Residual Stress on Concentric Laminated Fibrous Al2O3-ZrO2 Composites on Prolonged High Temperature Exposure

  • Sarkar, Swapan Kumar;Lee, Byong Taek
    • Korean Journal of Materials Research
    • /
    • v.23 no.9
    • /
    • pp.531-536
    • /
    • 2013
  • This paper investigates the effect of prolonged high temperature exposure on concentric laminated $Al_2O_3-ZrO_2$ composites. An ultrafine scale microstructure with a cellular 7 layer concentric lamination with unidirectional alignment was fabricated by a multi-pass extrusion method. Each laminate in the microstructure was $2-3{\mu}m$ thick. An alternate lamina was composed of 75%$Al_2O_3$-(25%m-$ZrO_2$) and t-$ZrO_2$ ceramics. The composite was sintered at $1500^{\circ}C$ and subjected to $1450^{\circ}C$ temperature for 24 hours to 72 hours. We investigated the effect of long time high temperature exposure on the generation of residual stress and grain growth and their effect on the overall stability of the composites. The residual stress development and its subsequent effect on the microstructure with the edge cracking behavior mechanism were investigated. The residual stress in the concentric laminated microstructure causes extensive micro cracks in the t-$ZrO_2$ layer, despite the very thin laminate thickness. The material properties like Vickers hardness and fracture toughness were measured and evaluated along with the microstructure of the composites with prolonged high temperature exposure.

Properties of Fe-based Soft magnetic Thin Film with Hybrid Structures (Hybrid 구조의 Fe계 연자성 박막의 특성)

  • 송재성;이원재;허정섭;김현식;오영우
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.11
    • /
    • pp.963-968
    • /
    • 2000
  • Magnetic properties and microstructures of Fe$\_$93-x/Zr$_3$B$_4$Ag$\_$x/ thin films were investigated as a function of addition of element Ag, (X$\_$Ag/=0 to 6 at.%) and annealing temperature, T$\_$a/=300$\^{C}$ to 600$\^{C}$. In the case of adding Ag, magnetic properties of Fe$\_$93-x/Zr$_3$B$_4$Ag$\_$x/ thin films were improved than those of Ag-free Fe$\_$93/Zr$_3$B$_4$thin films. The prominent soft magnetic properties with coercivity of 1.1 Oe, saturation magnetization of 2.2 T and permeability of 5400 at 50㎒ were obtained from Fe$\_$88/Zr$_3$B$_4$Ag$\_$5/ thin film annealed was lower than that of Fe-base or Co-base thin films reported previously. Such enhanced magnetic properties are presumably attributed to the format in ultra fine grains. Also, the reduced eddy current loss in the annealed sample is due to refined micro magnetic domains with increasing the amount of Ag in Fe$\_$93-x/Zr$_3$B$_4$Ag$\_$x/ thin films.

  • PDF

Electrical Resistivity and Fracture Toughness of SiC-ZrB2

  • Shin, Yong-Deok;Ju, Jin-Young;Kwon, Ju-Sung
    • The Korean Journal of Ceramics
    • /
    • v.5 no.4
    • /
    • pp.400-403
    • /
    • 1999
  • The mechanical and electrical properties of hot-pressed and annelaed $\beta$-SiC+39vol.% $ZrB_2$ electroconductive ceramic composites were investigated as a function of the liquid forming additives of $Al_2O_3+Y_2O_3$(6:4 wt%). In this microstructures, no reactions and elongated $\alpha$-SiC grains with equiaxed $ZrB_2$ grains were observed between $\beta$-SiC and $ZrB_2$. The properties of the $\beta$-SiC+39vol.%$ZrB_2$ composites with 4wt% $Al_2O_3+Y_2O_3$ at R.T. are as follows: fracture toughness is 6.37 MPa.m1/2, electical resistivity is $1.51\times10^{-4}\Omega \cdot\textrm{cm}$ and the relative density is 98.6% of the theoretical density. The fracture toughness of the $\beta$-SiC+39 vol.% $ZrB_2$ composites were weakly decreased with increasing amount of $Al_2O_3+Y_2O_3$ additives. Internal stresses due to the difference of $\beta$-SiC and $ZrB_2$ thermal expansion coefficient and elastic modulus mismatch appeared to contribute to fracture toughening in $\beta$-SiC+39vol.%$ZrB_2$ electroconductive ceramic composites.

  • PDF

Effect of Sn Addition on Corrosion Behavior of Zr-1.0 Nb-xSn Alloy System (Zr-1.0Nb-xSn 합금의 부식거동에 대한 Sn첨가의 영향)

  • Lee, Myeong-Ho;Choe, Byeong-Gwon;Jeong, Yong-Hwan
    • Korean Journal of Materials Research
    • /
    • v.12 no.5
    • /
    • pp.369-374
    • /
    • 2002
  • To investigate the corrosion behavior of Zr-1.0Nb-xSn (x=1.0, 1.5, 2.0 and 2.5wt. %)alloy system, the corrosion tests of Zr-1.0Nb-xSn alloys were carried out in steam at $400^{\circ}C$ for 125 days and in 70ppm LiOH solution at $360^{\circ}C$ for 180 days. The matrix microstructures of the test specimens were analyzed using TEM and the oxide structures on the test specimens were analyzed using XRD. It was found from the analyses that the more Sn content the alloy had, the faster it was corroded and with the increase of Sn content in the alloy the fraction of $t-ZrO_2$ to $m-ZrO_2$ was decreased. It was also found that the alloys having more Sn showed more dislocation density than those having less.

Magnetic Properties of FeZrN/$SiO_2$ Soft Magnetic Multilayer Thin Films (FeZrN/$SiO_2$ 연자성 다층 박막의 자기적 성질)

  • Kim, Taek-Su;Kim, Jong-O
    • Korean Journal of Materials Research
    • /
    • v.6 no.11
    • /
    • pp.1061-1066
    • /
    • 1996
  • RF magnetron reactive sputtering법으로 Fe75.5Zr8.3N16.2/SiO2(250$\AA$) 다층 박막을 FeZrN의 두께를 변화시키면서 제조하고, 제조된 박막을 진공 열처리하여 열처리 온도에 따른 포화자화, 보자력, 고주파에서의 투자율 그리고 열적 안정성을 조사하였다. Fe75.5Zr8.3N16.2/SiO2(250$\AA$) 다층박막은 FeZrN의 두께가 800$\AA$이상일 때 좋은 연자성을 나타내었다. Fe75.5Zr8.3N16.2/SiO2(250$\AA$)다층 박막을 45$0^{\circ}C$로 열처리 했을 때 포화자속밀도(1.08 T), 보자력 0.41 Oe, 1 MHz에서의 실효 투자율은 3000이상의 연자성을 나타내었다. 그 이유는 X-선 회절 분석 결과 열처리에 의해서 ZrN 미결정이 석출하여 $\alpha$-Fe 결정 성장이 억제되어 우수한 연자기적 성질이 나타난다고 판단된다. 이때 $\alpha$-Fe 입자 크기는 40-50$\AA$, ZrN의 입자 크기는 10-15$\AA$이다. 그리고 실효 투자율의 주파수 의존성에서 단층막에서는 5 MHz 이상에서 실효 투자율이 급격히 감소하는 경향을 보였으나, 다층막에서는 40MHz까지 실효 투자율이 1600이 되어 고주파에서의 연자성이 개선되었다.

  • PDF

Sintering Atmosphere Effect on the Grain Size and Phase Distribution of a Zirconia ($ZrO_2$ 의 입자크기과 상분포에 미치는 소결분위기 영향)

  • 백용균;안중호
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.11
    • /
    • pp.1198-1204
    • /
    • 1999
  • The effect of sintering atmosphere on the grain sizes and phase distributions in 3Y-ZrO2 and 8Y-ZrO2 was investigated O2 and N2 were used as sintering atmospheres. In the case of 3Y-ZrO2 the sintered density was higher in N2 than in O2 while in the case of 8Y-ZrO2 contrary results were obtained. The observation can be explained by the nitrogen solubility into the zirconia lattice. That is nitrogen gas can behave as a diffusive gas contrary to the behavior in other oxides depending on the amount of Y2O3. In 3Y-ZrO2 tetragonal phase was retained at room temperature irrespective of sintering atmospheres. Grain sizes of two specimens were below 2㎛ and larger in O2 thin in N2 Under a given stress the transformability of tetragonal phase into monoclinic phase was higher in O2 than N2. The results are discussed on the basis of an effect of the grain size and non-transformable ttragonal(t') phase.

  • PDF

Circumferential Creep Behaviors of Zr-Nb-O and Zr-Nb-Sn-Fe Alloy Cladding Tubes Manufactured by Pilgering (Pilgering 법에 의해 제조된 Zr-Nb-O 및 Zr-Nb-Sn-Fe 합금 피복관의 원주방향 Creep 거동)

  • Lee, S.Y.;Ko, S.;Choi, Y.C.;Kim, K.T.;Choi, J.H.;Hong, S.I.
    • Transactions of Materials Processing
    • /
    • v.17 no.5
    • /
    • pp.364-372
    • /
    • 2008
  • In this study, the circumferential creep behaviors ofpilgered advanced Zirconium alloy tubes such as Zr-Nb-O and Zr-Nb-Sn-Fe were investigated in the temperature range of $400\sim500^{\circ}C$ and in the stress range of 80$\sim$150MPa. The test results indicate that the stress exponent for the steady-state creep rate of the Zr-Nb-Sn-Fe alloy decreases with the increase of stress(from 6$\sim$7 to 4), while that of the Zr-Nb-O alloy is nearly independent of stress(5$\sim$6). The activation energy of creep deformation is found to be nearly the same as the activation energy for Zr self diffusion. This indicates that the creep deformation may be controlled by dislocation climb mechanism in Zr-Nb-O. On the other hand, the transition of stress exponent(from 6-7 to 4) in Zr-Nb Sn-Fe strongly suggests the transition of the rate controlling mechanism at high stresses. The lower stress exponent at high stresses in Zr-Nb-Sn-Fe can be explained by the dynamic deformation aging effect caused by interaction of dislocations with Sn substitutional atoms.

Improvement of Mechanical Properities in Al-Cu-Li-Ag-Mg-Zr Alloys by Thermomechanical Treatement (가공열처리에 의한 고강도 Al-Cu-Li-Ag-Mg-Zr 합금의 기계적 성질 개선)

  • Yu, C.H.;Namkung, I.;Lee, O.Y.;Kim, D.K.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.5 no.2
    • /
    • pp.103-110
    • /
    • 1992
  • This study is aimed to investigate the effect of various thermomechanical treatments($T_6$, $T_8$ and ITMT) on the microstructure and mechanical properties of an Al-Cu-Li-Ag-Mg-Zr alloy (Weldalite 049) which has been known to strong natural aging response, good weldablity and high strength in $T_6$ sand $T_8$ temper. This experiment was performed by means of differential scaning calorimetry, tensile test, optical and transmission electron microscopy. The tensile strength in the peak aged condition shows 620, 650 MPa in $T_6$ and $T_8$(40% cold work), respectively. Also, The tensile strength is increased with cold working in $T_8$ but decreased at 60% cold working. However, the tensile strength of the intermediate thermomechanical treated speciman(ITMT) is lower than that of $T_6$ temper about 20% but the elongation is higher than two times. It might be predicted that the ITMT is effective processing to improve the toughness of this alloy. In $T_6$, $T_8$ and ITMT, the major strengthening phase is $T_1(Al_2CuLi)$ phases. and the fine $T_1$ phase which are homogeneously precipited in matrix was observed much more in $T_8$ than $T_6$ and ITMT.

  • PDF

Sealing capability and marginal fit of titanium versus zirconia abutments with different connection designs

  • Sen, Nazmiye;Sermet, Ibrahim Bulent;Gurler, Nezahat
    • The Journal of Advanced Prosthodontics
    • /
    • v.11 no.2
    • /
    • pp.105-111
    • /
    • 2019
  • PURPOSE. Limited data is available regarding the differences for possible microleakage problems and fitting accuracy of zirconia versus titanium abutments with various connection designs. The purpose of this in vitro study was to investigate the effect of connection design and abutment material on the sealing capability and fitting accuracy of abutments. MATERIALS AND METHODS. A total of 42 abutments with different connection designs [internal conical (IC), internal tri-channel (IT), and external hexagonal (EH)] and abutment materials [titanium (Ti) and zirconia (Zr)] were evaluated. The inner parts of implants were inoculated with $0.7{\mu}L$ of polymicrobial culture (P. gingivalis, T. forsythia, T. denticola and F. nucleatum) and connected with their respective abutments under sterile conditions. The penetration of bacteria into the surrounding media was assessed by the visual evaluation of turbidity at each time point and the number of colony forming units (CFUs) was counted. The marginal gap at the implant- abutment interface (IAI) was measured by scanning electron microscope. The data sets were statistically analyzed using Kruskal-Wallis followed by Mann-Whitney U tests with the Bonferroni-Holm correction (${\alpha}=.05$). RESULTS. Statistically significant difference was found among the groups based on the results of leaked colonies (P<.05). The EH-Ti group characterized by an external hexagonal connection were less resistant to bacterial leakage than the groups EH-Zr, IT-Zr, IT-Ti, IC-Zr, and IC-Ti (P<.05). The marginal misfit (in ${\mu}m$) of the groups were in the range of 2.7-4.0 (IC-Zr), 1.8-5.3 (IC-Ti), 6.5-17.1 (IT-Zr), 5.4-12.0 (IT-Ti), 16.8-22.7 (EH-Zr), and 10.3-15.4 (EH-Ti). CONCLUSION. The sealing capability and marginal fit of abutments were affected by the type of abutment material and connection design.

A Study on the Dielectric and Piezoelectric properties of the Pb(SbS11/2TSnS11/2T)OS13T-PbTiOS13T-PbZrOS13T Ceramics (Pb(Sb1/2Sn1/2)O3-PbTiO3-PbZrO3 세라믹스의 유전 및 압전 특성에 관한 연구)

  • 정장호;류기원;이성갑;이영희
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.5
    • /
    • pp.517-524
    • /
    • 1992
  • In this study, 0.10Pb(SbS11/2TSnS11/2T)OS13T-(0.90-x)PbZrOS13T (0.25 x 0.40) ceramics were fabricated by the atmospheric method. The sintering temperature and time were 1250[$^{\circ}C$] and 2[2hr], respectively. The structureal, dielectric and piezoelectric properties with composition of PbTiOS13T were studied. As the results of XRD ans SEM, the crystal structure of a specimen was rhombohedral, lattice constant and average grain size were decreased with increasing the contents of PbTiOS13T. Relative dielectric constant and Curie temperature were increased with increasing the contents of PbTiOS13T, 0.10PSS-0.40PT-0.50PZ specimen had the highest values of 904 and 265[$^{\circ}C$], respectively. In increasing of PbTiOS13T contents form 25[mol%] to 40[mol%], piezoelectric charge constant and electromechanical coupling factors were increased form 114[pC/N] to 142[pC/N], 17[%] to 24[%] and mechanical quality factor were decreased with increasing the contents of PbTiOS13T. In the 0.10PSS-0.40PT-0.50PZ specimens, those values were 14.2[kV/cm] and 9.43[x10S0-6TC/cmS02T], resectively.