • pp.690-695
    • /
    • 1996
  • We have systematically investigated the characterization of V$_{2}$O$_{5}$ thin films as a counter electrode for lithium based complementary electrochromic devices. The V$_{2}$O$_{5}$ thin films were prepared by thermal vacuum evaporation with varing the substrate temperature and film thickness. In electrochromic devices for smart windows, the WO$_{3}$ thin films with 400-800 nm thickness require to be capable of reversibly injection 10-15 mC/cm$^{2}$ of lithium, which is readily accomplished charge-balanced switching in a V$_{2}$O$_{5}$ thin films with 100-150nm thick. The V$_{2}$O$_{5}$ thin films produces considerably small changes in optical modulation properties in the visible and near infrared region(500-1100 nm) compared to the amorphous WO$_{3}$ thin films on 10-15 mC/cm$^{2}$ of lithium injection and the V$_{2}$O$_{5}$ thin films can therefore act as a counter electrode to WO$_{3}$ in a lithium based complementary clectrochromic devices. After 10$^{5}$ coloration/bleaching switching time, the degradation does not occurs and the devices exhibit a stable optical modulation in V$_{2}$O$_{5}$ thin films. It has shown that the injected lithium ion amounts in crystalline V$_{2}$O$_{5}$ thin films with the same thickness is large by 3-5 mC/cm$^{2}$ of lithium compared to the amorphous thin films in the same driving conditions. Therefore, to optimize the device performance, it is necessary to choose an appropriate film thickness and crystallinity of V$_{2}$O$_{5}$ for amorphous WO$_{3}$ film thickness as a working electrode.

  • PDF

진공증착법에 의해 제작된 Cd2GeSe4와 Cd2GeSe4:Co2+ 박막의 물리적 특성 (Physical Properties of Cd2GeSe4 and Cd2GeSe4:Co2+ Thin Films Grown by Thermal Evaporation)

  • 이정주;성병훈;이종덕;박창영;김건호
    • 한국진공학회지
    • /
    • 제18권6호
    • /
    • pp.459-467
    • /
    • 2009
  • 진공증착법으로 $Cd_2GeSe_4$$Cd_2GeSe_4:Co^{2+}$ 박막을 ITO(indium tin oxide) 유리 기판 위에 제작하였다. 결정화는 증착된 박막들을 질소분위기의 전기로에서 열처리함으로서 이룰 수 있었다. X-선 회절 분석에 의하여 증착된 $Cd_2GeSe_4$$Cd_2GeSe_4:Co^{2+}$ 박막의 격자상수는 $a\;=\;7.405\;{\AA}$, $c\;=\;36.240\;{\AA}$$a\;=\;7.43\;{\AA}$, $c\;=\;36.81\;{\AA}$로서 능면체(rhombohedral) 구조이었고, 열처리 온도를 증가함에 따라 (113)방향으로 선택적으로 성장됨을 알 수 있었다. 열처리 온도를 증가시킴에 따라 입계 크기가 점차 커지고 판상구조로 결정화 되었다. 실온에서 측정한 광학적인 에너지 띠 간격은 열처리 온도의 증가에 따라 $Cd_2GeSe_4$ 박막의 경우 1.70 eV ~ 1.74 eV로 증가하였고, $Cd_2GeSe_4:Co^{2+}$ 박막의 경우 1.79 eV ~ 1.74 eV로 감소하였다. $Cd_2GeSe_4$$Cd_2GeSe_4:Co^{2+}$ 박막 내의 전하운반자들의 동역학적 거동을 광유기 방전 특성(PIDC : photoinduced discharge characteristics) 방법으로 조사하였다.

Sputtering방식을 이용한 Indium Thin oxide박막의 넓이에 따른 X-ray 검출기 특성 연구

  • 김대국;신정욱;오경민;김성헌;이영규;조성호;남상희
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제42회 동계 정기 학술대회 초록집
    • /
    • pp.321-322
    • /
    • 2012
  • 의료용 방사선 장비는 초기의 아날로그 방식의 필름 및 카세트에서 진보되어 현재는 디지털 방식의 DR (Digital Radiography)이 널리 사용되며 그에 관한 연구개발이 활발히 진행되고 있다. DR은 크게 간접방식과 직접방식의 두 분류로 나눌 수 있는데, 간접방식은 X선을 흡수하면 가시광선으로 전환하는 형광체(Scintillator)를 사용하여 X선을 가시광선으로 전환하고, 이를 Photodiode와 같은 광소자로 전기적 신호로 변환하여 방사선을 검출하는 방식을 말하며, 직접 방식은 X선을 흡수하면 전기적 신호를 발생 시키는 광도전체(Photoconductor)를 사용하여 광도전체 양단 전극에 고전압을 인가한 형태를 취하고 있는 가운데, X선이 조사되면 일차적으로 광도전체 내부에서 전자-전공쌍(Electron-hole pair)이 생성된다. 이들은 광도전체 양단의 인가되어 있는 전기장에 의해 전자는 +극으로, 전공은 -극으로 이동하여 아래에 위치한 Active matrix array을 통해 방사선을 검출하는 방식이다. 본 연구에서는 직접방식 X-ray 검출기에서 활용되는 a-Se을 ITO (Indium Thin oxide) glass 상단에 Thermal evaporation증착을 이용하여 두께 $50{\mu}m$, 33 넓이로 증착 시킨 다음, a-Se상단에 Sputtering증착을 이용하여 ITO를 11 cm, 22 cm, $2.7{\times}2.7cm$ 넓이로 증착시켜 상하부의 ITO를 Electrode로 이용하여 직접방식의 X-ray검출기 샘플을 제작하였다. 제작 과정 중 a-Se의 Thermal evaporation증착 시, 저진공 $310^{-3}_{Torr}$, 고진공 $2.210^{-5}_{Torr}$에서 보트의 가열 온도를 두 번의 스텝으로 나누어 증착 시켰다. 첫 번째 스텝 $250^{\circ}C$, 두 번째 스텝은 $260^{\circ}C$의 조건으로 증착하여 보트 내의 a-Se을 남기지 않고 전량을 소모할 수 있었으며, 스텝간의 온도차를 $10^{\circ}C$로 제어하여 균일한 박막을 형성 할 수 있었다. Sputtering증착 시, 저진공 $2.510^{-3}$, 고진공 $310^{-5}$에서 Ar, $O_2$를 사용하여 100 Sec간 플라즈마를 생성시켜 ITO를 증착하였다. 제작된 방사선 각각의 검출기 샘플 양단의 ITO에 500V의 전압을 인가하고, 진단 방사선 범위의 70 kVp, 100 mA, 0.03 sec 조건으로 X-ray를 조사시켜 ITO넓이에 따른 민감도(Sensitivity)와 암전류(Dark current)를 측정하였다. 측정결과 민감도(Sensitivity)는 X-ray샘플의 두께에 따른 $1V/{\mu}m$ 기준 시, 증착된 ITO의 넓이가 11 cm부터 22 cm, $2.7{\times}2.7cm$까지 각각 $7.610nC/cm^2$, $8.169nC/cm^2$, $6.769nC/cm^2$로 22 cm 넓이의 샘플이 가장 높은 민감도를 나타내었으나, 암전류(Dark current)는 $1.68nA/cm^2$, $3.132nA/cm^2$, $5.117nA/cm^2$로 11 cm 넓이의 샘플이 가장 낮은 값을 나타내었다. 이러한 데이터를 SNR (Signal to Noise Ratio)로 합산 하였을 시 104.359 ($1{\times}1$), 60.376($2{\times}2$), 30.621 ($2.7{\times}2.7$)로 11 cm 샘플이 신호 대 별 가장 우수한 효율을 나타냄을 알 수 있었다. 따라서 ITO박막의 면적이 클수록 민감도는 우수하나 그에 따른 암전류의 증가로 효율이 떨어짐을 검증 할 수 있었으며, 이는 ITO면적이 넓어짐에 따른 저항의 증가로 암전류에 영향을 끼침을 할 수 있었다. 본 연구를 통해 a-Se의 ITO 박막 면적에 따른 전기적 특성을 검증할 수 있었다.

  • PDF

Fabrication of Schottky Device Using Lead Sulfide Colloidal Quantum Dot

  • Kim, Jun-Kwan;Song, Jung-Hoon;An, Hye-Jin;Choi, Hye-Kyoung;Jeong, So-Hee
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.189-189
    • /
    • 2012
  • Lead sulfide (PbS) nanocrystal quantum dots (NQDs) are promising materials for various optoelectronic devices, especially solar cells, because of their tunability of the optical band-gap controlled by adjusting the diameter of NQDs. PbS is a IV-VI semiconductor enabling infrared-absorption and it can be synthesized using solution process methods. A wide choice of the diameter of PbS NQDs is also a benefit to achieve the quantum confinement regime due to its large Bohr exciton radius (20 nm). To exploit these desirable properties, many research groups have intensively studied to apply for the photovoltaic devices. There are several essential requirements to fabricate the efficient NQDs-based solar cell. First of all, highly confined PbS QDs should be synthesized resulting in a narrow peak with a small full width-half maximum value at the first exciton transition observed in UV-Vis absorbance and photoluminescence spectra. In other words, the size-uniformity of NQDs ought to secure under 5%. Second, PbS NQDs should be assembled carefully in order to enhance the electronic coupling between adjacent NQDs by controlling the inter-QDs distance. Finally, appropriate structure for the photovoltaic device is the key issue to extract the photo-generated carriers from light-absorbing layer in solar cell. In this step, workfunction and Fermi energy difference could be precisely considered for Schottky and hetero junction device, respectively. In this presentation, we introduce the strategy to obtain high performance solar cell fabricated using PbS NQDs below the size of the Bohr radius. The PbS NQDs with various diameters were synthesized using methods established by Hines with a few modifications. PbS NQDs solids were assembled using layer-by-layer spin-coating method. Subsequent ligand-exchange was carried out using 1,2-ethanedithiol (EDT) to reduce inter-NQDs distance. Finally, Schottky junction solar cells were fabricated on ITO-coated glass and 150 nm-thick Al was deposited on the top of PbS NQDs solids as a top electrode using thermal evaporation technique. To evaluate the solar cell performance, current-voltage (I-V) measurement were performed under AM 1.5G solar spectrum at 1 sun intensity. As a result, we could achieve the power conversion efficiency of 3.33% at Schottky junction solar cell. This result indicates that high performance solar cell is successfully fabricated by optimizing the all steps as mentioned above in this work.

  • PDF

하부전극 물질에 따른 CdTe박막 증착과 그에 따른 전기적 특성 평가

  • 김대국;신정욱;이영규;김성헌;이건환;남상희
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.327-328
    • /
    • 2012
  • 의료분야의 진단 방사선 장비는 초기의 필름방식 및 카세트에서 진보되어 현재는 디지털방식의 DR (Digital Radiography)이 널리 사용되며 이에 관한 연구개발이 활발히 진행 되고 있다. DR은 일반적으로 직접방식과 간접방식으로 나눌 수 있다. 직접방식의 원리는 X선을 흡수하면 전기적 신호를 발생 시키는 광도전체(Photoconductor)를 사용하여 광도전체 양단 전극에 전압을 인가하여 전기장을 유도한 가운데, X선을 조사하면 광도전체 내부에서 전자-전공쌍(Electron-hole pair)이 생성된다. 이것은 양단에 유도된 전기장의 영향으로 전자는 +극으로, 전공은 -극으로 이동하여 아래에 위치한 하부기판을 통하여 이미지로 변조된다. 간접방식은 X선을 흡수하면 가시광선으로 전환하는 형광체(Scintillator)를 사용하여 조사된 X선을 형광체에서 가시광선으로 전환하고, 이를 Photodiode와 같은 광변환소자로 전기적 신호로 변환하여 방사선을 검출하는 방식을 말한다. 본 연구에서는 직접방식에서 이용되는 광도전체 중 흡수효율이 높고 Mobility가 뛰어난 CdTe를 선정하여 PVD (Physical vapor deposition)방식으로 300 m의 두께를 목표로 하여 증착을 진행하였다. Chamber의 진공도가 $2.5{\times}10^{-2}$ Torr로 도달 시점부터, Substrate와 Boat에 열을 가하였다. Substrate온도는 $350^{\circ}C$, Boat온도는 $300^{\circ}C$도로 설정하여 11시간 동안 진행하였다. Substrate온도는 $303^{\circ}C$, Boat온도는 $297^{\circ}C$도부터 증착이 시작되어 선형적인 증가세 추이를 나타내어 Substrate 및 Boat온도가 설정 값에 도달 하였을 때, $25{\sim}34.4{\AA}/s$ 증착율을 나타내었다. 하부전극의 물질에 따른 CdTe증착 효율성 평가를 진행한 후, 그에 따른 전기적 특성을 알아보았다. 하부전극의 물질로는 ITO (Indium Tin Oxide), Parylene이 코팅 된 ITO, Au, Ag를 사용하였다. 하부전극의 물질 상단에 Thermal Evaporation System을 사용하여 CdTe를 증착한 후, Cdte 상단에 Au를 증착 시켜 민감도(Sensitivity)와 암전류(Dark current)를 측정하였다. 증착 결과 ITO와 Ag상단에 증착시킨 CdTe박막은 박리가 되었고, Au와 Parylene이 코팅 된 ITO에는 CdTe박막이 안정적이게 형성이 되었다. 이 두 샘플에 대하여 동일한 조건으로 민감도와 암전류를 측정 시, Parylene이 코팅된 ITO를 하부전극으로 사용한 CdTe박막은 0.1021 pA/$cm^2$의 암전류와 1.027 pC/$cm^2$의 민감도를 나타낸 반면, Au를 하부전극으로 사용한 CdTe박막은 0.0381 pA/$cm^2$의 암전류와 1.214 pC/$cm^2$의 민감도를 나타내어 Parylene이 코팅된 ITO보다 우수한 전기적 특성을 나타내었다. 따라서 Au는 CdTe박막 증착 시, 하부전극 기판으로서 뛰어난 특성을 나타내는 것을 알 수 있었다.

  • PDF

Interfacial reaction and Fermi level movements of p-type GaN covered by thin Pd/Ni and Ni/Pd films

  • 김종호;김종훈;강희재;김차연;임철준;서재명
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 1999년도 제17회 학술발표회 논문개요집
    • /
    • pp.115-115
    • /
    • 1999
  • GaN는 직접천이형 wide band gap(3.4eV) 반도체로서 청색/자외선 발광소자 및 고출력 전자장비등에의 응용성 때문에 폭넓게 연구되고 있다. 이러한 넓은 분야의 응용을 위해서는 열 적으로 안정된 Ohmic contact을 반드시 실현되어야 한다. n-type GaN의 경우에는 GaN계면에서의 N vacancy가 n-type carrier로 작용하기 때문에 Ti, Al, 같은 금속을 접합하여 nitride를 형성함에 의해서 낮은 접촉저항을 갖는 Ohmic contact을 하기가 쉽다. 그러나 p-type의 경우에는 일 함수가 크고 n-type와 다르게 nitride가 형성되지 않는 금속이 Ohmic contact을 할 가능성이 많다. 시료는 HF(HF:H2O=1:1)에서 10분간 초음파 세척을 한 후 깨끗한 물에 충분히 헹구었다. 그런 후에 고순도 Ar 가스로 건조시켰다. Pd와 Ni은 열적 증착법(thermal evaporation)을 사용하여 p-GaN에 상온에서 증착하였다. 현 연구에서는 열처리에 의한 Pd의 clustering을 줄이기 위해서 wetting이 좋은 Ni을 Pd 증착 전과 후에 삽입하였으며, monchromatic XPS(x-ray photoelectron spectroscopy) 와 SAM(scanning Auger microscopy)을 사용하여 열처리 전과 40$0^{\circ}C$, 52$0^{\circ}C$ 그리고 695$0^{\circ}C$에서 3분간 열처리 후의 온도에 따른 morphology 변화, 계면반응(interfacial reaction) 및 벤드 휨(band bending)을 비교 연구하였다. Nls core level peak를 사용한 band bending에서 Schottky barrier height는 Pd/Ni bi-layer 접합시 2.1eV를, Ni/Pd bi-layer의 경우에 2.01eV를 얻었으며, 이는 Pd와 Ni의 이상적인 Schottky barrier height 값 2.38eV, 2.35eV와 비교해 볼 때 매우 유사한 값임을 알 수 있다. 시료를 후열처리함에 의해 52$0^{\circ}C$까지는 barrier height는 큰 변화가 없으나, $650^{\circ}C$에서 3분 열처리 후에 0.36eV, 0.28eV 만큼 band가 더 ?을 알 수 있었다. Pd/Ni 및 Ni/Pd 접합시 $650^{\circ}C$까지 후 열 처리 과정에서 계면에서 matallic Ga은 온도에 비례하여 많은 양이 형성되어 표면으로 편석(segregation)되어지나, In-situ SAM을 이용한 depth profile을 통해서 Ni/Pd, Pd/Ni는 증착시 uniform하게 성장함을 알 수 있었으며, 후열처리 함에 의해서 점차적으로 morphology 의 변화가 일어나기 시작함을 볼 수 있었다. 이는 $650^{\circ}C$에서 열처리 한후의 ex-situ AFM을 통해서 재확인 할 수 있었다. 이상의 결과로부터 GaN에 Pd를 접합 시 심한 clustering이 형성되어 Ohoic contact에 문제가 있으나 Pd/Ni 혹은 Ni/Pd bi-layer를 사용함에 의해서 clustering의 크기를 줄일 수 있었다. Clustering의 크기는 Ni/Pd bi-layer의 경우가 작았으며, $650^{\circ}C$ 열처리 후에 barrier height는 Pd/Ni bi-layer의 경우에도 Ni의 영향을 받음을 알 수 있었다.

  • PDF

유전체 다이아프램을 이용한 다모드 광섬유 압력센서 (Multimode fiber-optic pressure sensor based on dielectric diaphragm)

  • 김명규;권대혁;김진섭;박재희;이정희;손병기
    • 한국진공학회지
    • /
    • 제6권3호
    • /
    • pp.220-226
    • /
    • 1997
  • 실리콘 미세가공기술로 형성된 프레임 모양의 실리콘 기판에 의해 지지되는 -$Si_3N_4/300 nm-SiO_2/150 nm-Si_3N_4$ 광반사막을 제조하였으며, 이것을 광섬유와 결합하여 강도형 다모드 광섬유 압력센서를 제작하고 그 특성을 조사하였다. $Si_3N_4/SiO_2/Si_3N_4$다아아 프램을 광반사막으로 사용하기 위하여 이 다이아프램의 뒷면에 NiCr 및 Au 박막을 각각 진 공증착하여 광반사막에서의 광투과에 의한 광손실을 수%로 감소시킬 수 있었다. 유전체 다 이아프램의 상하에 각각 있는 $Si_3N_4$막은 KOH 수용액에 의한 실리콘 이방성 식각시 자동식 각 정지층 역할을 하여 다이아프램 두께의 재현성이 우수하였다. 다이아프램의 크기가 3$\times$ 3$\textrm{mm}^2$, 4$\times$4$\textrm{mm}^2$ 및 5$\times$5$\textrm{mm}^2$인 센서는 각각 0~126.64kPa, 0~79.98kPa 및 0~46.66kPa의 압력범위에서 선형적인 광출력-압력 특성을 나타내었으며, 이들 센서의 압력감도는 각각 약 20.69nW/kPa, 26.70nW/kPa 및 39.33nW/kPa로서, 다이아프램의 크기가 증가할수록 압력감 도도 증가하였다.

  • PDF

UV-excited chlorine radical을 이용한 실리콘 웨이퍼상의 금속 오염물의 건식세정에 관한 연구 (A study of dry cleaning for metallic contaminants on a silicon wafer using UV-excited chlorine radical)

  • 손동수;황병철;조동률;김경중;문대원;구경완
    • 한국진공학회지
    • /
    • 제6권1호
    • /
    • pp.9-19
    • /
    • 1997
  • 본 연구에서는 실리콘 웨이퍼 표면에 존재하는 미량의 Zn, Fe, Ti 금속 오염물들이 UV-excited chlorine radical을 이용한 건식세정 방법으로 제거되는 반응과정을 찾아내고자 하였다. 실리콘 웨이퍼 상에 진공증착법으로 원형패턴이 있는 Zn, Fe, Ti 박막을 증착시켜 상온 및 $200^{\circ}C$에서 UV/$Cl_2$세정하였을 때, 염소 래디컬($Cl^*$)이 Fe, Zn, Ti와 반응하여 제거되 는 것을 반응 전후 광학현미경과 SEM을 통해 표면 형상 변화를 관찰하였고, in-line으로 연결된 XPS를 통해서 반응 후 웨이퍼 표면에 남아있는 화합물의 화학적 결합상태를 관찰 하였으며, UV/$Cl_2$ 세정 후 실리콘 기판이 손상받는 정도를 알기 위해 AFM으로 표면 거칠 기를 측정하였다. 광학현미경과 SEM의 분석 결과에 의하면 Zn와 Fe는 쉽게 제거되는 반면 염화물을 형성하기 보다는 휘발성이 적은 산화물을 형성하는 경향이 강한 Ti은 약간만 제 거되는 것을 확인하였다. XPS분석을을 통해서 이들 금속 오염물들이 chlorine radical과 반 응하여 웨이퍼 표면에 금속 염화물을 형성하고 있는 것을 확인하였고, UV/$Cl_2$세정처리를 하였을 때 실리콘 웨이퍼의 표면 거칠기가 약간 증가하는 것을 알 수 있었다. 지금까지의 결 과를 볼 때, 습식세정과 UV/$Cl_2$건식세정을 병행하면 플라즈마 및 레이저를 사용하는 다른 건식세정 방법에 비하여 보다 저온에서 실리콘 기판의 큰 손상 없이 비교적 용이하게 금속 오염물을 제거할 수 있음을 제안 하였다.

  • PDF